Structural Design and Analysis for Carbon/Epoxy Composite Wing of A Small Scale WIG Vehicle (소형 위그선의 탄소/에폭시 복합재 주익의 구조 설계 및 해석에 관한 연구)

  • Park, Hyun-Bum;Kang, Kuk-Jin;Kong, Chang-Duk
    • Composites Research
    • /
    • v.19 no.5
    • /
    • pp.12-19
    • /
    • 2006
  • In this paper, conceptual structural design of the main wing for a small scale WIG(Wing in Ground Effect) among high speed ship projects, which will be a high speed maritime transportation system for the next generation in Rep. of Korea, was performed. The Carbon/Epoxy material was selected for the major structure, and the skin-spar with a foam sandwich structural type was adopted for improvement of lightness and structural stability. As a design procedure for the present study, firstly the design load was estimated through the critical flight load case study, and then flanges of the front and rear spars from major bending loads and the skin and the spar webs from shear loads were preliminarily sized using the netting rule and the rule of mixture. Stress analysis was performed by a commercial FEA code, NASTRAN. From the stress analysis results for the first designed wing structure, it was confirmed that the upper skin between the front spar and the rear spar was unstable fer the buckling. Therefore in order to solve this problem, a middle spar and the foam sandwich type structure at the skin and the web were added. After design modification, the structural safety and stability for the final design feature was confirmed. In addition to this, the insert bolt type structure with eight high strength bolts to fix the wing structure to the fuselage was adopted for easy assembly and removal as well as in consideration of more than 20 years fatigue life.

CRYOGENIC AND ELEVATED TEMPERATURE CYCLING OF CARBON / POLYMER COMPOSITES FOR RESUABLE LAUNCH VEHICLE CRYOGENIC TANKS (왕복선 연료탱크 적용을 위한 탄소/고분자 복합재료의 극저온-고온 싸이클링)

  • 예병한;원용구
    • Proceedings of the Korean Society of Propulsion Engineers Conference
    • /
    • 2003.05a
    • /
    • pp.151-155
    • /
    • 2003
  • An apparatus was developed to repetitively apply a -196 $^{\circ}C$ thermal load to coupon-sized mechanical test specimens. Using this device, IM7/5250-4 (carbon / bismaleimide) cross-ply and quasi-isotropic laminates were submerged in liquid nitrogen (L$N_2$) 400 times. Ply-by-Ply micro-crack density, laminate modulus, and laminate strength were measured as a function of thermal cycles. Quasi-isotropic samples of IM7/977-3 (carbon / epoxy) composite were also manually cycled between liquid nitrogen and an oven set at 120 $^{\circ}C$ for 130 cycles to determine whether including elevated temperature in the thermal cycle significantly altered the degree or location of micro-cracking. In response to thermal cycling, both materials micro-cracked extensively in the surface plies followed by sparse cracking of the inner plies. The tensile modulus of the IM7/5250-4 specimens was unaffected by thermal cycling, but the tensile strength of two of the lay-ups decreased by as much as 8.5 %.

  • PDF

Interfacial Evaluation and Damage Sensing of Carbon Fiber/Epoxy-AT-PEI Composite using Electro-Micromechanical Techniques (Electro-micromechanical 시험법을 이용한 탄소섬유 강화 Epoxy-AT PEI 복합재료의 손상 감지능 및 계면물성 평가)

  • Kim, Dae-Sik;Kong, Jin-Woo;Park, Joung-Man;Kim, Minyoung;Kim, Wonho;Ahn, Byung-Hyun;Park, Jin-Ho
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2002.10a
    • /
    • pp.212-215
    • /
    • 2002
  • Interfacial evaluation and damage sensing of the carbon fiber/epoxy-amine terminated (AT)-polyetherimide (PEI) composites were performed using micromechanical test and electrical resistance measurement. As AT-PEI content increased, the fracture toughness of epoxy-AT-PEI matrix increased, and thus their interfacial shear strength (IFSS) was improved due to the improved toughness. After curing process, the changes in electrical resistance (ΔR) with increasing AT-PEI contents increased gradually because of the changes in thermal expansion coefficient (TEC) and thermal shrinkage of matrix. Matrix fracture toughness was correlated to the IFSS, residual stress and electrical resistance. The results obtained from the electrical resistance measurement during curing process, reversible stress/strain, and durability test were consistent with modified matrix toughness properties.

  • PDF

Development of Water-lubricated Plastic Bearings (수-윤활용 플라스틱 베어링 개발에 관한 연구)

  • Hosung Kong;Hung-gu Han
    • Tribology and Lubricants
    • /
    • v.39 no.6
    • /
    • pp.235-243
    • /
    • 2023
  • This paper presents the fabrication process of water-lubricated plastic bearings. Plastic bearings require good mechanical properties and tribological properties as well as elasticity and shock resistance, especially when lubricated in dirty water conditions. In this study, sleeve-type plastic bearings are produced by winding a prepreg sheet, which primary contains nitrile rubber (NBR)-modified epoxy, self-lubricating fillers, and various types of lattice-structured reinforcing fibers such as carbon, Aramid, and polyethylene terephthalate. A thermosetting epoxy is chemically modified with NBR to impart elasticity and low-friction characteristics in water conditions. Experimental investigations are conducted to examine the mechanical and tribological characteristics of the developed bearing materials, and the results are compared with the characteristics of a commercial plastic bearing (Thordon SXL), well known as a water-lubricated bearing. A Thordon bearing (mainly composed of polyurethane) exhibits an extremely low load-bearing capacity and is thus only suitable for medium loading (1~10MPa). The tribological characteristics of the test materials are evaluated through Falex block-on-ring (LFW-1) friction and wear tests. The results indicate that friction exhibited by the carbon-fiber-reinforced NBR-10wt.%-modified epoxy composite material, incorporated with the addition of 20wt.% UHMWPE and 6wt.% paraffin wax, is lower than that of the Thorden bearings, whereas its wear resistance surpass that of Thorden ones. Because of these features, the load carrying capacity of the fabricated composite (>10MPa) is higher than that of the Thorden bearings. These results confirm the applicability of water-lubricated plastic bearing materials developed in this study.

Behavior of 2-D Biaxial braided hollow composite under bending (굽힘 하중 하에서의 2-D Biaxial Braided 중공형 복합재료의 거동)

  • 서거원;임동진;윤희석
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2000.11a
    • /
    • pp.12-16
    • /
    • 2000
  • This study is about the effect of braiding on the 2-D biaxial braided hollow composite(BD) compared with unidirectional hollow composite(UD). The specimens were made of T700S Carbon/Epoxy prepreg and T700S dried Carbon yarns. Fiber volume fraction of UD and BD was obtained experimentally and analytically. Fiber volume fraction of BD was derived based on unit cell of braiding yarn section. Bending test was executed to investigate the effect of braiding part. The result of experiment and analysis of fiber volume fraction has good agreement. Bending strength of BD is about 20% higher than that of UD.

  • PDF

Failure Analysis on the Carbon/Epoxy Laminate Subjected to Low Velocity Impact (저속충격을 받는 Carbon/Epox 적층판의 손상 해석)

  • 이호철;이영신;김재훈;전제춘
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2000.11a
    • /
    • pp.98-101
    • /
    • 2000
  • Recently, composite material which has much excellent mechanical characteristics has been applied in many industries. However, it has a brittle characteristic under impact condition and its invisible characteristics of the damaged area has been the motivation of many engineers investigation. The modified failure criterion is implemented to predict the failure behavior of the composite plate subjected to low velocity impact using commercial finite element analysis code, ABAQUS-Ver. 5.8. The new criterion is in good agreement with experimental results and can predict the failure behavior of the composite plate subjected to low velocity impact more accurately.

  • PDF

Experimental and microstructural evaluation on mechanical properties of sisal fibre reinforced bio-composites

  • Kumar, B. Ravi;Hariharan, S.S.
    • Steel and Composite Structures
    • /
    • v.33 no.2
    • /
    • pp.299-306
    • /
    • 2019
  • The natural fibre composites are termed as bio-composites. They have shown a promising replacement to the current carbon/glass fibre reinforced composites as environmental friendly materials in specific applications. Natural fibre reinforced composites are potential materials for various engineering applications in automobile, railways, building and Aerospace industry. The natural fibre selected to fabricate the composite material is plant-based fibre e.g., sisal fibre. Sisal fibre is a suitable reinforcement for use in composites on account of its low density, high specific strength, and high hardness. Epoxy is a thermosetting polymer which is used as a resin in natural fibre reinforced composites. Hand lay-up technique was used to fabricate the composites by reinforcing sisal fibres into the epoxy matrix. Composites were prepared with the unidirectional alignment of sisal fibres. Test specimens with different fibre orientations were prepared. The fabricated composites were tested for mechanical properties. Impact test, tensile test, flexural test, hardness test, compression test, and thermal test of composites had been conducted to assess its suitability in industrial applications. Scanning electron microscopy (SEM) test revealed the microstructural information of the fractured surface of composites.

Comparison of Interfacial Aspects of Carbon and Glass Fibers/Epoxy Composites by Microdroplet Tests at Low and Room Temperatures (상온 및 저온에서의 탄소와 유리섬유/에폭시 복합재료의 계면특성 비교)

  • Wang, Zuo-Jia;GnidaKouong, Joel;Kim, Myung-Soo;Park, Joung-Man;Um, Moon-Kwang
    • Journal of Adhesion and Interface
    • /
    • v.10 no.4
    • /
    • pp.162-168
    • /
    • 2009
  • As a preliminary study of optimum composite properties under cryogenic temperature, the comparison of interfacial properties of carbon or glass fibers reinforced epoxy composites was evaluated at ambient and intermediate low temperature, i.e., 25 and $-10^{\circ}C$ by using micromechanical techniques. Under tensile and compressive loading conditions, their mechanical modulus at low temperature was higher than that atambient temperature. Interfacial shear strength (IFSS) at ambient and low temperatures was compared to each other, depending on epoxy matrix toughness and apparent modulus at the interface. The IFSS was much higher at low temperature than that at room temperature because of the increased epoxy matrix modulus. Statistical distributions of tensile strengths of glass and carbon fibers were evaluated for different temperature ranges, which is dependent upon fiber's inherent flaws and rigidity.

  • PDF

Effect of Combined Environmental Factors on Degradation Behavior of Carbon Fiber/Epoxy Composites (복합적인 환경인자의 영향에 따른 탄소섬유/에폭시 복합재의 열화 특성)

  • Hwang, Young-Eun;Lee, Gil-Hyung;Yoon, Sung-Ho
    • Composites Research
    • /
    • v.22 no.5
    • /
    • pp.37-42
    • /
    • 2009
  • Thermal analysis properties and chemical structure of carbon fiber/epoxy composites under environmental exposure were examined using an accelerated aging tester which can simulate real weather conditions such as temperature, moisture and ultraviolet. The composite specimens were exposed to combined environmental factors up to 3000 hours. Thermal analysis properties and chemical structure of the composites were evaluated with various exposure times through Modulated DSC and FTIR. According to the results of Modulated DSC, the glass transition temperature increased as exposure time increased due to the formation of network structures in the composites. Also endotherm peaks of enthalpy relaxation related to physical aging that can affect the properties of the composites were observed as exposure time increased. From the results of FTIR, it was found that the location of the peaks was little affected by exposure time, but the intensity of the peaks slightly decreased as exposure time increased due to the curing reaction in the epoxy group.

Analysis of Interfacial Shear Strength of Fiber/Epoxy Composites by Microbond Test and Finite Element Method (미소접합시험과 유한요소법을 통한 섬유/에폭시 복합재의 계면 전단강도 해석)

  • Kang, Soo-Keun;Lee, Deok-Bo;Choi, Nak-Sam
    • Composites Research
    • /
    • v.19 no.4
    • /
    • pp.7-14
    • /
    • 2006
  • Interfacial shear strength between epoxy and carbon fiber has been analyzed utilizing the microbond specimen with an epoxy micro-droplet adhered onto single carbon fiber. The interfacial shear stress distributions along the fiber/matrix interface were calculated by finite element analysis using three kinds of finite element models such as droplet model, circular-crosssection model and pull-out model. Conclusions were obtained as follows. (1) Interfacial shear stress distribution showed that larger stresses were concentrated in the fiber/matrix interface for microbond test than for pull-out test. Thus, debonding at the fiber/matrix interface during microbond test was liable to occur at low load level. (2) Microbond test showed higher interfacial strength which was caused by various effects of micro-droplet geometry and size as well as stress concentration in the region contacting with the micro-vise tip.