THE COMPARISON OF SHEAR STRENGTH AND BRACKET PLACEMENT BETWEEN BONDING TECHNIQUES (접착술식에 따른 전단강도 및 Bracket위치의 비교)

  • Pak, Yun-Kyong;Kook, Yoon-A;Kim, Sang-Cheol
    • The korean journal of orthodontics
    • /
    • v.21 no.3
    • /
    • pp.513-520
    • /
    • 1991
  • The purpose of this study was to compare the bracket placement and the shear bond strength of indirect-bonded brackets with those of direct-bonded ones. Forty eight extracted human teeth were collected and attached with brackets and tested on shear bond strength, using Instron. Fourteen patients from Wonkwang University Dental Hospital were selected for direct bonding of brackets and their teeth were measured on bracket angulation and bracket height. The obtained results were as follows: 1. The shear bond strengths of incisors were higher in direct-bonding,group, rather than in-direct-bonding group. But, the shear bond strength of premolars showed no significant differences between groups. 2. The bracket angulations of indirect-bonding group were preciser than those of direct-bonding group, especially in upper first premolars, lower lateral incisors, canines, premolars. 3. In bracket height, there were no significant differences between groups.

  • PDF

Shear bond strength between gold alloy and orthodontic metal bracket using light emitting diode curing light (Light emitting diode를 이용한 광중합 시 금합금과 교정용 금속 브라켓의 전단접착강도)

  • Jung, Min-Ho;Chung, Shin-Hye;Shon, Won-Jun
    • The korean journal of orthodontics
    • /
    • v.40 no.1
    • /
    • pp.27-33
    • /
    • 2010
  • Objective: The need to bond orthodontic brackets onto various alloys has increased because of the increasing demand for adult orthodontic treatment. This study tried to evaluate the shear bond strength between gold alloy and metal bracket using light emitting diode (LED) light curing after metal primer and silicoating surface conditioning. Methods: Half of the type III gold alloy plates were treated with sandblasting with aluminum oxide and metal primer containing 4-META. the other half were treated with silica and silane. Metal brackets were bonded with Transbond XT light curing adhesive on these plates and shear bond strength were evaluated 1 hour, 6 hours, and 24 hours later. The differences of shear bond strength between groups were evaluated with two-way ANOVA. Results: The results showed higher bond strength in the silicoating group and a tendency of bond strength increase over time. Conclusions: When using LED curing lights for metal bracket bonding to alloy surfaces, long curing time and silicoating can produce a reliable bonding strength.

Effect of tribochemical silica coating on the shear bond strength of rebonded monocrystalline ceramic brackets (단결정형 세라믹 브라켓의 재접착 시 tribochemical silica coating이 전단접착강도에 미치는 영향)

  • Jeon, Young-Mi;Son, Woo-Sung;Kang, Sang-Wook
    • The korean journal of orthodontics
    • /
    • v.40 no.3
    • /
    • pp.184-194
    • /
    • 2010
  • Objective: The purpose of this study was to investigate the effect of tribochemical silica coating on the shear bond strength (SBS) of rebonded ceramic brackets using nano-filled flowable composite resin. Methods: A total of 60 premolars were prepared and divided into 4 equal groups as follows: Tribochemical silica coating (TC) + Transbond XT (XT), TC + Transbond supreme LV (LV), Sandblast treatment (SA) + XT, SA + LV. Treated ceramic brackets were rebonded on the premolars using each adhesive. All samples were tested in shear mode on a universal testing machine. Results: SBS of silica coated groups were high enough for clinical usage (TCLV: 10.82 $\pm$ 1.82 MPa, TCXT: 11.50 $\pm$ 1.72 MPa). But, SBS of the sandblast treated groups had significantly lower values than the tribochemical silica coated groups (SALV, 1.23 $\pm$ 1.16 MPa; SAXT, 1.76 $\pm$ 1.39 MPa; p < 0.05). There was no difference between the shear bond strength by type of adhesive. In the silica coated groups, 77% of the samples showed bonding failure in the adhesive. In the sandblast treated group, all bonding failures occurred at the bracket-adhesive interface. Conclusions: The result of this study suggest that newly introduced nano-filled flowable composite resin and tribochemical silica coating application on debonded ceramic bracket bases can produce appropriate bond strengths for orthodontic bonding.

The Effect of Tin Ion-plating on the Bond Strength of Orthodontic Bracket (TiN Ion-Plating이 교정용 브라켓의 접착강도에 미치는 영향)

  • KIM, Seok-Yong;KWON, Oh-Won;KIM, Kyo-Han
    • The korean journal of orthodontics
    • /
    • v.27 no.1
    • /
    • pp.157-171
    • /
    • 1997
  • This study was conducted to see the effect of TiN ion-plating on the bond strength of orthodontic bracket. Three stainless-steel brackets with different base types were chosen; when TiN ion-plated brackets and non iorrplated brackets were bonded to the teeth, initial and long-term bond strength were measured, The observations oi bonding surface and failure sites through the scanning electron microscope were analysed and compared. The summary of this study was as follows; ${\cdot}$ When TiN ion-plating was not applied, the Micro-Loc type was the highest in bond strength atter 24 hours as $5.89{\pm}1.77$ MPa, followed by $4,27{\pm}1.12MPa$ for Foil Mesh type and $2.64{\pm}0.58MPa$ for Undercut type(P<0.05). ${\cdot}$ Under TiN ion-plating, the bond strength after 24 hours showed: Micro-Loc type $-6.26{\pm}1.51MPa$, Foil Mesh type $-7.45{\pm}2.01MPa$, Undercut type $-2.93{\pm}0.84MPa$. Unlike in the case of non ion-plating, Foil Mesh type showed a higher strength than Micro-Loc type, with Undercut type still showing the lowest bond strength(P<0.05). The bond strength, after 24 hours, increased in case of ion-plated in all 3 types, but a significant increase was shown only in Foil Mesh type(P<0.001). ${\cdot}$ Under a long-term immersion, regardless of ion or non ion-plating, bond strength in general increased over the initial bond strength(one day), with more stability. ${\cdot}$ Through scanning electron microscopic observation of bonding surface, it was found that, regardless of the bracket base type or the application of ion-plating, the resin was thoroughly spreaded into bracket base to form a solid bonding surface between the bracket and the tooth. This was also true in case of a long-term immersion. ${\cdot}$ The scanning electron microscopic observation of failure sites revealed diverse failure patterns.

  • PDF

A comparative study on bond strength and adhesive failure pattern in bracket bonding with self-etching primer (Self-etching Primer를 이용한 교정용 브라켓 부착시 전단결합강도와 파절양상에 관한 비교연구)

  • Kim, You-Kyoung;Lee, Jin-Woo;Cha, Kyung-Suk
    • The korean journal of orthodontics
    • /
    • v.34 no.4 s.105
    • /
    • pp.325-332
    • /
    • 2004
  • A self-etching primer that combines the etchant and primer in one chemical compound saves time and should be mote cost-effective to the clinician and patient. The purpose of this study was to evaluate the clinical effectiveness of a self-etching primer by measuring shear bond strengths according to various conditions and observing adhesive failure patterns. For this Investigation, 120 upper and lower premolars extracted for orthodontic purposes were used and randomly divided into six groups of twenty teeth each. Human premolars were embedded in a metal cylinder with orthodontic resin. Metal brackets and ceramic brackets were bonded with XT primer and self-etching primer by means of XT adhesive. Upon curing, plasma arc light and visible light were used. After bonding, the shear bond strength was tested by Instron universal testing machine, and the amount of residual adhesive that remained on the tooth after debonding was measured by stereoscope and assessed with an adhesive remnant index. The results were as fellows: 1. When brackets were bonded, if other conditions remained the same, there was no significant difference in shear bond strength due to the type of primer - either self-etching primer or XT primer. 2. When metal brackets were bonded, there was no significant difference in shear bond strength according to the source of light - plasma arc light or visible light - and type of primer. 3. There was a very significant difference in shear bond strength according to the type of brackets - metal or ceramic brackets. The shear bond strength of ceramic brackets was stronger than metal brackets. 4. When the adhesive failure patterns of metal brackets bonded with self-etching primer were observed by using the adhesive remnant index, the bond failure of the metal bracket occurred more frequently at the bracket-adhesive. The failure of the ceramic bracket, however, occurred more frequently at the enamel-adhesive interface. The adhesive failure patterns of metal brackets bonded with XT primer observed the same patterns. The above results suggest that self-etching primer can be clinically useful for bonding the brackets without fear of a decrease in shear bond strength.

Shear bond strength of ceramic brackets bonded with antimicrobial monomer-containing self-etching primer (항미생물제제를 포함한 self-etching primer로 접착한 세라믹 브라켓의 전단 결합 강도)

  • Kwon, Tae-Hun;Kang, Jang-Mi;Chang, Na-Young;Kang, Kyung-Hwa
    • The korean journal of orthodontics
    • /
    • v.41 no.1
    • /
    • pp.16-24
    • /
    • 2011
  • Objective: The purpose of this study was to determine (1) the shear bond strength (SBS) of an antimicrobial monomer-containing self-etching primer according to ceramic bracket types and (2) the bracket-adhesive failure mode using an adhesive remnant index (ARI). Methods: A total of 90 extracted human teeth were randomly divided into 6 groups. Each group consisted of one of two ceramic brackets (monocrystalline, polycrystalline) and one of three primers (Transbond XT primer, Transbond Plus SEP, Clearfil Protect Bond) with each group containing 15 specimens. The SBS was measured, and adhesive residues left on the tooth surface were assessed. Results: The SBS of polycrystalline ceramic bracket groups was Significantly higher than that of the monocrystalline ceramic bracket groups (p < 0.001). The SBS of Transbond XT primer groups was significantly higher than those of Transbond Plus SEP groups and Clearfil Protect Bond groups (p < 0.001). All the groups showed bonding failures between the bracket base and adhesive. Conclusions: The combination of a self-etching primer with a monocrystalline bracket is recommended for clinical use, considering its acceptable SBS and mode of failure.

The effect of chlorhexidine varnish application on the shear bond strength of orthodontic brackets (클로르헥시딘 바니쉬의 적용이 교정용 브라켓의 전단접착강도에 미치는 영향)

  • Im, Dong-Hyuk;Kim, Tae-Woo;Chang, Young-Il;Nahm, Dong-Suk;Yang, Won-Sik;Baek, Seung-Hak
    • The korean journal of orthodontics
    • /
    • v.30 no.2 s.79
    • /
    • pp.215-222
    • /
    • 2000
  • The purpose of this study was to determine whether the application of chlorhexidine varnish affects the shear bond strength and failure pattern of orthodontic brackets or not. The experimental group consisted of 22 human premolars which extracted after chlorhexidine varnish application (4 times for 1 week interval) in vivo, and the control group consisted of 22 human premolars which extracted without any pre-treatment. After all teeth were etched with $37\%$ phosphoric acid gel, metal orthodontic brackets (Q-3002, RMO, USA) were bonded to each tooth using auto-polymerizing orthodontic resin (Ortho-One, Bisco, USA) with the same bonding procedure. The shear bond strength was measured with Instron universal testing machine (model 4466, Instron Ltd., England), and the failure pattern of each bracket was examined with Scanning Electron Microscope (SM 840A, JEOL, Japan). The data were analysed statistically with t-test. The results were as follows : 1. Application of chlorhexidine varnish had no significant effect on the shear bond strength of the orthodontic bracket. 2. There was no significant difference in the failure pattern of orthodontic bracket between the experimental group and the control group.

  • PDF

A COMPARATIVE STUDY ON SHEAR BOND STRENGTHS INFLUENCED BY TIME ELAPSED AFTER BRACKET BONDING WITH A LIGHT-CURED GLASS IONOMER CEMENT (광중합형 글래스아이오노머 시멘트의 브라켓 접착후 시간 경과에 따른 전단결합강도의 비교연구)

  • Lee, Ki-Soo;Lim, Ho-Nam;Park, Young Guk;Shin, Kang-Seob
    • The korean journal of orthodontics
    • /
    • v.25 no.5 s.52
    • /
    • pp.605-611
    • /
    • 1995
  • The purpose of this study was to evaluate effects of time on shear bond strengths of a light-cured glass ionomer cement and chemically cured resin cement to enamel, and to observe the failure patterns of bracket bondings. Shear bond strength of a light-cured glass ionomer cement were compared with that of a resin cement. Metal brackets were bonded on the extracted human bicuspids. Specimens were subjected to a shear load(in an Instron machine) after storage at room temperature for 5 and 15 minutes; after storage in distilled water at $37^{\circ}C$ for 1 or 35 days. The deboned specimens were measured In respect of adhesive remnant index. The data were evaluated and tested by ANOVA, Duncan's multiple range test, and t-test, and those results were as follows. 1. The shear bond strength of light-cured glass ionomer cement is higher than that of resin cement at 5 and 15 minutes. 2. The shear bond strengths of both light-cured glass ionomer cement and resin cement increase with time. There was no significant difference in those of both 1 day group and 35 day group 3. Light-cured glass ionomer cement is suitable as orthodontic bracket adhesives

  • PDF

TENSILE STRENGTH OF DIRECT-BONDING BRACKETS (Direct-bonding bracket 의 인장강도(引張?度))

  • Kwon, Oh Won
    • The korean journal of orthodontics
    • /
    • v.12 no.2
    • /
    • pp.139-144
    • /
    • 1982
  • As adhesive systems were improved, a great variety of bracket bases were available. The purpose of this study was to evaluate the adhesive porperties of 3 types of direct-bonding brackets by testing the tensile stremgth. 60 noncarious premolars extracted for orthodontic treatment were used. The tensile strength was tested by Tensilon/UTM-1-10000C after 24 hours from bonding. Following results were obtained; There was no difference between the tensile strength of foil-mesh base bracket and photoetched base bracket statisstically. However, the accurate test result of plastic bracket could not be obtained due to the distortion of bracket wing during testing. Of the failure in fail-mesh base bracket and photo-etched base bracket, the combination type of failure, where part of the adhesive remained on the tooth and part on the bracket was the most common type (50%, 50%), The second type of failure occured at the bracket-adhesive interface (30%, 35%) and the last type of failure occured at the adhesive-tooth interface (20%, 15%).

  • PDF