DOI QR코드

DOI QR Code

Shear bond strength between gold alloy and orthodontic metal bracket using light emitting diode curing light

Light emitting diode를 이용한 광중합 시 금합금과 교정용 금속 브라켓의 전단접착강도

  • Jung, Min-Ho (Department of Orthodontics, School of Dentistry, Seoul National University, Samsung Medical Dental Center) ;
  • Chung, Shin-Hye (Department of Conservative Dentistry, Seoul National University) ;
  • Shon, Won-Jun (Department of Conservative Dentistry, Seoul National University)
  • 정민호 (서울대학교 치과병원 교정과, 삼성의료원 교정과) ;
  • 정신혜 (서울대학교 치의학대학원 보존학교실) ;
  • 손원준 (서울대학교 치의학대학원 보존학교실)
  • Published : 2010.02.28

Abstract

Objective: The need to bond orthodontic brackets onto various alloys has increased because of the increasing demand for adult orthodontic treatment. This study tried to evaluate the shear bond strength between gold alloy and metal bracket using light emitting diode (LED) light curing after metal primer and silicoating surface conditioning. Methods: Half of the type III gold alloy plates were treated with sandblasting with aluminum oxide and metal primer containing 4-META. the other half were treated with silica and silane. Metal brackets were bonded with Transbond XT light curing adhesive on these plates and shear bond strength were evaluated 1 hour, 6 hours, and 24 hours later. The differences of shear bond strength between groups were evaluated with two-way ANOVA. Results: The results showed higher bond strength in the silicoating group and a tendency of bond strength increase over time. Conclusions: When using LED curing lights for metal bracket bonding to alloy surfaces, long curing time and silicoating can produce a reliable bonding strength.

성인 교정환자의 수요가 증가하면서 보철물 표면에 교정장치를 부착해야 하는 빈도가 늘어나고 있다. 본 연구는 금속표면에 교정장치를 직접 접착하고자 할 때 사용하는 metal primer와 silicoating으로 각각 금합금의 표면을 처리한 후 light emitting diode (LED) 광중합기를 사용하여 광중합을 시행하여 접착력을 평가해 보고자 하였다. Type III gold alloy 표면에 aluminum oxide를 이용한 sandblasting 후 4-META 계열의 metal primer로 처리한 시편과 silica를 이용한 sandblasting 후 silane으로 처리한 시편에 광중합형 접착레진인 Transbond XT를 이용하여 금속 브라켓을 접착하고 접착 후 1시간, 6시간, 24시간 후 전단접착강도의 변화를 비교, 관찰하였다. 측정된 값을 이원분산분석(two-way analysis of variance)을 이용하여 비교하고 두 가지 표면처리 방법 간에 접착강도에 차이가 있는지도 살펴보았다. 연구결과, metal primer에 비하여 silicoating을 시행한 시편에서 높은 전단접착강도가 관찰되었으며, 시간이 경과할수록 접착강도가 증가하는 경향을 보였다. Adhesive remnant index (ARI)에서는 군 간 유의한 차이를 보이지 않았다. LED를 이용하여 광중합을 시행하는 경우 법랑질에 비하여 긴 시간의 광중합을 실시하고 metal primer보다는 silicoating 방법을 사용하는 것이 금합금표면에 교정장치를 부착할 때 더 높은 접착강도를 얻을 수 있을 것이다.

Keywords

References

  1. Jung MH. Current trends in orthodontic patients in private orthodontic clinics. Korean J Orthod 2009;39:36-42. https://doi.org/10.4041/kjod.2009.39.1.36
  2. Keim RG, Gottlieb EL, Nelson AH, Vogels DS 3rd. 2008 JCO study of orthodontic diagnosis and treatment procedures, part 1: results and trends. J Clin Orthod 2008;42:625-40.
  3. Newman GV. Epoxy adhesives for orthodontic attachments: progress report. Am J Orthod 1965;51:901-12. https://doi.org/10.1016/0002-9416(65)90203-4
  4. Zachrisson BU. Bonding in orthodontics. In: Graber TM, Vanarsdall RL Jr, editors. Orthodontics: current principles and techniques. 3rd ed. St. Louis: Mosby; 2000. p.557-646.
  5. Proffit WR, Fields HW, Nixon WL. Occlusal forces in normal- and long-face adults. J Dent Res 1983;62:566-70. https://doi.org/10.1177/00220345830620051201
  6. Zachrisson BU, Buyukyilmaz T. Recent advances in bonding to gold, amalgam and porcelain. J Clin Orthod 1993;27: 661-75.
  7. Sperber R, Watson P, Rossouw P, Sectakof P. Adhesion of bonded orthodontic attachments to dental amalgam: in vitro study. Am J Orthod Dentofac Orthop 1999;116:506-13. https://doi.org/10.1016/S0889-5406(99)70180-0
  8. Lee YK, Cha JY, Yu HS, Hwang CJ. Effect of metal primer and thermocycling on shear bonding strength between the orthodontic bracket and gold alloy. Korean J Orthod 2009;39:320-9. https://doi.org/10.4041/kjod.2009.39.5.320
  9. Nergiz I, Schmage P, Herrman W, Ozcan M. Effect of alloy type and surface conditioning on roughness and bond strength of metal brackets. Am J Orthod Dentofac Orthop 2004;125:42-50. https://doi.org/10.1016/S0889-5406(03)00507-9
  10. Mills RW, Jandt KD. Blue LEDs for curing polymer based dental filling materials. Lasers Electro-Opt Soc Inst Electr Electron Engr Newslett 1998;12:9-10.
  11. Mills RW, Jandt KD, Ashworth SH. Dental composite depth of cure with halogen and blue light emitting diode technology. Br Dent J 1999;186:388-91.
  12. Swanson T, Dunn WJ, Childers DE, Taloumis LJ. Shear bond strength of orthodontic brackets bonded with light-emitting diode curing units at various polymerization times. Am J Orthod Dentofacial Orthop 2004;125:337-41. https://doi.org/10.1016/j.ajodo.2003.04.011
  13. Krishnaswamy NR, Sunitha C. Light-emitting diode vs halogen light curing of orthodontic brackets: a l5-month clinical study of bond failures. Am J Orthod Dentofacial Orthop 2007;132: 518-23. https://doi.org/10.1016/j.ajodo.2005.09.038
  14. Niepraschk M, Rahiotis C, Bradley TG, Eliades T, Eliades G. Effect of various curing lights on the degree of cure of orthodontic adhesives. Am J Orthod Dentofacial Orthop 2007;132: 382-4. https://doi.org/10.1016/j.ajodo.2007.04.029
  15. Toroglu MS, Yaylali S. Effects of sandblasting and silica coating on the bond strength of rebonded mechanically retentive ceramic brackets. Am J Orthod Dentofacial Orthop 2008; 134:181 .el-181.e7.
  16. Artun J, Bergland S. Clinical trials with crystal growth conditioning as an alternative to acid-etch enamel pretreatment. Am J Orthod 1984;85:333-40. https://doi.org/10.1016/0002-9416(84)90190-8
  17. Cook WD, Beech DR, Tyas MJ. Structure and properties of methacrylate based dental restorative materials. Biometerials 1985;6:362-8. https://doi.org/10.1016/0142-9612(85)90094-8
  18. Kyldal KK, Ruyter IE. How different curing methods affect the degree of conversion of resin-based inlay/onlay materials. Acta Odontol Scand 1994;52:315-22. https://doi.org/10.3109/00016359409029044
  19. Lee SJ. Effects of light source, exposure time and post-irradiation time on the degree of conversion and shear bond strength of orthodontic adhesive [PhD thesis]. Seoul, Korea: Graduate School, Seoul National University; 2003.
  20. Stahl F, Ashworth SH, Jandt KD, Mills RW. Light-emitting diode (LED) polymerisation of dental composites: flexural properties and polymerisation potential. Biomaterials 2000;21: 1379-85. https://doi.org/10.1016/S0142-9612(00)00029-6
  21. Cheng L, Ferguson JW, Jones P, Wilson HJ. An investigation of the polymerization of orthodontic adhesives by the transillumination of tooth tissue. Br J Orthod 1989;16:183-8. https://doi.org/10.1179/bjo.16.3.183
  22. Ulusoy C, Irmak O, Bagis Y, Ilke O, Ulusoy A. Temperature rise and shear bond strength of bondable buccal tubes bonded by various light sources. Eur J Orthd 2008;30:413-7. https://doi.org/10.1093/ejo/cjn013
  23. Bradburn G, Pender N. An in vitro study of the bond strength of two light-cured composites used in the direct bonding of orthodontic brackets to molars. Am J Orthod Dentofacial Orthop 1992;102:418-26. https://doi.org/10.1016/S0889-5406(05)81188-6
  24. Reynolds IR. A review of direct orthodontic bonding. Br J Orthod 1975;2:171-8. https://doi.org/10.1080/0301228X.1975.11743666
  25. Buyukyilmaz T, Zachrisson BU. Improved orthodontic bonding to silver amalgam. Part 2. Lathe-cut, admixed, and spherical amalgams with different intermediate resins. Angle Orthod 1998;68:337-44.
  26. Tanaka T, Nagata K, Takeyama M, Atsuta M, Nakabayashi N, Masuhara E. 4-META opaque resin--a new resin strongly adhesive to nickel-chromium alloy. J Dent Res 1981;60:1697-706. https://doi.org/10.1177/00220345810600091101
  27. Hansson O. Strength of bond with Comspan Opaque to three silicoated alloys and titanium. Scand J Dent Res 1990;98: 248-56.
  28. Peutzfeldt A, Asmussen E. Silicoating: evaluation of a new method of bonding composite resin to metal. Scand J Dent Res 1988;96:171-6.
  29. Craig RG, Powers JM. Restorative dental materials. 11th ed. St. Louis: Mosby; 2002. p.67-l24.
  30. Buyukyilmaz T, Zachrisson Y, Zachrisson B. Improving orthodontic bonding to gold alloy. Am J Orthod Dentofacial Orthop 1995;108:510-8. https://doi.org/10.1016/S0889-5406(95)70051-X
  31. Reliance metal primer; instruction for use. Itaca, Reliance Orthodontic Products Inc.
  32. Super-Bond C&B; Pictorial instruction for use. Moriyama, Japan: Sun Medical Co.
  33. 3M ESPE Sil; instruction for use, St. Paul, 3M ESPE Dental Products.
  34. Patusco VC, Montenegro G, Lenza MA, Alves de Carvalho A. Bond strength of metallic brackets after dental bleaching. Angle Orthod 2009;79:122-6. https://doi.org/10.2319/072507-345.1
  35. Nebbe B, Stein E. Orthodontic brackets bonded to glazed and deglazed porcelain surfaces. Am J Orthod Dentofacial Orthop 1996;109:431-6. https://doi.org/10.1016/S0889-5406(96)70125-7

Cited by

  1. The effects of primer precuring on the shear bond strength between gold alloy surfaces and metal brackets vol.34, pp.1, 2010, https://doi.org/10.1093/ejo/cjq163