• Title/Summary/Keyword: atomizing reduction steel slag

Search Result 5, Processing Time 0.021 seconds

Characteristics of Concrete Polymer Composite Using Atomizing Reduction Steel Slag as an Aggregate (II) (Use of Polystyrene as a Shrinkage Reducing Agent) (아토마이징 제강 환원슬래그를 골재로 사용한 폴리머 콘크리트 복합재료의 특성(II) (폴리스티렌 수축저감재 사용))

  • Hwang, Eui-Hwan;Kim, Jin-Man
    • Applied Chemistry for Engineering
    • /
    • v.25 no.4
    • /
    • pp.380-385
    • /
    • 2014
  • Spherical atomizing reduction steel slag was prepared by atomizing technology using reduction steel slag (ladle furnace slag, LFS) generated from steel industry. In order to develop the mass-recycling technology of atomizing reduction steel slag, polymer concrete composite was prepared using spherical atomizing reduction steel slag instead of fine aggregate (river sand) and coarse aggregate (crushed aggregate), depending on the grain size. Different polymer concrete specimens were prepared with the various proportions of polymer binder and replacement ratios of atomizing reduction steel slag in order to investigate the characteristics of polymer concrete composite. Results showed that compressive strengths of polymer concrete specimens decreased with the increase of replacement ratios of atomizing reduction steel slag, but flexural strengths of the specimens showed a maximum strength at the 50% of replacement ratios of atomizing reduction steel slag. It was concluded that addition ratio of polymer binder, which affect greatly on the prime cost of production of polymer concrete, could be reduced by maximum 18.2 vol% because the workability of the polymer concrete was remarkably improved by using the atomizing reduction steel slag. However, further study is required because the mechanical strength of the specimen using atomizing reduction steel slag was greatly reduced in hot water resistance test.

Characteristics of Polyester Polymer Concrete Using Spherical Aggregates from Industrial By-Products(II)(Use of Fly Ash and Atomizing Reduction Steel Slag) (산업부산물 구형골재를 사용한 폴리에스테르 폴리머 콘크리트의 특성(II) (플라이 애쉬와 아토마이징 제강 환원슬래그 사용))

  • Hwang, Eui-Hwan;Kim, Jin-Man
    • Korean Chemical Engineering Research
    • /
    • v.53 no.3
    • /
    • pp.364-371
    • /
    • 2015
  • For the cost down of polymer concrete, It is very important to reduce the use amount of polymer binder, which occupies most of the production cost of polymer concrete. Fly ash and atomizing reduction steel slag are spherical materials obtained from industrial by-products. Spherical atomizing reduction steel slag was manufactured using steel slag from reduction process of ladle furnace by atomizing technology. To investigate the physical properties of polymer concrete, polymer concrete specimens were prepared with the various proportions of polymer binder and replacement ratios of atomizing steel slag. Results showed that compressive and flexural strengths of the specimens were remarkably increased with the addition amount of polymer binder and the replacement ratios of atomizing steel slag. In the hot water resistance test, compressive strength, flexural strength, bulk density and average pore diameter decreased but total pore volume and pore diameter increased. We found that polymer concrete developed in this study reduced the amount of polymer binder by 18.2% compared to the conventional product because of the remarkable improvement of workability of polymer concrete using spherical fly ash and atomizing reduction steel slag instead of calcium carbonate (filler) and river sand (fine aggregate).

Characteristics of Concrete Polymer Composite Using Atomizing Reduction Steel Slag (I) (Use of PMMA as a Shrinkage Reducing Agent) (아토마이징 제강 환원슬래그를 사용한 폴리머 콘크리트 복합재료의 특성 (I) (PMMA 수축저감재를 사용))

  • Hwang, Eui Hwan;Kim, Jin Man
    • Applied Chemistry for Engineering
    • /
    • v.25 no.2
    • /
    • pp.181-187
    • /
    • 2014
  • In order to use the spherical atomizing reduction steel slag (ladle furnace slag, LFS) instead of the fine aggregate of polymer concrete composites, various specimens were prepared with various replacement ratios of atomizing reduction steel slag and the addition ratios of polymer binder. Physical properties of these specimens were investigated through the absorption test, the compressive strength test, the flexural strength test, the hot water resistance test, the pore analysis and the micro-structure using scanning electron microscope. Results showed that the compressive strength and flexural strength of specimens with 7.5% of polymer binders increased with the increase of replacement ratios of atomizing reduction steel slag, but those of the specimens with 8.0% or more of polymer binders showed a maximum strength at a certain replacement ratio due to the material segregation causing the increase of fluidity. By hot water resistance tests, the compressive strength, flexural strength, average pore diameter, and bulk density decreased but the total pore volume and pore diameter increased. It was concluded that the amount of polymer binders could be reduced by maximum 23.8%, because the workability of the polymer concrete was remarkably improved by using the atomizing reduction steel slag instead of fine aggregate. However, since the use of atomizing reduction steel slag decreased the resistance of the polymer concrete to hot water, further studies are required.

Characteristics of Polyester Polymer Concretes Using Spherical Aggregates from Industrial By-Products (III) (Using an Atomizing Steel Slag as a Filler and Fine Aggregate) (산업부산물 구형골재를 사용한 폴리에스테르 폴리머 콘크리트의 특성(III) (아토마이징 제강슬래그를 충전재와 잔골재로 사용))

  • Hwang, Eui-Hwan;Kim, Jin-Man
    • Applied Chemistry for Engineering
    • /
    • v.26 no.1
    • /
    • pp.104-110
    • /
    • 2015
  • It is known that polymer concretes are 8~10 times more expensive than ordinary Portland cement concretes; therefore, in the production of polymer concrete products, it is very important to reduce the amount of polymer binders used because this occupies the most of the production cost of polymer concretes. In order to develop a technology for the reduction of polymer binders, smooth and spherical aggregates were prepared by the atomizing technology using the oxidation process steel slag (electric arc furnace slag, EAFS) and the reduction process steel slag (ladle furnace slag, LFS) generated by steel industries. A reduction in the amount of polymer binders used was expected because of an improvement in the workability of polymer concretes as a result of the ball-bearing effect and maximum filling effect in case the polymer concrete was prepared using the smooth and spherical atomized steel slag instead of the calcium carbonate (filler) and river sand (fine aggregate) that were generally used in polymer concretes. To investigate physical properties of the polymer concrete, specimens of the polymer concrete were prepared with various proportions of polymer binder and replacement ratios of the atomized reduction process steel slag. The results showed that the compressive strengths of the specimens increased gradually along with the higher replacement ratios of the atomized steel slag, but the flexural strength showed a different maximum strength depending on the addition ratio of polymer binders. In the hot water resistance test, the compressive strength, flexural strength, bulk density, and average pore diameter decreased; but the total pore volume and porosity increased. It was found that the polymer concrete developed in this study was able to have a 19% reduction in the amount of polymer binders compared with that of the conventional product because of the remarkable improvement in the workability of polymer concretes using the spherical atomized oxidation steel slag and atomized reduction steel slag instead of the calcium carbonate and river sand.

An Experimental Study on Rapid Repairing Mortar for Road with Steel Slag (철강 슬래그를 사용한 도로용 긴급보수 모르타르에 관한 실험적 연구)

  • Jung, Ui-In;Kim, Bong-Joo;im, Jin-Man;Kwak, Eun-Gu
    • Journal of the Korea Institute of Building Construction
    • /
    • v.18 no.5
    • /
    • pp.419-427
    • /
    • 2018
  • The purpose of this study is to recycle steel slag generated from the iron producing process and to use steel slag as a construction material which is currently landfilled Steel slag is subjected to aging treatment due to the problem of expansion and collapse when it reacts with water. The Slag Atomizing Technology (SAT) method developed to solve these problems of expanding collapse of steel slag. In this study, experimental study on the emergency repair mortar using the reducing slag, electric arc furnace slag and silicon manganese slag manufactured by the SAT method is Reduced slag was shown an accelerated hydration when it was replaced with rapidly-setting cement, and the rate of substitution was equivalent to 15%. It is shown that the electric furnace oxide slag is equivalent to 100% of the natural aggregate, and it can be replaced by 15-30% when the silicon manganic slag is substituted for the electric furnace oxide slag. With the above formulation, it was possible to design the rapidly repair mortar for road use. These recycling slags can contribute on achieving sustainability of construction industry by reducing the use of cement and natural aggregates and by reducing the generation of carbon dioxide and recycling waste slag.