Estimation of Fatigue Characteristics Using Weibull Statistical Analysis with Aramid Fiber on LNGC Secondary Barrier (LNGC 2차 방벽에 적용된 Aramid 섬유의 Weibull 통계 분석을 이용한 피로특성 평가)

  • Park, Jin Hyeong;Oh, Dong Jin;Kim, Min Gyu;Kim, Myung Hyun
    • Journal of the Society of Naval Architects of Korea
    • /
    • v.54 no.5
    • /
    • pp.415-420
    • /
    • 2017
  • Insulation systems in Liquefied Natural Gas Carriers (LNGC) are vulnerable to sloshing impact and fatigue loads because of waves. If gas leaks into the primary barrier, the Flexible Secondary Barrier (FSB) prevents the leakage of gas in this system. Fatigue strength of the FSB largely depends on the behavior of composite materials. In this study, a new system is applied to the FSB using aramid fiber to improve the fatigue strength of the secondary barrier, with the intention of replacing conventional E-glass fibers. The manufacturing method involved varying the ratio of the aramid fiber to the E-glass fiber for optimum design of the FSB. The fatigue tests results of the secondary barrier using aramid fiber were superior to that using E-glass fiber. The statistical analysis is performed to obtain the fatigue test results and estimate the probability of failure as well as the design guideline of LNGC secondary barriers.

Improving the Photo-stability of p-aramid Fiber by TiO2 Nanosol (TiO2 sol-gel 합성에 의한 파라 아라미드 섬유의 내광성 증진 연구)

  • Park, Sung-Min;Kwon, Il-Jun;Sim, Ji-Hyun;Lee, Jae-Ho;Kim, Sam-Soo;Lee, Mun-Cheul;Choi, Jong-Seok
    • Textile Coloration and Finishing
    • /
    • v.25 no.2
    • /
    • pp.126-133
    • /
    • 2013
  • Although para-aramid fibers poss higher mechanical properties, they show very low resistance to sunlight exposure. This paper studied on the effect of nano-sol coated $TiO_2$ to improve the photo-stability of p-aramid fibers. Titanium dioxides were prepared by sol-gel method from titanium iso-propoxide at different R ratio ($H_2O$/titanium iso-propoxide). All samples were characterized by XRD, TEM and UV-vis spectrometer. The mechanical properties of p-aramid fabrics by $TiO_2$ nano-sol coating before and after sunlight irradiation were measured with tensile tester. XRD pattern of titanium dioxide particles was observed by mixing phase together with rutile and anatase type. The results showed, after sunlight irradiation, the decreased mechanical properties of the fiber. Furthermore, the sunlight irradiation obviously deteriorated the surface and defected areas of the fiber severely by photo-induced chain scission and end group oxidation in air.

Improvement of the Strength Properties and Impact Resistance of the Cement Composite Materials by the use of Surface Modification of the Aramid Fibers (아라미드섬유의 표면개질에 의한 시멘트 복합재료의 강도특성 및 내충격성능의 향상효과)

  • Nam, Jeong-Soo;Yoo, Jae-Chul;Kim, Gyu-Yong;Kim, Hong-Seop;Jeon, Joong-Kyu
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.19 no.1
    • /
    • pp.100-108
    • /
    • 2015
  • The purpose of this study is to evaluate the effect of improvement on the impact resistance and strength properties of cement composites by surface modification of aramid fiber. For aramid fiber reinforced cement composites, therefore, dispersion capability and the bonding efficiency between the fibers and the cement composite material need to be improved. It is possible by modifying surface properties to hydrophobic, it is considered that oiling agent ratio of 1.2 % and improvement of performance is in need to be investigated. In this study, short aramid fibers were mixed by different fiber length and oiling agent ratio. And improvement of strength properties and impact resistance performance of hybrid cement composites were evaluated under the influence of steel fiber. As a result, strength properties of aramid fiber reinforced cement composites are different by mixing ratio of fiber, oiling agent ratio and length of fiber. In case of cement composites which have same volume fraction and fiber length, tensile strength and flexural strength were improved with increase of the emulsions throughput of the fiber surface. The results of evaluation on the static strength properties had effects on impact resistance performance by high-velocity impact. And it was observed that the scabbing of rear was suppressed with increase of the oiling agent ratio.

A Study on Material Properties of Composite Panel for Impact·Blast Resistance (방호·방폭 보강용 복합패널의 재료특성에 관한 연구)

  • Kim, Woonhak;Kang, Seokwon
    • Journal of the Society of Disaster Information
    • /
    • v.12 no.4
    • /
    • pp.373-380
    • /
    • 2016
  • In order to develop composite fiber panels that can maximize the protection and blast resistance of the existing structures by improving lightweight, high-strength and fireproof performances of the single layer material of precast panels, the basic properties of the inner and outer covers that are mixed with aramid fibers (AF) and polyester fibers (PF) were evaluated in this study. Also, a basic study was performed on the performance of composite fiber panels by testing Nano-sized composite materials that are lightweight and excellent in fire resistance for their compressive strength, bending strength and tensile strength.

A Study of Resistance of Fatigue Crack in Aluminum Alloy Plate Bonded with FRP (FRP 본딩한 알루미늄 판재의 피로균열 저항성에 관한 연구)

  • 윤한기;오세욱;박원조;허정원
    • Journal of Welding and Joining
    • /
    • v.12 no.4
    • /
    • pp.117-126
    • /
    • 1994
  • APAL (Aramid Patched ALuminum alloy) was manufactured, which was a material that was consisting of a A12024-T3 aluminum alloy plate bonded to single-side of it with aramid/epoxy laminates. The aramid/epoxy laminates were bonded to it in condition of 1, 2 ply and fiber orientation of .+-.45, 0.deg./90.deg. Fatigue crack propagation tests were performed at stress ratio R-0.2, 0.5 with Al 2024-T3, APAL 45-1P, APAL 0/90-1P, APAL 45-2P, APAL 0/90-2P specimens to examine behavior of retardation in fatigue crack propagation. All the APAL specimens showed superior fatigue crack resistance. Number of cycle spended for crack to propagate from $a_{M}$=37 to $a_{M}$=65 mm in case of APAL 0/90-2P specimen was half that of Al 2024-T3 specimen. Fatigue crack propagation rate of APAL 0/90 specimens were retarded more compared to APAL 45 specimens and the amounts of retardation at R=0.5 were larger than that at R=0.2. It was found that the retardation in fatigue crack propagation was caused by intact fibers in the wake of crack.ack.

  • PDF

The Behavior of Crack Growth Rate for APAL and CPAL Patched with FRP Laminate in Aluminum Alloy Plate (알루미늄 합금판재에 FRP 라미네이터를 보강한 APAL 및 CPAL 재의 균열전파속도 거동)

  • 윤한기;정해용;허정원
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.19 no.4
    • /
    • pp.1013-1022
    • /
    • 1995
  • A hybrid composite (APAL;Aramid Patched ALuminum alloy, CPAL;Carbon Patched ALluminum alloy), consisting of a Al 2024-T3 aluminum alloy plate sandwiched between two aramid/epoxy and carbon/epoxy laminate, was developed. Fatigue crack growth behavior was examined at stress ratios of R=0.2, 0.5. The APAL and CPAL showed superior fatigue crack growth resistance, which may be attributed to the crack bridging effect imposed by the intact fibers in the crack wake.

Synthesis of Zinc Oxide by a light resistance enhancement of p-aramid fibers (Zinc Oxide 합성에 의한 p-aramid 섬유의 내광성 증진)

  • Lee, Ji-Min;Kim, Min-Ji;Kim, Sam-Soo
    • Proceedings of the Korean Society of Dyers and Finishers Conference
    • /
    • 2012.03a
    • /
    • pp.58-58
    • /
    • 2012
  • 산소와 아연의 화합물인 산화아연은 UVA, UVB 산란효과가 있는 논케미컬 자외선 차단 성분으로 물, 알코올에는 녹지 않지만 산, 알칼리, 암모니아수 등에는 녹는다. 자외선을 방지하며 입자경은 500nm전후이다. 굴절률은1.9~2.0으로 내광성, 내건성, 내열성이 커서 햇빛이나 다른 자극으로 보호막을 형성하며 수렴, 방부, 항균작용을 한다. 이러한 특징을 띄는 금속산화물 산화아연을 내광성이 약한 p-aramid섬유에 코팅해 내광성 증진을 나타내려한다. 이에 따라 본 실험에서는 암모니아수와 Zinc acetate로부터 sol-gel 합성법에 따른 ZnO 합성 실험을 수행하였다. 반응물 농도에 따른 ZnO 입자의 형상과 입자 분포를 통해 결정크기를 알아보았다. 결과 분석을 위하여 X-ray 회절분석(XRD)를 이용해 ZnO입자의 결정성을 분석하였고, 패턴의 형상과 결정크기를 전계방출형 투과전자현미경(FE-TEM)을 통해 관찰하였다.

  • PDF

Investigation of Co-poly-para-aramid Fiber Dispersion in Chloroprene Rubber Matrix and Improvement of Dispersibility Through Fiber Surface Modification

  • Garam Park;Hyeri Kim;Gayeon Jeong;Dohyeong Kim;Seungchan Noh;Dajeong Gwon;Myung Chan Choi;Jaseung Koo
    • Elastomers and Composites
    • /
    • v.57 no.4
    • /
    • pp.175-180
    • /
    • 2022
  • To produce a co-poly-para-aramid fiber (AF, Technora®)-reinforced neoprene rubber composite, dispersion of AF in a neoprene matrix is investigated. The AF is then surface-modified by mercerization and acetone, plasma, and silane treatments to improve dispersibility. Finally, an internal mixer process is used to disperse the surface-modified fibers in the neoprene rubber matrix.

Structural Performance Evaluation of Reinforced Concrete Column Reinforced with Aramid Fibers and PET Fibers (아리미드섬유와 PET섬유시트로 보강한 철근콘크리트 기둥의 구조성능평가)

  • Dong-Hwan Kim;Min-Su Jo;Jin-Hyeung Choi;Woo-Rae Cho;Kil-Hee Kim
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.27 no.1
    • /
    • pp.78-85
    • /
    • 2023
  • This study evaluates the performance of reinforced concrete columns using hybrid fiber sheets for structural behavior. The purpose of this method is to improve the load-bearing capacity of the reinforced structure by impregnating a hybrid fiber sheet, which is woven by arranging aramid and glass fibers uniaxially and attached to an aged concrete structure requiring reinforcement with epoxy. In particular, not only the weight reduction of the material obtained by using a fiber lighter than the steel material, but also the low-strength, high-toughness fiber element among the fibers used delays the brittle fracture of the high-strength, low-toughness fiber element. The low-strength, high-toughness fiber element among the fibers used delays the brittle fracture of the high-strength, low-toughness fiber element, resulting in weight reduction compared to steel. The study conducted structural tests on four specimens, with the hybrid reinforcement method and failure mode as main variables. Specimen size and loading conditions were chosen to be comparable with previous studies. The structural performance of the specimen was evaluated using energy dissipation capacity and ductility. Analysis shows that excellent results can be obtained with the hybrid fiber sheet reinforcement.

Characteristics of Recycled m-Aramid and TPP Complex Solutions in Preparation and Cotton Fibers after Coating (재활용 메타 아라미드와 TPP 복합용액의 제조 및 면섬유 코팅 후 특성분석)

  • Kim, Sam Soo;Lee, Ji Min;Cho, Ho Hyun;Ryoo, Kyu Yul
    • Textile Coloration and Finishing
    • /
    • v.25 no.4
    • /
    • pp.292-302
    • /
    • 2013
  • Cotton fabrics treated with hybrid materials were developed and prepared. A halogen-free flame retardant and an aromatic amide were blended and applied to cotton fabrics. Thermal and physical properties of the treated cotton fabrics were investigated. The surface of the pure and coated cotton fabrics was characterized by Fourier transform infrared spectroscopy. The elemental composition of the coated surface of the cotton fabric was measured using X-ray photoelectron spectroscopy and compared with that of pure cotton fabric. After being solved in N,N-dimethylacetamide, m-aramid and triphenylphosphine oxide (TPP) were applied to cotton fabrics through a dip-pad-coagulation process. The treated cotton fabrics with recycled m-aramid/TPP resulted in increased limited oxygen index values and thermal resistance.