Effects of Suspension Composition on Defects in Aqueous Tape Casting of Alumina Ceramics: A Rheological Study

  • Shin, Hyo-Soon
    • 한국세라믹학회지
    • /
    • 제42권1호
    • /
    • pp.1-6
    • /
    • 2005
  • In aqueous alumina tape casting, the effects of altering the composition of the suspensions, the binders and the casting thickness were studied. The rheological behavior of the suspensions and the defects of the dried tapes were examined and the relationships between them are discussed. The changes in the defect regions reported in the previous paper were related with the rheological properties with variations of the binder, the composition and the casting thickness. The shear thinning factor increased with the organic content and the solid content (the decrease of water content). The apparent viscosity increased with the shear thinning factor. The relation between the shear thinning factor and the log apparent viscosity was similar for all binder types. In the relation between the defect free region and the rheological properties, the defect free region became narrower with increasing casting thickness. The defect free region is independent of binder type. Therefore, the thicker tape is more difficult to produce in aqueous alumina tape casting. Knowledge of the rheological properties of the suspensions could help Predict the defect type and the possibility of defect free dried tapes.

수계 테이프 케스팅 법에 의한 봉상 γ-LiAlO2 입자 강화 MCFC 매트릭스 제조 공정의 최적화 (Optimization of Rod-shaped γ-LiAlO2 Particle Reinforced MCFC Matrices by Aqueous Tape Casting)

  • 최현종;신미영;현상훈;임희천
    • 한국세라믹학회지
    • /
    • 제46권3호
    • /
    • pp.282-287
    • /
    • 2009
  • Rod-shaped particle reinforced $LiAlO_2$ matrices for MCFC were fabricated by an aqueous tape-casting technique. The hydrolysis reaction and agglomeration of $\gamma-LiAlO_2$ particles in aqueous slurries were inhibited by additions of $LiOH{\cdot}H_2O$ and glycerin to the aqueous $\gamma-LiAlO_2$ slurry. The tape-casting, performed using the aqueous slurry containing protein albumin, was fast and led to an effective drying at casting temperature range of $60{\sim}65^{\circ}C$. The strength of the particle reinforced matrix was improved about 4 times compared to that of matrix without reinforcement. Pore size distribution ($0.1{\sim}0.4{\mu}m$) and porosity ($50{\sim}60%$) of the reinforced matrices were determined to be appropriate for the MCFC matrix. The aqueous tape casting process is not only environmental-friendly but also efficient for fabricating MCFC matrices compared to non-aqueous tape casting.

용매세척건조법에 의한 PZT 테입 제조 (Preparation of PZI Tapes by Solvent Washing Dry Method)

  • 신효순;윤석진;김현재
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1999년도 춘계학술대회 논문집
    • /
    • pp.300-303
    • /
    • 1999
  • For the fast dry of the aqueous tape, the process which water was replaced by organic solvent was proposed. So-called, it was the solvent washing dry, Three organic solvents (methanol, ethanol, and acetone) were selected for the washing solvent. The weight loss of the washed tapes was measured to evaluate the dry rate of the tapes and dried tapes were examined the generation of the cracks with the variations of the organic solvent and the washing time. Methanol, ethanol, and acetone were all available organic solvents for this method. The tapes washed in methanol, ethanol, and acetone were dried rapidly for twenty minutes. After thirty minutes, the weight losses were not any more. The solvent of the lower surface tension can decreases the crack of dried tape. If solvent substitutes water completely, though it was fast dried, crack can be eliminated. The tape casting system was designed for the solvent washing dry and prepared. An homogeneous tape was established by continuous tape casting process.

  • PDF

The Effects of Suspension Composition on Defects in Aqueous Tape Casting of Alumina Ceramics

  • Shin, Hyo-Soon
    • 한국세라믹학회지
    • /
    • 제41권9호
    • /
    • pp.647-652
    • /
    • 2004
  • In aqueous tape casting of alumina slurry systems, the relationships between the suspension compositions and the defects of the dried tapes were discussed. The suspensions compositions were controlled with the ratios of the solids, water and organics binder contents. The effects of the thickness of dried tape and kinds of binder system were also examined. In the defect free region, the apparent viscosity showed nearly same value due to the count balancing effect of solid and organic binder content on the apparent viscosity. When water content was constant, increasing solid led to decrease of organic binder content. The defect free region was narrowed with increasing of casting thickness. When linear type acrylic emulsion binders system (D1000 and D 1035) were used, defect free zone formed the belt type in the triangle of solid, water and organic binder content according to the line of constant water contents. However the defect free region was not found in the cross-link type emulsion binder system (D 1050).

수계공정에 의한 알루미나 테이프로 제조한 세라믹 인공치관용 알루미나 유리 복합체의 기계적 물성 (Mechanical Properties of Alumina-Glass Dental Composites Prepared from Aqueous-Based Tape Casting)

  • 이명현;김대준;이득용;이정훈;김창은
    • 한국세라믹학회지
    • /
    • 제36권10호
    • /
    • pp.1123-1131
    • /
    • 1999
  • Alumina-glass composites which are considered as the material of the choice for all dental crown was prepared by aqeous-based tape casting and sintering for 2h at 1120$^{\circ}C$ followed by glass infiltration for 2h at 1100$^{\circ}C$ Biaxial strength and fracture toughness of the composites were evaluated to determine the optimum composition of the tape as a function of the amount of constituent such as alumina binder and plasticizer. The strength and the fracture toughness of the alumina tape increased with increasing the contents of alumina and binder. These observations are consistent with in fluence of the constituents on mean alumuna particle distance in tapes suggesting that high strength of the glass infiltrated alumina composites is related to toughening by crack bowing. The biaxial strength and the fracture toughness of the composite containing the optimum constituent composition were 523 MPa and 3.3 MPa$.$1/2 respectively.

  • PDF

Rheology of Slurries and Effects of Polymer Volume Ratio in Aqueous PZT Tape Casting

  • Yoon, Seok-Jin;Shin, Hyo-Soon;Lee, Dong-Kyun;Kang, Chong-Yun;Park, Ji-Won;Kim, Hyun-Jai
    • The Korean Journal of Ceramics
    • /
    • 제7권1호
    • /
    • pp.16-19
    • /
    • 2001
  • For the fast dry of the aqueous tape, the process which water was reaplaced by organic solvent was proposed. Socalled, it was the solvent washing dry. Three organic solvents (methanol, ethanol and acetone) were selected for the washing solvent. The weight loss of the washed tapes was measured to evaluate the dry rate of the tapes and dried tapes were examined the generation of the cracks with the variations of the organic solvent and the washing time. Methanol, ethanol and acetone were available organic solvents for this method. The tapes washed in methanol, ethanol and acetone were dried rapidly for twenty minutes. After thirty minutes, the weight losses were not found any more, The solvent of the lower surface tension can decreases the crack of dried tape. If solvent substitutes water completely, though it was fast dried, crack can be eliminated.

  • PDF

Solvent Washing Dry Method for Aqueous Tape Casting

  • Yoon, Seok-Jin;Shin, Hyo-Soon;Park, Ji-Won;Kang, Chong-Yun;Kim, Tae-Song;Kim, Hyun-Jai
    • The Korean Journal of Ceramics
    • /
    • 제7권2호
    • /
    • pp.55-57
    • /
    • 2001
  • For the fast dry of the aqueous tape, the process which water was replaced by organic solvent was proposed. Socalled, it was the solvent washing dry. Three organic solvents (methanol, ethanol and acetone) were selected for the washing solvent. The weight loss of the washed tapes was measured to evaluate the dry rate of the tapes and dried tapes were examined the generation of the cracks with the variations of the organic solvent and the washing time. Methanol, ethanol and acetone were available organic solvents for this method. The tapes washed in methanol, ethanol and acetone were dried rapidly for twenty minutes. After thirty minutes, the weight losses were not found any more. The solvent of the lower surface tension can decreases the crack of dried tape. If solvent substitutes water completely, though it was fast dried, crack can be eliminated.

  • PDF

Acrylate를 결합제로 사용한 수계 테이프 캐스팅에서 알루미나 슬러리의 분산 및 점성 특성 (Dispersion and Rheological Characteristics of Alumina Slurries in Aqueous Tape-casting Using Acrylate Binder)

  • 조유정;박일석;문주호;김대준
    • 한국세라믹학회지
    • /
    • 제39권2호
    • /
    • pp.164-170
    • /
    • 2002
  • Acrylate 수계 결합제를 사용한 알루미나 테이프 캐스팅용 슬러리의 완전분산을 위한 최적의 분산제와 분산제량을 결정하기 위해 침강실험, 분말 함유량 실험, 점도 및 zeta 전위 측정을 행하였다. 알루미나 슬러리의 완전분산은 분산제를 polycarboxylic acid로 했을 때 얻어졌으며, 최적의 첨가량은 알루미나 100에 대하여 0.23∼0.24g 이었다. 분말에 대한 분산제량이 증가할수록 분산은 잘 이루어졌으나, 일정량 이상이 첨가되면 분산제가 용매 안에 과잉으로 존재하여 분산을 저해하는 요인으로 작용하였다. 테이프 캐스팅용 슬러리는 100g의 알루미나 분말에 0.2g의 polycarboxylic acid를 첨가하였을 때 분산 및 테이프 특성이 가장 우수하였고, 이 때 혼합한 결합제는 acrylate였고, 가소제는 Benzoflex를 사용하였다. 이 때 슬러리 최적 점도는 약 570 cps였고, 테이프 내 알루미나 량은 57 vol%이었다.

MARGINAL FIT RELATED TO MARGIN TYPES OF GLASS INFILTRATED ALUMINA CORE FABRICATED FROM AQUEOUS-BASED ALUMINA TAPE

  • Oh, Nam-Sik;Yu, Byeung-Su;Kim, Il-Kyu;Choi, Jin-Ho;Kim, Dae-Joon;Park, Il-Seok;Lee, Myung-Hyun;Lee, Keun-Woo
    • 대한치과보철학회지
    • /
    • 제40권3호
    • /
    • pp.262-268
    • /
    • 2002
  • Statement of problem. In-Ceram system is one of the all-ceramic crowns that can be used in anterior 3 unit fixed partial dentures and posterior single crowns. The alumina core used in In-Ceram system is manufactured using slip-casting technique. The slip-casting technique is difficult and technique sensitive. To improve this problem, tape-casting method was introduced into dentistry. There were no studies to examine the effect of margin design on the margin fitness of all-ceramic crowns fabricated from alumina tape. Purpose. The purpose of this study was to compare the marginal fitness of glass infiltrated alumina core fabricated from aqueous-based alumina tape according to different margin types ($90^{\circ},\;110^{\circ},\;135^{\circ}$ shoulder margin). Material and method. Three upper central resin incisors were prepared with $90^{\circ},\;110^{\circ}$, and $135^{\circ}$ shoulder margins for all-ceramic crowns, respectively. The resin teeth were duplicated and master die and special plaster die were made as usual. After alumina cores were fabricated from aqueous-based alumina tape, cores were cemented to each 15 epoxy dies replicated from three resin teeth with resin cement. These cemented cores were embedded in epoxy resin. Specimens were cut mesiodistally and buccolingually. Marginal gap and discrepancy were measured under microscope. Results. The marginal gap and discrepancy of $90^{\circ}$ marginal angle was $75.1{\mu}m,\;86.6{\mu}m,\;110^{\circ}$ marginal angle was $41.5{\mu}m,\;50.7{\mu}m$ and $135^{\circ}$ marginal angle was $51.7{\mu}m,\;54.2{\mu}m$, respectively. The smallest value was seen in 110 (angle, which was statistically significant compared to that of $90^{\circ}$ angle (p<0.05). Conclusion. Marginal fitness of alumina cores made of alumina tape with $110^{\circ}$ shoulder margin was best and others were clinically acceptable.