• Title/Summary/Keyword: aggregate exposure ratio

Search Result 18, Processing Time 0.027 seconds

Residual Mechanical Properties of Ultra High Strength Concrete with Aggregate Factor (골재요인에 따른 초고강도 콘크리트의 잔존역학적 특성)

  • Lee, Hee-Kwang;Kim, Gyu-Yong;Lee, Tae-Gyu;Nam, Jeong-Soo;Koo, Kyung-Mo;Youn, Yong-Sang
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2011.11a
    • /
    • pp.211-212
    • /
    • 2011
  • It was very important to evaluate concrete experimentally at elevated temperature because concrete was filled with aggregate of concrete volume about 70 percent. Concrete exposure to high temperatures produces changes in its internal structure, for instance loss of its strength and deformation capacity, in extreme cases risking the service life of the structure. The work of this paper is performed to evaluate the thermal behavior of ultra-high strength concrete having different water to cement ratio (strength), fine aggregate to aggregate ratio and maximum size of coarse aggregate. For exposure to 500℃ during 1 hour, residual mechanical properties of the ultra-high strength concrete decreased as the s/a ratio decreases and the maximum size of coarse aggregate increases.

  • PDF

Residual behavior of SRRAC beam and column after exposure to high temperatures

  • Zhou, Ji;Chen, Zongping;Zhou, Chunheng;Zheng, Wei;Ye, Peihuan
    • Steel and Composite Structures
    • /
    • v.45 no.3
    • /
    • pp.369-388
    • /
    • 2022
  • Composite effect between steel and recycled aggregate concrete (RAC) in steel reinforced-RAC (SRRAC) structures can effectively improve RAC's adverse mechanical properties due to the natural defects of recycled coarse aggregate (RCA). However, the performance of SRRAC after thermal exposure will have a great impact on the safety of the structure. In this paper, firstly, the mechanical properties of SRRAC structures after high temperatures exposure were tested, including 24 SRRAC columns and 32 SRRAC beams. Then, the change rules of beams and columns performance with the maximum temperature and replacement percentage were compared. Finally, the formulas to evaluate the residual bearing capacity of SRRAC beams and columns after exposure to high temperatures were established. The experimental results show that the maximum exposure temperature can be judged by the apparent phenomenon and mass loss ratio of RAC. After high temperatures exposure, the mechanical properties of SRRAC beams and columns change significantly, where the degradation of bearing capacity and stiffness is the most obvious. Moreover, it is found that the degradation degree of compression member is more serious than that of flexural member. The formulas of residual bearing capacity established by introducing influence coefficient of material strength agree well with the experimental results.

Effect of Aggregate on Mechanical Properties of Ultra-High Strength Concrete Exposed to High Temperature (고온을 받은 초고강도 콘크리트의 역학적 특성에 관한 골재의 영향)

  • Kim, Young-Sun;Choi, Hyoung-Gil;Ohmiya, Yoshifumi;Kim, Gyu-Yong
    • Journal of the Korea Concrete Institute
    • /
    • v.23 no.4
    • /
    • pp.431-440
    • /
    • 2011
  • Concrete structures exposed to fire produce changes in their internal structure, resulting in their service life reduction due to the deterioration of its strength and performance capacity. The deterioration level are dependent on the temperature, exposure time, concrete mix proportions, aggregate property, and material properties. This study was performed to evaluate the thermal behavior of ultra-high strength concrete for the parameters of water to cement ratio (compressive strength), fine to total aggregate ratio, and maximum coarse aggregate size. At room temperature and $500^{\circ}C$, tests of ultrasonic pulse velocity, resonance frequency, static modulus of elasticity, and compressive strength are performed using ${\varnothing}100{\times}200\;mm$ cylindrical concrete specimens. The results showed that the residual mechanical properties of ultra-high strength concrete heated to $500^{\circ}C$ is influenced by variation of a water to binder ratio, fine to total aggregate ratio, and maximum coarse aggregate size.

Residual behavior of recycled aggregate concrete beam and column after elevated temperatures

  • Chen, Zongping;Zhou, Ji;Liang, Ying;Ye, Peihuan
    • Structural Engineering and Mechanics
    • /
    • v.76 no.4
    • /
    • pp.513-528
    • /
    • 2020
  • This paper presents the results of an experimental study on the residual behavior of reinforced recycled aggregate concrete (RRAC) beam-columns after exposure to elevated temperatures. Two parameters were considered in this test: (a) recycled coarse aggregate (RCA) replacement percentages (i.e. 0, 30, 50, 70 and 100%); (b) high temperatures (i.e. 20, 200, 400, 600, and 800℃). A total of 25 RRAC short columns and 32 RRAC beams were conducted and subjected to different high temperatures for 1 h. After cooling down to ambient temperature, the following basic physical and mechanical properties were then tested and discussed: (a) surface change and mass loss ratio; (b) strength of recycled aggregate concrete (RAC) and steel subjected to elevated temperatures; (c) bearing capacity of beam-columns; (d) load-deformation curve. According to the test results, the law of performance degradation of RRAC beam-columns after exposure to high temperatures is analyzed. Finally, introducing the influence coefficient of RCA replacement percentage and high temperatures, respectively, to correct the calculation formulas of bearing capacity of beam-columns in Chinese Standard, and then the residual bearing capacity of RRAC beam-columns subjected elevated temperatures is calculated according to the modified formulas, the calculated results are in good agreement with the experimental results.

Surface Properties of Exposed-Aggregate Concrete Depending on Retarder and Water Jet Washing Timing (지연제 살포량과 물씻기 시간이 골재노출 콘크리트의 표면성상에 미치는 영향)

  • Park, Jun Hui;Han, Cheon-Goo
    • Journal of the Korea Institute of Building Construction
    • /
    • v.15 no.2
    • /
    • pp.169-175
    • /
    • 2015
  • Recently, a stone is preferred as a cladding materials because of its outstanding durability and luxurious character. However, because of running out of natural resources and restriction of production, it is expected that difficulty of stable supply, and thus alternative cladding materials for concrete wall is needed. Therefore, in this research, as an alternative cladding materials, exposed-aggregate concrete is studied using saccharin based retarder. For evaluating factors, changing water-to-cement ratio, dosages of saccharin-based retarder, and timing of water jet washing were tested on the surface properties of exposed-aggregate concrete. As a result, the most favorable surface performance was obtained at 0.75 day after the placing in 25% of water-to-cement ratio, and at one day after the placing in 35 and 55% of water-to-cement ratio, 1.5 day after the placing in 65% of water-to-cement ratio with $24m{\ell}/m^2$ of retarder application.

An Experimental Study on The Differential Dry Shrinkage of Concrete Using Artificial Lightweight Aggregate (인공 경량골재를 사용한 콘크리트의 부등 건조수축에 관한 실험적 연구)

  • Lee, Chang-soo;Kim, Young-ook;Lin, Yan
    • Journal of the Society of Disaster Information
    • /
    • v.6 no.1
    • /
    • pp.78-90
    • /
    • 2010
  • Exposure to the outside, the concrete is differential moisture distribution depending on the depth. Such a differential moisture distribution causes the differential drying shrinkage in concrete structures. This thesis is researched to compare the shrinkage of lightweight concrete depending on depth to normal concrete. It is used artificial lightweight aggregate which has 20% of pre-absorb value by lightweight concrete. When water-binder ratio is 30%, average shrinkage of lightweight concrete section decreased than normal concrete, but differential shrinkage of lightweight concrete section increased. However water-binder ratio is 40% and 50% average shrinkage and differential shrinkage of lightweight concrete section decreased than normal concrete.

A Study on the Evaluation of the Durability of Concrete Using Copper Slag Aggregates (동슬래그 골재를 함유한 콘크리트의 내구성 평가 연구)

  • Lee, Mun-Hwan
    • Journal of the Korea Concrete Institute
    • /
    • v.20 no.6
    • /
    • pp.773-784
    • /
    • 2008
  • Even if the exploitation of copper slag produced during the smelting process of copper as aggregate for construction purpose has been permitted since 2004 in Korea, the lack of sufficient data enabling to evaluate its long-term stability that is its durability has to date impeded its application. This study intends to investigate experimentally the durability characteristics of 18 and 27 MPa-class commercial concretes in which natural sand (fine aggregates) has been partially replaced by copper slag through accelerated and exposure tests so as to provide bases promoting the application of copper slag concrete. The experimental results revealed insignificant difference of the durability characteristics in most of the mix proportions in which 30% of natural sand was replaced by copper slag. In the case where crushed sand was adopted, tests verified similar characteristics for replacement ratio of 50%. Particularly, the results of the exposure test conducted during 8 years demonstrated that equivalent level of durability was secured compared to the case using natural sand. In the case of 18MPa-class lower grade concrete, exposure test verified also that the physical lifetime similar to 50 years could be secured until carbonation reaches cover depth of 20 mm.

A novel prediction model for post-fire elastic modulus of circular recycled aggregate concrete-filled steel tubular stub columns

  • Memarzadeh, Armin;Shahmansouri, Amir Ali;Poologanathan, Keerthan
    • Steel and Composite Structures
    • /
    • v.44 no.3
    • /
    • pp.309-324
    • /
    • 2022
  • The post-fire elastic stiffness and performance of concrete-filled steel tube (CFST) columns containing recycled aggregate concrete (RAC) has rarely been addressed, particularly in terms of material properties. This study was conducted with the aim of assessing the modulus of elasticity of recycled aggregate concrete-filled steel tube (RACFST) stub columns following thermal loading. The test data were employed to model and assess the elastic modulus of circular RACFST stub columns subjected to axial loading after exposure to elevated temperatures. The length/diameter ratio of the specimens was less than three to prevent the sensitivity of overall buckling for the stub columns. The gene expression programming (GEP) method was employed for the model development. The GEP model was derived based on a comprehensive experimental database of heated and non-heated RACFST stub columns that have been properly gathered from the open literature. In this study, by using specifications of 149 specimens, the variables were the steel section ratio, applied temperature, yielding strength of steel, compressive strength of plain concrete, and elastic modulus of steel tube and concrete core (RAC). Moreover, parametric and sensitivity analyses were also performed to determine the contribution of different effective parameters to the post-fire elastic modulus. Additionally, comparisons and verification of the effectiveness of the proposed model were made between the values obtained from the GEP model and the formulas proposed by different researchers. Through the analyses and comparisons of the developed model against formulas available in the literature, the acceptable accuracy of the model for predicting the post-fire modulus of elasticity of circular RACFST stub columns was seen.

Weathering Properties of Shale Aggregate in Daegu-Kyeongbuk region and Freezing-Thawing Characteristics of Concrete in response to Usage of Shale Aggregate (대경권 셰일 골재의 풍화특성 및 셰일 골재 사용량에 따른 콘크리트의 동결융해 특성)

  • Lee, Seung-Han;Jung, Yong-Wook;Yeo, In-Dong;Choi, Jong-Oh
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.14 no.8
    • /
    • pp.4033-4038
    • /
    • 2013
  • Sedimentary rocks from construction waste are discarded through open storage and landfilling, which causes an increase in construction cost and inefficient of execution of works. Some sandstone are selected and utilized as aggregates, but shale is buried as industrial waste. Therefore, in this research, we evaluated weathering properties of shale aggregate that is widely distributed throughout Daegu-Kyeongbuk region and freeze-thaw characteristics of concrete according to the replacement ratio of shale aggregate, in an effort to stabilize aggregate supply-demand in Daegu-Kyeongbuk region and develop alternative aggregates. We used red shale and black shale in the experiment, which were exported from a construction site in Deagu. We verified the usage of shale as a concrete aggregate by comparing andesite, which is broadly used as a thick aggregate for concrete, to hornfels, which is a metamorphic sedimentary rock. As a result of the experiment, we observed no degradation phenomenon for andesite and hornfels. However, a part of country rock containing black shale was found to be exfoliated. Red shale started having cracks in the direction of stratification after 1.5 months of direct exposure, and it broke into smaller pieces after approximately 4 months. After 300 cycles of freeze-thaw process on the concrete manufactured according to the replacement ratio of shale aggregate, the modulus of elasticity was 97% for plain and 95% for hornfels. In the case of RS_100, it was 57% after 210 cycles, and for BS_100, it was 54% after 240 cycles. Therefore, we established that, as the number of repetition increases, the freeze-thaw resistance decreases dramatically.

Axial compression mechanical properties of steel reinforced recycled concrete column exposure to temperatures up to 800℃

  • Chen, Zongping;Liang, Yuhan;Mo, Linlin;Ban, Maogen
    • Steel and Composite Structures
    • /
    • v.41 no.5
    • /
    • pp.731-746
    • /
    • 2021
  • The purpose of this paper is to investigate the axial bearing capacity and residual properties of steel reinforced recycled aggregate concrete (SRC) column after elevated temperature. A total of 48 SRC columns were designed for the static loading test after elevated temperature. The variables include replacement ratios, designed temperature, target duration, thicknesses of cover concrete, steel ratios and stirrup spacing. From this test, the mass loss ratio and stress load-deformation curve were obtained, and the influence of various parameters on residual bearing capacity were analyzed. ABAQUS was used to calculate the temperature field of specimens, and then got temperature damage distribution on the cross-section concrete. It was shown that increasing of the elevated temperatures leaded to the change of concrete color from smoky-gray to grayish brown and results in reducing the bearing capacity of SRC columns. The axial damage and mechanism of SRC columns were similar to those of reinforced natural aggregate concrete columns at the same temperatures. Finally, the calculation method of axial compressive residual bearing capacity of SRC columns recycled concrete columns after high temperature was reported based on the test results and finite element analysis.