Sung, Hyo Kyung;Shin, Sang Yong;Cha, Wooyeol;Oh, Kyungshik;Lee, Sunghak;Kim, Nack J.
Korean Journal of Metals and Materials
/
v.48
no.10
/
pp.875-883
/
2010
This study assessed the Charpy impact properties of the heat-affected zones (HAZs) of API X80 linepipe steels containing complex oxides. Three types of steel were fabricated by adding Mg and $O_2$ to form complex oxides and their microstructures and Charpy impact properties were investigated. The number of complex oxides increased with the amount of excess Mg and $O_2$ that was included in the steels. Simulated HAZs containing a number of oxides showed a high volume fraction of acicular ferrite (AF) because the oxides acted as nucleation sites for AF, thereby leading to an improvement in the Charpy impact properties. According to a correlation study between the heat input, the volume fraction of the AF, and the Charpy impact properties, ductile fractures occurred predominantly when the fraction of the AF was 20% or higher; moreover, the Charpy absorbed energy was excellent at more than 100 J. These findings suggest that the improvement of the Charpy impact properties of the HAZs was associated with the active nucleation of AF in the oxide-containing steel HAZs.
Hong, Seokmin;Shin, Sang Yong;Lee, Sunghak;Kim, Nack J.
Korean Journal of Metals and Materials
/
v.48
no.8
/
pp.705-716
/
2010
Effects of specimen thickness and notch shape on fracture mode appearing in drop weight tear test (DWTT) specimens of API X70 and X80 linepipe steels were investigated. Detailed microstructural analysis of fractured DWTT specimens showed that the fractures were initiated in normal cleavage mode near the specimen notch, and that some separations were observed at the center of the fracture surfaces. The Chevron-notch (CN) DWTT specimens had broader normal cleavage surfaces than the pressed-notch (PN) DWTT specimens. Larger inverse fracture surfaces appeared in the PN DWTT specimens because of the higher fracture initiation energy at the notch and the higher strain hardening in the hammer-impacted region. The number and length of separations were larger in the CN DWTT specimens than in the PN DWTT specimens, and increased with increasing specimen thickness due to the plane strain condition effect. As the test temperature decreased, the tendency to separations increased, but separations were not found when the cleavage fracture prevailed at very low temperatures. The DWTT test results, such as upper shelf energy and energy transition temperature, were discussed in relation with microstructures and fracture modes including cleavage fracture, shear fracture, inverse fracture, and separations.
Shin, Sang Yeol;Lee, Ji In;Chung, Woon Jin;Cho, Sung-Hoon;Choi, Yong Gyu
Current Optics and Photonics
/
v.3
no.5
/
pp.415-422
/
2019
Retroreflection of vehicle headlights, as induced by spherical glass beads, is a key optical phenomenon that provides road-surface markings with greatly enhanced visibility, thus better securing a driver's safety in the nighttime as well as in unclear daytime. Retroreflectance of glass beads is a quite sensitive function of their refractive index, so that measurement of the refractive index of glass specifically in the shape of spherical beads needs to be performed within a reasonable uncertainty that is tolerable for road-marking applications. The Becke line method has been applied in assessing refractive index of such glass beads as e.g. an industrial standard in the Republic of Korea; however, the reference refractive-index liquids are not commercially available these days for refractive index greater than 1.80 due to the toxicity of the constituent materials. As such, high-refractive-index glass beads require an alternate method, and in this regard we propose a practically serviceable technique with uncertainty tantamount to that of the Becke line method: Based on comparison of calculated and measured retroreflectance values of commercial glass beads, we discover that their refractive index can be determined with reasonable precision via the retroreflectance measurement. Specifically, in this study the normalized retroreflectance originating from a single glass sphere is computed as a function of refractive index using the Fresnel equations, which is then validated as coinciding well with retroreflectance values measured from actual specimens, i.e. glass-bead aggregates. The uncertainties involved are delineated in connection with radius and imperfections of the glass beads.
In this study, surface composites were fabricated with Fe-based amorphous alloy powders and VC powders by high-energy electron beam irradiation, and the correlation of their microstructure with hardness and fracture toughness was investigated. Mixture of Fe-based metamorphic powders and VC powders were deposited on a plain carbon steel substrate, and then electron beam was irradiated on these powders without flux to fabricate surface composites. The composite layers of 1.3~1.8 mm in thickness were homogeneously formed without defects and contained a large amount (up to 47 vol.%) of hard $Cr_2B$ and $V_8C_7$ crystalline particles precipitated in the solidification cell region and austenite matrix, respectively. The hardness of the surface composites was directly influenced by hard $Cr_2B$ and $V_8C_7$ particles, and thus was about 2 to 4 times greater than that of the steel substrate. Observation of the microfracture process and measurement of fracture toughness of the surface composites indicated that the fracture toughness increased with increasing additional volume fraction of $V_8C_7$ particles because $V_8C_7$ particles effectively played a role in blocking the crack propagation along the solidification cell region heavily populated with $Cr_2B$ particles. Particularly in the surface composite fabricated with Fe-based metamorphic powders and 30 % of VC powders, the hardness and fracture toughness were twice higher than those of the surface composite fabricated without mixing of VC powders.
Shin, Sang Yong;Hong, Suckmin;Bae, Jin-ho;Kim, Kisoo;Lee, Sunghak
Korean Journal of Metals and Materials
/
v.47
no.3
/
pp.155-168
/
2009
In this study, microstructural investigation was conducted on the separation phenomenon occurring during Charpy impact tests of API X80 linepipe steels. Particular emphasis was placed on the role of microstructural phases present in the API X80 steels such as acicular ferrite, bainite, and hard secondary phases. Detailed microstructural analysis of fractured impact specimens showed that highly elongated bainite worked as prior initiation sites for separations, and that the number and length of separations increased with increasing volume fraction of bainite. In the steels having high work hardenability, tearing-shaped separations were found because the hammer-impacted region was seriously hardened during the impact test, which led to the reduction in the impact toughness. As the test temperature decreased, the tendency of separations increased, but separations were not observed when the cleavage fracture prevailed at very low temperatures. Thus, the minimization of the formation of bainite and secondary phases in the steels would be beneficial for preventing or minimizing separations because separations deteriorated low-temperature impact toughness.
Han, Seung Youb;Shin, Sang Yong;Lee, Sunghak;Kim, Nack J.;Kwak, Jai-Hyun;Chin, Kwang-Geun
Korean Journal of Metals and Materials
/
v.48
no.5
/
pp.377-386
/
2010
An investigation was conducted into the effects of $\kappa$-carbides on the cracking phenomenon, which often occurred in cold-rolled light-weight steel plates. Three kinds of steels were fabricated by varying the C content, and their microstructures and tensile properties were investigated. In the two steels that contained a high carbon content, the band structures of ferrites and $\kappa$-carbides that were severely elongated along the rolling direction were well developed, whereas continuous arrays of $\kappa$-carbides were formed in the steel that contained a low carbon content. Detailed microstructural analyses of the deformed region beneath the tensile fracture surface showed that the cracks initiated at arrays of $\kappa$-carbides or $\kappa$-carbides formed interfaces between the band structures, which initiated cleavage fractures in the ferrite bands, while the bands populated with a number of $\kappa$-carbides did not play an important role in propagating the cracks. Thus, the minimization of interfacial $\kappa$-carbides or $\kappa$-carbide arrays by increasing the carbon content was essential for preventing cracking from occurring during cold rolling.
Ha, Dae Jin;Sung, Hyo Kyung;Lee, Sunghak;Lee, Jong Seog;Lee, Yong Deuk
Korean Journal of Metals and Materials
/
v.46
no.11
/
pp.737-746
/
2008
Mechanisms of sticking phenomena occurring during hot rolling of a modified STS 430J1L ferritic stainless steel have been investigated in this study by using a pilot-plant-scale rolling machine. As the rolling pass proceeds, the Fe-Cr oxide layer formed in a reheating furnace is destroyed, and the destroyed oxides penetrate into the rolled steel to form a thin oxide layer on the surface region. The sticking does not occur on the surface region containing oxides, whereas it occurs on the surface region without oxides by the separation of the rolled steel at high temperatures. This indicates that the resistance to sticking increases by the increase in the surface hardness when a considerable amount of oxides are formed on the surface region, and that the sticking can be evaluated by the volume fraction and distribution of oxides formed on the surface region. The lubrication and the increase of the rolling speed and rolling temperature beneficially affect to the resistance to sticking because they accelerate the formation of oxides on the steel surface region. In order to prevent or minimize the sticking, thus, it is suggested to increase the thickness of the oxide layer formed in the reheating furnace and to homogeneously distribute oxides along the surface region by controlling the hot-rolling process.
Han, Seung Youb;Shin, Sang Yong;Lee, Sunghak;Bae, Jin-ho;Kim, Kisoo
Korean Journal of Metals and Materials
/
v.47
no.9
/
pp.523-532
/
2009
In this study, four API X80 linepipe steel specimens were fabricated with varying cooling rates and finish cooling temperatures, and their microstructures and crystallographic orientations were analyzed to investigate the effects of cooling conditions on their tensile and Charpy impact properties. All the specimens consisted of acicular ferrite, granular bainite, and secondary phases such as martensite and martensiteaustenite constituent. The volume fraction of secondary phases increased with increasing cooling rate, and the higher finish cooling temperature resulted in the reduction in volume fraction and grain size of secondary phases. According to the crystallographic orientation analysis data, the effective grain size and unit crack path decreased as fine acicular ferrites having a large amount of high-angle grain boundaries were homogeneously formed, thereby leading to the improvement of Charpy impact properties. The specimen fabricated with the higher cooling rate and lower finish cooling temperature had the highest upper shelf energy and the lowest energy transition temperature because it contained a large amount of fine secondary phases homogeneously distributed inside fine acicular ferrites, while its tensile properties well maintained.
Ha, Dae Jin;Sung, Hyo Kyung;Park, Joon Wook;Lee, Sunghak
Korean Journal of Metals and Materials
/
v.47
no.7
/
pp.406-415
/
2009
A study was conducted on the effects of carbon, tungsten, and vanadium on the wear properties and surface roughness of four High Speed Steel (HSS) rolls manufactured by the centrifugal casting method. Hot-rolling simulation tests were carried out using a high-temperature wear tester capable of controlling speed, load, and temperature. HSS rolls contained a large amount (up to 25 vol.%) of carbides such as MC, $M_{2}C$, $M_{7}C_{3}$, and $M_{6}C$ carbides formed in the tempered martensite matrix. The matrix consisted mainly of lath tempered martensite when the carbon content in the matrix was small, and contained a considerable amount of plate tempered martensite when the carbon content increased. The high-temperature wear test results indicated that the wear properties and surface roughness of the rolls improved when the amount of hard MC carbides formed inside solidification cells increased. The rolls distribution was also homogeneous. The best wear properties and surface roughness were obtained from a roll where a large amount of MC carbides was homogeneously distributed in the lath tempered martensite matrix. The proper contents of carbon equivalent, tungsten equivalent, and vanadium were 2.0~2.3%, 9~10%, and 5~6%, respectively.
Allison, Darcy L.;Morris, Craig C.;Schetz, Joseph A.;Kapania, Rakesh K.;Watson, Layne T.;Deaton, Joshua D.
Advances in aircraft and spacecraft science
/
v.2
no.1
/
pp.17-44
/
2015
A modular multidisciplinary analysis and optimization framework has been built with the goal of performing conceptual design of an advanced efficient supersonic air vehicle. This paper addresses the specific challenge of designing this type of aircraft for a long range, supersonic cruise mission with a payload release. The framework includes all the disciplines expected for multidisciplinary supersonic aircraft design, although it also includes disciplines specifically required by an advanced aircraft that is tailless and has embedded engines. Several disciplines have been developed at multifidelity levels. The framework can be readily adapted to the conceptual design of other supersonic aircraft. Favorable results obtained from running the analysis framework for a B-58 supersonic bomber test case are presented as a validation of the methods employed.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.