• 제목/요약/키워드: a-C:Ti

검색결과 3,740건 처리시간 0.032초

고내압용 Au/Ni/Ti/3C-SiC 쇼트키 다이오드의 제작과 그 특성 (Fabrication of a Au/Ni/Ti/3C-SiC Schottky Diode and its Characteristics for High-voltages)

  • 심재철;정귀상
    • 한국전기전자재료학회논문지
    • /
    • 제24권4호
    • /
    • pp.261-265
    • /
    • 2011
  • This paper describes the fabrication and characteristics of a Au/Ni/Ti/3C-SiC Schottky diode with field plate (FP) edge termination. The Schottky contacts were annealed for 30 min at temperatures ranging from 0 to $800^{\circ}C$. At annealing temperature of $600^{\circ}C$, it showed an inhomogeneous Schottky barrier and had the best electrical characteristics. However, the annealing of $800^{\circ}C$ replaced it with ohmic behaviors because of the formation of many different types of nickel silicides. The fabricated Schottky diode had a breakdown voltage of 200 V, Schottky barrier height of 1.19 eV and worked normally even at $200^{\circ}C$.

CO Oxidation Activities of Ni and Pd-TiO2@SiO2 Core-Shell Nanostructures

  • Do, Yeji;Cho, Insu;Park, Yohan;Pradhan, Debabrata;Sohn, Youngku
    • Bulletin of the Korean Chemical Society
    • /
    • 제34권12호
    • /
    • pp.3635-3640
    • /
    • 2013
  • We prepared Ni and Pd-modified $TiO_2@SiO_2$ core-shell nanostructures and then analyzed them by scanning electron microscopy, optical microscopy, X-ray diffraction crystallography, FT-IR and UV-Visible absorption spectroscopy. In addition, their CO oxidation performance was tested by temperature-programmed mass spectrometry. The CO oxidation activity showed an order of Ni-$TiO_2@SiO_2$ ($900^{\circ}C$) < Ni-$TiO_2@SiO_2$ ($90^{\circ}C$) < Ni-$TiO_2@SiO_2$ ($450^{\circ}C$) in the first CO oxidation run, and greatly improved activity in the same order in the second run. The $T_{10%}$ (the temperature at 10% CO conversion) corresponds to the CO oxidation rate of $2.8{\times}10^{-5}$ molCO $g{_{cat}}^{-1}s^{-1}$. For Ni-$TiO_2@SiO_2$ ($450^{\circ}C$), the $T_{10%}$ was observed at $365^{\circ}C$ in the first run and at $335^{\circ}C$ in the second run. For the Pd-$TiO_2@SiO_2$ ($450^{\circ}C$), the $T_{10%}$ was observed at a much lower temperature of $263^{\circ}C$ in the first CO oxidation run, and at $247^{\circ}C$ in the second run. The CO oxidation activities of transition metal modified $TiO_2@SiO_2$ core-shell nanostructures presented herein provide new insights that will be useful in developing catalysts for various environments.

화학증착법에 의한 여러 가지 강들위에 증착된 TiC의 결정학적 특성 (The Crystallographic Properties of TiC Deposited on Different Substrate Steel by Chemical VaporDeposition)

  • 윤순길;김호기
    • 한국세라믹학회지
    • /
    • 제24권6호
    • /
    • pp.519-526
    • /
    • 1987
  • TiC was deposited onto several substrate steels by the Chemical Vapor Deposition technique from TiCl4-CH4-H2 gas mixtures in the horizontal resistance furnace. Deposition rates and morphologies of the coatings were investigated with the carbon contents. Deposition thickness increased linearly with the deposition time in the Presence of CH4 gas. The various interlayers of coating by EDS and X-ray Diffraction were proved as Cr7C3 and Fe3C. Chromium contents did not affect the preferred orientation of TiC deposit. The deposition was controlled by a mass transport and a surface reaction in case of 1 wt% C-5.25 wt% Cr steel irrespective of deposition temperature.

  • PDF

Highly Luminescent Aniline and TiO2 Composite: The Effect of Weight Ratio of Aniline and TiO2

  • Kim, Byoung-Ju;Park, Eun-Hye;Kang, Kwang-Sun
    • Current Photovoltaic Research
    • /
    • 제4권1호
    • /
    • pp.8-11
    • /
    • 2016
  • Strong deep ultraviolet emitting aniline and $TiO_2$ composite has been synthesized via hydrolysis and condensation reactions of titaniumisopropoxide ($Ti(OPr)_4$), aniline, and acetic anhydride. Three different weight ratios of aniline and $Ti(OPr)_4$ including 3:1 ($TiO_2An-A$), 2:1 ($TiO_2An-B$), and 1:1 ($TiO_2An-C$) were synthesized and characterized their optical properties. The FTIR spectra of the $TiO_2An-A$, -B, and -C showed the absorption intensities of the benzene ring stretching and bending vibrations, and benzene ring -CH stretching, bending, and deformation vibrations increased with the increase of the amount of aniline. The UV-visible absorption spectra showed that the UV region absorption was slightly increased with the increase of the amount of aniline. The photoluminescence (PL) intensities were exponentially increased with the increase the excitation wavelength from 307 to 317 nm, steadily increased from 300 to 313 nm and slowly increased from 302 to 308 nm for $TiO_2An-A$, -B, and -C, respectively and decreased thereafter. Therefore, the PL intensity is strongly dependent on the weight ratio of $Ti(OPr)_4$ and aniline.

초청정한 Si 기판 위에서 Ti의 초기 반응 (Initial Reactions of Ti on the Atomically Clean Si Substrates)

  • 전형탁
    • 분석과학
    • /
    • 제5권3호
    • /
    • pp.303-308
    • /
    • 1992
  • Ti과 Si의 초기 반응이 Titanium Silicide의 표면 거칠기 (Surface roughness)를 고찰하기 위해 연구하였다. 형성기구는 In-situ AES와 LEED의 측정장비로 연구하였다. Ti의 하나나 두 원자층이 초고진공에서 원자적으로 깨끗한 Si 기판 위에 증착되었다. Reconstruction이 된 $7{\times}7$ Si(111) 표면이 초 고진공하에서 얻어졌으며 박막의 증착은 Quartz Crystal Oscillator로 측정되었다. In-situ 측정 결과 Ti과 Si의 초기 반응이 실온에서 일어났으며 Disorder막을 형성하였다. 낮은 온도($200^{\circ}C{\sim}300^{\circ}C$)에서 Ti과 Si의 Intermixing이 고찰되었고 $400^{\circ}C$ 근처에서 $1{\times}1$ Si(111) LEED 패턴이 관찰되었다. 이것은 Disorder막이 Order막으로 변화가 생긴 것을 나타낸다. 더 높은 온도에서 $7{\times}7$ Si(111) LEED 패턴이 재관찰되었는데 이것은 3차원적인 $TiSi_2$의 형성을 증명하는 것이다.

  • PDF

고에너지 볼밀링된 BaCO3와 TiO2 혼합분말의 고상반응에 의한 나노결정 BaTiO3 분말 합성 (Synthesis of Nanocrystalline BaTiO3 Powder by the Combination of High Energy Ball Milling of BaCO3-TiO2 Mixture and Solid-State Reaction)

  • 류성수
    • 한국분말재료학회지
    • /
    • 제19권4호
    • /
    • pp.310-316
    • /
    • 2012
  • Nanocrystalline $BaTiO_3$ powder could be synthesized by solid-state reaction using the mixture which was prepared by a high energy milling process in a bead mill for $BaCO_3$ and nanocrystalline $TiO_2$ powders mixture. Effect of the milling time on the powder characteristic of the synthesized $BaTiO_3$ powder was investigated. Nanocrystalline $BaTiO_3$ with a particle size of 50 nm was obtained at $800^{\circ}C$. High tetragonal $BaTiO_3$ powder with a tetragonality(=c/a) of 1.009 and a specific surface area of $7.6m^2/g$ was acquired after heat-treatment at $950^{\circ}C$ for 2 h. High energy ball milling was effective in decreasing the reaction temperature and increasing the tetragonality.

Fabrication of Sintered Compact of Fe-TiB2 Composites by Pressureless Sintering of (FeB+TiH2) Powder Mixture

  • Huynh, Xuan-Khoa;Kim, Ji Soon
    • 한국분말재료학회지
    • /
    • 제23권4호
    • /
    • pp.282-286
    • /
    • 2016
  • A sintered body of $TiB_2$-reinforced iron matrix composite ($Fe-TiB_2$) is fabricated by pressureless-sintering of a mixture of titanium hydride ($TiH_2$) and iron boride (FeB) powders. The powder mixture is prepared in a planetary ball-mill at 700 rpm for 3 h and then pressurelessly sintered at 1300, 1350 and $1400^{\circ}C$ for 0-2 h. The optimal sintering temperature for high densities (above 95% relative density) is between 1350 and $1400^{\circ}C$, where the holding time can be varied from 0.25 to 2 h. A maximum relative density of 96.0% is obtained from the ($FeB+TiH_2$) powder compacts sintered at $1400^{\circ}C$ for 2 h. Sintered compacts have two main phases of Fe and $TiB_2$ along with traces of TiB, which seems to be formed through the reaction of TiB2 formed at lower temperatures during the heating stage with the excess Ti that is intentionally added to complete the reaction for $TiB_2$ formation. Nearly fully densified sintered compacts show a homogeneous microstructure composed of fine $TiB_2$ particulates with submicron sizes and an Fe-matrix. A maximum hardness of 71.2 HRC is obtained from the specimen sintered at $1400^{\circ}C$ for 0.5 h, which is nearly equivalent to the HRC of conventional WC-Co hardmetals containing 20 wt% Co.

TiC-Mo 공정복합재료의 고온 변형특성 (Deformation Properties of TiC-Mo Eutectic Composite at High Temperature)

  • 신순기
    • 한국재료학회지
    • /
    • 제23권10호
    • /
    • pp.568-573
    • /
    • 2013
  • The deformation properties of a TiC-Mo eutectic composite were investigated in a compression test at temperatures ranging from room temperature to 2053 K and at strain rates ranging from $3.9{\times}10^{-5}s^{-1}$ to $4.9{\times}10^{-3}s^{-1}$. It was found that this material shows excellent high-temperature strength as well as appreciable room-temperature toughness, suggesting that the material is a good candidate for high-temperature application as a structure material. At a low-temperature, high strength is observed. The deformation behavior is different among the three temperature ranges tested here, i.e., low, intermediate and high. At an intermediate temperature, no yield drop occurs, and from the beginning the work hardening level is high. At a high temperature, a yield drop occurs again, after which deformation proceeds with nearly constant stress. The temperature- and yield-stress-dependence of the strain is the strongest in this case among the three temperature ranges. The observed high-temperature deformation behavior suggests that the excellent high-temperature strength is due to the constraining of the deformation in the Mo phase by the thin TiC components, which is considerably stronger than bulk TiC. It is also concluded that the appreciable room-temperature toughness is ascribed to the frequent branching of crack paths as well as to the plastic deformation of the Mo phase.

Ti-33.8wt% Al 금속간 화합물의 고온 산화거동 (High temperature oxidation behavior of Ti-33.8wt% Al intermetallic compounds)

  • 최송천;조현준;이동복
    • 한국표면공학회지
    • /
    • 제26권5호
    • /
    • pp.235-244
    • /
    • 1993
  • The oxidation behavior of a two-phase(Ti3Al+TiAl) intermetallic compound, Ti-33.8wt%Al, has been in-vestigated in air at 800, 900 and $^1000{\circ}C$. Though the isothermal oxidation behavior followed a parabolic law up to 100$0^{\circ}C$ indicating that protective oxide scales were formed, the cyclic oxidation behavior followed a lin-ear law in the entire temperature range tested because flaky or stratified scales were usually spalled from the surface during cooling. During oxidation at 80$0^{\circ}C$, the alloy showed excellent oxidation resistance because continuous protective Al2O3 films were formed on the outermost surface of the alloy. However, above $900^{\circ}C$, the oxidation resistance of the alloy was decreased gradually because relatively non-protective TiO2 scales as well as some of Al2O3 scales were formed on the outer oxide scale. The oxidation mechanism of the alloy at different temperature was proposed.

  • PDF

Al2TiO5-점토 복합체를 이용한 원적외선방사재질의 개발 (Development of Al2TiO5-Clay Composites for Far Infrared Radiator)

  • 한상목;신대용
    • 산업기술연구
    • /
    • 제20권A호
    • /
    • pp.239-245
    • /
    • 2000
  • Sintered $Al_2TiO_5$ has a very low thermal expansion and an infrared radiative selectively emitting large amounts of far infrared rays. However, it is week in mechanical strength. Spectral infrared emittance, thermal expansion coefficient, and mechanical strength of $Al_2TiO_5$-clay composites were studied to develop a material for far infrared radiators. The composites containing 10~50 mass% Jungsan clay had high emittance in the range of 2,000~500cm-1. The bending strength of the $Al_2TiO_5$-clay composites increased with increasing clay content. The $Al_2TiO_5$-clay composites with a clay content of 50mass% and heat-treated at $1,200^{\circ}C$ had a large strength for infrared radiators ; 86MPa. The average linear thermal expansion coefficient from $200{\sim}1,000^{\circ}C$ of the 50mass% jungsan clay containing compo sited heat-treated at $1,200^{\circ}C$ was lower than $3.87{\times}10-6/^{\circ}C$.

  • PDF