핵 연료 피복관 재료로 샤용되고 었는 Zr 합금의 부식특성을 개선하기 위하여 Zn-xSn 2원계 합금과 Zr-0.4Nb-xSn 3원계 합금을 제조하여 부식특성을 평가하였다. 부식 실험은 $360^{\circ}C$ 물 분위기의 mini-autoclave에서 수행하였다. 2원계 합금의 경우 Sn이 0.5, 0.8, 1.5wt.% 첨가된 합금에서는 15일에서 속도천이가 발생한 후 급격한 부식 가속 현상이 나타녔으나, 2.0wt.% 가 첨가된 합금의 경우 80일까지의 부식 실험에서도 천이 현상을 보이지 않는 매우 높은 부식 저항성을 보였다. 3원계 합금에서는 Sn 함량이 증가할수록 부식이 증가하는 경향을 보였다. 이러한 경향은 2원계 합금과 3원계 합금에서 Sn의 고용도 차, 미량 첨가된 Nb의 영향 및 석출물의 특성과 관련이 잇는 것으로 생각된다. 또한 Zr-xSn, Zr-O.4Nb-xSn 합금의 부식은 tetragonal-$ZrO_2$의 분율과 수소 흡수율에 의해서 제어될 수도 있다.
Commercially pure titanium(cp-Ti) and Ti-15wt%Zr-4wt%Nb-4wt%Ta alloy were melted in vacuum induction furnace. According to the chemical analysis, the content of carbon was above ASTM standard in the cast ingots because of using graphite crucible. The TEM micostructures of cp-Ti and Ti alloy shows that chemically stable TiC precipitates distribute in ${\alpha}-Ti$ matrix. In order to examine the properties of cp-Ti and Ti-Zr-Nb-Ta alloy for dental applications, mechanical properties and corrosion resistance were investigated. The anodic polarization properties of Ti-Zr-Nb-Zr alloy were almost same as that of cp-Ti in 1% lactic acid. However, as the results of the anodic polarization test in 5% HCl, it was known that Ti-Zr-Nb-Zr alloy showed a rapid decrease in current density at higher potential in comparison with cp-Ti. The yield stress and tensile strengh in Ti-Zr-Nb-Ta were ${\sigma}_{0.2}=623\;MPa$, ${\sigma}_{T.S.}=708\;MPa$ and these results showed 30% increase in yield stress in comparison with cp-Ti.
To investigate the corrosion behavior of Zr-1.0Nb-xSn (x=1.0, 1.5, 2.0 and 2.5wt. %)alloy system, the corrosion tests of Zr-1.0Nb-xSn alloys were carried out in steam at $400^{\circ}C$ for 125 days and in 70ppm LiOH solution at $360^{\circ}C$ for 180 days. The matrix microstructures of the test specimens were analyzed using TEM and the oxide structures on the test specimens were analyzed using XRD. It was found from the analyses that the more Sn content the alloy had, the faster it was corroded and with the increase of Sn content in the alloy the fraction of $t-ZrO_2$ to $m-ZrO_2$ was decreased. It was also found that the alloys having more Sn showed more dislocation density than those having less.
The Zr-0.2Sn-0.8Nb-X(X = 0~200ppm Si, 0~0.4wt.% Mo and Mn respectively) ingots for test specimens were manufactured by a vacuum arc re-melting method to find out the effect of Si, Mo, and Mn on the corrosion characteristics of the Zr-0.2Sn-0.8Nb alloy. After being heat-treated and rolled repeatedly out to be flat materials, they were finally heat-treated at 51$0^{\circ}C$ for three hours and used as the specimens for corrosion tests. The corrosion behavior of the specimens was studied in both 40$0^{\circ}C$ steam for 200 days and in aqueous 70 ppm LiOH solution at 36$0^{\circ}C$ for 90 days. From the study it was found that Si from 80 to 200 ppm contributed to increasing the corrosion resistance of Zr-0.2Sn-0.8Nb alloy in both steam and LiOH solution. This study also showed that Mn from 0.1 to 0.4% caused to go up the corrosion resistance, whereas Mo played a apart in improving the corrosion resistance only between 0.05 and 0.2 wt.%.
Kim, Tae-Kyu;Choi, Pyung-Sik;Yang, Sung-Ki;Lee, Chong-Tak;Sohn, Dong-Seong
Nuclear Engineering and Technology
/
제40권6호
/
pp.505-510
/
2008
The correlation between the tensile strength and corrosion behavior of Zr-1.0wt%Nb alloy heat treated at $480^{\circ}C$ for up to 32 hours was evaluated. The tensile strength at $400^{\circ}C$ was continuously reduced with an increasing heat treatment time, mainly due to a grain growth and a decreased area fraction of the precipitates. However, the corrosion resistance in an aqueous ammonia solution at $360^{\circ}C$ was enhanced, mainly due to the formation of $\beta$-Nb precipitates. It is thus concluded that a longer heat treatment time provides a better corrosion resistance while degrading the tensile strength.
Saji, Viswanathan S.;Jeong, Yong Hoon;Choe, Han Cheol
Corrosion Science and Technology
/
제8권4호
/
pp.139-142
/
2009
Recently, quaternary titanium alloys of the system Ti-Nb-Ta-Zr received considerable research interest as potential implant materials because of their excellent mechanical properties and biocompatibility. However, only few reported works were available on the corrosion behavior of such alloys. Hence, in the present work, electrochemical corrosion of Ti-35Nb-5Ta-7Zr alloy, which has been fabricated by arc melting and heat treatment, was studied in 0.9 wt% NaCl at $37\pm1^{\circ}C$, along with biomedical grade Ti-6Al-4V and CP-Ti. The phase and microstructure of the alloys were investigated employing XRD and SEM. The results of electrochemical studies indicated that the corrosion resistance of the quaternary alloy was inferior to that of Ti-6Al-4V and CP Ti.
Purpose: The purpose of this study was to investigate the electrochemical characteristics of nanotubular Ti-25Nb-xZr ternary alloys for dental implant materials. Materials and Methods: Ti-25Nb-xZr alloys with different Zr contents (0, 3, 7, and 15 wt.%) were manufactured using commercially pure titanium (CP-Ti), niobium (Nb), and zirconium (Zr) (99.95 wt.% purity). The alloys were prepared by arc melting in argon (Ar) atmosphere. The Ti-25Nb-xZr alloys were homogenized in Ar atmosphere at $1,000^{\circ}C$ for 12 hours followed by quenching into ice water. The microstructure of the Ti-25Nb-xZr alloys was examined by a field emission scanning electron microscope. The phases in the alloys were identified by an X-ray diffractometer. The chemical composition of the nanotube-formed surfaces was determined by energy-dispersive X-ray spectroscopy. Self-organized $TiO_2$ was prepared by electrochemical oxidation of the samples in a $1.0M\;H_3PO_4+0.8wt.%$ NaF electrolyte. The anodization potential was 30 V and time was 1 hour by DC supplier. Surface wettability was evaluated for both the metallographically polished and nanotube-formed surfaces using a contact-angle goniometer. The corrosion properties of the specimens were investigated using a 0.9 wt.% aqueous solution of NaCl at $36^{\circ}C{\pm}5^{\circ}C$ using a potentiodynamic polarization test. Result: Needle-like structure of Ti-25Nb-xZr alloys was transform to equiaxed structure as Zr content increased. Nanotube formed on Ti-25Nb-xZr alloys show two sizes of nanotube structure. The diameters of the large tubes decreased and small tubes increased as Zr content increased. The lower contact angles for nanotube formed Ti-25NbxZr alloys surfaces showed compare to non-nanotube formed surface. The corrosion resistance of alloy increased as Zr content increased, and nanotube formed surface showed longer the passive regions compared to non-treatment surface. Conclusion: It is confirmed that corrosion resistance of alloy increased as Zr content increased, and nanotube formed surface has longer passive region compared to without treatment surface.
Zr-xNb alloys (x = 0.2, 0.8, 1.5 wt.%) were prepared to study the characteristics of the phase transformation in Zr-Nb system. The samples were heat treated at ${\beta}$-temperature ($1020^{\circ}C$) for 20 min and then cooled with different cooling rate. The microstructures of the specimens having the same compositions were changed with cooling rate and Nb content. The Widmanst$\ddot{a}$tten structure was observed on the furnace-cooled sample. The relationship between ${\alpha}$-Widmanst$\ddot{a}$tten and ${\beta}$-phase was the {0001}${\alpha}$//{110}${\beta}$, <11$\bar{2}$0>//<111>. The ${\beta}$-phase in Widmanst$\ddot{a}$tten structure of Zr-Nb alloys containing Nb more than solubility limit was identified as ${\beta}_{Zr}$ phase which was a stable phase at high temperature. In the water quenched samples, two kinds of martensite structures were observed depending on the Nb-concentration. The lath martensite was formed in Zr-0.2, 0.8 wt.% Nb alloys and the plate martensite having twins was formed in Zr-1.5 wt.% Nb alloy.
고연소도 핵연료피복관용 신합금 재료를 개발하기 위한 연구로 Zr-0.8Sn-xNb(x = 0.2,0.4,0.8, 1.0) 계 합금을 제조하여 Nb 첨가량이 Zr 합금의 미세구조 및 부식특성에 미치는 영향을 조사하였다. 미세조직 관찰결과 Nb첨가량이 증가함에 따라 결정립의 크기는 강소하였고 석출물의 량은 증가하였다. $360^{\circ}C$ 물 분위기에서 부식시험 한 결과 Nb 함량이 적을수록 부식저항성이 증가하는 경향을 나타냈으며며, Zr-0.8Sn-0.2Nb 합금이 가장 우수한 부식저항성을 보였다. 동얼 두께의 산화막에 대하여 XRD 분석한 결과, 내식성이 우수한 0.2 wt.% Nb 합금에서는 산화막내 tetra-$ZrO_2$의 분율이 높게 관찰되었다. 합금설계 관점에서 Zr-O.8Sn-xNb 합금계에 Nb올 첨가할때 Nb은 고용도 이하로 첨가되어야 한다고 사료된다.
Ti-13Nb-13Zr (TNZ) alloy has attracted considerable research attention in the last decade as a suitable substitute for the commercially used Ti-6Al-4V (TAV) alloy for orthopedic and dental implant applications. Hence, in the present work, a comparative evaluation has been performed on the electrochemical corrosion behavior of TNZ and TAV alloys in 0.9 wt.% NaCl solution. The result of the study showed that both the alloys had similar electrochemical behavior. The corrosion resistance of TAV alloy is found to be marginally superior to that of TNZ alloy.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.