The Coating Materials of Electrode Materials on Machinability of W-EDM (와이어전극의 도금재료가 W-EDM 가공성에 미치는 영향)

  • 김창호;허관도
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2000.05a
    • /
    • pp.735-738
    • /
    • 2000
  • The characteristics of wire electrical discharge machining (WEDM) are governed by many factors such as the power supply type, operating condition and electrode material. This work deals with the effect of wire electrode materials on the machining characteristics such as, metal removal rate, surface characteristics and surface roughness during WEDM A wire's thermal physical properties are melting point, electrical conductivity and vapor pressure. One of the desired qualities of wire is a low melting point and high vapor pressure to help expel the contaminants from the gap. They are determined by the mix of alloying elements (in the case of plain brass and coated wire) or the base core material(i.e. molybdenum). Experiments have been conducted regarding the choice of suitable wire electrode materials and influence of the properties of these materials on the machinability and surface characteristics in WEDM, the experimental results are presented and discussed from their metallurgical aspect. And the coating effect of various alloying elements(Au, Ag, Cu, Zn, Cr, Mn, etc.) to the Cu or 65-35 brass core on them was reviewed also. The removal rate of some coated wires are higher than that of 65-35 brass electrode wire because the wire is difficult to break due to the wire cooling effect of Zn evaporation latent heat and the Zn oxide on the surface is effective in preventing short circuit. The removal rate increases with increasing Zn content from 35, 40 and Zn coated wire

  • PDF

Chlorination of Metal Sulfide with Chlorine Gas (금속황화물의 염소화 반응)

  • Song, Yon-Ho;Hong, Jung-Seun;Lee, Chul-Tae
    • Applied Chemistry for Engineering
    • /
    • v.5 no.6
    • /
    • pp.1078-1091
    • /
    • 1994
  • Thermodynamic calculations have been made from existing literature data to show that it is reasonable to expect to recover metal chlorides from the chlorination of metal sulfides with chlorine gas. The reactions between 12 metal sulfides, such as, $Ag_2S$, $As_2S_3$, CdS, CuS, $Cu_2S$, FeS, HgS, $MoS_2$, $Ni_3S_2$, PbS, $Sb_2S_3$ and chlorine gas were investigated by means of thermogravimetric method. The theorical calculation and the experimental investigation showed that chlorination of sulfide is a better alternative process for the extraction metallurgical process of sulfide ores.

  • PDF

Freibergite from the Yeonhwa 1 Mine (제 1 연화광산에서 산출되는 프라이버자이트)

  • 정재일;이영엽;이광식
    • Journal of the Mineralogical Society of Korea
    • /
    • v.7 no.2
    • /
    • pp.81-90
    • /
    • 1994
  • 연화 광산 동점 및 묘봉 광체에서 산출되는 프라이버자이트는 후기 광화 시기에 방연석, 피라지라이트, 황철석, 자철석, 알라반다이트, 함망간, 자철석, 섬아연석, 황선석, 석영 등과 밀접하게 공존하고 있다. 화학조성을 보면 Ag가 최고 40.5 wt%까지 높은 함량을 보이고, Zn은 극소량 또는 microprobe의 측정 한계 이하이다. 어떤 입자들에서 Pb가 최고 1.70 wt% 함유되어 있다. 연화 프라이브자이트의 화학 조성상의 다소 고유한 특성은 Me12Sb4S13을 기준으로 할 때 S가 부족하고 Sb가 많이 포함되는 점이다.

  • PDF

EXPERIMENTAL STUDY ON THE DISSOLUTION COMPONENTS AND CORROSION PRODUCTS OF SEVERAL AMALGAMS IN ARTIFICIAL SALIVA (인공타액에서 수종 아말감의 부식시 용해성분 및 표면 부식 생성물에 관한 실험적 연구)

  • Cho, Seung-Joo;Lee, Myung-Jong
    • Restorative Dentistry and Endodontics
    • /
    • v.19 no.1
    • /
    • pp.1-26
    • /
    • 1994
  • The purpose of this study was to investigate the dissolution components during corrosion of amalgams and to identify surface corrosion products in the modified Fusayama artificial saliva. Four type of amalgam alloys were used: low copper lathe cut amalgam alloy (Cavex 68), low copper spherical amalgam alloy (Caulk Spherical Alloy), high copper admixed amalgam alloy (Dispersalloy) and high copper single composition amalgam alloy (Tytin). Each amalgam alloy and Hg were triturated according to the manufacturer's direction by means of mechanical amalgamator (Capmaster, S.S.White), and then the triturated mass was inserted into the cylindrical metal mold which was 10mm in diameter and 2.0mm in height and condensed with compression of 150kg/$cm^2$ using oil pressor. The specimens were removed from the mold and stored at room temperature for 7 days and cleansed with distiled water for 30 minutes in an ultrasonic cleaner. The specimens were immersed in the modified Fusayama artificial saliva for the periods of 1 month, 3 months and 6 months. The amounts of Hg, Cu, Sn and Zn dissolved from each amalgam specimen immersed in the artificial saliva for the periods of 1 month, 3 months and 6 months were measured using Inductivity Coupled Plasma Atomic Emission Spectrometry (ICPQ-1000, Shimadzu, Japan) and amount of Ag dissolved from amalgam specimen was measured using Atomic Absorption Spectrophotometry (Atomic Absorption/Flame emission spectrophotometer M-670, Shimadzu, Japan). A surface corrosion products of specimens were analysed using Electron Spectroscopy Chemical Analyser (ESCA PHI-558, PERKIN ELMER, U.S.A.). The secondary image and back scattered image of corroded surface of specimens was observed under the SEM, and the corroded surface of specimens was analysed with the EDX. The following results were obtained. 1. The dissolution amount of Cu was the most in high copper admixed amalgam(Dispersalloy) and the least in high copper single composition amalgam(Tytin). 2. Sn and Zn were dissolved during all the experiment periods, and dissolution amounts were decreased as the time elapsed. 3. Initial surface corrosion products were ZnO and SnO. 4. Corrosion of ${\gamma}$ and ${\gamma}_2$ phase in low copper amalgams was observed and Ag-Cu eutectic alloy phase was corroded in low copper spherical amalgam(Caulk Sperical Alloy). 5. Corrosion of ${\gamma}$ and $\eta$' phase in high copper amalgams was observed and Ag-Cu eutectic alloy phase was corroded in high copper admixed amalgam(Dispersalloy). 6. Sn-Cl was produced in the subsurface of low copper amalgams and high copper admixed amalgam.

  • PDF

Effect of Nano Particles on the Hathcing rate of Artemia sp. Cyst Zooplankton (나노입자가 알테미아(Artemia sp.) Cyst 부화율에 미치는 영향)

  • Jeong, Yeon-Kyu;Lee, Byeong-Woo;Park, Chan-Il;Choi, Kwang-Soo;Kim, Mu-Chan
    • Journal of the Korean Society for Marine Environment & Energy
    • /
    • v.12 no.4
    • /
    • pp.302-306
    • /
    • 2009
  • 9 kinds of nanoparticle used for this study was a particle with the size of less than 100 nm of diameter, and Artemia sp. cyst examined what kind of influence to have upon the process hatched out in nauplius. 82% hatched in nauplius at the opposition ward where a nanoparticle wasn't added after 24 time course. AGZ020, Nano silver, P-25, Sb and SnO nanoparticle showed hatching rate of 18%, 20%, 13%, 50% and 0% respectively by the 20mg/L density, and it became clear that a harmful effect is big, but I had a harmful effect compared with the opposition ward by 75%, 60%, 73% and 73% respectively by Ag-$TiO_2$, In, Sn and Zn nanoparticle, but a feeble thing was known relatively compared with AGZ020, Nano silver, P-25, Sb and SnO nanoparticle. The difference has caused this with the ingredient a nanoparticle has. Ag is included 2 % and AGZ020, Nano silver and P-25 nanoparticle are used widely as anti-fungus agent, and the SnO nanoparticle which became combination is a light catalyst pill, and oxygen is used for a Sn particle. This and others, a possibility that use is generalized and flows into aquatic environment in sequence the home electronics, functionality cosmetics, anti-fungus agent and a light catalyst pill at present becomes high for nanoparticles and others. The anxiety which has an influence on the ecology world in the water with this can be generated, so I'd have to study the potential danger a nanoparticle has continuously.

  • PDF

Effect of Nano Particles on the Hathcing rate of Artemia sp. Cyst (알테미아(Artemia sp.) Cyst 부화율에 미치는 나노입자의 영향)

  • Lee, Byeong-Woo;Cho, Sang-Man;Park, Chan-Il;Jeong, Woo-Gun;Kim, Mu-Chan
    • Proceedings of KOSOMES biannual meeting
    • /
    • 2008.05a
    • /
    • pp.137-141
    • /
    • 2008
  • 9 kinds of nanoparticle used for this study was a particle with the size of less than 100 nm of diameter, and Artemia sp. cyst examined what kind a influence to have upon the process hatched out in nauplius. 82% hatched in nauplius at the opposition ward where a nanoparticle wasn't added after 24 time course. AGZ020, Nano silver, P-25, Sb and SnO nanoparticle showed hatching rate of 18%, 20%, 13%, 50% and 0% respectively by the 20mg/L density, and it became clear that a harmful effect is big, but I had a harmful effect compared with the opposition ward by 75%, 60%, 73% and 73% respectively by Ag-$TiO_2$, In, Sn and Zn nanoparticle, but a feeble thing was known relatively compared with AGZ020, Nano silver, P-25, Sb and SnO nanoparticle. The difference was mused this with the ingredient a nanoparticle has. Ag is included 2% and AGZ020, Nano silver and P-25 nanoparticle are used widely as anti-fungus agent, and the SnO nanoparticle which became combination is a light catalyst pill, and oxygen is used for a Sn particle. This and others, a possibility that use is generalized and flows into aquatic environment in sequence the home electronics, functionality cosmetics, anti-fungus agent and a light catalyst pill at present becomes high for nanoparticles and others. The anxiety which has an influence on the ecology world in the water with this can be generated, so I'd have to study the potential danger a nanoparticle has continuously.

  • PDF

Selective Leaching Process of Precious Metals (Au, Ag, etc.) from Waste Printed Circuit Boards (PCBs) (廢 PCBs부터 귀금속(Au, Ag 등)의 선택적 침출공정)

  • 오치정;이성오;국남표;김주환;김명준
    • Resources Recycling
    • /
    • v.10 no.5
    • /
    • pp.29-35
    • /
    • 2001
  • This study was carried out to recover gold, silver and valuable metals from the printed circuit boards (PCBs) of waste computers. PCBs samples were crushed under 1 mm by a shredder and separated into 30% conducting and loft nonconducting materials by an electrostatic separator. The conducting materials contained valuable metals which were then used as feed materials for magnetic separation. 42% of magnetic materials from the conducting materials was removed by magnetic separation as nonvaluable materials and the others, 58% of non magnetic materials, was used as leaching samples containing 0.227 mg/g Au and 0.697 mg/g Ag. Using the materials of leaching from magnetic separation, more than 95% of copper, iron, zinc, nickel and aluminium was dissolved in 2.0M sulfuric acid solution, added with 0.2M hydrogen peroxide at $85^{\circ}C$. Au and Ag were not extracted in this solution. On the other hand, more than 95% of gold and 100% of silver were leached by the selective leaching with a mixed solvent (0.2M($NH_4$)$_2$$S_2$$O_3$,0.02M $CuSO_4$,0.4M $NH_4$OH). Finally, the residues were reacted with a NaCl solution to leach Pb whereas sulfuric acid was used to leach Sn. Recoveries reached 95% and 98% in solution, respectively.

  • PDF

Preparations and characteristics of the ceramic balls for heavy metals absorption and antibacterial activities in the drinking water (음용수중의 중금속흡착과 항균성용 세라믹 볼의 제조 및 특성평가)

  • Park, Chun-Won;Park, Ra-Young;Park, Sun-Min
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.15 no.6
    • /
    • pp.263-268
    • /
    • 2005
  • The ceramic balls impregnated with $20{\sim}40nm$ sized Ag colloid were examined for heavy metals absorption and antibacterial activities in the drinking water. The preparation conditions of ceramic ball that the porosity was excellent were as follows: starting material: 85 wt% $Ca_{10}(PO_4)_6(OH)_2$, binder: 5 wt% PVA and 15 wt% ${\alpha}-Ca_3(PO_4)_2$, heating temperature: $1000^{\circ}C$, duration: 3 hrs. The ceramic balls obtained under these conditions showed specific surface area of $110m^2/g$, pore size of $120{\mu}m$ and porosity of 80%. Also, as the results of a performance test on a rate of adsorbing and removing heavy metals in the drinking water by using the.AAS, heavy metals such as Zn, Mn, Fe and Cu were removed to the extent that their content became 0.03mg/l or lower after 1 day and they showed an excellent bactericidal activity that all coliforms were killed after 3 hrs.

Corrosion Behavior of Ti-6Al-4V Alloy after Plasma Electrolytic Oxidation in Solutions Containing Ca, P and Zn

  • Hwang, In-Jo;Choe, Han-Cheol
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2016.11a
    • /
    • pp.120-120
    • /
    • 2016
  • Ti-6Al-4V alloy have been used for dental implant because of its excellent biocompatibility, corrosion resistance, and mechanical properties. However, the integration of such implant in bone was not in good condition to achieve improved osseointergraiton. For solving this problem, calcium phosphate (CaP) has been applied as coating materials on Ti alloy implants for hard tissue applications because its chemical similarity to the inorganic component of human bone, capability of conducting bone formation and strong affinity to the surrounding bone tissue. Various metallic elements, such as strontium (Sr), magnesium (Mg), zinc (Zn), sodium (Na), silicon (Si), silver (Ag), and yttrium (Y) are known to play an important role in the bone formation and also affect bone mineral characteristics, such as crystallinity, degradation behavior, and mechanical properties. Especially, Zn is essential for the growth of the human and Zn coating has a major impact on the improvement of corrosion resistance. Plasma electrolytic oxidation (PEO) is a promising technology to produce porous and firmly adherent inorganic Zn containing $TiO_2(Zn-TiO_2)$coatings on Ti surface, and the a mount of Zn introduced in to the coatings can be optimized by altering the electrolyte composition. In this study, corrosion behavior of Ti-6Al-4V alloy after plasma electrolytic oxidation in solutions containing Ca, P and Zn were studied by scanning electron microscopy (SEM), AC impedance, and potentiodynamic polarization test. A series of $Zn-TiO_2$ coatings are produced on Ti dental implant using PEO, with the substitution degree, respectively, at 0, 5, 10 and 20%. The potentiodynamic polarization and AC impedance tests for corrosion behaviors were carried out in 0.9% NaCl solution at similar body temperature using a potentiostat with a scan rate of 1.67mV/s and potential range from -1500mV to +2000mV. Also, AC impedance was performed at frequencies ranging from 10MHz to 100kHz for corrosion resistance.

  • PDF

Production and Characteristics of Pullulanase from Bacillus cereus (Bacillus cereus에 의한 Pullulanase의 생산 및 특성)

  • 정만재;임계숙;조대선;우정숙
    • Microbiology and Biotechnology Letters
    • /
    • v.20 no.4
    • /
    • pp.409-416
    • /
    • 1992
  • The optimum cultural temperature and time for the pullulanase production by Bacillus cereus were $15^{\circ}C$ and 72 hrs, respectively. The addition of casein, nutrient broth and egg albumin to the basal medium, respectively, increased greatly the enzyme production. The enzyme was purified by ammonium sulfate fractionation, CM-cellulose and DEAE-cellulose column chromatographies. The specific activity of the purified enzyme was 29.09 U/mg protein and the yield of enzyme activity was 17.1% The purified enzyme showed a single band on polyacrylamide disc gel electrophoresis and its molecular weight was estimated to be 61,000 by SDSpolyacrylamide disc gel electrophoresis. The isoelectric point for the purified enzyme was pH 7.0. The optimum temperature and pH were $40^{\circ}C$ and 6.5. The purified enzyme was stable below $35^{\circ}C$ and in the pH range of 6.5-11.0. It was greatly inhibited by $Ag^{+}$, $Hg^{2+}$ and $Zn^{2+}$, and its thermal stability was increased by the addition of $Ca^{2+}$ Among various substrates, pullulan was favorably hydrolyzed by the purified enzyme and the hydrolysis product 011 pulluIan was maltotriose.

  • PDF