Probabilistic Characteristics of Fatigue Behavior Parameter of Paris-Erdogan Law in Mg-Al-Zn Alloy (Mg-Al-Zn 합금의 Paris-Erdogan 법칙에 따른 피로거동 파라미터의 확률론적 특성)

  • Choi, Seon-Soon
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.35 no.4
    • /
    • pp.375-381
    • /
    • 2011
  • The primary aim of this study is to investigate the probabilistic characteristics of the fatigue parameters that describe the fatigue crack growth behavior in magnesium alloy. Statistical fatigue crack propagation experiments have been performed on rolled AZ31 magnesium alloy CT specimens with different specimen thickness, load ratio, and maximum load at ambient temperature in a laboratory. Using the statistical fatigue data obtained from these experiments, the goodness-of-fit of the probability distribution of the fatigue behavior parameters is evaluated in this study by performing statistical analyses. The crack growth rate coefficient is a fatigue parameter having a very large COV(Coefficient of Variation), but the variation of a crack growth rate exponent is not substantial. It is considered that a crack growth rate exponent can be a material constant. It is also found that the best fit probability distribution of the parameters such as the crack growth rate coefficient and crack growth rate exponent for a magnesium alloy is a three-parameter Weibull distribution, and two-parameter Weibull distribution is a good distribution only for the crack growth rate coefficient.

Properties and Casting Characteristics of Al-Zn-Fe-Si Alloys (Al-Zn-Fe-Si 합금의 물성 및 주조특성)

  • Yun, Ho-Seob;Kim, Jeong-Min;Park, Joon-Sik;Kim, Ki-Tae
    • Journal of Korea Foundry Society
    • /
    • v.33 no.1
    • /
    • pp.8-12
    • /
    • 2013
  • Although aluminum-silicon based commercial casting alloys have been used in applications that demand high electrical or thermal conductivity, new aluminum casting alloys that possess higher conductivities are currently required for advanced applications. Therefore, there is much research into the development of new high conductivity aluminum casting alloys that contain lower amounts of or no silicon. In this research, the properties and casting characteristics of Al-Zn-Fe-Si alloys with various Fe and Si contents were investigated. Two types of AlFeSi phases were formed depending on the Fe and Si contents. As the silicon content increased, the tensile strength of the Al-Zn-Fe-Si alloy increased slightly, while the electrical conductivity decreased slightly. It was also observed that both the fluidity and hot cracking susceptibility of the investigated alloys were closely related to the formation of the AlFeSi phases.

Mechanism of Crack Formation in Pulse Nd:YAG Laser Spot Welding of Al Alloys (Al합금 펄스 Nd:YAG 레이저 점 용접부의 균열 발생기구)

  • 하용수;조창현;강정윤;김종도;박화순
    • Journal of Welding and Joining
    • /
    • v.18 no.2
    • /
    • pp.86-94
    • /
    • 2000
  • This study was performed to investigate types and formation mechanism of cracks in two Al alloy welds, A5083 and A7N01 spot-welded by pulse Nd : YAG laser, using SEM, EPMA and Micro-XRD. In the weld zone, three types of crack were observed : center line crack({TEX}$C_{C}${/TEX}), diagonal crack({TEX}$C_{D}${/TEX}), and U shape crack({TEX}$C_{U}${/TEX}). Also, HAZ crack({TEX}$C_{H}${/TEX}) was observed in the HAZ region, furthermore, mixing crack({TEX}$C_{M}${/TEX}) consisting of diagonal crack and HAZ crack was observed. White film was formed at th hot crack region in the fractured surface after it was immersed to 10% NaOH water. In the case of A5083 alloy, white films in {TEX}$C_{C}${/TEX} crack and {TEX}$C_{D}${/TEX} crack region were composed of low melting phases, {TEX}$Fe_{2}SiAl_{8}${/TEX} and eutectic phases, $Mg_2$Al$_3$ and $Mg_2$Si. Such films observed $CuAl_2$, {TEX}$Mg_{32}(Al,Zn)_{3}${/TEX}, MgZn$_2$, $Al_2$CuMg and $Mg_2$Si were observed in the whitely etched films near {TEX}$C_{C}${/TEX} crack and {TEX}$C_{D}${/TEX} crack regions. The formation of liquid films was due to the segregation of Mg, Si, Fe in the case of A5083 alloy and Zn, Mg, Cu, Sim in the case of A7N01 alloy, respectively. The {TEX}$C_{C}${/TEX} and {TEX}$C_{D}${/TEX} cracks were regarded as a result of the occurrence of tensile strain during the welding process. The formation of {TEX}$C_{M}${/TEX} crack is likely to be due to the presence of liquid film at the grain boundary near the fusion line in the base metal as well as in the weld fusion zone during solidification. The {TEX}$C_{U}${/TEX} crack is considered a result of the collapsed keyhole through incomplete closure during rapid solidification.

  • PDF

Reaction-Bonded Al2O3 Ceramics Using Oxidation of Al Alloy Powder

  • Lee, Hyun-Kwuon
    • Korean Journal of Materials Research
    • /
    • v.24 no.5
    • /
    • pp.236-242
    • /
    • 2014
  • Fabrication of reaction-bonded $Al_2O_3$ (RBAO) ceramics using Al-Zn-Mg alloy powder was studied in order to improve traditional RBAO ceramic processing using Al powder. The influence on reaction-bonding and microstructure, as well as on physical and mechanical properties, of the particulate characteristics of the $Al_2O_3$-Al alloy powder mixtures after milling, was revealed. Variation of the particulate characteristics of this $Al_2O_3$-Al alloy powder mixture with milling time was reported previously. To start, the $Al_2O_3$-Al alloy powder mixture was milled, reaction-bonded, post-sintered, and characterized. During reaction-bonding of the $Al_2O_3$-Al alloy powder mixture compacts, oxidation of the Al alloy took place in two stages, that is, there was solid- and liquid-state oxidation of the Al alloy. The solid-state oxidation exhibited strong dependence on the density of surface defects on the Al-alloy particles formed during milling. Higher milling efficiency resulted in less participation of the Al alloy in reaction-bonding. This was because of its consumption by chemical reactions during milling, and subsequent powder handling, and could be rather harmful in the case of over-milling. In contrast to very little dependence of oxidation of the Al alloy on its particle size after milling, the relative density, microstructure, and flexural strength were strongly dependent on particle size after milling (i.e., on milling efficiency). The relative density and 4-point flexural strength of the RBAO ceramics in this study were ~98% and ~365 MPa, respectively, after post-sintering at $1,600^{\circ}C$.

Corrosion Behavior of Mg-Al-Zn-CaO Alloy (Mg-Al-Zn-CaO 합금의 부식 거동)

  • Moon, Jung-Hyun;Jun, Joong-Hwan;Kim, Young-Jik
    • Journal of Korea Foundry Society
    • /
    • v.33 no.3
    • /
    • pp.127-133
    • /
    • 2013
  • The influences of a small amount of CaO addition on the microstructure and corrosion behavior of AZ81 casting alloy have been investigated by means of optical microscopy, scanning electron microscopy, X-ray photoelectron spectroscopy, immersion and electrochemical tests. The added CaO led to the refinement of ${\alpha}$-Mg grains and the decrease in ${\beta}$ precipitate content by the formation of an $Al_2Ca$ phase. The AZ81-CaO alloy had a better corrosion resistance than the AZ81 alloy. The microstructural characterization on the corroded surface revealed that the enhanced corrosion resistance of the CaO-containing alloy may well be ascribed to the increased barrier effect of precipitates formed more continuously along the grain boundaries and the incorporation of Al and Ca elements into the corrosion film, by which it became more protective.

Effect of Al and Mg Contents on Wettability and Reactivity of Molten Zn-Al-Mg Alloys on Steel Sheets Covered with MnO and SiO2 Layers

  • Huh, Joo-Youl;Hwang, Min-Je;Shim, Seung-Woo;Kim, Tae-Chul;Kim, Jong-Sang
    • Metals and materials international
    • /
    • v.24 no.6
    • /
    • pp.1241-1248
    • /
    • 2018
  • The reactive wetting behaviors of molten Zn-Al-Mg alloys on MnO- and amorphous (a-) $SiO_2$-covered steel sheets were investigated by the sessile drop method, as a function of the Al and Mg contents in the alloys. The sessile drop tests were carried out at $460^{\circ}C$ and the variation in the contact angles (${\theta}_c$) of alloys containing 0.2-2.5 wt% Al and 0-3.0 wt% Mg was monitored for 20 s. For all the alloys, the MnO-covered steel substrate exhibited reactive wetting whereas the $a-SiO_2$-covered steel exhibited nonreactive, nonwetting (${\theta}_c>90^{\circ}$) behavior. The MnO layer was rapidly removed by Al and Mg contained in the alloys. The wetting of the MnO-covered steel sheet significantly improved upon increasing the Mg content but decreased upon increasing the Al content, indicating that the surface tension of the alloy droplet is the main factor controlling its wettability. Although the reactions of Al and Mg in molten alloys with the $a-SiO_2$ layer were found to be sluggish, the wettability of Zn-Al-Mg alloys on the $a-SiO_2$ layer improved upon increasing the Al and Mg contents. These results suggest that the wetting of advanced high-strength steel sheets, the surface oxide layer of which consists of a mixture of MnO and $SiO_2$, with Zn-Al-Mg alloys could be most effectively improved by increasing the Mg content of the alloys.

Effect of Scancium Content on The Hot Extrusion of Al-Zn-Mg-(Sc) Alloy (Al-Zn-Mg-(Sc) 합금의 고온가공성에 미치는 Sc 함량의 영향)

  • Kim, Jin-Ho;Kim, Jeoung-Han;Yeom, Jong-Taek;Lee, Dong-Geun;Park, Nho-Kwang
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2006.05a
    • /
    • pp.184-187
    • /
    • 2006
  • The effects of scandium content and extrusion parameters on Al-Zn-Mg-(Sc) alloys were examined. Three kinds of Al-Zn-Mg-(Sc) alloys with up to 0.30 wt.% Sc were prepared. The compression test was conducted to investigate the microstructure evolution during hot deformation. Despite of microstructural differences in the alloys, deformation behaviors were very similar. After extrusion at $350^{\circ}C$ with the ram speed of 15mm/sec, AA7075 showed a moderate surface quality compared with other Sc containing alloys, which was attributed to low flow stresses. AA7075 showed coarse-grained bands in surface region. With the ram speed of 1.5mm/sec at $350^{\circ}C$, the surface quality of the alloys was sound due to low friction stresses and deformation heating. As the Sc content increased, tensile strengths and elongations at room temperature improved.

  • PDF

An Electrochemical Evaluation on the Corrosion Property of Metallizing Film (용사 도막의 내식성에 관한 전기화학적 평가)

  • Moon, Kyung-Man;Shin, Joong-Ha;Lee, Myung-Hoon;Lee, Sung-Yul;Kim, Yun-Hae
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.34 no.5
    • /
    • pp.670-677
    • /
    • 2010
  • There are many surface protection methods for numerous steel structures being used under severely corrosive environment, one of them, metallizing(thermal spray) is a available protection method which is comparatively and recently developed for surrface protection of various steel structures. However coating film obtained by spraying is to be needed increasingly more good corrosion resistance due to accelerating of environmental contamination. In this study, coating films(DFT:$200{\mu}m$) are performed with arc spray by wire metal and their types of films are pure zinc, pure aluminum, alloy film(Al:Zn=85:15) and alloy film(Al:Zn=95:5). And corrosion resistance of their films was investigated with electrochemical methods in seawater solution. Pure aluminum film showed a relatively somewhat good corrosion resistance compared to among those of other films and alloy films also showed a good corrosion resistance compared to pure zinc film. Especially it was observed that pure aluminum film showed a comparatively good corrosion resistance than that of alloy film named as galvarium spray(Al:Zn=85:15) in seawater solution. Morphology of corroded surface of pure zinc film appeared the pattern like intergranlar corrosion, however films of pure aluminum and alloy metal showed a general corrosion pattern.

Weld Cracking of High Strength Al-Zn-Mg Alloy Weldment (용접구조용 7000 계열 고장력 Al-Zn-Mg 합금의 용접특성과 용접균열에 관한 고찰)

  • 김환태;황선효;남수우
    • Journal of Welding and Joining
    • /
    • v.12 no.1
    • /
    • pp.28-37
    • /
    • 1994
  • 본 소고에서는 Al-Zn-Mg 계통의 고강도 알루미늄합금의 제조과정에서 실시하는 열처리 공정을 통해 얻어지는 시효경화 효과, 합금원소 첨가에 따른 석출물의 생성과 이에 따른 석출경화 효과와 용착금속의 응고균열 발생과의 상호관계를 조사하고 용접열영향부의 용질원자 확산과 입계의 liquid film에 의한 액화(liquation) 균열의 생성을 분석하여 설명하고자 한다.

  • PDF

Microstrucual Characterization of Vacuum Gas Gas Atomized AZ31+1%MM Alloy Powders (진공가스분무한 AZ31+1%MM 합금 분말의 미세조직 특성)

  • 김연옥
    • Journal of Powder Materials
    • /
    • v.6 no.3
    • /
    • pp.231-237
    • /
    • 1999
  • In this study, the characteristics of gas atomized Mg-3wt%Al-1wt%Zn-1wt%MM alloy powders under vacuum condition were investigated. In spite of the low fluidity and easy oxidation of the molten magnesium, the spherical powders could be successfully produced by using a modified three pieces nozzle attached to the gas atomization unit. It was found that most of the solidified powders less than 50$\mu$m in diameter were single crystal and the solidified structure showed a typical dendritic morphology due to supercooling prior to nucleation. The secondary dendrite arm spacing decreased as the size of powders decreased. The Mg-Al-Ce intermetallic compounds with chemically stable phase were found in the interdendritic regions of $\alpha$-Mg. It is considered that formation of the chemically stable phase may possibly affect to improve the corrosion resistance. Therefore, it is expected that the materials formed of these Mg-Al-Zn-MM alloy powders shows better mechanical properties and corrosion resistance due to the structural refinement.

  • PDF