Fruits Extracts Mediated Synthesis of Zinc Oxide Nanoparticles Using Rubus coreanus and its Catalytic Activity for Degradation of Industrial Dye

  • Rupa, Esrat Jahan;Gokulanathan, Anandapadmanaban;Ahn, Jong-Chan;Mathiyalagan, Ramya;Markus, Josua;Elizabeth, Jimenez Perez Zuly;Soshnikova, Veronika;Kim, Yeon-Ju;Yang, Deok-Chun
    • Proceedings of the Plant Resources Society of Korea Conference
    • /
    • 2018.04a
    • /
    • pp.93-93
    • /
    • 2018
  • This study disclosed the aqueous fruits extract of Rubus coreanus as a sustainable agent for the synthesis of Rubus coreanus zinc oxide nanoparticle (Rc-ZnO Nps) using as a reducing and capping precursor for co-precipitation method. The development of Rc-ZnO was assured by white precipitated powder and analyzed by spectroscopic and analytical instruments. The UV-visible (UV-Vis) studies indicate the maximum absorbance at 357nm which confirmed the formation of ZnO Nps and the purity, functional group and monodispersity were assured by field emission transmission electron microscopy (FE-TEM), Fourier Transform Infrared (FTIR) Spectroscopy and dynamic light scattering (DLS). The X-ray powder diffraction (XRD) data revealed the Nps is 23.16 nm in size, crystalline in nature and possess hexagonal wurtzite structure. The Rc-ZnO Nps were subjected for catalytic studies. The Malachite Green dye was degraded by Rc- ZnO NPs in both dark and light (100 W tungsten) conditions and it degraded about 90% at 4 hours observation in both cases. The biodegradable, low cost Rc-ZnO NPs can be a better weapon for waste water treatment.

  • PDF

Resistance Spot Weldability of Surface Roughness Textured Galvannealed Steel Sheets (표면조도처리 된 합금화 용융아연도금강판의 저항 점 용접성)

  • Park, Sang-Soon;Kim, Ki-Hong;Kang, Nam-Hyun;Kim, Young-Seok;Rhym, Young-Mok;Choi, Yung-Min;Park, Yeong-Do
    • Korean Journal of Metals and Materials
    • /
    • v.46 no.8
    • /
    • pp.495-505
    • /
    • 2008
  • With the high proportion of zinc coated steels in body-in-white assembly, newly developed surface roughness textured galvannealed steel sheets have been introduced. In this study, zinc coated and surface roughness textured steel sheets were welded by resistance spot welding to investigate its weldability including electrode wear test. Based on the results of tensile-shear test, nugget diameter changes, and electrode tip growth test, it was clear that both surface roughness textured steels (GA-T and GA-E) showed good weldability. Also, there was no large difference in weldability and electrode wear behavior between GA-T and GA-E steels which have different surface roughness morphology. An analysis of electrode degradation showed Fe and Zn penetration through the electrode tip surface at 2400 welds reached $55{\sim}60{\mu}m$ and $75{\sim}80{\mu}m$, respectively. Therefore, there is no significant effect of surface roughness morphology on spot weldability of surface roughness textured galvannealed steel sheets. However, slight difference in thickness of alloying layers existing on electrode tip was found between GA-T and GA-E steels.

Influence of NiO, $TiO_2$ on ZnO-$SnO_2$ System Spinel Pigment (ZnO-$SnO_2$계 Spinel 채료에 대한 NiO, $TiO_2$의 영향)

  • 이응상;황성윤
    • Journal of the Korean Ceramic Society
    • /
    • v.14 no.3
    • /
    • pp.187-192
    • /
    • 1977
  • For the purpose researching to the influence of tetrahedral and octahedral preference of cations of $Ni^{2+}$, $Ti^{4+}$ upon the formation and the color development of the $ZnO-SnO_2$ spinel containing $Ni^{2+}$ and $Ti^{4+}$ ions, the gradual substitution of $Ni^{2+}$ ions for $Zn^{2+}$ ions and of $Ti^{4+}$ ions for $Sn^{4+}$ ions of the spinel in NiO-ZnO-$SnO_2$-$TiO_2$ system was carried out. On samples prepared by calcining the oxide and basic cabonate mixtures at $1300^{\circ}C$ for 2 hours, the X-ray analysis, measurement of reflectance and the test of their stabilaity as a glaze pigment were also carried out. The results are summarized as follows 1) Single spinel was formed completely to x=1 in the $xNiO\cdot(2-x)ZnO\cdot{SnO}_2$system, and gave brilliant lightgreen hue. Moreover, $NiO\cdot{ZnO}\cdot{SnO}_2$ formed easily spinel than $NiO\cdot{MgO}\cdot{SnO}_2$ because Zn^{2+}$ ions had more strong tetrahedral preference than $Mg^{2+}$ ions. 2) As the gradual substitution of $Ti^{4+}$ ions for $Sn^{4+}$ ions in $NiO\cdot{MgO}\cdot{SnO}_2$ system, the spinels formed well and was nearly not changed in the hue. 3) The results of glaze test. (1) As the gradual substitution of $Ni^{2+}$ ions for $Zn^{2+}$ ions, the color changed from dull white to graish broun gradually in calcium-zinc glaze and calcium glaze, and from white to beige in tile glaze. (2) As the gradual substitution of $Ti^{4+}$ ions for $Sn^{4+}$ ions in $NiO-ZnO-SnO_2-TiO_2$ system, the color was become dull generally and was not change in tile glaze.

  • PDF

Multiple Brain Calcification in Chronic Lead Poisoning (만성 연중독자에서의 다발성 뇌석회화 병변)

  • Kim, Sung-Ryul;Kim, Byoung-Gwon;Hong, Young-Seoub;Dam, Do-Won;Choi, Soon-Seob;Jung, Kap-Yull;Kim, Joon-Youn
    • Journal of Preventive Medicine and Public Health
    • /
    • v.28 no.2 s.50
    • /
    • pp.398-405
    • /
    • 1995
  • We experienced a case of occupational lead poisoning employed in a secondary lead smelting plant for 12 years. The patient was 39-year-old male and had been felt dizziness, recent memory impairment and intermittent severe abdominal pain for 2 years. On admission, blood lead level was $92.9{\mu}g/dl$, urinary lead level was $19.9{\mu}g/l$ and zinc protoporphyrin level was $226.0{\mu}g/dl$. On the blood test, hemoglobin was 10.6g/dl and showed normocytic normochromic anemia. There were no abnormal findings in the biochemical and hormonal tests. Decrease of I.Q. and use of words in speaking were found in the psychiatric and psychologic examinations. We observed the finding of motor polyneuropathy in the nerve conduction velocity test. Computed tomographic finding showed calcification lesions in the basal ganglia, dentate nuclei, caudate nuclei, and especially characteristic multiple calcifications were located in the subcortical white matter.

  • PDF

A Study on the change of Ecological Environment in Cave cause by the Pollution of Cave Environment and Analysis of Environmental Pollutants in Cave (환경오염으로 인한 동굴생태환경의 변화와 환경오염물질 분석에 관한 연구)

  • 이경호
    • Journal of the Speleological Society of Korea
    • /
    • no.61
    • /
    • pp.5-16
    • /
    • 2000
  • Recently many environmental researcher are concerned about the ecological environment and the issue of environmental pollution in cave. In this paper we discuss about air pollution, water pollution, state of water quality, ecological environment and situation of environmental public damage in cave The concerning of air pollution in cave is mainly to the type of secondary contamination, which much is developed in various fields recently. The natural water in the most of cave is no problems but ground water has slitting with natural water during much raining period. The state of water quality is gradually contaminated with artificial environmental pollution, that is, the contents of kinds of Aluminum, Nickel, Copper, Zinc and Calcium are higher than before. On the other hand it is very important things to keep the control of constant temperature, darkness and humidity in cave. The contamination by lamp flora and even black colored contamination are appeared nowadays. The ecological environment in cave destructed by growing of mi coorganism. In fact the internal of cave is shielded with the state of climate of cave external but the environment of internal cave is contaminated, because blowing from external climate state. In addition to environmental pollution caused by carbon dioxide and body temperature of tourists. By the way eco-examination of cave is black color public damage, green color one and white color one has been discovered, so we need to have the situation of demand of environmental reservation alternatives.

  • PDF

The Development of Corrosion Standard System of Water and Wastewater in Soil Environment (상·하수도 배관재의 토양환경에서의 부식표준시스템 개발)

  • Park, Kyeong-Dong;Shin, Yeong-Jin;Lee, Ju-Yeong
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.5 no.4
    • /
    • pp.7-12
    • /
    • 2006
  • Galvanized steel pipe, copper pipe and stainless steel pipe, which is being used in waterworks piping materials. In case of galvanized steel pipe, the precipitation of a product is being generated due to the pollution of the tap water, a white water phenomenon, and various corrosion reaction because a zinc ion is melted by tap water. And in case of a cupper pipe, many problems which is harm in sanitation appeared because of a inflow of harmfulness substance by a frequent accident of a water leakage. So, to prevent these problems, it is substituted for stainless steel pipe. However, those problems is still occurring because of badness of welding, a problem of a water leakage in connection part, and a increment of construction expenses. Therefore, this research has examined the laying period according to each piping thickness and a corrosion shape according to each laying depth after laying in various soils(sandy loam, loamy, clay loam, clay) using galvanized steel pipe, copper pipe, and stainless steel pipe. That is, we has studied the data which is necessary for a rational method of preserving the quality of water by examining the corrosion properties of piping materials in the soil environment which waterworks piping materials is being used.

  • PDF

Virtual Screening of Penicillin-derived Inhibitors for the Metallo-β-lactamase from Bacillus cereus

  • Lee, Jong-Sun;White, Ethan;Kim, Sang-Gon;Kim, Sung-Kun
    • Bulletin of the Korean Chemical Society
    • /
    • v.31 no.12
    • /
    • pp.3644-3652
    • /
    • 2010
  • The metallo-$\beta$-lactamases ($M{\beta}Ls$) are clinically significant enzymes which readily hydrolyze most $\beta$-lactam antibiotics. Discovering potential inhibitors for the $M{\beta}Ls$ is an expensive, time consuming endeavor. Virtual screening can sieve out inhibitor candidates with incompatible features prior to synthesis, decreasing these costs. Using Autodock 4.0, the binding locations and energies of four previously-studied potential inhibitors and four additional compounds obtained from the National Cancer Institute (NCI) database were computationally calculated. Based on the docking models of these eight compounds, we then designed several hypothetical inhibitor structures, compounds A through F, and performed their respective docking experiments. The docking results for compound F showed that it binds to the zinc containing active sites with a lowest predicted binding energy of -6.70 kcal/mol, suggesting F is the most likely potential $M{\beta}L$ inhibitor.

Porosity Reduction during Gas Tungsten Arc-Gas Metal Arc Hybrid Welding of Zinc Coated Steel Sheets (II) - Hybrid Welding Results (GTA-GMA 하이브리드공정에 따른 자동차용 아연도금강판의 용접부 기공감소 (II) - 하이브리드공정 적용 결과)

  • Ahn, Young-Nam;Kim, Cheolhee
    • Journal of Welding and Joining
    • /
    • v.34 no.4
    • /
    • pp.48-54
    • /
    • 2016
  • The use of Zn coated steel has increased in the automotive industry due to its excellent corrosion resistance. Conventionally the BIW(body-in-white) structure and the hang-on parts have been made of Zn coated steel and more recently Zn coated steel began to be applied in the chassis parts. During gas metal arc (GMA) welding of the chassis part, lap fillet joint used to be adopted but spatter generation and porosities are most important concerns. In the industrial applications, an intentional joint gap was made to avoid the weld defects but it is not easy to control the size of joint gap. In this research, gas tungsten arc (GTA) is combined with GMA welding where GTA precedes GMA. As pulsed arc was adopted as GMA, GTA was oscillated along the longitudinal direction by pulsing GMA, but the arc oscillation did not disturb the molten droplet transfer of GMA welding. By increasing the distance between GTA and GMA, the length of weld pool increased and porosity could be reduced. Moreover porosity in the welds was fully removed when the distance between two arcs was 15 mm.

Chemical enhancement of footwear impressions in urine on the surface of tiles

  • Kim, Sung Jin;Hong, Sungwook
    • Analytical Science and Technology
    • /
    • v.32 no.3
    • /
    • pp.113-119
    • /
    • 2019
  • Enhancement of footwear impressions in urine on the surface of tiles by using p-dimethylaminocinnamaldehyde (DMAC), which react with urea, and ninhydrin, 1,8-diazafluoren-9-one (DFO), 1,2-indanedione/zinc (1,2-IND/Zn), which react with amino acid, was studied. As a result of comparing the application methods of reagents, the ninhydrin and the 1,2-IND/Zn were suitable for application with spray method, which is spray directly on footwear impression, DFO and DMAC were suitable for application with dry contact method, which is applying heat with press to DMAC impregnated paper on footwear impression. In addition, DMAC applied with dry contact method showed best contrast and enhancement result in both white and black colored tiles by comparing of the sensitivity by different dilution ratio of urine and the aging time of footwear impressions in urine. And the result of applied with DMAC (with dry contact method) on the floor tiles collected at various places in a building's men's and women's bathrooms, it can be successfully enhanced that footwear impressions in urine. So it is believed that the method can be used to recover footwear impressions in urine from real crime scenes.

Fluid Inclusion and Stable Isotope Studies of the Kwangsin Pb-Zn Deposit (광신 연 - 아연 광상의 유체포유물 및 안정동위원소 연구)

  • Choi, Kwang-Jun;Yun, Seong-Taek;So, Chil-Sup
    • Economic and Environmental Geology
    • /
    • v.30 no.6
    • /
    • pp.505-517
    • /
    • 1997
  • Lead and zinc mineralization of the Kwangsin mine was formed in quartz and carbonate veins that filled fault-related fractures in the limestone-rich Samtaesan Formation of the Chosun Supergroup and the phyllite-rich Suchangni Formation of unknown age. A K-Ar date of alteration sericite indicates that the Pb-Zn mineralization took place during Late Cretaceous (83.5 Ma), genetically in relation to the cooling of the nearby Muamsa Granite (83~87 Ma). Mineral paragenesis can be divided into three stages (I, II, III): (I) the deposition of barren massive white quartz, (II) the main Pb-Zn mineralization with deposition of white crystalline quartz and/or carbonates (rhodochrosite and dolomite), and (III) the deposition of post-ore barren calcite. Mineralogic and fluid inclusion data indicate that lead-zinc minerals in middle stage II (IIb) were deposited at temperatures between $182^{\circ}$ and $276^{\circ}C$ from fluids with salinities of 2.7 to 5.4 wt. % equiv. NaCl and with log $fs_2$ values of -15.5 to -11.8 atm. The relationship between homogenization temperature and salinity data indicates that lead-zinc deposition was a result of fluid boiling and later meteoric water mixing. Ore mineralization occurred at depths of about 600 to 700 m. Sulfur isotope compositions of sulfide minerals (${\delta}^{34}S_{CDT}=9.0{\sim}14.5$ ‰) indicate a relatively high ${\delta}^{34}S_{{\Sigma}S}$ value of ore fluids (up to 14 ‰), likely indicating an igneous source of sulfur largely mixed with an isotopically heavier sulfur source (possibly sulfates in surrounding sedimentary rocks). There is a remarkable decrease of calculated ${\delta}^{18}O$ value of water in hydrothermal fluids with increasing paragenetic time: stage I, 14.6~10.1 ‰; stage IIa, 5.8~2.2 ‰; stage IIb, 0.8~2.0 ‰; stage IIc, -6.1~-6.8 ‰, This indicates a progressive increase of meteoric water influx in the hydrothermal system at Kwangsin. Measured and calculated hydrogen and oxygen isotope values indicate that the Kwangsin hydrothermal fluids was formed from a circulating (due to intrusion of the Muamsa Granite) meteoric waters which evolved through interaction mainly with the Samtaesan Formation (${\delta}^{18}O=20.1$ to 24.9 ‰) under low water/rock ratios.