• Title/Summary/Keyword: Zinc leaching

Search Result 68, Processing Time 0.025 seconds

Characterizations of Precipitated Zinc Powder Produced by Selective Leaching Method

  • Marwa F. Abd;F. F. Sayyid;Sami I. Jafar Al-rubaiey
    • Corrosion Science and Technology
    • /
    • v.23 no.1
    • /
    • pp.54-63
    • /
    • 2024
  • This work investigated the influence of concentration and applied potential on the characteristics of zinc powder (purity, apparent density, morphology, particle size distribution, and particle zeta potential) produced by the electrochemical process from waste brass. High-purity zinc powder is obtained using selective leaching of industrial brass waste in acidic, neutral, and alkaline solutions. The free immersion method with and without voltage using linear polarization technique is used. In the electrochemical process, hydrochloric acid HCl in three different concentrations (0.1, 0.2, and 0.3) M is used. The time and the distance between the electrodes are set to be 30 min and 3 cm, respectively. It has been found that the percentage purity is 98%, 96%, and 94% for the acidic, neutral, and alkaline solutions, respectively. In addition, the morphology of zinc powder analyzed by SEM was dendritic and mossy. It has been recorded that the purity of zinc increases with the increase of the concentration and applied potential. The highest value of purity for zinc powder was %98.58 in 1000 mV and 0.3M concentration for graphite cathode.

Fixation and Leaching Characteristics of CCA- and CCFZ- Treated Domestic Softwood Species

  • Kim, Jae-Jin;Kim, Hyung-Jun;Ra, Jong-Bum;Chun, Su Kyoung;Kim, Gyu-Hyeok
    • Journal of the Korean Wood Science and Technology
    • /
    • v.31 no.6
    • /
    • pp.55-59
    • /
    • 2003
  • The fixation and leaching characteristics of chromated copper arsenate (CCA Type C) and chromium- copper-fluoride-zinc (CCFZ) in domestic softwood (Japanese red pine, Korean pine, and Japanese larch) sapwood were investigated using the expressate method to follow chromium fixation and the American Wood-Preservers' Association (AWPA) leaching procedure to determine leaching properties after fixation. The rates of fixation were affected by preservative types; CCA was fixed much faster than CCFZ for all species evaluated. There were definite differences in the fixation rates of different species, with Korean pine requiring shorter to fix than the other species evaluated. Chromium fixation was greatly enhanced by elevated temperatures, and fixation time can be estimated according to fixation temperatures applied. The percentage of arsenic and zinc leached from domestic softwoods was relatively high compared to chromium and copper, indicating that there is still a relatively high unfixed arsenic and zinc components after complete chromium fixation in CCA-and CCFZ-treated samples, respectively.

Toward high recovery and selective leaching of zinc from electric arc furnace dust with different physicochemical properties

  • Lee, Han Saem;Park, Da So Mi;Hwang, Yuhoon;Ha, Jong Gil;Shin, Hyung Sang
    • Environmental Engineering Research
    • /
    • v.25 no.3
    • /
    • pp.335-344
    • /
    • 2020
  • This work describes highly efficient recovery and selective leaching of Zn from electric arc furnace dust (EAFD) with different physicochemical properties, induced by acid leaching at ambient conditions. The chemical compositions, mineralogical phases, and particle sizes of the EAFDs were analyzed and compared. The effects of leaching time, liquid/solid ratio, acid type, and acid concentration on the selective leaching of Zn were also studied. The EAFD with high Fe/Zn ratio (> 1, EAFD3) was richer in ZnFe2O4 and exhibited larger particle size than samples with low Fe/Zn ratio (< 1, EAFD1,2). ANOVA analysis revealed that the Fe/Zn ratios of the EAFDs also have a significant effect on Zn extraction (p < 0.005). Selective leaching of Zn with minimum Fe dissolution was obtained at pH > 4.5, regardless of other parameters or sample properties. The maximum Zn extraction rate obtained by the pH control was over 97% for EAFD1 and EAFD2, 76% for EAFD3, and 80% for EAFD4. The present results confirm that the Fe/Zn ratio can be used to identify EAFDs that permits facile and high-yield Zn recovery, and pH can be used as a process control factor for selective leaching of Zn regardless of any differences in the properties of the EAFD sample.

Recovery of Gallium and Indium from Zinc Residues by Acid Leaching (산침출에 의한 아연제련잔사로부터 갈륨 및 인디움의 회수)

  • 이화영;김성규;오종기
    • Resources Recycling
    • /
    • v.2 no.2
    • /
    • pp.22-26
    • /
    • 1993
  • The flowsheet for the recovery of gallium and indium from zinc residues has been established based on the sulfuric acid treatment. In comparison with the alkali treatment, the method proposed in this work allowed the recovery of indium together with gallium. The majority of iron contained in leach liquor could be removed through the two-stage neutrallization under oxidative or reductive atmosphere. Crude gallium and indium could be obtained through the alkali and/or acid leaching of the products generated from the above treatment. In addition, cementation of indium with zinc powders could also be used for the concentration of it from weak acid solutions.

  • PDF

Preparation of High Purity ZnO Powder from zinc-bearing waste by the Hydrometallurgical Process (함아연 폐기물로부터 습식법에 의한 고순도 ZnO 분말의 제조)

  • 이재천;이강인;유효신
    • Resources Recycling
    • /
    • v.1 no.1
    • /
    • pp.58-68
    • /
    • 1992
  • A process development for direct synthesis of high pure ZnO powders from zinc-bearing waste was investigated. This waste contains a 55% of zinc and it was extracted by the sulfuric acid(leaching). After removal of iron ion by precipitation from the zinc solution, the purification through a solvent extraction by the use of D2EHPA as an extractant was carried out. Then, loaded zinc in organic solution was stripped and precipitated simultaneously using a precipitant such as oxalic acid. Then, loaded zinc in organic solution was stripped and precipitated simulataneously using a precipitant such as oxalic acid. The synthesized $ZnC_2O_4$ powders by the precipitation stripping method was calcined to obtain more than 99.9% of ZnO powders. The effect of sulfuric acid concentration, leaching time, pulp density on the extraction of zinc was studied and the optimum conditions for the solvent extraction were obtained through the investigation of purification of zinc solution. The size, morphology and size distribution of synthesized $ZnC_2O_4$ powders were studied in terms of oxalic acid concentration, temperature, surfactant added, precipitation time, etc.

  • PDF

Recovery of Valuable Metals from Spent Alkaline Manganese Batteries using Sulfuric Acid (폐알카리 망간전지로부터 황산을 이용한 유가금속 회수)

  • Shin, Shun-Myung;Kang, Jin-Gu;Sohn, Jeong-Soo;Yang, Dong-Hyo
    • Applied Chemistry for Engineering
    • /
    • v.17 no.5
    • /
    • pp.517-520
    • /
    • 2006
  • The leaching behaviors of zinc and manganese oxides of spent alkaline manganeses battery in sulfuric acid solution by using $H_{2}O_{2}$ as a reducing agent were investigated according to the concentration of $H_{2}SO_{4}$, temperature, reaction time, and the amount of $H_{2}O_{2}$. The experimental results of zinc and manganeses dissolution rates obtained without a reducing agent at 100 g/L solid/liquid ratio, 3.0 M $H_{2}SO_{4}$, $60^{\circ}C$ and 200 r.p.m. were 97.7% and 43.5%, respectively. On the other hand, zinc and manganeses dissolution rates obtained by adding 30 mL reducing agent at $60^{\circ}C$ were 99.6% and 97.1%, respectively. The addition of the reducing agent increased the leaching of manganese by two-fold compared to the absence of a reducing agent. In case of adding over 30 mL $H_{2}O_{2}$, however, the leaching rates of zinc and manganeses were independent of reducing agent amounts.

Environmental Assessment of Vitrified Mine Tailing Aggregate Using Various Leaching Methods (고농도 중금속 함유 광미를 이용한 유리화 처리 골재의 장기 용출특성에 따른 환경안전성 평가)

  • Lee, Sang-Woo;Chun, Sa-Ho;Lee, Ki-Kang;Lee, Sanghoon
    • Journal of Environmental Impact Assessment
    • /
    • v.16 no.1
    • /
    • pp.35-43
    • /
    • 2007
  • Vitrified aggregates obtained by using mine tailings were evaluated using various leaching methods to assess their environmental safety. The leaching tests in this study include continuous batch leaching, Dutch availability leaching, pH-stat and tank diffusion test as well as TCLP (Toxicity Characteristic Leaching Procedure), which is commonly adopted. Vitrification technique has successfully been applied treating some solid wastes containing high level of heavy metals, such as EAF (Electric Arc Furnace) dust and mine tailings. The potentially most leachable element among trace metals was As and theoretically about 7% of total concentrations in the aggregate can be released under extreme condition. Zinc was leached about 4% and the other trace metals including Cd, Cr and Pb were hardly released from the vitrified mine tailing aggregate.

Dissolution Kinetics of Sphalerite in Aqueous Ferric Chloride Solution (염화제이철 수용액에서 섬아연광의 용해에 관한 속도론적 연구)

  • Yoo, Seung-Joon;Park, Hyung-Sang;Choi, Cheong-Song;So, Chil-Sup
    • Economic and Environmental Geology
    • /
    • v.26 no.3
    • /
    • pp.421-429
    • /
    • 1993
  • Dissolution reactions of chemical grade zinc sulfide and natural sphalerite were studied in ferric chloride solution as an oxidant. To enhance the leaching reaction, ultrasonic technique was employed in this investigation. For the reaction with pure zinc sulfide, chemical reaction was the rate limiting step in the range of low conversion irrespective of applying ultrasonic wave. And the diffusion through liquid film instead of diffusion through product layer of free sulfur was the rate determining step because ultrasonic vibration removes the product from reaction zone. In the case of sphalerite with the ultrasonic vibrator, it was found that inert mineral layer diffusion was the rate determining step, in which the elemental sulfurs formed were removed by the ultrasonic action. Experimental results showed that the ultrasonic technique proved to be the methods which can significants improve the leaching performance.

  • PDF

The Effect of pH on Citric Acid Leaching of Soil Contaminated with Heavy Metals (중금속(重金屬) 오염토양(汚染土壤)의 구산(枸酸) 침출(浸出)에 대한 pH의 영향(影響))

  • Jung, Kyungbae;Park, Hongki;Yoo, Kyoungkeun;Park, Jay Hyun;Choi, Ui Kyu
    • Resources Recycling
    • /
    • v.22 no.5
    • /
    • pp.13-19
    • /
    • 2013
  • The effect of pH on the citrate leaching behavior of heavy metal ion was investigated to develop an eco-friendly process for removing heavy metals from soil contaminated with copper, zinc, and lead. The leaching tests were performed using citrate solution with pH adjusted by mixing citric acid and sodium citrate under the following leaching conditions: particle size, under $75{\mu}m$; temperature, $50^{\circ}C$; citrate concentration, $1kmol/m^3$; pulp density, 5%; shaking speed, 100 rpm; leaching time, 1 hour. The difference of pH before and after the leaching test was not observed, and this result indicates the direct effect of hydrogen ion concentration on the leaching of metals was insignificant. The removal ratios of copper, zinc, and lead from the contaminated soil decreased with increasing pH. The thermodynamic calculation suggests that the leaching behaviors of metal ions were determined by two reactions; one is the reaction to form complex ions between heavy metal ions and citrate ion species, and the other is the reaction to form metal hydroxide between heavy metal ions and hydroxide ion.