Preparation of Yttria Stabilized zirconia Films by the Electrochemical Vapor Deposition (전기화학증착에 의한 이트리아 안정화 지르코니아 박막의 제조)

  • 정지원;박동원;전치훈;최병진;김대룡
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.5
    • /
    • pp.477-484
    • /
    • 1994
  • The yttria stabilized zirconia(YSZ) thin films for solid oxide fuel cell (SOFC) were fabricated by an electrochemical vapor deposition(EVD) technique using YCl3+ZrCl4+H2O gas system. The YSZ films were deposited under reduced pressure at the temperature of 1000~120$0^{\circ}C$ on the porous alumina substrates. The deposition rate, chemical composition and growth morphology were investigated by SEM, XRD, EDS. The growth rates of the films obeyed a parabolic rate law, representing that the growing process is controlled by an electrochemical transport through the YSZ film. The Y2O3 content of the films was about 10 mol%, equal to the composition of metal chloride reactant gases, approximately. The YSZ films were highly dense, the growing features showed columnar structure and surface morphologies were changed with the EVD conditions.

  • PDF

Crack-Free Fabrications of Yttria-Stabilized Zirconia Films Using Successive-Ionic-Layer-Adsorption-and-Reaction and Air-Spray Plus Method

  • Taeyoon Kim;Sangmoon Park
    • Korean Journal of Materials Research
    • /
    • v.34 no.2
    • /
    • pp.79-84
    • /
    • 2024
  • Thin films of yttria-stabilized zirconia (YSZ) nanoparticles were prepared using a low-temperature deposition and crystallization process involving successive ionic layer adsorption and reaction (SILAR) or SILAR-Air spray Plus (SILAR-A+) methods, coupled with hydrothermal (175 ℃) and furnace (500 ℃) post-annealing. The annealed YSZ films resulted in crystalline products, and their phases of monoclinic, tetragonal, and cubic were categorized through X-ray diffraction analysis. The morphologies of the as-prepared films, fabricated by SILAR and SILAR-A+ processes, including hydrothermal dehydration and annealing, were characterized by the degree of surface cracking using scanning electron microscopy images. Additionally, the thicknesses of the YSZ thin films were compared by removing diffusion layers such as spectator anions and water accumulated during the air spray plus process. Crack-free YSZ thin films were successfully fabricated on glass substrates using the SILAR-A+ method, followed by hydrothermal and furnace annealing, making them suitable for application in solid oxide fuel cells.

Optimization of anode and electrolyte microstructure for Solid Oxide Fuel Cells (고체산화물 연료전지 연료극 및 전해질 미세구조 최적화)

  • Noh, Jong Hyeok;Myung, Jae-ha
    • Korean Chemical Engineering Research
    • /
    • v.57 no.4
    • /
    • pp.525-530
    • /
    • 2019
  • The performance and stability of solid oxide fuel cells (SOFCs) depend on the microstructure of the electrode and electrolyte. In anode, porosity and pore distribution affect the active site and fuel gas transfer. In an electrolyte, density and thickness determine the ohmic resistance. To optimizing these conditions, using costly method cannot be a suitable research plan for aiming at commercialization. To solve these drawbacks, we made high performance unit cells with low cost and highly efficient ceramic processes. We selected the NiO-YSZ cermet that is a commercial anode material and used facile methods like die pressing and dip coating process. The porosity of anode was controlled by the amount of carbon black (CB) pore former from 10 wt% to 20 wt% and final sintering temperature from $1350^{\circ}C$ to $1450^{\circ}C$. To achieve a dense thin film electrolyte, the thickness and microstructure of electrolyte were controlled by changing the YSZ loading (vol%) of the slurry from 1 vol% to 5 vol. From results, we achieved the 40% porosity that is well known as an optimum value in Ni-YSZ anode, by adding 15wt% of CB and sintering at $1350^{\circ}C$. YSZ electrolyte thickness was controllable from $2{\mu}m$ to $28{\mu}m$ and dense microstructure is formed at 3vol% of YSZ loading via dip coating process. Finally, a unit cell composed of Ni-YSZ anode with 40% porosity, YSZ electrolyte with a $22{\mu}m$ thickness and LSM-YSZ cathode had a maximum power density of $1.426Wcm^{-2}$ at $800^{\circ}C$.

The Low-field Tunnel-type Magnetoresistance Characteristics of Thin Films Deposited on Different Substrate (기판 효과에 따른 저 자장 영역에서의 자기저항 효과에 관한 연구)

  • Lee, Hi-Min;Shim, In-Bo;Kim, Chul-Sung
    • Journal of the Korean Magnetics Society
    • /
    • v.12 no.2
    • /
    • pp.41-45
    • /
    • 2002
  • The low-field tunnel-type magnetoresistance (MR) properties of sol-gel derived $La_{0.7}Pb_{0.3}MnO_3(LPMO)$ thin film deposited on different substrate have been investigated. Polycrystalline thin films were fabricated by spin-coating on $SiO_2/Si(100)$ substrate and that with yttria-stabilized zirconia (YSZ) buffer layer, while c-axis-oriented thim film was grown on $LaAlO_3(001)$ (LAO) single crystal substrate. The full width half maximum (FWHM) of the rocking curve scan of LPMO/LAO film is $0.32^{\circ}$. Tunnel-type MR ratio is 0.52 % in $LPMO/SiO_2/Si$(100) film and that of $LPMO/YSZ/SiO_2/Si$(100) film is as high as 0.68 %, whereas that of LPMO/LAO(001) film is less than 0.4 % under the applied field of 500 Oe at 300 K. Well-pronounced MR hysteresis was registered with an MR peak in the vicinity of the coercive field. The low-field tunnel-type MR characteristics of thin films deposited on different substrates originates from the behavior of grain boundary properties.

Fabrication of $(La, Sr)MO_3$ (M=Mn or Co)/YSZ Nanocomposite Thin Film Electrodes for the Exhaust Gas Purification by a Chemically-Modified Sol-Gel Process

  • Hwang, H.J.;Moon, J.W.;Awano, M.;Maeda, K.
    • Journal of Powder Materials
    • /
    • v.8 no.3
    • /
    • pp.201-206
    • /
    • 2001
  • $>LaMnO_3$$(La, Sr)MO_3$, and $(La, Sr)MO_3/YSZ$ gel films were deposited by spin-coating technique on scandium-doped zirconia (YSZ) substrate using the precursor solution prepared from $La(O-i-C_3H_7)_3$, $Co(CH_3COO)_2$or $Mn(O-i-C_3H_7)_2$,2-methoxyethanol, and polyethylene glycol. By heat-treating the gel films, the electrochemical cells, $(La, Sr)MnO_3{\mid}ScSZ{\mid}Pt$ were fabricated. The effect of polyethylene glycol on the microstructure evolution of $$LaCoO_3and $LaMnO_3$thin films was investigated, and NOx decomposition characteristics of the electrochemical cells were investigated at $500^{\circ}C$ to $600^{\circ}C$. By applying a direct current to the $(La, Sr)MnO_3{\mid}ScSZ{\mid}Pt$ electrochemical cell, good NOx conversion rate could be obtained relatively at low current value even if excess oxygen is included in the reaction gas mixture.

  • PDF

The characteristics of Organic Thin Film Transistors with high-k dielectrics

  • Kim, Chang-Su;Kim, Woo-Jin;Jo, Sung-Jin;Baik, Hong-Koo
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2005.07b
    • /
    • pp.1288-1290
    • /
    • 2005
  • We report on the structural and electrical properties of amorphous Yttria-stabilized zirconia (YSZ) thin films which are the potential high-k gate dielectric material of organic thin film transistor (OTFT). To investigate the influence of the oxygen flow rate on the structural and electrical properties of the YSZ films, XRD, XPS, J-E, I-V were carried out in this work. Oxygen vacancies are expected to be the most predominant type of defect in metal-oxide dielectrics. The leakage current density decreased mainly because of the reduction of oxygen vacancies with increasing oxygen flow rate.

  • PDF

Bi-electrolyte Carbon Dioxide Gas Sensor Based on Paste Sodium-Beta Alumina and Yttria-stabilized Zirconia

  • Han, Hyeuk Jin;Park, Chong Ook
    • Journal of Sensor Science and Technology
    • /
    • v.23 no.3
    • /
    • pp.170-172
    • /
    • 2014
  • $CO_2$ sensor was used only one solid electrolyte in many cases. To improve the sensing characteristics of $CO_2$ sensors, solid electrolyte $CO_2$ sensor has been developed by bi-electrolyte type sensor using Na-Beta-alumina and YSZ. However, in many further studies, bi-electrolyte type sensor was made by pellet pressed by press machine and additional treatment for formation of interface. In the aspect of mass production, using thick film and additional treatment is not suitable. In this study, $CO_2$ sensor was fabricated by bi-electrolyte structure which was made by an NBA paste layer deposited on YSZ pellet and fired at $1650^{\circ}C$ for 2 hour. The formation of stable interface between YSZ and NBA were confirmed by SEM image. When the type IV electrochemical cell arrangement represented by $CO_2,O_2,Pt{\mid}Li_2CO_3-CaCO_3{\parallel}NBA{\parallel}YSZ{\mid}O_2,Pt$ is used to measure the $CO_2$ concentration in air. This sensor EMF should depend only on the concentration of $CO_2$ by logarithmic. Also, sensor shows $P_{CO_2}$ and EMF relationship like nerstian reaction at a temperature of $450^{\circ}C$.