Study on the Color Characteristics of Korean Red (한국산 적포도주의 색도 변화에 관한 연구 (II))

  • Lee, Jang-Eun;Shin, Yong-Sub;Sim, Jun-Ki;Kim, Sung-Soo;Koh, Kyung-Hee
    • Korean Journal of Food Science and Technology
    • /
    • v.34 no.2
    • /
    • pp.164-169
    • /
    • 2002
  • Five kinds of red wine from three different grape varieties, such as Gerbong (G), Campbell (C), Moru (M), Gerbong+Moru (70:30, GM), and Gerbong+Campbell(70:30, GC) were prepared in the year of 2000. The total phenolic content and color changes were monitored using hunter colorimeter and spectrophotometry methods during wine processing. The total phenolic content of Gerbong (G), Campbell (C), Moru (M), Gerbong+Moru(70:30, GM), and Gerbong+Campbell(70:30, GC) were 712.6 mg/L, 3472.9 mg/L, 2209.4 mg/L, 2019.4 mg/L, and 1184.5 mg/L, respectively. Between total phenolic content and hunter colorimeter value (L, a, and b) of red wine showed no significant difference, but that of spectrophotometry color value (hue and intensity) were significantly different (p<0.001). The total phenolic content, hue, and intensity values represented significantly different between grape varieties (p<0.01, p<0.001). the hue showed a negative correlation relationship $(r^2=0.8660,\;p<0.0001)$, and that of intensity was a positive $(r^2=0.8304,\;p<0.0001)$ between total phenolic contents. The total phenolic content of red wine could be estimated simply using these equations, $Y_{Total\;phenolic\;content\;(mg/L)}=3319.3-X_{Hue}/2208.36,\;and\;Y_{Total\;phenolic\;content\;(mg/L)}=1230.97-X_{intensity}/98.93$

Enzyme-Linked Immunosorbent Assay for Detection of Nivalenol (Nivaleno의 검출을 위한 효소 면역 측정법)

  • 손동화;이향범;곽보연;김수호;권창희
    • Journal of Food Hygiene and Safety
    • /
    • v.13 no.2
    • /
    • pp.129-134
    • /
    • 1998
  • To develop an enzyme-linked immunosorbent assay (ELISA) for nivalenol (NIV), we produced polyclonal antibodies against tetraacetyl nivalenol (Ac4-NIV) and established ELISA conditions. Ac4-NIV-hemisuccinate conjugated to bovine serum albumin (Ac4-NIV-HS-BSA) was immunized with Freund's adjuvants into rabbits subcutaneously several times. By use of the antiserum showing the highest titer and Ac4-NIV-HS-HRP conjugate, we established competitive direct ELISA (cdELISA). Standard curve of cdELISA showed that the detection range of Ac4-NIV was about 10~5,000 ng/ml (ppb). The cross-reactivities of the polyclonal antibody towards Ac4-NIV and acetyl T-2 were 100 and 70% respectively, and those towards NIV, deoxynivalenol, 3-acetyl deoxynivalenol, 15-acetyl deoxynivalenol, triacetyl deoxynivalenol, fusarenonX, and T-2 were less than 0.1%. When cdELISA was applied to NIV-spiked corns followed by extraction with 70% acetonitrile and acetylation with acetic anhydride in pyridine, the recovery rates of the Ac4-NIV were 108, 143, and 70% (average, 107%) in the levels of 100, 300, and 1,000 ng/g (ppb), respectively.

  • PDF

The Compound Refractive Lens for Hard X-ray Focusing

  • Choi, J.;Jung, J.;Park, S.;Kwon, T.
    • Journal of the Optical Society of Korea
    • /
    • v.11 no.2
    • /
    • pp.76-81
    • /
    • 2007
  • The compound refractive X-ray lens (CRL) for focusing hard X-rays is investigated to determine the parameters such as the focal length, the focal spot size, and spatial distribution at the focal spot using a simple theoretical calculations and CRLs fabricated by the self-assembly method. The number of individual compound lenses are defined for the given focal length of 1 m. The X-ray energy of 1 to 40 keV is used in the calculations. The CRL for focusing hard X-rays which generated from the X-ray tube is fabricated by nanoparticle-polymer composite in the form of circular concaves. The self-assembly method is applied to form the nanoaluminum-poly (methly meth-acrylate) composite and carbon-polymer composite CRL lenses. Aluminum nanoparticles of 100 nm and carbon microparticles are diffused in the polymer solution then the high gravity up to 6000G is applied in it to form the concave lens shape. X-ray energy at 8 keV is used for characterization of the composite CRLs. The FWHM of intensity for the fabricated nanoaluminium composite CRL system, N=10 is measured as 1.8 mm, which would give about $70{\mu}m$ in FWHM at 1 m of the focal length.

New Data on the Synthetic $Pt_{34}Sb_7$ and $Pt_3Sb$ Phases (합성화합물 $Pt_{34}Sb_7$$Pt_3Sb$에 대한 새로운 자료)

  • 김원사
    • Journal of the Mineralogical Society of Korea
    • /
    • v.1 no.1
    • /
    • pp.15-19
    • /
    • 1988
  • In the process of re-checking the phase relations of the Pt-Sb system the previously reported Pt4+Sb phase did not occur. Instead, Pt34Sb7 phase with an average chemical composition (wt%) Pt 89.3, Sb 11.4, total 100.7, has been newly found to exist, and the formula Pt34Sb7 has been tentatively assigned to it, It is pale brownish grey to yellowish grey under refloecting microscope and non-bireflectant, VHN100=225 (206-243). X-ray powder patterns are (d(I/Io)): 2.318(100), 2.293(100), 2.110(30), 1.440(50), 1.390(15), 1.283(5), 1.203(70) and 1.192(40)$\AA$. They are indexable on the basis of tertragonal cell with $\alpha$=3.948(3), c=16.85(1)$\AA$. A question whether the tetragonal Pt34Sb7 is the new phase or a polymorph of the cubic Pt4+Sb phase remains unclear and awaits better X-ray diffraction, electron microprobe analysis and DTA for the Pt4+Sb phase. The Pt3Sb phase reported to be of tetragonal symmetry has been confirmed to exist. It is greyish yellow in air and in oil, very weakly bireflectant, and weakly anisotropic. VHN25=216 (183-240). Its X-ray powder data have been successively indexed on a tetragonal cell with $\alpha$=3.9455(7), c=16.959(5)$\AA$.

  • PDF

Growth and electrical properties of $Sr_2$$({Ta_{1-x}},{Nb_x})_2$)$O_7$ thin films by RF sputtering (RF Sputtering을 이용한 $Sr_2$$({Ta_{1-x}},{Nb_x})_2$)$O_7$ 박막의 성장 및 전기적 특성)

  • In, Seung-Jin;Choi, Hoon-Sang;Lee, Kwan;Choi, In-Hoon
    • Korean Journal of Materials Research
    • /
    • v.11 no.5
    • /
    • pp.367-371
    • /
    • 2001
  • In this paper, theS $r_2$(T $a_{1-x}$ , N $b_{x}$)$_2$ $O_{7}$(STNO) films among ferroelectric materials having a low dielectric constant for metal-ferroelectric-semiconductor field effect transistor(MFS-FET) were discussed. The STNO thin films were deposited on p-type Si(100) at room temperature by co-sputtering with S $r_2$N $b_2$ $O_{7(SNO)}$ ceramic target and T $a_2$ $O_{5}$ ceramic target. The composition of STNO thin films was varied by adjusting the power ratios of SNO target and T $a_2$ $O_{5}$ target. The STNO films were annealed at 8$50^{\circ}C$, 90$0^{\circ}C$ and 9$50^{\circ}C$ temperature in oxygen ambient for 1 hour. The value of x has significantly influenced the structure and electrical properties of the STNO films. In the case of x= 0.4, the crystallinity of the STNO films annealed at 9$50^{\circ}C$ was observed well and the memory windows of the Pt/STNO/Si structure were 0.5-8.3 V at applied voltage of 3-9 V and leakage current density was 7.9$\times$10$_{08}$A/$\textrm{cm}^2$ at applied voltage of -5V.of -5V.V.V.

  • PDF

Amorphous Cr-Ti Texture-inducing Layer Underlying (002) Textured bcc-Cr alloy Seed Layer for FePt-C Based Heat-assisted Magnetic Recording Media

  • Jeon, Seong-Jae;Hinata, Shintaro;Saito, Shin
    • Journal of Magnetics
    • /
    • v.21 no.1
    • /
    • pp.35-39
    • /
    • 2016
  • $Cr_{100-x}Ti_x$ amorphous texture-inducing layers (TIL) were investigated to realize highly (002) oriented $L1_0$ FePt-C granular films through hetero-epitaxial growth on the (002) textured bcc-$Cr_{80}Mn_{20}$ seed layer (bcc-SL). As-deposited TILs showed the amorphous phase in Ti content of $30{\leq}x(at%){\leq}75$. Particularly, films with $40{\leq}x{\leq}60$ kept the amorphous phase against the heat treatment over $600^{\circ}C$. It was found that preference of the crystallographic texture for bcc-SLs is directly affected by the structural phase of TILs. (002) crystallographic texture was realized in bcc-SLs deposited on the amorphous TILs ($40{\leq}x{\leq}70$), whereas (110) texture was formed in bcc-SLs overlying on crystalline TILs (x < 30 and x > 70). Correlation between the angular distribution of (002) crystal orientation of bcc-SL evaluated by full width at half maximum of (002) diffraction (FWHM) and a grain diameter of bcc-SL indicated that while the development of the lateral growth for bcc-SL grain reduces FWHM, crystallization of amorphous TILs hinders FWHM. $L1_0$ FePt-C granular films were fabricated under the substrate heating process over $600^{\circ}C$ with having different FWHM of bcc-SL. Hysteresis loops showed that squareness ($M_r/M_s$) of the films increased from 0.87 to 0.95 when FWHM of bcc-SL decreased from $13.7^{\circ}$ to $3.8^{\circ}$. It is suggested that the reduction of (002) FWHM affects to the overlying MgO film as well as FePt-C granular film by means of the hetero-epitaxial growth.

The characteristic study of hybrid X-ray detector using ZnS:Ag phosphor (ZnS:Ag phosphor를 이용한 hybrid 형 X-ray detector 특성 연구)

  • Park, Ji-Koon;Gang, Sang-Sik;Lee, Dong-Gil;Cha, Byeong-Yeol;Nam, Sang-Hee;Choi, Heung-Kook
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.05b
    • /
    • pp.27-30
    • /
    • 2002
  • Photoconductor for direct detection flat-panel imager present a great materials challenge, since their requirements include high X -ray absorption, ionization and charge collection, low leakage current and large area deposition. Selenium is practical material. But it needs high thickness and high voltage in selenium for high ionization rate. We report comparative studies of detector sensitivity. One is an a-Se with $70{\mu}m$ thickness on glass. The other has hybrid layer of depositting ZnS phosphor with $100{\mu}m$ on a-Se. The leakage current of hybrid is similar to it of a-Se, but photocurrent is lager than a-Se. Both of them have high spatial resolution, but hybrid has higher sensitivity than a-Se at comparable bias voltage.

  • PDF

Design of a specimen holder for living cell in the soft X-ray microscopy (연 X-선 현미경을 위한 생체시료 고정장치 설계)

  • 권영만;김경우;윤권하
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2003.06a
    • /
    • pp.705-708
    • /
    • 2003
  • To observe a hydrated biological specimen, an environmental chamber was necessary to keep the specimen in a wet state under vacuum surroundings. The specimen holder is as follows designed consequently. The specimen holder consisted of two Si wafers, the centers of which were Si$_3$N$_4$(100nm thickness) windows of a 0.3mm square. The windows were made by a photo-lithographic method. The transmission of a window at 400eV is about 70%. A hydrated biological specimen was put between the two windows. When the chamber was closed, two wafers were contact at the metal mesh by the pressure of O-rings, and the specimen holder moved by the three micrometers.

  • PDF

Fabrication of High-Tc Superconducting $YBa_2Cu_3O_{7-x}$ Thin Films by Off-Axis RF Magnetron Sputtering (Off-Axis RF 마그네트론 스퍼터링에 의한 $YBa_2Cu_3O_{7-x}$ 고온 초전도 박막의 제조)

  • 성건용;서정대;강광용;장순호
    • Journal of the Korean Ceramic Society
    • /
    • v.28 no.3
    • /
    • pp.243-251
    • /
    • 1991
  • High-Tc YBa2Cu3O7-x superconducting thin films have been prepared by single-target off-axis RF magnetron sputtering. Optimal ratio of Y : Ba : Cu of the single-target was determined as 1 : 1.65 : 3.35 in order to obtain the stoichiometric films. Tc, crystalline phase, and microstructures of the surface and cross-section of the ex-situ YBa2Cu3O7-x thin films on MgO(100) had a Tc, zero of 80K, and the films on LaAlO3/Si had a Tc, on-set of 90 K and a Tc, zero of 70 K.

  • PDF

The Effect of La Concentration on The PLZT(x/30/70) Thin Films for NVRAM Memory Device (비휘발성 메모리 소자를 위한 PLZT(x/30/70) 박막에 대한 La 농도변화의 효과)

  • 김성진;윤영섭
    • Proceedings of the IEEK Conference
    • /
    • 2000.06b
    • /
    • pp.28-31
    • /
    • 2000
  • In this paper, the effects of La addition of PLZT(x/30/70) thin films Prepared by sol-gel method are investigated for NVFRAM application. The tetragonality (c/a), the grain size, and the surface roughness of PLZT thin films decrease with an increase of La concentration. As the La concentration increases, the dielectric constants at 10 kHz increase from 450 to 600, while the loss tangent decrease from 0.075 to 0.025. Also, the leakage current density at 100kV/cm decrease from 5.83$\times$10$^{-7}$ to 1.38$\times$10$^{-7}$ 4/$\textrm{cm}^2$. In the results of hysteresis loops measured at $\pm$170kV/cm, the remanent polarization and the coercive field of PLZT thin films with La concentration from 0 to 10㏖% decrease from 20.8 to 10.5 $\mu$C/cm and from 54.48 to 32.12kV/cm, respectively. After a fatigue measurement by applying 10$^{9}$ square pulses with $\pm$5V, the remanent polarizations of PLZT thin films with 0 and 10㏖% La concentration decrease about 64 and 42 % from initial state. In the results of retention measurement after 10$^{5}$ s, PLZT thin films with 0 to 10mo1% La concentration show that the remanent polarization is decreased about 43% and 9% from initial state, respectively.

  • PDF