• 제목/요약/키워드: Wrought

검색결과 106건 처리시간 0.034초

AZ31과 AZ91의 마찰교반용접부 결정립 크기 제어 (Control of Grain Size on Friction Stir Welded AZ31 and AZ91)

  • 권기수;이창우;김목순;;김정한
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2007년 추계학술발표대회 개요집
    • /
    • pp.328-331
    • /
    • 2007
  • It was carried out to evaluate microstructure and mechanical properties of friction stir welded(FSW) on magnesium alloys. Two types magnesium alloy was used in this work, AZ31 wrought and AZ91 cast magnesium alloy. Microstructure near the weld zone showed general weld structures such as stir zone(SZ), thermo-mechanically affected zone(TMAZ) and heat affected zone(HAZ). In the AZ91 alloy, the SZ had a fine grain size and $\beta$ phase particles which were well distributed in matrix. It was characterized to redistribute by partial or full re-solution of the $\beta$ phase which is coarse in base metal during FSW processing. The hardness of the SZ slightly increase than the base metal in AZ31 Mg alloy.

  • PDF

분말고속도공구강을 활용한 베어링 레이스 열간 단조 금형의 수명 및 기계적 특성 (Life and Mechanical Properties of Hot Former Die for Bearing Race using P/M High Speed Steel)

  • 홍성연;배종수
    • 한국분말재료학회지
    • /
    • 제14권6호
    • /
    • pp.367-371
    • /
    • 2007
  • P/M high speed steel (1.26% C, 4.42% Cr, 6.54% W, 4.92% Mo, 3.21 % V, 8.77% Co, bal. Fe) was applied to hot former die. It showed that the die life became 2.7 times higher than that of cast/wrought SKH 55 tool steel which is commercially used. The increase of die life was corresponding to the improved hardness and transverse rupture strength of PM high speed steel due to the finer grain and carbide as well as the uniform carbide distribution. The P/M high speed steel with the promoted die life could be an alternative to the conventional SKH55.

Al-Mg-(Ca) 합금에서 결정립의 열적 안정성 (Thermal Stability of Grains in Al-Mg-(Ca) Alloys)

  • 전중환
    • 열처리공학회지
    • /
    • 제25권4호
    • /
    • pp.175-180
    • /
    • 2012
  • Role of Ca in grain growth behavior has been investigated in hot-rolled Al-3%Mg and Al-3%Mg-0.5%Ca wrought alloys. When annealed for 1 hr from 723 to 823 K, grain size of the Al-3%Mg alloy increased rapidly above 723 K, whereas grains were relatively stable up to 773 K for the Ca-containing alloy. Grain homogeneity of the Ca-containing alloy was better than that of the Ca-free alloy both in hot-rolled and annealed states. Calculated activation energies for grain growth were 77.6 and 85.9 kJ/mole in the range of 723 to 823 K for the alloys with 0 and 0.5%Ca, respectively. Taking SEM images and EDS results into account, enhanced thermal stability in response to Ca addition would be associated with Al4Ca compounds located along the grain boundaries, which eventually play a role in restricting grain growth at elevated temperatures.

열처리온도 및 시간에 따른 알루미늄 주조재의 고상확산 접합 특성 (Solid State Diffusion Brazing of the Aluminum Alloy Castings According to the Heat Treatment Conditions)

  • 선주현;신승용;홍주화
    • 열처리공학회지
    • /
    • 제21권6호
    • /
    • pp.300-306
    • /
    • 2008
  • Solid state diffusion brazing of aluminum castings (AC4C) and wrought alloys (Al6061) was conducted in order to improve thermal conductivity and temperature uniformity of the aluminum heater which was generally fabricated by casting method. Tensile strength and thermal conductivity are raised with increasing brazing temperature, obtaining 122.5 MPa and $206W/m{\cdot}K$ at $540^{\circ}C$ 5hrs brazing conditions, respectively. The diffusion brazed heater, shows maximum temperature difference of $4^{\circ}C$, exhibits a enhanced temperature uniformity compared with the cast heater having the maximum temperature difference of $11^{\circ}C$.

Effect of Oxygen on Mechanical Properties of Metal Injection Molded Titanium and Titanium Alloy

  • Doi, Kenji;Hanami, Kazuki;Tanaka, Hideki;Teraoka, Tsuneo;Terauchi, Shuntaro
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.771-772
    • /
    • 2006
  • Mechanical properties of metal injection molded titanium and titanium alloy parts were investigated in this study. Material powders with low oxygen content and spherical shape were obtained by electrode induction-melting gas atomization which could melt and atomize titanium and titanium alloy bars with no touch on crucible or tundish. Tensile specimens were fabricated from obtained powders by metal injection molding process. Tensile strength of the specimens increases with increasing oxygen content. This result corresponds to a tendency of wrought metal.

  • PDF

Establishment of Process of Manufacture of Ti-6Al-4V Alloy Sintering Body by MIM

  • Otsuka, A.;Suzuki, K.;Achikita, M.
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.759-760
    • /
    • 2006
  • Ti-6Al-4V has low specific gravity, high corrosion resistance and superior mechanical properties but it is very difficult to control oxygen content in MIM process. It is necessary to use powders with coarse particle size to decrease oxygen content of powders, so feedstocks with poor fluidity and sintered bodies with lower density are obtained in such cases. Fine titanium hydride-dehydride powders were blended with atomized powders to accomplish higher fluidity and sintered density. Sintered bodies had higher sintered density and mechanical properties equivalent to those of wrought materials by controlling oxygen content less than 0.35mass%.

  • PDF

분말 압연에 의해 제조된 퍼말로이(PB, PC)의 자성 특성 (Magnetic Properties of Permalloy(PB, PC) Strips Fabricated by Powder Rolling Process)

  • 이동원
    • 한국분말재료학회지
    • /
    • 제3권1호
    • /
    • pp.13-24
    • /
    • 1996
  • Two grades of Permalloy strips, Fe-45Ni(PB) and Fe-78Ni-4Mo-5Cu(PC) were fabricated by powder rolling process from elemental powder mixtures. The roll compacted green strips were sintered, homogenized, cold rolled with or without an intermediate annealing and finally heat treated to measure magnetic properties. For a given thickness reduction, rolling with an intermediate annealing was found more effective to achieve a full densification with no visible micropores and also to obtain better magnetic properties. Increasing the final rolling reduction also produced a marked improvement of the magnetic properties whereas the cooling rate during the final heat treatment has little effect in both grades. Addition of a small amount, 0.4% Mn slightly degraded the properties. As an overall, The PM strips produced via powder rolling yielded the similar soft magnetic properties to the corresponding commercial grades produced via wrought processing.

  • PDF

자동차 경량화를 위한 다이캐스팅용 알루미늄합금 브레이크 페달의 강도해석 (Strength Analysis of Die-cast Aluminum-alloy Brake Pedals for use in Lightweight Cars)

  • 조승현;장준영
    • 한국생산제조학회지
    • /
    • 제25권2호
    • /
    • pp.138-142
    • /
    • 2016
  • In this study, a strength analysis was performed to assess die-cast aluminum alloy brake pedals as an improved alternative to wrought alloys. Aluminum brake pedal shapes are considered to be suitable for the die-casting process. The strength criterion of Volvo trucks was used as the criterion for the pedal strength. The results of this analysis showed that the frame thickness of the aluminum brake pedal must be increased from 12 mm to 18 mm to have a strength superior to that of a steel brake pedal. Additionally, the stress and weight of the aluminum brake pedal were found to be approximately 24% and 26% lower than those of the steel brake pedal, respectively. Mounting tests and strength assessments verified that the proposed die-cast aluminum alloy brake pedal demonstrated sufficient strength.

국소의치금속상과 Fe-Cr계 wire를 soldering 할때 발생한 계면의 성분변화 (Interfacial Elemental Change When Soldering the Nico-crally and Fe-Cr-Ni Alloy)

  • 조성암;고현권
    • 대한치과보철학회지
    • /
    • 제27권1호
    • /
    • pp.49-54
    • /
    • 1989
  • The purpose of this study was to investigate the interfacial elemental change when solding the Ni-Co-Cr dental removable partial denture alloy and Fe-Cr-Ni wrought wire alloy with Ag-Cu-Zu Silver solder, by EDXA, EPMA, to investigate the appropriateness of clinical usefullness for repair the fractured clasps of removable partial dentive. The result of this study was as follows: 1. The Ni element of major component of Ticonium penetrate into the silver solder 2. The movement Age element of silver solder into Fe-Cr-Ni wire was not significant, by EDXA and EPMA.

  • PDF

Research on Aesthetic Characteristics of Fabric Expression Technique of Art to Wear - Focusing on Art to Wear artists in the U.S.A. -

  • Jin, Kyung-Ok
    • 패션비즈니스
    • /
    • 제11권3호
    • /
    • pp.133-151
    • /
    • 2007
  • The role of fabric now directly related with the expression of the beauty of clothing and it provides new and creative ideas. This study was aimed at reviewing basic data that can be used in systematic design development through fabric expression for today's fashion designers who must study unique, original fashion design development. For systematic development of design technique through fabric expression, fabric expression methods and characteristics, aesthetic characteristics and fabric design of 'art to wear' were reviewed and the results are as follows. First, the highly wrought fabric expression of art to wear was confirmed to be comprehending a message within itself. Second, aesthetic characteristics of fabric expression used in art to wear can be classified as decorativeness, extensity, 2-D pictorialness, handicraft, compounding and rearrangement, and 3-D characteristics. Third, the 6 aesthetic characteristics have unique design features and aesthetic categories. The understanding the fabric expression techniques through study on the classification of the fabric expression in 'art to wear' is expected to be extended to proposition of creative direction and inspiration of modern fashion.