Studies on the Effect of Diffusion Process to Decay Resistance of Mine Props (간역(簡易) 처리법(處理法)에 의한 갱목(坑木)의 내부효력(耐腐效力)에 관(關)한 연구(硏究))

  • Shim, Chong-Supp;Shin, Dong-So;Jung, Hee-Suk
    • Journal of the Korean Wood Science and Technology
    • /
    • v.10 no.3
    • /
    • pp.166-166
    • /
    • 1982
  • This study has been made to make an observation regarding present status of the coal mine props which is desperately needed for coal production, despite of great shortage of the timber resources in this country, and investigate the effects of diffusion process on the decay resistances of the mine props as applied preservatives of Malenit and chromated zinc chloride. The results are as follows. 1. Present status of the coal mine props Total demand of coal mine props in the year of 1975 was approximately 456 thousand cubic meters. The main species used for mine props are conifer (mainly Pinus densiflora) and hardwood (mainly Quercus). Portions between them are half and half. With non fixed specification, wide varieties of timber in size and form are used. And volume of wood used per ton of coal production shows also wide range from 0.017 cubic meter to 0.03 cubic meter. 2. Decay resistance test a) The oven dry weight decreased between untreated specimen and treated specimen has not shown any significantly, although it has shown some differences in average values between them. It may be caused by the shorter length of the test. b) The strength of compression test between untreated specimen and treated specimen has also shown the same results as shown in case of weight decrease. Reasons assumed are the same. c) The amounts of the extractives in one percent of sodium hydroxide (NaOH) between untreated and treated specimen have shown the large value in case of untreated specimen than that of treated. 3. The economical benifit between untreated and treated wood when applied in field has seen better in long tenn base in case of treated wood, although the primary cost of treated wood add a little bit more cost than that of the untreated wood.

  • PDF

Measurment of Copper Concentration in ACQ, CUAZ, and CB-HDO Solutions by Using a Spectrophotometer

  • Ra, Jong-Bum
    • Journal of the Korean Wood Science and Technology
    • /
    • v.38 no.5
    • /
    • pp.450-456
    • /
    • 2010
  • This research was performed to develop the simple techniques to predict the copper concentration in alkaline copper quat (ACQ), copper azole (CUAZ), and bis-(N-cyclohexyl-diazeniumdioxy)-copper (CB-HDO) solutions. Two simple methods measuring the color due to copper compounds were evaluated by using a spectrophotometer. One is to directly measure the color of the preservative solutions. The other is to measure the color developed on the surface of a treated sample with the preservatives. The $L^*$ of the measured color values appeared to be the most sensitive to the change of copper concentration. The $a^*$ values of the preservative solutions tended to be decreased at above a certain concentration condition, and the $b^*$ values showed no trend with the concentration of copper compounds in preservative solutions. The surface color of the treated samples were changed from bluish to greenish as time passed. Both methods showed the high $R^2$ values of the regression models determined by using the lightness, which suggested that the methods might be applicable in preservative-treatment mills for the easy and fast prediction of the copper concentration.

Evaluation of Deterioration of Larix kaempferi Wood Heat-treated by Superheated Steam through Field Decay Test for 12 Months (12개월 야외 내후성 시험에 의한 과열증기 열처리된 낙엽송재의 열화 평가)

  • Park, Yonggun;Han, Yeonjung;Park, Jun-Ho;Chung, Hyunwoo;Kim, Hyunbin;Yang, Sang-Yun;Chang, Yoon-Seong;Yeo, Hwanmyeong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.46 no.5
    • /
    • pp.497-510
    • /
    • 2018
  • In this study, the decay resistance of larch wood, which was heat treated by superheated steam, was evaluated by the field decay test. During the field decay test of 12 months, non-treated wood has been severely damaged by termite, however, no visible damage has occurred in the preservative-treated wood and superheated steam heat-treated wood. Results of field decay test showed approximately 5% mass loss of the non-treated wood and the preservative-treated wood, and approximately 1% mass loss of the superheated steam heat-treated wood. After the field decay test for 12 months, the residual amount of preservatives remaining in the preservative-treated wood was lower than that before the field decay test. It was considered that the preservative was partially eluted during the field decay test, and the mass loss of the preservative-treated wood was thought to be similar to that of the non-treated wood. Through this study and additional long-term monitoring test, superheated steam heat treatment can be considered to be an environmental-friendly method to enhance the decay resistance of wood against rot fungi and/or insect without chemical treatment such as preservative injection.

Current Researches on the Protection of Exterior Wood from Weathering (목재의 기상열화 방지에 관한 최근의 연구 동향)

  • Kim, Yeong-Suk
    • Journal of the Korean Wood Science and Technology
    • /
    • v.46 no.5
    • /
    • pp.449-470
    • /
    • 2018
  • A review of research trends on wood surface protection for exterior use obtained the following conclusions: It has been reported that inorganic compounds such as chrome and copper used as wood preservatives can protect wood from weathering. It has been shown that precoating with hydrophobic substances such as wax and oil, UV absorbers, and HALS (Hindered Amine Light Stabilizers) enhances weathering resistance on the surface of ACQ-treated wood. Opaque coatings of paint/stains and semitransparent stains on the surface of preservative treated wood can increase the synergistic effects on prevention of weathering deterioration. Also the need for repainting periodically for the protection of the preservative treated wood surface has also been suggested. ZnO or $TiO_2$ of fine particles, metal ions such as Co, Cr, Fe, Mn, Ni and Ti, and UV absorbers such as tris-resorcinol triazine derivatives, triazine and benzotriazole were introduced as additives for preventing UV in the transparent coating on wood. Several reports showed that chemical modification such as methylation, acetylation, or alkylations have made some increases the effects of preventing weathering with the increasing weight gain of chemical formulas. In heat-treated wood, there were various contradictory reports on the resistance of weathering, and there were some other reports emphasizing the necessity of painting with UV resistance, which leads to the necessity of more advanced studies.

Heavy Metals of Landfilled Biomass and Their Environmental Standard, Including CCA-treated Wood for Eco-housing Materials (방부처리 목재를 포함한 토양매립 바이오메스의 중금속 함량과 안전성 문제)

  • Lim, Kie-Pyo;Lee, Jong-Tak;Bum, Jung-Won
    • Journal of the Korean Wood Science and Technology
    • /
    • v.34 no.4
    • /
    • pp.37-45
    • /
    • 2006
  • Recently, wood-framed houses has been built in the Korea for pension. Wood is good material for human healthy, while the construction lumbers are treated with preservative such as CCA (chromated copper arsenate), which contain some toxic elements for human body. However, if the waste woody biomass treated with various heavy metals, which has been collected from house construction or demolition, was fired in the field, and incinerated or landfilled after mass collection, such components will result in the toxic air pollutants in the burning or land fills, and spreaded into other areas. So the careful selection of wood and chemicals are required in advance for house construction, in particular, for environment-friendly housings. Therefore, this study was carried out to determine the content of toxic heavy metals in woody materials such as domestic hinoki and imported hemlock treated with CCA for housing materials, and the post-treated wood components such as organic fertilizer, sludge, dry-distilled charcoal and carbonized charcoal, to be returned finally into soil. The results are as follows. 1) The chemical analysis of toxic trace elements in various solid biomass required accurate control and management of laboratory environment, and reagents and water used, because of the error of data due to various foreign substances added in various processing and transporting steps. So a systematic analyzers was necessary to monitor the toxic pollutants of construction materials. 2) In particular, the biomass treated with industrial biological or thermal conditions such as sludge or charcoals was not fully dissolvable after third addition of $HNO_3$ and HF. 3) The natural woody materials such as organic fertilizer, sludge. and charcoals without any treatment of preservatives or heavy metal components were nontoxic in landfill because of the standard of organic fertilizers, even after thermal or biological treatments. 4) The CC A-treated wood for making the construction wood durable should not be landfilled, because of its higher contents of toxic metals than the criterion of organic fertilizer for agriculture or of natural environment. So the demolished waste should be treated separately from municipal wastes.

Influence of Copper Azole Retention Level to Wood Decay (목재 내 Copper Azole 보유량이 목재부후에 미치는 영향)

  • Lee, Hyun-Mi;Son, Dong-Won;Lee, Han-Sol;Hwang, Won-Joung
    • Journal of the Korean Wood Science and Technology
    • /
    • v.43 no.1
    • /
    • pp.112-121
    • /
    • 2015
  • In this study, Copper Azole (CuAz), a domestically available wood preservative for pressure treatment, was employed to perform an experimental research on its infiltration and decay properties in Japanese Red Pine. Test specimens were pressure-injected with CuAz-2 preservative to measure its preservative effectiveness, and then its impact on weight and mass losses. Furthermore, wood specimens were treated with CuAz-2 preservatives of various concentration levels before they were decayed with brown-rot-fungi in order to observe decay properties on light microscope (LM) and field emission scanning electron microscope (FE-SEM). As a result, untreated specimen by Fomitopsis palustris showed the mass loss of more than 40%, and the value of preservative effectiveness of CuAz-2 by indoor decay was $1,73-3.32kg/m^3$. The concentration levels of CuAz-2 preservative were shown to cause significant variations in terms of decay progresses in the cross section, radial section, and tangential section. By contrast, untreated specimens had underwent serious decays in early wood, late wood, longitudinal resin canals, and ray, which led to vertical destruction of wood texture. As for the radial section, ray tracheid, ray parenchyma cell, and window like pits were decayed and destroyed. In the case of tangential section, uniseriate rays and vertical resin canals were seriously decayed. In conclusion, this study indicates that the adequacy of the current CuAz injection amount should be reviewed in the domestic environment because there are significantly different decays at different decay conditions.

A Study on the Fabrication of the Laminated Wood Composed of Poplar and Larch (포푸라와 일본잎갈나무의 집성재 제조에 관한 연구)

  • Jo, Jae-Myeong;Kang, Sun-Goo;Kim, Ki-Hyeon;Chung, Byeong-Jae
    • Journal of the Korean Wood Science and Technology
    • /
    • v.2 no.2
    • /
    • pp.25-31
    • /
    • 1974
  • 1. Various gluing qualities applying Resorcinol Plyophen #6000 were studied on aiming the strength relationships of laminated woods resulted by single species [poplar (Populus deltoides), larch(Larix leptolepis)], mixed species of (poplar and larch), preservatives, treated poplar the scarf joint with mixed species of poplar and larch and the scarf joint treated with preservatives. 1. 1 On the block shear and on the DVL tension test, the mean wood failure ratio showed an excellent value i.e., above 65% and the tangential strength for larch was higher than that of radial, but it was reversed for poplar as shown in Tables 1 and 2. 1. 2 The lamina treated with Na-PCP reduced slightly the strength but the limited strength allowed for manufacturing laminated wood was not influenced by treating Na-PCP as shown in Tables 3 and 4. 1. 3 The safe scarf ratio in the plane scarf joint was above 1/12 for larch and 1/6 for poplar regard less of the chemical treatment or untreatment as shown in Tables. 5, 6, 7 and 8. 2. In the normal and boiled state, the gluing quality of the laminated wood composed of single[poplar (Populus deltoides), larch (Larix leptolepis)] and double species (poplar and larch) glued with Resorcinol Plyophen #6000 were measured as follow, and also represented the delamination of the same laminated wood. 2.1 The normal block shear strength of the straight and curved laminated wood (in life size) were more than three times of the standards adhesion strength. And, the value of the boiled stock was decreased to one half of the standard shear adhesion strength, but it was more than twice the standard strength for the boiled stock. Thus, it was recognized that the water resistance of the Resorcinol Plyophen #6000 was very high as shown in Tables 9 and 10. 2. 2 The delamination ratio of the straight and curved laminated woods in respect of their composition were decraesed, in turn, in the following order i. e., larch, mixed stock (larch+poplar) and poplar. The maximum value represented by the larch was 3.5% but it was below the limited value as shown in Table 11. 3. The various strengthes i.e., compressive, bending and adhesion obtainted by the straight laminaced wood which were constructed by five plies of single and double species of lamina i. e., larch (Larix leptolepis) and poplar (Populus euramericana), glued with urea resin were shown as follows: 3. 1 If desired a higher strength of architectural laminated wood composed of poplar (P) and larch (L), the combination of the laminas should be arranged as follows, L+P+L+P+L as shown in Table 12. 3.2 The strength of laminated wood composed of laminas which included pith and knots was conside rably decreased than that of clear lamina as shown Table 13. 3.3 The shear strength of the FPL block of the straight laminated wood constructed by the same species which were glued with urea adhesives was more than twice the limited adhesion strength, thus it makes possible to use it for interior constructional stock.

  • PDF

International Movement of Biocides Regulation (Biocides의 국제적 규제동향)

  • 박정규
    • Environmental Analysis Health and Toxicology
    • /
    • v.15 no.4
    • /
    • pp.115-122
    • /
    • 2000
  • Biocides, or non-agricultural pesticides, are a broad class of chemical. They are including biological agents used to disinfect/sanitize, pesticides for non-agricultural use, wood preservatives, antifoulants, etc. Since the early 1980s, many adverse effects of biocides to human health and ecosystem have been found in the world. Especially, antifouling biocide like TBT caused serious toxic effects on the marine organisms. Therefore, OECD began to work on biocides in mid 1996 to help Member countries co-operate in the assessment and registration of these products. EU also announced the Biocidal Products Directive (BPD, 98/8/EC) in 1998 to harmonize regulatory approaches to allow EU countries to conduct evaluations of biocides more efficiently. Korea just start to consider of biocides regulation. Some biocides products are regulated, but not all the biocides which are using in Korea. Therefore, we need to make a appropriate regulation for the all biocides categories. In addition, there are necessary to develop risk assessment tools, to survey the use pattern and amount, to research on the ecosystem contamination by the biocides .

  • PDF

Decay Efficacies of Plywoods Manufactured by ACQ-treated Veneers of Domestic Softwood and Hardwood Species

  • Suh, Jin Suk;Lee, Hyun Mi;Hwang, Won Jung;Hwang, Sung Wook;Lee, Dong Heub;Park, Sang Bum
    • Journal of the Korea Furniture Society
    • /
    • v.25 no.3
    • /
    • pp.233-237
    • /
    • 2014
  • The eco-friendly preservatives such as ACQ or CUAZ have been used in landscape architectural facilities these days. In this study, the decay efficacies of ACQ treatments were evaluated according to domestic veneer species, concentration of ACQ, weathering test, adhesive type, and fungus type. In case of veneer species, hinoki cypress and yellow poplar showed the highest and lowest decay resistance, respectively. And the decay resistance appeared to be greater in plywoods bonded by resorcinol resin-bonded plywood and non-weathering treated plywood than polyurethane resin-bonded plywood and weathering treated plywood.

  • PDF

Treatment Characteristics of Japanese Larch Heartwood with CCA or CCFZ and Improving its CCA Treatability by Incising Techniques (낙엽송(落葉松) 심재(心材)의 CCA와 CCFZ 처리특성(處理特性) 및 자상처리(刺傷處理)에 의(依)한 CCA 처리도(處理度) 개선(改善))

  • Kang, Sung-Mo;Kim, Gyu-Hyeok;Paik, Ki-Hyon
    • Journal of the Korean Wood Science and Technology
    • /
    • v.23 no.4
    • /
    • pp.60-66
    • /
    • 1995
  • The treatability of Japanese larch heartwood was assessed by pressure treatment of non-incised dimension material with CCA or CCFZ. The effectiveness of incising(conventional, high density, and needle incising) for improving CCA treatability on refractory Japanese larch heartwood was also investigated. Preservative retention and penetration were somewhat greater with CCFZ treatment, although those was generally poor in both preservatives. The retention gradients for both CCA and CCFZ-treated stock were essentially the same shape. Treatment of non-incised material with CCA acheived the recommended treatability for using treated wood at the regions of hazard class H2 in the Japanese Agricultural Standards. However, Japanese larch heartwood would require incising as a pretreatment for enhancing treatability, if CCA-treated larch is intended to be used at the regions of hazard class H3 and H4. As expected, incising resulted in a considerable improvement of preservative treatability, particularly penetration, and the effect of incising on the improvement of treatability was excellent at the sequence of needle incising, high density incising, and conventional incising. Among incising techniques investigated in this study, high density and needle incising enhanced CCA treatability beyond the point where it did meet a minimum requirements specified by the Japanese Agricultural Standards for using CCA-treated Japanese larch at the regions of hazard class H3 and even H4.

  • PDF