Review on Water Vapor Diffusion through Wood Adhesive Layer

  • Omar Saber ZINAD;Csilla CSIHA
    • Journal of the Korean Wood Science and Technology
    • /
    • v.52 no.4
    • /
    • pp.301-318
    • /
    • 2024
  • Contrary to other materials like metals, glass, etc., wood continuously interacts with the environment, increasing and decreasing its moisture content according to the humidity of the air and changing its dimensions by swelling or shrinking. Water diffusion through laminated solid wood is crucial in wood bonding processes. The adhesive layer might block the diffusion if the water vapor diffusion is perpendicular to the bond line. As a result of this blockage, different proportions of deformation appear on the two sides of the bond line, which causes stresses in the bonded assembly. The question arises of how long the bonded structure will keep its integrity due to moisture diffusion blockage, inevitable tensions appearing in the glue line, and how these stresses could be avoided. With cross laminated timber (CLT) solid wood panel production, this question gains new importance. Despite the relevance, only a limited number of publications are available. Comprehensive research would also be necessary considering both the molecular structure and diffusion properties of the adhesive adjusted to the wood species (covering possible substituting wood species, too). Overall, this review serves as a resource for enhancing our understanding of water vapor diffusion through wood adhesive layers and provides insights that have implications for reducing stresses in bonded wood assemblies and the performance of the bonded group over time. Furthermore, identifying knowledge gaps is necessary to establish the basis for investigating the diffusion property of CLT panels.

Study on the Neutral Axis of Glulam and its Mechanical Properties (적층목질재(積層木質材)(Glulam)의 중립축(中立軸)과 강도적(强度的) 성질(性質)에 관한 연구(硏究))

  • Park, Heon
    • Journal of the Korean Wood Science and Technology
    • /
    • v.18 no.3
    • /
    • pp.42-52
    • /
    • 1990
  • In this study, thick 24mm glulams were composed of thick. 3, 4, 6, 8mm Larch laminas to study that the theoretical analysis and the experimental analysis regarding the location of neutral axis of the glulams were compared, and to study on the effect of location of neutral axis on mechanical properties of glulam. The variation of location of neutral axis after proportional limit(or elastical limit) was studied to offer basic data to make the better composition method of glulam. The result obtained can be summarized as follows: 1. The theoretical neutral axis was 0.547 in solid wood, and also 0.547 in glulams because glulams were composed of only Larch laminas. 2. In solid wood, the deviation of the theoretical and the experimental neutral axis location was 0.1%, But in glulams, the deviation from-12.2% to + 7.8% showed nonuniform pattern but no large deviation. Because laminas was only of Larch and so the mechanical properties of laminas were monotonous. 3. The neutral axis exerted no influance on the elasticity of glulam, which meaned that the maximum shear strength in the neutral axis showed no influance on elasticity limit. 4. The only minutely lower elasticities of glulam than that of solid wood were shown. This was because of influance of glue lines of glulam on the elasticlties. 5. The failure type of glulam was wholly simple tension failure and the horizontal shear failure near neutral axis was not taken place, which was that glue line was complete in bonding and the strength of the lamina was not various but uniform. 6. The ratio of tension strain($^{\varepsilon}t$) I compression strain($^{\varepsilon}c$) initially showed uniform level After the elasticity limit. the ratio was increased with the flow of time and so the tension strain was more increased than compression strain. So this proved tension lamination technique, which is that the mechanical properties of glulam could be improved, if the lamina of more superior strength would he added on the bottom side of the glulam.

  • PDF

Properties of Glued Laminated Timber Made from Fast-growing Species with Mangium Tannin and Phenol Resorcinol Formaldehyde Adhesives

  • Hendrik, Jessica;Hadi, Yusuf Sudo;Massijaya, Muh Yusram;Santoso, Adi;Pizzi, Antonio
    • Journal of the Korean Wood Science and Technology
    • /
    • v.47 no.3
    • /
    • pp.253-264
    • /
    • 2019
  • This study characterized the chemical compounds in tannin from mangium (Acacia mangium) bark extract and determined the physical-mechanical properties of glued laminated timber (glulam) made from sengon (Falcataria moluccana), jabon (Anthocephalus cadamba), and mangium wood. The adhesives used to prepare the glulam were based on mangium tannin and phenol resorcinol formaldehyde resin. Five-layer glulam beams measuring $5cm{\times}6cm{\times}120cm$ in thickness, width, and length, respectively, were made with a glue spread of $280g/m^2$ for each glue line, cold pressing at $10.5kgf/cm^2$ for 4 h and clamping for 20 h. Condensed mangium tannin consisted of 49.08% phenolic compounds with an average molecular weight of 4745. The degree of crystallinity was 14.8%. The Stiasny number was 47.22%. The density and the moisture content of the glulams differed from those of the corresponding solid woods with mangium having the lowest moisture content (9.58%) and the highest density ($0.66g/cm^3$). The modulus of rupture for all glulam beams met the JAS 234-2003 standard but the modulus of elasticity and the shear strength values did not. Glulam beams made with tannin had high delamination under dry and wet conditions, but glulam made from sengon and jabon wood met the standard's requirements. All glulam beams had low formaldehyde emissions and were classified as $F^{****}$ for formaldehyde emissions according to the JAS 234 (2003) standard.

Effect of Glue and Alum Mixing Ratio on the Color Variation of Traditional Sizing Hanji (아교포수 방법이 전통한지의 색상 변화에 미치는 영향)

  • Lee, Yu-Ju;Choi, Tae-Ho
    • Journal of Conservation Science
    • /
    • v.35 no.2
    • /
    • pp.153-158
    • /
    • 2019
  • The traditional sizing treatment for the Hanji is performed to give the following functions. Those are to stabilize the paint of the painting, to prevent the paint of painting and moisture from smearing into the painting itself, to prevent the paint of the painting and moisture from passing to the lining paper, and to make the colors of painting match the surrounding.This study analyzed a result of the effect of Hanji sizing characteristic according to glue and alum mixing ratio and applying times, affects to pigments of painting and fastness of Hanji using accelerated aging test. As a result of color measurement of sizing treated Hanji, the concentration of glue and the number of application increased, the brightness and the $L^*$ value decreased but the yellowness index increased.

Investigation on The Cause of Interception of Regulated Pest from Imported Glue-laminated Boards Through In-situ Inspection of Their Manufacturing Processes (생산공정 현장실사를 통한 수입 집성재로부터 규제해충 검출 원인 조사)

  • Kim, Min-Ji;Shin, Hyun-Kyeong;Choi, Yong-Seok;Salim, Sabiha;Kim, Gyu-Hyeok
    • Journal of the Korean Wood Science and Technology
    • /
    • v.44 no.5
    • /
    • pp.617-621
    • /
    • 2016
  • On-site survey on glue-laminated board (GLB) manufacturers of Malaysia, Indonesia, and China was conducted to identify the cause of interception of regulated pest from imported GLBs from those countries, and to suggest optimal manufacturing processes of GLB for preventing quarantine risk associated with imported GLBs. The cause of pest interception was improper manufacturing processes, such as air drying or inadequate kiln drying of green laminae, improper storage of dried laminae before finger jointing and edge gluing, and/or incomplete packing of GLBs. In particular, Paulownia GLB manufacturing processes used in China, including air drying of laminae, were mostly poor in terms of preventing quarantine risk associated with imported GLBs. From now on, for preventing quarantine risk associated with imported GLBs, importers have to ask foreign manufacturers spontaneously to use proper manufacturing processes (adequate kiln drying of green laminae, proper storage of dried laminae, and complete packaging of final GLBs).

Comparative Studies on Physical and Mechanical Properties of Domestic Wood-Based Panels (국산목질판상재료(國産木質板狀材料)의 물리적(物理的) 및 기술적성질(機械的性質)에 관(關)한 비교연구(比較硏究))

  • Lee, Phil-Woo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.18 no.2
    • /
    • pp.67-78
    • /
    • 1990
  • This study was performed to determine the characteristics of physical and mechanical properties of domestic wood based materials; plywood, particleboard, medium density fiberboard. Main items of tested properties were panel size, moisture content, water absorption, linear expansion and thickness swelling, glue bond shear strength, bending properties(stress at proportional limit, modulus of rupture. modulus of elasticity), tensile strength, screw holding strength, and internal bond as neccessary. the results were discussed mainly with Korean Standards. The obtained conclusions are as follows; 1. Length and width of 3mm thin plywood(3-ply) and 12mm thick plywood(7-ply) were satished with KS-standard, but thicknesses of these panels were not- passed tolerance limit except one of eight makers. 2. Length and width of particleboard and medium density fiberboard were greater than the tolerance limit value of KS standard, but the thicknesses of these panels were passed this value. 3. Moisture contents of 12mm thick and 3mm thin plywood were satisfied with KS-standard except one mill made 3mm thin plywood. 4. Moisture absortion of plywood was not passed tolerance limit of KS-standard but particleboard was satisfied with this standard value. 5. Dry and wet shear strengths in glue bond of 3mm thin plywood were not reached to KS-standard, but those of 12mm thick plywood were sufficiently satisfied with KS standrad. 6. Modulus of ruptures, parallel to grain and perpendicular to grain of plywood, and particleboard and medium density fiberboard were satisfied with KS-standard. 7. Tensile strengths, parallel to grain and perpendicular to grain of plywood were satisfied with allowance stress of US product standard PS 1-74. 8. Screw holding strength of particleboard was not reached to KS standard, but internal bond was satisfied with KS standard.

  • PDF

Characterization and Comparison of Oriental Ink Sticks (동양 전통 먹(墨)의 이화학적 성상 비교 분석)

  • Kim, Kang-Jae;Eom, Tae-Jin
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.40 no.4
    • /
    • pp.74-81
    • /
    • 2008
  • The writing brush, ink stick, paper, and ink stone were the four precious things of the studying and recording in oriental world until even nowaday. The oriental paper was comparatively well evaluated in many papers and reviews, but it is difficult to find some scientific reports or reviews about the ink stick. In this paper, the scientific aspect of ink sticks of oriental maine three country(Korea, China, Japan) were evaluated by the physical, chemical and microscopic analysis. The result could summarized as fellows; 1. The Korean lampblack ink stick contains more carbon and less nitrogen and the Chinese ink sticks contain less carbon and more oxygen. 2. The Korean lampblack and cowhide glue contain relatively higher amount of sulphur. 3. The particle size distribution of carbon in the ink stick was not change after grinding in the ink stone. 4. The particle size of carbon and the pore size in the charcoal ink sticks of three country were larger than those of the lampblack ink sticks. 5. The ink solution of the charcoal ink sticks shows high roundness on Hanji while the ink solution of the lampblack ink sticks is spread readily to Hanji surface. 6. The change of whiteness in printing of the ink sticks is notable in thermal treatment.

Effects of Adhesion Conditions on Bonding Strength of Pitch Pine Woods for Glued-Laminated Wood (리기다소나무 판재(板材)의 접착조건(接着條件)이 집성재(集成材)의 접착성능(接着性能)에 미치는 영향(影響))

  • Park, Sang-Bum;Kong, Young-To;Jo, Jae-Myeong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.16 no.4
    • /
    • pp.48-53
    • /
    • 1988
  • This study was carried out to investigate the effects of pressing time and spreading amount, moisture content, gap-distance with butt to butt joint and adhesives on bonding strength in manufacturing the laminated wood with Pitch pine (Pinus rigida). The results obtained were as follows: 1) The pressing time of 12 hours, 10 kilogram per square centimeter of pressure and 200 gram per square meter of spreading amount were required to reach over 50 kilogram per square centimeter (block shear strength) in manufacturing the laminated wood by aqueous vinyl urethane adhesive. 2) The bonding strength decreased with the increase of moisture content of wood. The block shear strength, however, showed over 100 kilogram per square centimeter when the strength test was carried out after air-drying the laminated wood in high moisture content (30-70%). 3) Regardless of direction of load, every flexural property decreased with the increase of gap-distance with butt to butt joint. However, little of every flexural property was changed at 0.5 millimeter of joint-gap distance. The flexural property of vertically laminated wood (perpendicular to glue line to load direction: 1) showed more than that of horizontally laminated wood (parallel to glue line to load direction: //). 4) Among five adhesives used at this experiment, the bonding strength of aqueous vinyl urethane adhesive was the highest in dry bond and wet tests.

  • PDF

Evaluation of Shear Strength by Direction of Wood Grain for Korean Pine Using PRF Adhesive (페놀레조시놀공축합수지로 접착된 국산 잣나무의 목리방향별 전단성능평가)

  • Park, Sun-Hyang;Kim, Kwang-Mo;Pang, Sung-Jun;Kong, Jin Hyuk;Lee, Sang-Joon
    • Journal of the Korean Wood Science and Technology
    • /
    • v.45 no.3
    • /
    • pp.243-249
    • /
    • 2017
  • This study was performed to find out the optimum adhesive conditions on manufacturing a cross-laminated timber (hereinafter CLT) with using domestic Korean Pine (Pinus koraiensis). The adhesive conditions including a applied amount of the glue and a Pressure are the one of the most important key factors on establishing CLT production process. The shear strength was examined with differing the adhesive conditions while using Phenol Resorcinol Formaldehyde Resin Adhesive (PRF resin). The optimum adhesive conditions was confirmed to be: glue spread of $250g/m^2$ and Pressure of 0.8 MPa respectively. The grain directions of glued specimens were also considered, perpendicularly bonded and parallelly bonded groups. Shear strength of the former group showed lower values than the latter group which is considered to be the effect of a rolling shear. Meanwhile the shear strength of both group satisfied the Korean Standard (KS F 3021) and the European Standard (EN 14080 and EN 16351). The results derived from this study can be used as the basic data for manufacturing the CLT with domestic Korean Pine. And additional researches for the other species including domestic Korean Larch and Pitch Pine is also now being performed.

Experimental Evaluation of Shear Bonding Performance of Wood-Steel Composite Members (목재-강재 합성 부재의 전단 부착 성능에 대한 실험적 평가)

  • Park, Keum-Sung;Lee, Sang-Sup;Kwak, Myong-Keun
    • Journal of Korean Association for Spatial Structures
    • /
    • v.19 no.4
    • /
    • pp.53-60
    • /
    • 2019
  • In this study, an experimental study was carried out to evaluate the bond shear performance according to the shear connector between the glue-laminated timber and steel interface. Ten block shear specimens were fabricated according to the configuration of the adhesive surface of wood and steel. In addition, four test specimens were produced according to the main variable shape of the wood-concrete shear connector. As a result of the block shear test, the shear strength of the steel-wood adhesive is shown to have a shear performance greater than the wood-wood shear strength. As a result of the push-out test according to the shape of the shear connector, the shear strength increased linearly with the attachment area. The complete composite behavior between the glued-laminated timber and the steel can be secured.