• 제목/요약/키워드: Wood Fiber

검색결과 477건 처리시간 0.029초

난기류 혼합법을 이용한 목섬유-열가소성 섬유 복합재에 관한 연구(I) - 공정변수가 복합재의 물리적 성질에 미치는 영향 - (Wood Fiber-Thermoplastic Fiber Composites by Turbulent Air Mixing Process(I) - Effects of Process Variables on the Physical Properties of Composites -)

  • 윤형운;이필우
    • Journal of the Korean Wood Science and Technology
    • /
    • 제24권3호
    • /
    • pp.101-109
    • /
    • 1996
  • Effects of process variables were evaluated in physical properties of the wood fiber-thermoplastic fiber composites using nonwoven web method. Turbulent air mixer using compressed air was employed to mix wood fiber with two types of thermoplastic polypropylene and nylon 6 fibers. The optimal hot press temperature and time were found to be $190^{\circ}C$ and 9 minutes in wood fiber-polypropylene fiber composite and to be $220^{\circ}C$ and 9 minutes in wood fiber-nylon 6 fiber composite. As the density of wood fiber-polypropylene fiber composite and wood fiber-nylon 6 fiber composite increased, the physical properties were improved The density appeared to be the most significant factor on physical properties in the statistical analysis. The composition ratio of polypropylene or nylon 6 fiber to wood fiber was considered not to be statistically significant factor. The thickness swelling decreased somewhat in wood fiber-polypropylene fiber composite and wood fiber-nylon 6 fiber composite as the content of synthetic fiber increased. As the increase of mat moisture content, dimensional stability was improved in wood fiber-polypropylene fiber composite but not in wood fiber-nylon 6 fiber composite.

  • PDF

난기류 혼합법을 이용한 목섬유-열가소성 섬유 복합재에 관한 연구(II) - 공정변수가 복합재의 기계적 성질에 미치는 영향 - (Wood Fiber-Thermoplastic Fiber Composites by Turbulent Air Mixing Process(II) - Effect of Process Variables on The Mechanical Properties of Composites -)

  • 윤형운;이필우
    • Journal of the Korean Wood Science and Technology
    • /
    • 제25권3호
    • /
    • pp.58-65
    • /
    • 1997
  • This research was carried out to evaluate the effect of process variables on mechanical properties of the wood fiber-thermoplastic fiber composites by turbulent air mixing method. The turbulent air mixer used in this experiment was specially designed in order to mix wood fiber and thermoplastic polypropylene or nylon 6 fiber, and was highly efficient in the mixing of relatively short plastic fiber and wood fiber in a short time without any trouble. The adequate hot - pressing temperature and time in our experimental condition were $190^{\circ}C$ and 9 minutes in 90% wood fiber - 10% polypropylene fiber composite and $220^{\circ}C$ and 9 minutes in 90% wood fiber 10% nylon 6 fiber composite. Both in the wood fiber - polypropylene fiber composite and wood fiber- nylon 6 fiber composite, the mechanical properties improved with the increase of density. Statistically, the density of composite appeared to function as the most significant factor in mechanical properties. Within the 5~15% composition ratios of polypropylene or nylon 6 fiber to wood fiber, the composition ratio showed no significant effect on the mechanical properties. Bending and tensile strength of composite, however, slightly increased with the increase of synthetic fiber content. The increase of mat moisture content showed no significant improvement of mechanical properties both in wood fiber - polypropylene fiber composite and wood fiber nylon 6 fiber composite. Wood fiber - nylon 6 fiber composite was superior in th mechanical strength to wood fiber-polypropylene fiber composite, which may be related to higher melt flow index of nylon 6 fiber(22g/10min) than of polypropylene fiber(4.3g/10min).

  • PDF

목질(木質)과 비목질계(非木質系) 섬유(纖維)를 활용한 복합재(複合材) 연구(硏究) - 폴리프로필렌의 섬유장(纖維長)과 공정변수(工程變數)의 영향(影響)을 중심(中心)으로 - (Studies on Composites Using Wood and Nonwood Fibers - Effects of Polypropylene Fiber Length and Process Variables -)

  • 이필우
    • Journal of the Korean Wood Science and Technology
    • /
    • 제25권2호
    • /
    • pp.33-44
    • /
    • 1997
  • This study was executed to examine the effects of polypropylene fiber length and process variables of the composites made from wood fiber and nonwood fiber mixed formulations. As a nonwood fiber the polypropylene with 3 denier thickness of tow condition was selected and cut into each length of 0.5, 1.0, 1.5, 2.0 and 2.5cm to mix with wood fiber. And also western hemlock wood fiber for medium density fiberboard was prepared. First, to decide an adequate polypropylene mixing fiber length, the composites of 1.0g/$cm^3$ density were made from 10% polypropylene fiber by each of five lengths and 90% western hemlock fiber mixed formulations. Thereafter as the experiments of process variable, the composites applied with adequate polypropylene fiber length(1.5cm) were made from 4 density levels (0.6, 0.8, 1.0, 1.2g/$cm^3$). 3 mixed formulations of wood fiber to polypropylene fiber(95 : 5, 90 : 10, 85 : 15), and 3 mat moisture contents(5, 10, 20%). According to the results and discussions it was concluded as follows ; The physical and mechanical properties were shown improved tendency. as polypropylene fiber length was increased in the range from 0.5 to 1.5cm, but shown decreasing tendency from 2.0 to 2.5 cm. Accordingly, it was shown that polypropylene fiber length is limited to 1.5cm or less length in mixing wood fiber and polypropylene fiber by turbulent air mixing process. As the densities of wood fiber-polypropylene fiber composites were increased, the physical and mechanical properties were clearly improved. Also they were shown significantly increasement statistically between densities respectively. In the mixed formulations, physical and mechanical properties were shown only slightly improvement, as they changed from 95 : 5 to 85 : 15 in wood fiber to polypropylene fiber. Despite of increasement of mat moisture content, mechanical properties were not improved significantly but physical properties were improved somewhat in wood fiber-polypropylene fiber composites.

  • PDF

한지 슬러시-목재 섬유 또는 목재 파티클 복합재의 인장강도 (Tensile Strength of Composites from Hanji(Korean paper) Sludge Mixed with Wood Fiber or Pariticle)

  • 이필우;손정일;이영규
    • 한국가구학회지
    • /
    • 제10권1호
    • /
    • pp.51-56
    • /
    • 1999
  • This research was carried out to investigate the Hanji sludge(black color)-wood fiber and wood particle composited applied by waste sludges arising from the making process of Hanji (Korea paper). In experimental design, four levels of the mixed ratio of Hanji sludge to wood fiber or wood particle(10:90, 20:80, 30:70 and 40:60), three kinds of the resin(PMDI, urea and phenol resin)and three kinds of the specific gravity(0.6, 0.75 and 0.9) were designed to determine the tensile strength of Hanji sludge-wood fiber and wood particle composites. From the results and discussion, it may be concluded as follows: In Hanji sludge-wood fiber and wood particle composites, tensile strengths showed decreasing tendency absolutely by increasing Hanji sludge additive, but clearly increase with the increase of specific gravity. In Hanji sludge-wood fiber composites, there were no differences between PMDI and urea resin-bonded composites, but phenol resin-boned composites were made possibly until the addition of 30% Hanji sludge. On the other hand, Hnji sludge-wood particle composites(SpGr=0.6) have very low tensile strength values. But they were made favorably until the addition of 20% Hanji sludge in Hanji sludge-wood particle composites(SpGr=0.9).

  • PDF

스티렌계 수지(樹脂)를 매트릭스로 사용한 목재 - 플라스틱 복합체(複合體)의 물성(物性)에 미치는 상용화제(相溶化劑)의 효과(效果) (Effect of Compatibilizers on Mechanical Properties of Wood-Plastic Composites Using Styrene Polymers as Matrix Polymers)

  • 한규성
    • Journal of the Korean Wood Science and Technology
    • /
    • 제21권2호
    • /
    • pp.31-37
    • /
    • 1993
  • Composites of styrene polymers with woody fibers were prepared, and the effect of compatibilizers on their mechanical properties was evaluated. To improve the compatibility of wood fibers and the matrix polymers, styrene-maleic anhydride copolymer(SMA) and maleic anhydride-modified polymers were used as compatibilizers. As results, maleic anhydride-modified polystyrene and SMA were proved to improve the tensile strength of the molded composites, and also were evaluated as good compatibilizers for the wood fiber polystyrene composite. Cellulosic fiber (dissolving pulp) provided better reinforcement than lignocellulosic fiber(thermomechanical pulp). On the contrary in the case of the composite of wood fiber and acrylonitrile-butadiene styrene copolymer(ABS), SMA and maleic anhydride-modified acrylonitrile-butadiene-styrene copolymer(MABS) did not act as compatibilizers. However, MABS was evaluated as a good polymer matrix to make wood fiber reinforced composite. The tensile properties of the composites of wood fiber and MABS were superior than those of wood fiber-ABS composites.

  • PDF

Development and Evaluation of Turbulent Air Mixing Process for Manufacturing Wood Fiber and Thermoplastic Fiber Composites

  • Yoon, Hyoung-Un;Eom, Young-Geun;Park, Jong-Young;Kong, Young-To
    • Journal of the Korean Wood Science and Technology
    • /
    • 제26권2호
    • /
    • pp.38-44
    • /
    • 1998
  • A new device that uses turbulent air for mixing wood fibers with thermoplastic fibers was designed and its mixing effectiveness was evaluated in wood fiber and polypropylene fiber composites. Composites made by the turbulent air mixing (TAM) process performed better than composites made by the conventional Rando-Webber forming or nonwoven web process with an additional needling step. Thus, the TAM process proved to be a simple and efficient method in mixing wood fibers with short thermoplastic fibers for the production of wood fiber and thermoplastic fiber composites.

  • PDF

Physical and Mechanical Properties of Wood Fiber-Polypropylene Fiber Composite Panel

  • Kim, Jee-Woong;Eom, Young-Geun
    • Journal of the Korean Wood Science and Technology
    • /
    • 제29권3호
    • /
    • pp.36-46
    • /
    • 2001
  • This study was to find a way of reusing wood and plastic wastes, which considered as a troublesome problem to be solved in this age of mass production and consumption, in manufacturing wood fiber-polypropylene fiber composite panel. And the feasibility of this composite panel as a substitute for existing headliner base panel of automobile was also discussed, especially based on physical and mechanical performance. Nonwoven web composite panels were made from wood fiber and polypropylene fiber formulations of 50 : 50, 60 : 40, and 70 : 30, based on oven-dry weight, with densities of 0.4, 0.5, 0.6, and 0.7 g/$cm^3$. At the same density levels, control fiberboards were also manufactured for performance comparison with the composite panels. Their physical and mechanical properties were tested according to ASTM D 1037-93. To elucidate thickness swelling mechanism of composite panel through the observation of morphological change of internal structures, the specimens before and after thickness swelling test by 24-hour immersion in water were used in scanning electron microscopy. Test results in this study showed that nonwoven web composite panel from wood fibers and polypropylene fibers had superior physical and mechanical properties to control fiberboard. In the physical properties of composite panel, dimensional stability improved as the content of polypropylene fiber increased, and the formulation of wood fiber and polypropylene fiber was considered to be a significant factor in the physical properties. Water absorption decreased but thickness swelling slightly increased with the increase of panel density. In the mechanical properties of composite panel, the bending modulus of rupture (MOR) and modulus of elasticity (MOE) appeared to improve with the increase of panel density under all the tested conditions of dry, heated, and wet. The formulation of wood fiber and polypropylene fiber was considered not to be a significant factor in the mechanical properties. All the bending MOR values under the dry, heated, and wet conditions met the requirements in the existing headliner base panel of resin felt.

  • PDF

한지슬러지-목재섬유 복합보드의 제조연구 II. 한지슬러지-목재섬유 복합보드의 기계적 성질 (Study on Manufacture of Korean Paper(Hanji) Sludge-Wood Fiber Composite Boards II. Mechanical Properties of Korean Paper(Hanji) Sludge-Wood Fiber Composite Boards)

  • 이필우;이학래
    • Journal of the Korean Wood Science and Technology
    • /
    • 제27권2호
    • /
    • pp.31-37
    • /
    • 1999
  • 한지제지 공정 중에서 발생하는 백색슬러지와 흑색슬러지를 각각 일정비율(10:90, 20:80, 30:70, 40:60)로 목재 섬유와 혼합하고 PMDI, 요소 및 폐놀수지를 이용하여 목표비중 0.60, 0.75, 0.90 별로 복합보드를 제조한 결과 전반적으로 볼 때 PMDI수지를 적용한 백색슬러지-목재섬유 복합보드나 요소수지를 적용한 흑색슬러지-목재섬유 복합보드의 경우 20% 정도까지의 슬러지 첨가는 거의 통상적인 보드에 대용하는 기계적 성질을 지닌다고 믿어진다.

  • PDF

목섬유(木纖維)와 열가소성(熱可塑性) 플라스틱 복합재료(複合材料)의 기계적(機械的) 성질(性質) (Mechanical Properties of Wood-Fiber Thermoplastic Composites)

  • 박병대;임기표;김윤수
    • Journal of the Korean Wood Science and Technology
    • /
    • 제22권2호
    • /
    • pp.46-53
    • /
    • 1994
  • 본 연구(硏究)는 목섬유(木纖維)와 열가소성(熱可塑性) 플라스틱의 복합재료(複合材料)를 제조하고 그 기계적(機械的) 성질(性質)을 평가하기 위하여 실행되었다. 강도가 높고 밀도가 낮아 플라스틱의 보강재료로써 잠재성을 갖는 목섬유를 2종의 열가소송 플라스틱(폴리프로필렌과 폴리에틸렌)과 혼합(混合)하여 복합재료(複合材料)를 만들었다. 흡습성(吸濕性)인 목섬유와 비흡습성(非吸濕性)인 플라스틱과 친화성을 위해 계면활성제(界面活性劑)를 사용하였다. 또한 낮은 밀도의 목섬유를 플라스틱내에서 혼합하기 위해 고속 플라스틱믹서를 사용하였다. 사출성형(射出成形)한 샘플을 사용하여 기계적(機械的) 성질(性質)을 시험(試驗)한 결과 인장및 휨강도는 목섬유 혼합량에 따라 크게 향상되었다. 휨 강도(强度)는 인장강도(引張强度)보다 훨씬 크게 나타났으며 인장(引張)및 휨탄성(彈性) 계수(係數)는 플라스틱내 목섬유 혼합량과 비례적으로 증가하였다. 목섬유는 복합재료의 강도(强度)와 탄성계수(彈性係數)를 향상시킴으로서 플라스틱을 보강할 수 있었다. 이와는 반대로 인장시험에서 시편 파괴점까지의 신장율과 파괴에너지는 목섬유 혼합량이 증가함에 따라 감소하였다. 충격강도(衝擊强度) 역시 유사한 경향을 보였다.

  • PDF

Evaluation of The Moment Resistance Joint Strength of Larch Glulam Using Glass Fiber Reinforced Wood Plate

  • Song, Yo-Jin;Jung, Hong-Ju;Park, Hyun-Ho;Lee, Hak-Young;Hong, Soon-Il
    • Journal of the Korean Wood Science and Technology
    • /
    • 제42권5호
    • /
    • pp.571-578
    • /
    • 2014
  • As a way of developing wooden joint development, a glass fiber reinforced wood plate was manufactured to replace a steel plate. Also, the fracture toughness was evaluated. Through application to a cantilever-type specimen made of a column and a beam, the moment resistance performance was evaluated. For the fracture toughness specimen of the wood plate, 12 types were manufactured by varying the combination of a main member (veneer and plywood) and reinforcement (glass fiber sheet and glass fiber cloth). The results of the fracture toughness test indicated that the 5% yield load of the specimen using plywood was 18% higher than that of the specimen using veneer, and that the specimen reinforced by inserting glass fiber sheets between testing materials (Type-3-PS) had the highest average 5% yield load 4841 N. Thus, a moment resistance strength test was performed by applying Type-3-PS to a column-beam joint. The results of the test indicated that compared to the specimen using a steel plate and a drift pin (Type-A), the maximum moment ratio of the specimen using a glass fiber reinforced wood plate (Type-3-PS) and a drift pin (Type-B) was 0.79; and that a rupture occurred in the wood plate due to high stiffness of the drift pin. The maximum moment ratio of the specimen using a glass fiber reinforced wood plate (Type-3-PS) and a glass fiber reinforced wooden laminated pin (Type-C) was 0.67, which showed low performance. However, unlike Type-A, a ductile fracture occurred on Type-C, and the load gradually decreased even after the maximum moment.