The Effect of Gelatin Coating and Sonication on the Quality Properties of Wet-Aging Pork Loins

  • Yea-Ji Kim;Tae-Jun Jung;Tae-Kyung Kim;Jae Hoon Lee;Dong-Min Shin;Hwan Hee Yu;Yun-Sang Choi
    • 한국축산식품학회지
    • /
    • 제43권2호
    • /
    • pp.269-281
    • /
    • 2023
  • In this study, we evaluate the effect of gelatin coating and sonication of wet-aged pork loin on quality. The moisture content of wet-aged pork loin with sonication and gelatin coating was the highest in the G5S sample (5% gelatin coating and sonication), while the moisture content of wet-aged pork loin with sonication was higher than that without sonication. The pH of wet-aged pork loin with sonication was lower than that without sonication. The aging loss of 5% gelatin coating with sonication was significantly lower than that of G0 (control), while the cooking loss was the lowest in G0 wet-aged pork loin. The water holding capacity of the wet-aged pork loin was the highest in G1. The thiobarbituric acid reactive substances value of wet-aged pork loin was significantly decreased with coating and not affected by sonication. The gelatin coating and sonication treatment significantly increased the myofibrillar fragmentation index of the samples. Shear force of wet-aged pork loin significantly decreased as the samples were gelatin-coated and sonicated. The myofibrillar and total protein solubilities were not significantly different between samples. In conclusion, the 1% gelatin coating with sonication can enhance the quality of wet-aged pork loin.

광섬유 WOW 액상코팅 공정의 코팅액 유동특성 해석연구 (Analysis of Coating Flow Characteristics in Wet-on-Wet Optical Fiber Liquid Coating Process)

  • 김경진;박중윤
    • 반도체디스플레이기술학회지
    • /
    • 제16권4호
    • /
    • pp.91-96
    • /
    • 2017
  • In this computational study of optical fiber manufacturing, WOW (wet-on-wet) double coating process on freshly drawn glass fiber has been numerical modelled and simulated using a simplified geometry of typical optical fiber coating apparatus. The numerical domain includes primary and secondary coating dies along with secondary coating cup and the interface between primary and secondary coating liquids are investigated using level set method. Coating liquid viscosity is an important parameter and its dependence on temperature is also considered. Since there would be possibility for pressure and temperature of primary coating liquid to be increased substantially at high fiber drawing speed, the effects of increased pressure and temperature of primary coating liquid are examined on flow patterns of coating liquids in secondary coating cup. In case that both pressure and temperature of primary coating liquid are high enough, liquid interface becomes noticeably unstable and this flow instability could adversely affect the uniform coatings and final quality of produced optical fiber.

  • PDF

벼 무논직파재배의 종자 코팅소재별 발아 및 유묘생육 특성 (Effect of Different Seed Coating Materials on Seedling Establishment and Growth in Direct Seeded Rice under Puddled Wet Soil Condition)

  • 박광호;김양식;장진택
    • 현장농수산연구지
    • /
    • 제15권1호
    • /
    • pp.63-73
    • /
    • 2013
  • Pot시험에서 코팅소재별 벼 종자의 발아 및 유묘생육 특성을 구명하기 위하여 무처리, 규산코팅, 천매암코팅, 철분코팅, 규산복토, 철분코팅+규산복토 처리에서 유묘의 입모율, 경시적 입묘양상의 변화, 초장의 특성을 벼 무논점파와 무논조파재배에서 조사결과를 요약하면 다음과 같다. 입모율 1. 벼 무논점파재배의 경우 규산복토, 무처리 100%, 천매암코팅 91.5%, 규산코팅 88%, 철분코팅+규산복토 86%, 철분코팅 75.5%이었다. 2. 벼 무논조파재배에서는 무처리, 규산복토 100%, 철분코팅+규산복토 97.5%, 천매암코팅 96%, 규산코팅 94.8%, 철분코팅 86%로 각각 나타났다. 본 시험에서는 규산복토와 무처리에서 가장 높게 나타났지만 실제 각종 제한요인(새 피해, 건조, 부묘현상 등)이 많은 포장조건에서는 무처리 조건이 상반된 결과가 나타나고 있으며 천매암코팅, 규산코팅 또는 복토조건에서 철분코팅보다 높은 입묘율을 각각 보였다. 유묘의 초장 생장 1. 벼 무논점파재배에서 유묘의 초장생장은 파종 후 35일 조사한 유묘 초장의 경우 벼 무논점파재배에서는 규산복토 23.8cm, 무처리 23.6cm, 규산코팅 21.4cm, 천매암코팅 20.3cm, 철분코팅+규산복토 16.8cm, 철분코팅 15.4cm이었다. 2. 벼 무논조파재배에서 파종 후 35일 조사한 유묘의 초장생장은 규산복토 22.1cm, 무처리 21.2cm, 규산코팅 20.0cm, 천매암코팅 19.0cm, 철분코팅 17.7cm, 철분코팅+규산복토 17.0cm 순으로 각각 나타났다.

스크린 프린팅 기술을 적용한 피스톤 스커트의 브레이드 코팅공정에 관한 기초연구 - 매개변수 연구 (A Basic Study on Blade Coating Process of Piston Skirt by Applying the Technology of Screen Printing - Parametric Study)

  • 전상명
    • Tribology and Lubricants
    • /
    • 제25권6호
    • /
    • pp.414-420
    • /
    • 2009
  • In this study, using the general expressions predicting the pressure under a blade and the volume of coating fluid passing through the blade edge, it is predicted the change of the coating wet film thickness related with various parameters determining the characteristics of this blade coating process. Using the results of this research, it can be found the optimized coating wet film thickness taking into account the parameters related with various coating process on various metal surfaces will be able to be predicted.

습식법으로 제조된 BN 중간층을 가진 Cf/SiC 복합재의 제조 및 물성 평가 (Fabrication and Characterization of Cf/SiC Composite with BN Interphase Coated by Wet Chemical Process)

  • 구준모;김경호;한윤수
    • 한국표면공학회지
    • /
    • 제50권6호
    • /
    • pp.523-530
    • /
    • 2017
  • In this study, we developed the h-BN interphase for ceramic matrix composites (CMCs) through a wet chemical coating method, which has excellent price competitiveness and is a simple process as a departure from the existing high cost chemical vapor deposition method. The optimum condition for nitriding an h-BN interphase using boric acid and urea as precursors were derived, and the h-BN interphase coating through a wet method on a carbon preform of 2.5 D was conducted to apply the optimum conditions to the CMCs. In order to control the coating property via the wet coating method, four parameters were investigated such as dipping time of the specimen in the precursor solution, the ratio of boric acid and urea in the precursor, the concentration of solution where the precursor was dissolved, and the cycle of dipping and dry process. The CMCs was fabricated through polymer impregnation and pyrolysis (PIP) processes and a three-point flexural strength test was conducted to verify the role of the coated h-BN interphase.

SB latex 대체용 친환경 전분계 바이오바인더 및 합성바인더의 적용 기술 개발 (제1보) - 대체용 바인더의 Pre-coating 적용 - (Application Technology of Environmental-friendly Starch-based Biobinder and Synthesized Binder in order to Substitute SB Latex for Paper Coating (1) - Application of Substitute Binder for Pre-coating Layer -)

  • 이용규;김선구;원종명;김영훈
    • 펄프종이기술
    • /
    • 제47권5호
    • /
    • pp.134-140
    • /
    • 2015
  • This study was carried out to evaluate whether EVAc, acryl latex and biobinder could substitute the part of SB latex for pre-coating color formula or not. Different coating colors prepared through the substitution of 30% SB latex with EVAc, acryl latex, and biobinder were applied for pre-coating layer. 100% SB latex is used as a binder for top coating color. The optical properties, gloss, roughness, stiffness, dry- and wet-pick strength were measured. There were no significant differences in the brightness, whiteness, opacity, roughness, ink set-off and gloss of paper coated with 5 different coating colors. However the stiffness, dry- and wet-pick strength were somewhat lower than those of conventional coating color which 100% SB latex was used as a binder. Although the part of SB latex could be substituted with EVAc, acryl latex and biobinder without sacrificing the qualities of coated paper. Further researches on the improvement of stiffness, dry- and wet-pick strength, and the optimization of rheology of coating color in order to improve the qualities of coated paper are strongly recommended.

The Origin of the Residual Carbon in LiFePO4 Synthesized by Wet Milling

  • Park, Sung-Bin;Park, Chang-Kyoo;Hwang, Jin-Tae;Cho, Won-Il;Jang, Ho
    • Bulletin of the Korean Chemical Society
    • /
    • 제32권2호
    • /
    • pp.536-540
    • /
    • 2011
  • This study reports the origin of the electrochemical improvement of $LiFePO_4$ when synthesized by wet milling using acetone without conventional carbon coating. The wet milled $LiFePO_4$ delivers 149 $mAhg^{-1}$ at 0.1 C, which is comparable to carbon coated $LiFePO_4$ and approximately 74% higher than that of dry milled $LiFePO_4$, suggesting that the wet milling process can increase the capacity in addition to conventional carbon coating methods. UV spectroscopy, elemental microanalysis, and evolved gas analysis are used to find the root cause of the capacity improvement during the mechanochemical reaction in acetone. The analytical results show that the improvement is attributed to the conductive residual carbon on the surface of the wet milled $LiFePO_4$ particles, which is produced by the reaction of $FeC_2O_4{\cdot}2H_2O$ with acetone during wet milling through oxygen deficiency in the precursor.

일부 합성피혁 근로자들의 Dimethylformamide, Methyl Ethyl Ketone, Toluene 노출에 따른 요중 대사물질 (Urinary Metabolites of Dimethylformamide, Methyl Ethyl Ketone, and Toluene exposed Workers in Synthetic Leather Factories)

  • 최호춘;김강윤;안선희;이영자;정규철
    • 한국산업보건학회지
    • /
    • 제11권2호
    • /
    • pp.135-144
    • /
    • 2001
  • This study was performed to measure airborne dimethylformamide(DMF), methyl ethyl ketone(MEK) and toluene and their urinary metabolites concentrations and to determine the relationship between airborne and urinary concentration. Airborne samples and their urinary metabolites were measured 98 male workers who work for 8 synthetic leather factories in a portion of Kyoung-In area. Urine samples were collected at end-of-shift to estimate the exposure levels. 1. The concentration of airborne DMF by process was 8.81 ppm for wet-mixing, 15.05 ppm for wet-coating, 6.03 ppm for dry-mixing, 5.58 ppm for dry-coating, 5.37 ppm for printing, and 9.03 ppm for total. There was statistically significant difference by process. Urinary NMF concentrations of wet-mixing, wet-coating, dry-mixing, dry-coating and printing were $90.55mg/{\ell}$, $79.80mg/{\ell}$, $39.86mg/{\ell}$, $25.23mg/{\ell}$, and $38.15mg/{\ell}$, respectively, and total geometric mean was $56.24mg/{\ell}$. There was significant difference by process. 2. The concentration of airborne MEK by process was 1.89 ppm for wet-mixing, 1.96 ppm for wet-coating, 10.33 ppm for dry-mixing, 29.24 ppm for dry-coating, 14.98 ppm for printing, and 4.87 ppm for total. There was statistically significant difference by process. Urinary MEK concentrations of wetmixing, wet-coating, dry-mixing, dry-coating and printing were $0.93mg/{\ell}$, $0.70mg/{\ell}$, $3.29mg/{\ell}$, $3.29mg/{\ell}$, and $1.06mg/{\ell}$, respectively, and total geometric mean was $1.25mg/{\ell}$. There was statistically significant difference by process. Urinary MEK 3. The concentration of airborne toluene by process was 0.35ppm for wet-mixing, 0.42ppm for wet-coating, 2.95ppm for dry-mixing, 11.67ppm for dry-coating, 4.88ppm for printing, 1.24ppm for total. There was statistically significant difference by process. Urinary hippuric acid concentrations of wet-mixing, wet-coating, dry-mixing, dry-coating and printing were 0.24g/g creatinine, 0.21g/g creatinine, 0.34g/g creatinine, 0.52g/g creatinine, and 0.29g/g creatinine, respctively and total geometric mean was 0.28g/g creatinine. There was statistically significant difference by process. 4. No. of exceeded KPEL was 40 workers(40.8%) for DMF(10ppm), 1 worker(1.0%) for MEK(200ppm), and no worker for toluene(100ppm). No. of exceeded KBEI was 62 workers(63.3%) for urinary NMF($40mg/{\ell}$), 29 workers(29.6%) for urinary MEK, 1 worker(1.0%) for urinary hippuric acid. 5. The regression equations were Log(NMF)=0.4094*Log(DMF)+1.3587(r=0.4516) for DMF, Log(MEKU)=0.1859*Log(MEK)-0.0324(r=0.3303) for MEK, Log(HA)=0.2106*Log(Toluene)-0.5685(r=0.4497) for toluene. Synthetic leather factory workers expose to 3 kinds of organic solvents which are DMF, MEK and toluene. Their urinary NMF and MEK levels were higher than their concentration levels through respiratory. It seems that the urinary levels were affected skin absorption for working habit and alcohol intake.

  • PDF

광섬유 2차 코팅다이 형상 변화에 따른 유리섬유 고속 코팅공정 영향성 해석연구 (Numerical Study of Secondary Coating Die Geometry Effects on High Speed Optical Glass Fiber Coating Process)

  • 김경진;박중윤
    • 반도체디스플레이기술학회지
    • /
    • 제18권3호
    • /
    • pp.12-18
    • /
    • 2019
  • The protective double layer polymer coatings on silica optical fibers are realized by wet-on-wet liquid coating process and they play an important role in final quality of mass produced optical fibers. This numerical study aims to analyze the effects of secondary coating die design parameters by employing two dimensional axisymmetric model of coating cup and coating die geometry and computational fluid dynamics simulations which include temperature dependent viscosity of polymer coating liquids and viscous dissipation heating. Under high speed fiber drawing conditions and pressurized coating liquid supply, the effects of converging die angle are investigated in order to appreciate the change of coating liquid flow patterns such as flow recirculation zone near coating die as well as primary and secondary coating layer thicknesses. The auxiliary coating die to converging coating die is also tested and the results find that this concept is advantageous in achieving stable double layer coatings on silica glass fiber.