Development of 3-Dimensional Stress Measurement System by Bore hole Bottom Deformation Method (공저변형법에 의한 3차원응력측정 시스템의 개발)

  • Lee, Ki-Ha;Ishijima, Yoji;Fujii, Yoshiaki
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 2006.03a
    • /
    • pp.34-41
    • /
    • 2006
  • A 3-dimensional stress measurement system based on the bore hole bottom deformation method, which is one of the stress relief methods, was developed. A pilot bore hole is drilled from the bottom of a bore hole and the stress meter is inserted into the pilot bore hole in the method. The bore hole is advanced as an over coring and the deformations in seven directions are measured by cantilever type-sensors. Using the cantilever type-sensors saves time for hardening of glue. No cable connection between the stress meter and a data logger is necessary since a compact data logger is installed in the stress meter. The accuracy of the stress meter was confirmed by a biaxial test for a Shikotsu welded tuff block although in-situ tests have not been carried out yet.

  • PDF

Experimental Study on Strength of Austentic Stainless Steel (STS 304L) Fillet-Welded Connection with Weld Metal Fracture According to Welding Direction (용접방향에 따른 오스트나이트계 스테인리스강(STS304L) 용착금속파단 용접접합부의 내력에 관한 실험적 연구)

  • Kim, Tae Soo;Lee, Hoochang;Hwang, Bokyung;Cho, Taejun
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.22 no.1
    • /
    • pp.81-89
    • /
    • 2018
  • Austenitic stainless steels have excellent corrosion resistance, durability and fire resistance. Especially, since STS304L among austenitic types is a low-carbon variation of STS304 and has excellent intergranular corrosion resistance, it can often be used under the welded condition without heat treatment after field welding. This paper investigated ultimate behaviors such as ultimate strength and weld metal fracture mechanism of STS304L fillet-welded connections with TIG(tungsten inert gas) welding through test results. Main variables of specimens are weld length and welding direction against loading. Fracture of specimens are classified into three modes(tensile fracture, shear fracture and block shear fracture). Ultimate strengths were compared according to the welding direction and weld length and TFW series with transverse fillet weld had the highest strength compared with other types(LFW series with longitudinal fillet weld and FW series with all round weld). It is known that current design specifications such as KBC 2016 and AISC2010 underestimated the strength of TFW and LFW specimens and provided unconservative estimates for FW specimens. Finally, strength equations were proposed considering material properties of STS 304L material.

Fatigue Strength Evaluation of Bogie Frame of Urban Maglev Train (도시형 자기부상열차 대차 프레임의 피로강도 평가)

  • Han, Jeong Woo;Kim, Heung Sub;Bang, Je Sung;Song, See Yeob
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.37 no.7
    • /
    • pp.945-951
    • /
    • 2013
  • This study evaluated the fatigue strength of the bogie frame of an urban maglev train through fatigue analysis, cumulative damage, and fatigue tests based on a proposed fatigue evaluation method. The results of FEM analysis in which various load combinations were adopted showed that all data were under the fatigue limit of a butt welded joint made of A6005 in a Goodman diagram. The cumulative fatigue damage was calculated at the highest level from a bolt connecting the area of the electromagnetic pole in the casting block; however, the total sum was evaluated as D=0.808 based on $1{\times}10^7$ cycles, which indicates that it did not exceed the failure criteria. In addition, the results of the fatigue testshowed that there was no crack at any position in the bogie frame, which corresponded to the results of fatigue analyses.