산성안개가 내후성강재의 녹형성 및 피로강도에 미치는 영향 (Effect of Acid Fog on Rust Formation and Fatigue Strength of Weathering Steel)

  • 김민건;구은회
    • 산업기술연구
    • /
    • 제22권B호
    • /
    • pp.13-20
    • /
    • 2002
  • The purpose of this study is to investigate the effect of acid fog on the rust formation behavior of weathering steel (SMA50) which is used in uncoated bridges. Weathering steel didn't form the passive film under the environment of acid fog(pH5,6), whereas the environment of distilled water formed the protective oxide film. Therefore, the construction of weathering steel under the environment extremely exposed to SOx and NOx which are the main compositions of acid fog is not adequate. Fatigue limits of weathering steel under acid fog environment are remarkably decreased as compared with environment of distilled water. The corrosive constituents in acid fog has piled up the corrosion products on specimen surface and generated the corrosion pits. Because of the high stress concentration arising at this corrosion pit, relatively low fatigue limits were obtained for acid fog specimens.

  • PDF

무도장 교량에 사용되는 내후성강재의 부식 및 피로거동에 미치는 산성안개의 영향 (Effect of Acid Fog on Rust Formation and Fatigue Behavior of Weathering Steel Used in Un-Coated Bridge)

  • 김민건
    • 대한기계학회논문집A
    • /
    • 제32권1호
    • /
    • pp.13-20
    • /
    • 2008
  • The purpose of this study is to investigate the effect of acid fog on the rust formation behavior of weathering steel (SMA50) which is used in un-coated bridges. Weathering steel didn't form the passive film under the environment of acid fog(pH5,6), whereas the environment of distilled water formed the protective oxide film. Therefore, the construction of weathering steel under the environment extremely exposed to SOx and NOx which are the main compositions of acid fog is not adequate. Fatigue limits of weathering steel under acid fog environment are remarkably decreased as compared with environment of distilled water. The corrosive constituents in acid fog has piled up the corrosion products on specimen surface and generated the corrosion pits. Because of the high stress concentration arising at this corrosion pit, relatively low fatigue limits were obtained for acid fog specimens.

Experimental approach to evaluate weathering condition of granite using electrical resistivity

  • Oh, Tae-Min;Cho, Gye-Chun;Son, Thai An;Ryu, Hee-Hwan;Lee, Changho
    • Geomechanics and Engineering
    • /
    • 제8권5호
    • /
    • pp.675-685
    • /
    • 2015
  • Weathering is the breaking/cutting down process of rocks due to physical and chemical processes in natural as well as artificial environment including $CO_2$ injection for storage in the sediment, or natural resource recovery process. This study suggests an alternative method to estimate the degree of weathering for granites. A series of laboratory and field experiments are performed to measure electrical resistivities on various rock samples experienced different degrees of weathering and their residual soils under different saturation conditions. It is found that the normalized electrical resistivity increases with a decrease in water absorption and the saturation. Simple boundaries are suggested to identify the weathering degree of granites, based on limited data. Field test results for three sites confirm that the suggested method could be estimated well the degree of weathering of granites compared with the other methods suggested previously. Although further research is required, this study suggests that an electrical resistivity could be an effective approach to estimate the degree of weathering of granites compared with the other methods suggested previously.

목타르와 목초액로 처리한 낙엽송재의 Weathering 특성 (Weathering of Larch Wood treated with Wood tar and Wood vinegar)

  • 권구중;권성민;장재혁;전근우;김남훈
    • Journal of Forest and Environmental Science
    • /
    • 제27권1호
    • /
    • pp.55-60
    • /
    • 2011
  • This study has been carried out to investigate the preservation characteristics and weathering of larch wood treated with wood tar and wood vinegar, neglected under the circumstance of outdoor exposure, buried under ground, and deposited under water. Earlywood cell wall observed by optical microscope has been collapsed due to the fungi deterioration. This phenomenon occurred more frequently in the case of woods treated with wood tar and buried under ground. Relative crystallinity of woods treated with wood tar, exposed outdoors, and untreated wood buried under ground was highest at 63% while wood tar treated wood buried under ground was lowest at 46%.

팔공산 화강암내 흑운모의 풍화과정에서 생성되는 고령토광물들의 광물학적 특성 및 생성 환경 (Mineralogical Characteristics and Formation Environment of Kaolin Minerals in the Weathering of Granitoids: Weathering of Biotite in Palgongsan Granite)

  • 정기영
    • 한국광물학회지
    • /
    • 제11권2호
    • /
    • pp.97-105
    • /
    • 1998
  • Weathering of biotite in Palgonsan granite was studied by using X-ray diffraction, optical microscopy, scanning electron microscopy, and electron probe micro analysis. Biotite altered to biotite/vermiculite regular mixed layer mineral (B/V) in the early stage of weathering. Although partially replaced by kaolinite with the progress of weathering. B/V is the major weathering product of biotite throughout the profile. During the formation of B/V, Mg, Fe and K are removed from a biotite layer to form a vermiculite layer by about 28%, 44% and 88%, respectively, whereas the Ti content is not changed. Considerable volume increase after the kaolinitization of B/V suggests that Al and Si are largely introduced from the external weathering solution. The silicate lattice templet of a weathering biotite facilitated the nucleation and growth of kaolinite. In the Palgongsan granite weathering profile, plagioclase weathered mostly into halloysite whereas biotite greatly contributes to the kaolinite crystallization though its small content in fresh rock.

  • PDF

누전차단기 하우징의 내후성에 관한 연구 (A Study on the Weathering of RCD'S Housing)

  • 김창환;신진용;강병철;김상명
    • 한국표면공학회지
    • /
    • 제47권6호
    • /
    • pp.335-340
    • /
    • 2014
  • This study selected an outdoor RCD'S and verified behavior of change in the housing with time. Weathering tests were carried out as outdoor exposure test (90 degrees, 37 degrees) and laboratory test (xenon lamp), and the results were evaluated based on color difference, gloss, contact angle, and optical microscope. This study can provide basic data for standardization of development and performance evaluation on RCD'S housing products.

암반풍화도에 따른 지질공학적 특성 저감효과 (Effects of Rock Weathering on the Degradation of Engineering Properties)

  • 이창섭;조태진
    • 터널과지하공간
    • /
    • 제15권6호
    • /
    • pp.411-424
    • /
    • 2005
  • 풍화작용은 심부에서 생성된 암석이 지표에서 파괴되고 변질되어 현재의 환경조건과 평형을 이루는 산물을 형성하는 과정이다. 본 연구에서는 국내에서 가장 분포면적이 넓은 화강암질암의 풍화단계별 시료를 채취하여 편광현미경관찰, X-선 회절분석, 전자현미경관찰, 화학분석, 물성시험등을 수행하였다. 실험결과에 의거하여 풍화에 의해 형성되는 2차광물, 특히 점토광물의 형성과정을 확인하였고, 풍화에 따른 암석의 공학적인 성질변화와 물성저하의 메카니즘을 규명하였다.

Evaluation of geochemical processes affecting groundwater chemistry in Namwon, Korea

  • Kim, Kang-Joo;Natarajan Rajmohan;Kim, Hyung-Jung;Kim, Suk-Hwi;Hwang, Gab-Soo;Cho, Min-Joe;Lee, Sang-Ho
    • 한국지하수토양환경학회:학술대회논문집
    • /
    • 한국지하수토양환경학회 2004년도 임시총회 및 추계학술발표회
    • /
    • pp.334-337
    • /
    • 2004
  • Groundwater chemistry in Namwon area, Korea, was investigated to understand the contribution of geochemical processes on groundwater chemistry. For this study, a total of 279 groundwater samples were collected from 93 wells distributed over the study area. Higher concentrations of major ions are generally encountered in the shallow alluvial wells, suggesting that these chemicals are originated from the surface contamination sources. Mass balance analysis based on reaction stoichiometry reveals that the water chemistry is regulated by three major chemical processes: weathering of silicate/ carbonate minerals, input of C1/SO$_4$ salts, and nitrate generating processes. The results show that mineral weathering is the most dominating factor regulating the groundwater chemistry. However, the groundwaters with the higher salt concentration indicate the larger mineral weathering effect, suggesting that some part of the mineral weathering effect is also associated with the anthropogenic activities such as limes applied to the cultivated lands, carbonates (CaCO$_3$) in the cement materials.

  • PDF

Evaluation method for time-dependent corrosion depth of uncoated weathering steel using thickness of corrosion product layer

  • Kainuma, Shigenobu;Yamamoto, Yuya;Ahn, Jin-Hee;Jeong, Young-Soo
    • Structural Engineering and Mechanics
    • /
    • 제65권2호
    • /
    • pp.191-201
    • /
    • 2018
  • The corrosion environments in a steel structure are significantly different depending on the individual parts of the members. To ensure the safety of weathering steel structures, it is important to evaluate the time-dependent corrosion behavior. Thus, the progress and effect of corrosion damage on weathering steel members should be evaluated; however, the predicted corrosion depth, which is affected by the corrosion environment, has not been sufficiently considered until now. In this study, the time-dependent thicknesses of the corrosion product layer were examined to quantifiably investigate and determine the corrosion depth of the corroded surface according to the exposure periods and corrosion environments. Thus, their atmospheric exposure tests were carried out for 4 years under different corrosion environments. The relationship between the thickness of the corrosion product layers and mean corrosion depth was examined based on the corrosion environment. Thus, the micro corrosion environments on the skyward and groundward surfaces of the specimens were monitored using atmospheric corrosion monitor sensors. In addition, the evaluated mean corrosion depth was calculated based on the thickness of the corrosion product layer in an atmospheric corrosion environment, and was verified through a comparison with the measured mean corrosion depth.