Material Characteristics and Quantitative Deterioration Assessment of the Sinwoldong Three-storied Stone Pagoda in Yeongcheon, Korea (영천 신월동삼층석탑의 재질특성과 훼손도 정량평가)

  • Yi, Jeong-Eun;Lee, Chan-Hee;Chae, Seong-Tae;Jung, Young-Dong
    • Journal of Conservation Science
    • /
    • v.26 no.4
    • /
    • pp.349-360
    • /
    • 2010
  • The Yeongsheon Sinwoldong three-storied stone pagoda (Treasure No. 465) composed mainly of drusy alkali-granite. The major rock-forming minerals are biotite, quartz, amphiboles, orthoclase and plagioclase. Yellowish brown and black discoloration are formed at the eight sculpture Buddha of the stylobate. A broken rock fragments in the roof material were repaired using epoxy resin and cement mortar in the past. As a result of the infrared thermography analysis from the pagoda, cracks and exfoliation were not serious. Also, P-XRF analysis showed that concentration of Fe (mean 5,599ppm) and S (mean 3,270ppm) were so high in yellowish discoloration parts. Black discoloration area was detected highly Mn (mean 2,155ppm) concentration around the eight sculpture Buddha of the stylobate. The main reason for these are inorganic contaminants from disengaged rock ingredient and organic contaminants from withered plant body. Degree of physical weathering is relatively high in the southern and northern side. The eastern and western side had similar with weathering condition. The northern and eastern side were serious discoloration and biological weathering relatively. Therefore, we suggest that the pagoda need to do cleaning of biological contaminant and conservation treatment to weakened materials of rock and long term monitoring.

Evaluation and Weathering Depth Modeling of Thermally Altered Pelitic Rocks based on Chemical Weathering and Variations: Ulju Cheonjeon-ri Petroglyph (화학적 풍화작용과 조성변화에 따른 열변질 이질암의 풍화심도 모델링 및 평가: 울주 천전리 각석)

  • LEE Chan Hee;CHUN Yu Gun
    • Korean Journal of Heritage: History & Science
    • /
    • v.56 no.4
    • /
    • pp.160-189
    • /
    • 2023
  • The Cheonjeon-ri petroglyph is inscribed with shale formation belonging to the Daegu Formation of the Gyeongsang Supergroup in the Cretaceous of the Mesozoic Era. This rock undergoes thermal alteration to become hornfels, and has a high hardness and dense texture. Rock-forming minerals have almost the same composition as quartz, alkali felspar, plagioclase, calcite, mica, chlorite and opaque minerals, but calcite is rarely detected in the weathered zone. The petroglyph forms a weathered zone with a certain depth, and there is a difference in mineral and chemical composition between weathered and unweathered zones, respectively. The CaO contents of the weathered zone were reduced by more than 90% compared to that of the unweathered zone, because calcite reacted with water and dissolved. As a result of calculating the surface weathering depth for the petroglyph with the transmission characteristics of X-rays, depth of the parts in falling off and exfoliation showed a depth of about 0.5 to 1 mm, but the weathering depth in most areas was calculated to be about 3 to 4 mm. This can be proved by the contents and changes of Ca and Sr. The surface discolorations of the petroglyph are distributed with different color density, and the yellowish brown discoloration is alternated with a thin biofilm layer, showing a coverage of 79.6%. Therefore, periodic preservation managements and preventive conservation monitoring that can effectively control the physicochemical and biological damages of the Cheonjeonri petroglyph will be necessary.

Conservation Scheme and Deterioration States of the Wanggung-ri Five-storied Stone Pagoda in the Iksan, Korea (익산 왕궁리 5층 석탑의 훼손현황과 보존방안 연구)

  • Yang, Hee-Jae;Lee, Chan-Hee;Kim, Sa-Dug;Choi, Seok-Won
    • 보존과학연구
    • /
    • s.25
    • /
    • pp.171-195
    • /
    • 2004
  • This research presents an evaluation of the weathering and deterioration state of the Wanggung-ri five-storied stone pagoda in the Iksan (National Treasure No. 289) and suggests conservational schemes. A deterioration map of the pagoda was drawn from the aspects of petrological, physical, chemical, biological, structural and artificial weathering.The rock properties consisting of the pagoda were medium-grained biotite granite that had leucocratic phenocryst developed in parts. The body of each story suffered severely from the secondary contamination that turned the colors into light grey, pitch dark, yellowish brown, and reddish brown as well as granular decomposition, exfoliation and peel-off. The roof stones were heavy exfoliated or peeled off in most of the cases. In addition to the fine cracks, there were layered cracks on the corners. The roof stones of the3rd and 4th story in the north and west side had some stones fall-off, while those of the 2ndstory in the north side had steel reinforcement filled for a fixing purpose. Those of the 5th story showed big gaps that must have originated from cracks and were easily subject to granular decomposition and rainfall. The inside clay filler was missing in the lower part of the roof stones of the 4th and 5th story and the supporting stones, which were thus covered by light grey or pitch dark sediments. The contact area of the materials was about 70 % in the parts where there was a space due to the filler missing and washigher than 90 % in the lower parts of the pagoda. About 90 % or more of the roof stones surface of each story were covered by aerial plants that formed a thick biological mat. Thus it seemed necessary to come up with the conservational measures to remove the plans living on the surface of the stone materials, with the plans to prevent rain from falling inside, and with the water repellent and hardening treatments to postpone the surface weathering of the rock properties. All those measures and plans must be based on the results of long-term monitoring and thorough detail investigations.

  • PDF

Mass Interception Fractions and Weathering Half-lives of Iodine-131 and Radiocesium in Leafy Vegetables Observed after the Fukushima Daiichi Nuclear Power Plant Accident

  • Tagami, Keiko;Uchida, Shigeo
    • Journal of Radiation Protection and Research
    • /
    • v.46 no.4
    • /
    • pp.178-183
    • /
    • 2021
  • Background: This study was carried out to provide environmental transfer parameter values to estimate activity concentrations of these radionuclides in agricultural crops when direct contamination occurred. Materials and Methods: Mass interception fractions (FBs) and weathering half-lives (Tws) of 131I and radiocesium were calculated using openly available monitoring data obtained after the Fukushima Daiichi Nuclear Power Plant accident. FB is the ratio between the initial radioactivity concentration of a radionuclide retained by the edible part of the plant (Bq·kg-1 fresh weight [FW]) and the amount of deposited radionuclide in that area (Bq·m-2). Tw values can be calculated using activity concentrations of crops decreased with time after the initial contamination. Results and Discussion: Calculated FB and Tw values for 131I and radiocesium were mostly obtained for leafy vegetables. The analytical results showed that there was no difference of FBs between 131I and radiocesium by t-test; geometric mean values for leafy vegetables cultivated under outdoor conditions were 0.058 and 0.12 m2·kg-1 FW, respectively. Geometric mean Tw value of 131I in leafy vegetables grown under outdoor conditions was 8.6 days, and that of radiocesium was 6.6 days; there was no significant difference between Tw values of these radionuclides by Wilcoxon rank sum test. Conclusion: There was no difference between 131I and radiocesium for FBs and Tws. By using these factors, we would be able to carry out a rough estimation of the activity concentrations of 131I and radiocesium in the edible part of leafy crops when a nuclear accident occurred.

Material Characteristics and Ultrasonic Velocity Diagnosis of the Five-storied Stone Pagoda in Tamni-ri, Uiseong (의성 탑리리 오층석탑의 재질특성과 초음파 물성진단)

  • Lee, Myeong Seong;Lee, Jae Man;Kim, Jae Hwan
    • Korean Journal of Heritage: History & Science
    • /
    • v.45 no.1
    • /
    • pp.70-85
    • /
    • 2012
  • Uiseong Tamni-ri Five-storied Stone Pagoda is composed of andesitic tuff and partially combined with tuff breccia and fine-grained granite. The andesitic tuff is identical to basement rock of Geumseongsan Mountain based on lithological, mineralogical and geochemical characteristics. The pagoda has suffered physical weathering such as crack and scaling, discoloration and biological colonization with complex reaction. Expecially, dark gray and brown discoloration appeared whole over the surface of the pagoda, and three to five-layered exfoliation and granular disintegration dominantly occurred in the fourth and fifth roof stones. It is assuming that the stone elements of the pagoda are evaluated as third to forth grades (average third grade) of weathering compared to fresh rock in Geumseongsan Mountain. The physical strength of the stone elements shows low values in the south and west sides of the pagoda that corresponds high weathering degree of the west side due to exfoliation, crack and granular disintegration. It is necessary to investigate the pagoda for precise deterioration assessment, monitoring and conservation treatment.

Performance indicator of the atmospheric corrosion monitor and concrete corrosion sensors in Kuwait field research station

  • Husain, A.;Al-Bahar, Suad Kh.;Salam, Safaa A. Abdul
    • Smart Structures and Systems
    • /
    • v.17 no.6
    • /
    • pp.981-994
    • /
    • 2016
  • Two field research stations based upon atmospheric corrosivity monitoring combined with reinforced concrete corrosion rate sensors have been established in Kuwait. This was established for the purpose of remote monitoring of building materials performance for concrete under Kuwait atmospheric environment. The two field research sites for concrete have been based upon an outcome from a research investigation intended for monitoring the atmospheric corrosivity from weathering station distributed in eight areas, and in different regions in Kuwait. Data on corrosivity measurements are essential for the development of specification of an optimized corrosion resistance system for reinforced concrete manufactured products. This study aims to optimize, characterize, and utilize long-term concrete structural health monitoring through on line corrosion measurement and to determine the feasibility and viability of the integrated anode ladder corrosion sensors embedded in concrete. The atmospheric corrosivity categories supported with GSM remote data acquisition system from eight corrosion monitoring stations at different regions in Kuwait are being classified according to standard ISO 9223. The two nominated field sites where based upon time of wetness and bimetallic corrosion rate from atmospheric data where metals and rebar's concrete are likely to be used. Eight concrete blocks with embeddable anodic ladder corrosion sensors were placed in the atmospheric zone adjacent to the sea shore at KISR site. The anodic ladder corrosion rate sensors for concrete were installed to provide an early warning system on prediction of the corrosion propagation and on developing new insights on the long-term durability performance and repair of concrete structures to lower labor cost. The results show the atmospheric corrosivity data of the environment and the feasibility of data retrieval of the corrosion potential of concrete from the embeddable sets of anodic ladder corrosion sensors.

Field Experiments of Scientific Conservation Treatment for Bangudae Petroglyphs in Ulsan, South Korea (울산반구대암각화 보존처리를 위한 현장적용실험)

  • Lee, Tae-jong;Oh, Jung-hyeon;Kim, Sa-dug
    • 보존과학연구
    • /
    • s.33
    • /
    • pp.69-83
    • /
    • 2012
  • Field experiments for Conservation damage on selected spots were carried out prior to direct conservation treatments for Bangudae Petroglyphs in Ulsan. It was found that there is a big difference in treatment effects according to the treatment technique and application rather than on the treatment material use. Based on the results of this study, a plan for the conservation treatment of Bangudae Petroglyphs will be suggested by providing new materials and application techniques for cracks, adhesive application and consolidation by conducting artificial weathering tests and continued monitoring.

  • PDF

The trial Test for the Estimation System of Deterioration of Exterior Wall by Infrared Theromography (적외선탐사기를 사용한 외벽열화평가 시스템의 구축)

  • Kwon, Young-Jin;Nishigawa, Tadashi;Oh, Sang-Keun;Park, Deuk-Kon;Choi, Long
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1996.04a
    • /
    • pp.398-401
    • /
    • 1996
  • It is the aim of this study to introduce the application method for the new estimation system of deterioration caused performance decrement of exterior wall by infrared theromography. With this help of this trial test, the defect such as void and honeycomb of esveria wall can be shown easily. Espicially by selecting the weathering condition, it becomes easier to identify defect than with original image. It was confirmed that this trial monitoring system is very useful to identify the defect of exterior wall.

  • PDF

Deterioration Diagnosis and Petrogenesis for Rock Properties of the Stone Lantern in the Gwanchoksa Temple, Nonsan, Korea (논산 관촉사 석등의 훼손도 진단 및 기원암의 성인적 해석)

  • Lee, Myeong Seong;Yi, Jeong Eun;Pyo, Su Hee;Song, Chi Young;Lee, Chan Hee
    • Journal of Conservation Science
    • /
    • v.17 s.17
    • /
    • pp.5-18
    • /
    • 2005
  • Rock materials of the Stone Lantern in the Gwanchoksa temple was composed of dark grey granodiorite. This Stone Lantern is partly structural distortion as S-shape, especially, rocks of the upper supports and under the roof materials were highly deterioration due to the surface exfoliation, and strong secondary contaminations owing to the discoloration by oxidation of inserted iron plates between the rock properties, and white grey to dark black contaminants along the rain path way. Rock surface of the Stone Lantern occurred as partly green patches because of coated by algae, lichen and moss. This biological problems are need for cleaning and treatments. The Stone Lantern have to be considered to conservation method that can reduce weathering factors with long-term monitoring about environmental change for structural stability, surface degradation and mechanical weathering. Materials of the Stone Lantern and basement rocks of the area are consisted of same petrogenetic granodiotite based on occurrences, petrological and geochemical characteristics.

  • PDF

Material and Deterioration Characteristic Analysis for Stone Sculptures in Gyeongbokgung Royal Palace, Seoul (경복궁 석조조형물의 재질 및 손상특성 분석)

  • Kim, Jiyoung;Jo, Young Hoon;Lee, Chan Hee
    • Journal of Conservation Science
    • /
    • v.29 no.4
    • /
    • pp.407-420
    • /
    • 2013
  • The stone sculptures in Gyeongbokgung Royal Palace are mainly composed of granite (884 sculptures, 96.7%) and marble (25 sculptures, 2.7%) that originated in several different quarries. Main deterioration forms are crack (24%), break-out (21%), exfoliation (36%), granular disintegration (9%) and blackening (20%). Crack and break-out are dominant contributors to high physical deterioration degree, and blackening is major weathering form of intensive discoloration. The Gyeonghoeru, Geunjeongjeon and Pumgyeseok areas require urgent and high conservation maintenance with short-term periodic monitoring since proportions of 3-grade deterioration were calculated higher than others as 55% for Gyeonghoeru, 29% for Geunjeongjeon, 11% for Pumgyeseok area. The Pumgyeseok (officials' rank stone), especially, needs intervention for protective facility due to its material vulnerability to weathering in outdoor environment.