• Title/Summary/Keyword: Wear of ceramics

Search Result 187, Processing Time 0.03 seconds

Fracture Mechanics Study on Wear Mechanism of Ceramics -Discussions on Experimental Results of Wear Test- (세라믹의 마멸기구에 관한 파괴역학적 연구 -마멸실험 결과의 고찰-)

  • 김석삼;김재호
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.14 no.3
    • /
    • pp.636-645
    • /
    • 1990
  • Analytically induced wear mechanism of elastic body under Hertzian contact is applied in acutual wear test of ceramics. There are two types of wear in ceramics, a large scale wear and a small scale wear. The large scale wear is commensurable with Hertzian contact area and the small scale wear with real contact area. Nondimensional parameter, S$_{c}$, is introduced and fully examined to estimate or predict wear rate of ceramics. Ceramic wear for S$_{c}$.leq.0.8 is in small scale wear and for S$_{c}$;geq.1.6 in large scale wear. wear.

Tribological Behavior of Silicon Carbide Ceramics - A Review

  • Sharma, Sandan Kumar;Kumar, B. Venkata Manoj;Kim, Young-Wook
    • Journal of the Korean Ceramic Society
    • /
    • v.53 no.6
    • /
    • pp.581-596
    • /
    • 2016
  • A comprehensive review on sliding and solid particle erosion wear characteristics of silicon carbide (SiC) ceramics and SiC composites is provided. Sliding or erosion wear behavior of ceramics is dependent on various material characteristics as well as test parameters. Effects of microstructural and mechanical properties of SiC ceramics are particularly focused to understand tribological performance of SiC ceramics. Results obtained between varieties of pairs of SiC ceramics indicate complexity in understanding dominant mechanisms of material removal. Wear mechanisms during sliding are mainly divided in two groups as mechanical and tribochemical. In solid particle erosion conditions, wear mechanisms of SiC ceramics are explained by elastic-plastic deformation controlled micro-fracture on the surface followed by radial-lateral crack propagation beneath the plastic zone.

A Study on the Wear Mechanism of the Alumina Ceramics for the Wear of STB2 (베어링 강(STB2)의 마멸에 미치는 알루미나 세라믹스의 마멸기구)

  • Nam, Joon-Woo;Jun, Tae-Ok;Jin, Dong-Kyu
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.12 no.3
    • /
    • pp.62-72
    • /
    • 1995
  • The present study was undertaken to investigate the dry wear mechanism of the alumina ceramics in the purity variation for the wear of STB2. The wear test was carried out under different experimental condition various sliding speed, contact pressure and sliding distance. According as the alumina purity increased, wear volume of the STB2 decreased and minimum value of wear volume was over to high speed side. According as the sliding speed and sliding distance increased, friction coefficient decreased owing to drop of the shear strength, it decresed largely owing to decreased of elastic modulus and thermal conductivity with decrease in alumina purity. Indicative of minimum, value of wear volume, low speed side was abrasive wear, high speed side was wear of heat softening. The friction surface of ceramics protacted by oxide was transfer from STB2.

  • PDF

Friction and Wear of Ceramic-Steel Pairs in Boundary-Lubricated and Unlubricated Line-Contact Sliding (경계윤활 및 무윤활 상태에서 선접촉을 하는 세라믹과 강의 마찰과 마멸 특성)

  • 이영제;김영호;장선태
    • Tribology and Lubricants
    • /
    • v.12 no.3
    • /
    • pp.12-25
    • /
    • 1996
  • The friction and wear behaviors of ceramics against steels with lubricants were investigated and compared with those observed in air. Lubrications wbre done by a water and a commercial engine oil as received. The investigated ceramics were $Al_{2}O_{3}$, SiC, and $Si_{3}N_{4}$. Steels with 0.2 wt.% C were heat treated to obtain tempered structure. A cylinder-on-plate tribometer with rotated sliding motion was used to carry out the experiments. In the experiments reported here, the ranges of different testing speeds and loads were used. It was found that the friction and wear characteristics of tested pairs were significantly influenced by environments. In water and oil environments the wear of ceramics was reduced from 10$^{-6}$ g/s down to 10$^{-8}$ g/s in dry sliding at the same values of the frictional power which are the products of the friction coefficient, the load and the sliding speed. SiC showed excellent wear resistant behavior in water sliding, which was the lowest among tested ceramics, but it was, very poor in oils. In case of $Si_{3}N_{4}$, the wear rates were very low under oil environment, but the highest in water. The wear rates of $Al_{2}O_{3}$ were very low in both lubricating conditions at low values of the frictional power, but high at high values of the frictional power.

Tribological Performance of Laser Textured Translucent Duplex α/β-Sialon Composite Ceramics

  • Joshi, Bhupendra;Tripathi, Khagendra;Gyawali, Gobinda;Lee, Soo Wohn
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2014.11a
    • /
    • pp.180-181
    • /
    • 2014
  • Optically translucent Sialon ceramics was fabricated by hot pressed sintering method. The Sialon ceramics was laser textured and their tribological performance was observed. Starved lubrication method was applied on Sialon ceramics with different dimple spacing under a load of 10N and at room temperature. The material having high dimple spacing ($200{\mu}m$) shows low coefficient of friction. The material shows mild wear and therefore, wear rate of steel ball (meeting partner) was observed to measure wear rate. Different phases Sialon ceramics were analyzed by XRD patterns. Moreover, the mechanical properties of the Sialon ceramics were observed.

  • PDF

Effect of Cutting Condition on the Tool Wear in Turning of the Presintered Low Purity Alumina Ceramics (저순도 알루미나 세라믹 예비소결체의 선삭에서 공구 마멸에 미치는 절삭 조건의 영향)

  • Lee, Jae-Woo
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.27 no.5
    • /
    • pp.14-21
    • /
    • 2010
  • In this study, presintered low purity alumina ceramics were machined with various tools to clarify the effects of the tool material, cutting condition and tool geometry on machinability. The main conclusions obtained were as follows. (a)The wear of tungsten carbide tool becomes smaller with the increase of the feed and clearance angle, and with the decrease of rake angle, especially exhibiting considerably smaller wear with both the decrease of rake angle and the increase of clearance angle. (b) So far as turning the ceramic presintered at low temperature, the diamond tool shows the best performance with higher feed. (c) The effect on the tool wear of the feed, clearance angle and rake angle becomes smaller in turning the ceramic presintered at higher temperature. (d) The tool wear is not severely affected by the depth of cut.

A Study on The Wear Process and Wear Mechanism of the Alumina Ceramics with Different Alumina Purity (순도를 달리한 알루미나 세라믹스의 마멸과정 및 이의 기구에 관한 연구)

  • 전태옥;진동규
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.18 no.12
    • /
    • pp.3404-3412
    • /
    • 1994
  • The present study was undertaken to investigate the dry wear process and wear mechanism of the alumina ceramics in the purity variation which are used for the mechanical seal, roll, liner and dies. The wear test was carried out under different experimental condition using the wear testing device and in which the annular surface rubbed on dry sliding condition various sliding speed, contact pressure and sliding distance. In case of alumina purity 95%, there was speed range which wear loss increased rapidly owing to enlargement of heat impact force and temperature rise of wear surface. According as the alumina purity increased, wear loss decreased but alumina purity 85% with much void and defect had the most wear loss than any other alumina purity. The friction coefficient of sliding initial stage of wear curves has a large value but according to increase of sliding distance, it decreased owing to drop of the shear strength of wear surfaces.

A Study on the Machinability and Machining properties of Composite Ceramics$(iC-Al_2O_3)$ by EDM (복합 세라믹스$(iC-Al_2O_3)$의 방전가공특성에 관한 연구)

  • 윤병주
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.4 no.4
    • /
    • pp.61-68
    • /
    • 1995
  • TiC-Al2O3 composite ceramics has high hardness, high strength, high wear and corrosion resistance. Therefore, composite ceramics have been concerned significantly with some excellent properties and many functions as new industrial materials to the industry at large. In present research, experiments are carried out to obtain the machinability and machining properties by EDM. As a result, the most suitable machining conditions of TiC-Al2O3 composite ceramics was that the pulse duration is 10-60$mutextrm{s}$, the peak current is 10-16A. The machining speed and the wear of the tool electrode increased with the increase in peak current.

  • PDF

Wear Patterns and Mechanisms of Cutting Tool in Cutting of Machinable Ceramics (가공성 세라믹 절삭에서 공구의 마멸 패턴과 메카니즘)

  • Jang, Sung-Min;Baek, Seung-Yub
    • Journal of the Korean Society of Safety
    • /
    • v.25 no.5
    • /
    • pp.1-6
    • /
    • 2010
  • When the ceramic material is being machined, micro crack and brittle fracture dominate the process of material removal. Generally, ceramics are very difficult-to-cut materials and machined using conventional method such as grinding and polishing. However, such processes are generally cost-expensive and have low material removal rate. Machinable ceramics used in this study contain BN powder to overcome these problem and for productivity elevation. This paper focuses on machinability evaluation during end mill process with CNC machining center in this study. Experiment for this purpose is performed for tool wear patterns and mechanism.

Evaluation of Wet Machining Characteristics of the Presintered Low Purity Alumina with the Ceramic, CBN and Diamond Tools (저순도 알루미나 예비소결체의 절삭유제에 따른 세라믹, CBN, 다이아몬드공구의 가공 특성 평가)

  • Lee, Jae-Woo
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.24 no.2 s.191
    • /
    • pp.33-40
    • /
    • 2007
  • In this study, presintered and full sintered low purity alumina ceramics were machined with various tools to clarify the effect of cutting fluid in machinability. The main conclusions obtained were as follows. When the presintered ceramics were wet machined with sintered diamond tool, the tool wear becomes extremely large, and higher cutting speed can be used than in the case of full sintered ceramics. The productivity of wet cutting with the sintered diamond tool is much higher than that of dry cutting. In the case of the CBN and ceramic tools, the tool wear were smaller at wet cutting than at dry cutting, especially exhibiting considerably larger grooved tool wear in wet cutting with ceramic tool.