  • Machining pressed compacts of ceramic and WC-Co materials can be the most cost effective way of forming the bodies prior to sintering when the required number of pieces is small. In this study, in order to clarify the machinability for turning, the $Si_3N_4$ and the WC-Co green compacts unsintered were machined under different cutting conditions with various tools. Absorbing chips by vacuum hose decreases tool wear. The tool wear becomes larger in the order of the ceramic, CBN and cemented carbide tools in machining the $Si_3N_4$ green compacts. In machining the WC-Co green compacts, the tool wear becomes larger in the order of the ceramic, cemented carbide and CBN tools. The land of cutting edge does not affect tool wear. When machining with cemented carbide tool, the tool wear i equal cutting length is nearly identical in spite of the increase of cutting spee, and the roughness of machined surface was the best in the cutting speed of 90 m/min. The tool wear decreases with the increase of rake angle and relief angle and with the decrease of nose radius. The machined surfaces become worse with the increase of feed rate and depth of cut, and with the decrease of rake angle and relief angle. The tool wear is not affected by the feed and depth of cut.

세라믹 마멸에 있어서의 새로운 파라메터 제안 (I) 질화규소와 지르코니아의 마찰$\cdot$마멸 특성 (A Propotition of a New Parameter in Ceramic Wear(I) Friction and Wear Characteristics of Silicon Nitride and Zirconia)

  • 김석삼;김상우
    • 대한기계학회논문집
    • /
    • 제17권6호
    • /
    • pp.1441-1455
    • /
    • 1993
  • 본 연구에서는 최신기법에 의해서 제조된 HIP제 질화규소와 지르코니아를 실험재료로 하여 무윤활하에서의 미끄럼마찰·마멸실험을 수행하여 마찰·마멸특성을 규명하고, SEM을 이용한 마멸면의 미시적 관찰을 통해서 세라믹의 마멸기구를 조사하 여 세라믹마멸기구의 마멸모델을 제시하고자 한다. 제시된 마멸모델에서 파괴역학을 도입하여 이론해석과 고찰을 수행하여 보다 실용적인 세라믹의 마멸율울 평가할 수 있 는 새로운 무차원 파라메터를 제안하고자 한다.

인공 고관절 골두용 세라믹 복합재료에 대한 세라믹-세라믹 접촉 마멸 특성 분석 (Ceramic-Ceramic Wear Zirconia/Alumina Composites For The Application Of Total Hip Joint Implant)

  • 김환;이권용;김대준;이명현;서원선
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2004년도 학술대회지
    • /
    • pp.355-361
    • /
    • 2004
  • Ceramic femoral heads in the total hip replacement have been developed to reduce the polyethylene liner wear, Alumina and zirconia (3Y-TZP) having the excellent tribological properties are coupled against acetabular cups of polyethylene and are used in clinical application worldwide. However, alumina has a risk of catastrophic failure, and zirconia has the low temperature degradation in spite of enhanced fracture toughness. Recently, novel zirconia/alumina composite is very attractive due to the low temperature degradation (LTD)-free character and high fracture toughness. In the present study, we focus on the wear of ceramic on ceramic, which are able to be used as femoral heads and acetabular cups. Therefore, LTD-free zirconia/alumina composites with three compositions are made in a form of disk and cylinder, and the wear of the composites is performed on pin-on-disk type wear tester. The wear is conducted with or without lubricant. All the composites fabricated with the different composition show the good wear resistance.

  • PDF

질화규소의 입계상에 존재하는 불순물이 마모에 미치는 영향 (Effect of Impurities in Grain Boundary Phases on Wear Behavior of $Si_3N_4$)

  • 오윤석;임대순;이경호
    • 한국세라믹학회지
    • /
    • 제33권3호
    • /
    • pp.277-284
    • /
    • 1996
  • The water test results indicated that the impurities had detrimetal effect on the wear resistance of silicon nitride and the effects were getting severe as the temperature increased. Especially when Ca existed as an impurity the detrimental effects was the most severe. These results were resulted from the fact that impurities lowered the mechanical properties of the grain boundary phase of silicon nitride. The wear test results of glass/glass-ceramic specimens having a similar composition to the grain boundary phase of silicon nitride revea-led that the specimen containing CaO showed the lowest wear resistance. The existence of Fe and Ca at the grain boundary phase assisted forming a grain boundary phase with relatively low refractoriness. Therefore at a given wear condition the removal of deformed layer would be easier. The results showed that the glass phases could be modified by heat-treatment and this modification improved tribological characteristics of the silicon nitride.

  • PDF

Friction and Wear of Pressureless Sintered Ti(C,N)-WC Ceramics

  • Park, Dong-Soo;Yun, Shin-Sang;Han, Byoung-Dong;Kim, Hai-Doo
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2002년도 proceedings of the second asia international conference on tribology
    • /
    • pp.211-212
    • /
    • 2002
  • Friction and wear of pressureless sintered Ti(C,N)-WC ceramics were studied using a ball-on-reciprocating flat apparatus in open air. The silicon nitride ball and the cemented carbide (WC-Co) ball were used against the Ti(C,N)-WC plate samples. The friction coefficients of the Ti(C,N)-WC samples against the silicon nitride ball and the cemented carbide ball were about 0.57 and 0.3, respectively. The wear coefficient of the sample without WC addition was 5 times as large as that of the sample with 10 mole % WC addition when tested against the silicon nitride ball under 98 N. The higher wear coefficient of Ti(C,N)-0WC was explained in part by larger grain size. Wear occurred mainly by grain dislodgment after intergranular cracking mainly caused by the accumulated stress within the grains.

  • PDF

Al2O3에서 미끄럼시의 마모 및 마모천이 기구 (Wear and Wear Transition Mechanisms During Sliding in Al2O3)

  • 조성재;김종집;한준희;문한규
    • 한국세라믹학회지
    • /
    • 제26권1호
    • /
    • pp.51-58
    • /
    • 1989
  • Wear and wear transition mechanisms during sliding as a function of time in Al2O3 have been studied to understand the wear behaviour of brittle ceramic materials. Commercial Si3N4 ball was rotated against flat Al2O3 specimens which were hot pressed and polished using upto 1${\mu}{\textrm}{m}$ diamond paste. Paraffin oil was used as a lubricant. Experimental data show that wear of Al2O3 is separated into distinct two stages, i.e., initial stage of slow wear and final stage of rapid wear. Microstructural observations at worn surface show that wear occurs through grooving and grain pull-out in the initial and final stage respectively. TEM observations beneath the worn surfaces show that grain pull-out starts to occur by the propagation of grain boundary cracks induced by dislocation pile-up throughthe surface.

  • PDF

Wear of primary teeth caused by opposed all-ceramic or stainless steel crowns

  • Choi, Jae-Won;Bae, Ik-Hyun;Noh, Tae-Hwan;Ju, Sung-Won;Lee, Tae-Kyoung;Ahn, Jin-Soo;Jeong, Tae-Sung;Huh, Jung-Bo
    • The Journal of Advanced Prosthodontics
    • /
    • 제8권1호
    • /
    • pp.43-52
    • /
    • 2016
  • PURPOSE. This study was conducted to evaluate the effects of full-coverage all-ceramic zirconia, lithium disilicate glass-ceramic, leucite glass-ceramic, or stainless steel crowns on antagonistic primary tooth wear. MATERIALS AND METHODS. There were four study groups: the stainless steel (Steel) group, the leucite glass-ceramic (Leucite) group, the lithium disilicate glass-ceramic (Lithium) group, and the monolithic zirconia (Zirconia) group. Ten flat crown specimens were prepared per group; opposing teeth were prepared using primary canines. A wear test was conducted over 100,000 chewing cycles using a dual-axis chewing simulator and a 50 N masticating force, and wear losses of antagonistic teeth and restorative materials were calculated using a three-dimensional profiling system and an electronic scale, respectively. Statistical significance was determined using One-way ANOVA and Tukey's test (P<.05). RESULTS. The Leucite group ($2.670{\pm}1.471mm^3$) showed the greatest amount of antagonist tooth wear, followed by in decreasing order by the Lithium ($2.042{\pm}0.696mm^3$), Zirconia ($1.426{\pm}0.477mm^3$), and Steel groups ($0.397{\pm}0.192mm^3$). Mean volume losses in the Leucite and Lithium groups were significantly greater than in the Steel group (P<.05). No significant difference was observed between mean volume losses in the Zirconia and Steel groups (P>.05). CONCLUSION. Leucite glass-ceramic and lithium disilicate glass-ceramic cause more primary tooth wear than stainless steel or zirconia.

The Wear Rate and Survivorship in Total Hip Arthroplasty Using a Third-generation Ceramic Head on a Conventional Polyethylene Liner: A Minimum of 15-year Follow-up

  • Bum-Jin Shim;Sung-Jin Park;Chan Ho Park
    • Hip & pelvis
    • /
    • 제34권2호
    • /
    • pp.115-121
    • /
    • 2022
  • Purpose: The purpose of this study was to evaluate the wear and survival rates of third-generation ceramic heads on a conventional ultra-high molecular weight polyethylene liner. Materials and Methods: A total of 160 hips (147 patients with a mean age of 55.9 years) who underwent total hip arthroplasty using the third-generation ceramic head on a conventional polyethylene liner from March 1998 to August 2003 were reviewed retrospectively. Evaluation of the wear rate for 56 hips (49 patients) followed-up for at least 15 years was performed using the PolyWare program version 8 (Draftware Developers, USA). The Kaplan-Meier survivorship was also evaluated. Results: Linear wear and volumetric wear rates were 0.11±0.47 mm/year and 32.75±24.50 mm3/year, respectively. Nine revisions were performed during the follow-up period because of cup or stem loosening. The Kaplan-Meier survival rate, using cup revision or total revision total hip arthroplasty (THA) as the endpoint of analysis, was 93.7% at 15 years and 73.6% at 20 years. Conclusion: Because all revisions were performed between 15 and 20 years in our study, surgeons should pay greater attention to patients who underwent THA with ceramic-on-polyethylene bearing from 15 years postoperatively. Contemporary alumina ceramic on highly cross-linked polyethylene could certainly be a good alternative bearing couple providing better longevity.

유기변성 하이브리드 세라믹 물질을 결합제로 이용한 고체피막윤활제의 마찰마모 특성 (Friction and Wear Characteristics of Bonded Film Lubricants of Organically Modified Hybrid Ceramic Binder Materials)

  • 한흥구;공호성;윤의성
    • Tribology and Lubricants
    • /
    • 제19권4호
    • /
    • pp.203-210
    • /
    • 2003
  • In order to enhance the thermal stability of binder materials of bonded type solid lubricants, several metal-alkoxide based sol-gel materials such as methyltrimethoxysilane(MTMOS), titaniumisopropoxide (Ti(Opr$\^$i/)$_4$), zirconiumisopropoxide (Zr(Opr$\^$i/)$_4$) and aluminumbutoxide (Al(Obu$\^$t/)$_4$) were modified chemically by both epoxy and acrylic silane compounds. Friction and wear characteristics of the bonded solid lubricants, whose binders were of several hybrid ceramic materials, were tested with a reciprocating tribo-tester. Wear life was evaluated with respect to the heat-curing temperature, friction temperature, type of supplement lubricants, and ratio of binder materials. Test results showed that the Si-Zr hybrid ceramic materials modified by epoxy-silane compounds had a higher wear life compared to others. Sb$_2$O$_3$ was the most effective supplement lubricants in the high temperature, and BUS analyses revealed that it was caused mainly by a strong anti-oxidation effect to MoS$_2$ particles. The higher heat-curing temperature resulted in the higher wear life, and the higher friction temperature resulted in the lower wear life.

Braking Performance of Ceramic Coated Discs

  • Kang, B.B.;Lee, H.S.
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2002년도 proceedings of the second asia international conference on tribology
    • /
    • pp.429-430
    • /
    • 2002
  • In this study, three kinds of brake: discs including two coated brake discs and one steel disc were tested under the same experimental conditions on a reduced scale braking test bench. Plasma spray coating technique was used to coat ceramic powder on the discs. In the test, four commercial sintered brake pads were coupled with discs. Ceramic coated discs have shown good stability in friction coefficient at high speed and high energy braking conditions. However, ceramic coated discs caused more wear loss of pad mass than the steel disc. It was shown that thermal barrier effect in ceramic coated discs adjusted the thermal partition between pad and disc. Steel disc showed fluctuating friction coefficient at high speed but less wear loss of pad mass than ceramic coated discs.