FTIR and Moisture Effects on Optical Information Transfer at Interface of Air and Glass (공기-유리 계면에서 광학정보 전달에 미치는 불완전 반사 및 수분 효과)

  • Han, Won Heum;Han, Ji Heum;Kim, Jee Hyen;Jung, Hyung Sik;Lee, Moon Ho
    • Journal of Adhesion and Interface
    • /
    • v.13 no.2
    • /
    • pp.73-84
    • /
    • 2012
  • The transfer mechanism of optical information at the interface of air and glass (the air-glass IF) has been investigated by thoroughly fulfilling the theoretical and experimental analyses regarding the FTIR (Frustrated Total Internal Reflection) and moisture effects on the fingerprint onto a glass cup with water. As for the fingerprint onto a glass cup with water its image was observed to be very vivid, which turned out to be due to the difference between the two light intensities reflected on the air-glass IF and the wet fingerprint ridge by manipulating the optical theories such as Fresnel relation, Snell's law, FTIR, GT (general transmission) and so on. In addition, the experimental inspection for FTIR and moisture effects on the fingerprint image also evidenced the fact that the vivid fingerprint image originated from the moisture effect rather than the FTIR phenomenon.

Effect of various cleaners and mordants to bond strength of light curing glass ionomer cements to dentin (Smear layer 제거와 금속 이온 처리가 광중합형 글라스아이오노머와 상아질간의 결합강도에 미치는 영향)

  • Lee, Won-Seob;Park, Sang-Jin
    • Restorative Dentistry and Endodontics
    • /
    • v.19 no.1
    • /
    • pp.45-63
    • /
    • 1994
  • 128 freshly extracted human molars were used to study the interaction between dentinal smear layer removal with various agents, and the shear bond strength of a light cured glass ionomer cement to dentin. It was proposed that the removal of smear layers using acidic cleaners followed by incorporation of Fe mordant with dentin could enhanced the infiltration of monomer component in light curing glass ionomer cement and resulted in a high bond strength. For the first treatment process for removal of smear layers on the surfaces of dentin, 50 % citric acid, 10% maleic acid and 10 % phosphoric acid were used, and for the second treatment process, 15% ferric chloride, 6.8% ferric oxalate or 30% potassium oxalate were used. Distilled water was used as a control. After double sequential treatment on dentin, a light curing glass ionomer cement was bonded to dentin. After being immersed in water at 31'C for 24 hours, shear bond strengths were measured Instron testing machine(Model No.4202, USA). Surface changes were also observed using SEM (Hitachi, S-2300, Japan) after treatment process with each agents. The following conclusions were drawn : 1. Dentin surface cleaned with maleic acid and treated with ferric oxalate showed the highest bond strength with light curing glass ionomer cement. 2. Bond strengths of glass ionomer cement to dentin treated with maleic acid or citric acid were the highest, and that treated with phosphoric acid showed the lowest. 3. The effect of ferric oxalate on shear bond strength to dentin was always higher than that of ferric chloride. 4. The smear layers were clearly removed and the orifices of dentinal tubules were opened widely by the citric acid, maleic acid and phosphoric acid. 5. The orifices of dentinal tubules opened after using the first solution were closed with the treatment of ferric chloride. 6. The precipitate like crystals were formed on dentin surfaces and tubules, but a significant decrease in bond strength of glass ionomer cement to dentin surface treated with potassium oxalate.

  • PDF

A STUDY ON BONDING STRENGTH OF DENTAL AMALGAM TO GLASS IONOMER CEMENT FOLLOWING SURFACE TREATMENT (글라스아이오노머 시멘트 표면 처리에 따른 치과용 아말감의 전단 결합 강도에 관한 연구)

  • Shin, Young-Joo;Choi, Ho-Young
    • Restorative Dentistry and Endodontics
    • /
    • v.19 no.1
    • /
    • pp.217-230
    • /
    • 1994
  • The purpose of this study was to assess the 24-hour shear bond strength of amalgam to glass ionomer cement, using five different intermediaries. The intermediaries used in this study were Scotchbond 2 (light curing dentin adhesive), Panavia (resin cement), liquid' of glass ionomer cement (chemical curing & light curing), and uncured mixture of light curing glass ionomer cement. This study was operated with 48 specimens devided into 6 groups. The experimental groups are as follows: Group 1 : Bonded Amalgam to chemical curing glass ionomer cement with liquid of chemical curing glass ionomer. Group 2 : Bonded Amalgam to light curing glass ionomer cement with liquid of chemical curing glass ionomer. Group 3: Bonded Amalgam to light curing glass ionomer cement with resin cement. Group 4: Bonded Amalgam to light curing glass ionomer cement with light curing dentin adhesive. Group 5: Bonded Amdlgam to light curing glass ionomer cement with liquid of light curing glass ionomer. Group 6: Bonded Amalgam to light curing glass ionomer cement with uncured mixture of light curing glass ionomer cement. 30 minutes after amalgam condensation, all specimens were stored for 24 hours in water at $37^{\circ}C$ and tested with Instron (1122). The following results obtained: 1. The shear bond strength of group 6 was higher than those of the other groups (46.7 kgf/$cm^2$, p<0.05). 2. The shear bond strength of resin cement intermediary group was lower than that of the group using uncured mixture of light curing glass ionomer cement. 3. The results of group 1 and group 2 were different, even though the inter-me diaries used were same. 4. Intermediary of Group 5 did not show complete set in Scanning Electromicroscopic examination. 5. Light-curing dentin adhesive did not show any bonding ability to amalgam.

  • PDF

Properties of artificial aggregates of coal bottom ash-dredged soil system added with waste glass (폐유리가 첨가된 석탄바닥재-준설토 계 인공골재의 특성)

  • Jo, Sinae;Kang, Seunggu
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.23 no.3
    • /
    • pp.146-151
    • /
    • 2013
  • In this study, the effect of addition of waste glassy slag produced from recycling of spent catalyst (denoted as waste glass hereafter) on the physical properties of artificial aggregates made of coal bottom ash and dredged soil (7 : 3 by weight base) was evaluated. Especially, the bloating behavior of artificial aggregates was analyzed by performing the relation study between the apparent density, water absorption and microstructure. The apparent density of artificial aggregates increased slightly with sintering temperature at $1050{\sim}1150^{\circ}C$, but decreased above $1150^{\circ}C$ showing bloating phenomenon. The bloating behavior of artificial aggregates was decreased so the apparent density increased with amount of waste glass added. Also, the water absorption of artificial aggregates decreased with sintering temperature. Above $1200^{\circ}C$, big fissure and much liquid were formed at the surface of artificial aggregates and these phenomena could be suppressed by increasing amount of waste glass added. The artificial aggregates fabricated in this study had an apparent density of 1.1~1.6 and water absorption of 8~22 % which meet KS requirements for the artificial lightweight aggregates.

Optical and mechanical properties of silicate film using a water glass (물유리를 이용한 실리카계 박막의 광학적 및 기계적 특성)

  • Lee, K.M.;Lim, Y.M.;Hwang, K.S.
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.5 no.2
    • /
    • pp.187-192
    • /
    • 2000
  • We prepared $SiO_2-Na_2O-R_mO_n$ thin films based on economics of water glass and investigated optical, mechanical properties of product thin films. Coating sol stabilized with 1 N HCl and 1 N $NH_4OH$, was fabricated by using water glass and calcium nitrate, and aluminum nitrate as starting materials. As-coated films on stainless steel, Si wafer and soda-lime-silica glass by spinning were finally annealed at 500, 750 and $900^{\circ}C$. Micro hardness and nitrogen content in film surface of annealed films were measured by Knoop hardness tester and EDX, respectively. Field Emission Scanning Electron Microscope (FE-SEM) and UV-VIS spectroscopy were adopted to analyze surface morphology and thickness and reflectance of our films.

  • PDF

Effects of salt water environment on the mechanical behavior of composites (복합재료의 기계적 거동에 염수환경이 미치는 영향에 관한 연구)

  • Moon, Jin-Bum;Kim, Soo-Hyun;Kim, Chun-Gon
    • Composites Research
    • /
    • v.23 no.1
    • /
    • pp.44-50
    • /
    • 2010
  • In this paper, two different experiments, namely, salt water spray and salt water immersion, were performed to reproduce the contact of composites with the seawater for three kinds of woven fabric composite material systems which would be used for the WIG(wing in ground effect)craft. After aging 140 days in the salt water environment, material properties of carbon/epoxy and glass/epoxy composite such as tensile, compressive and shear stiffness and strength, and inter-laminar shear strength (ILSS) were measured. By comparing baseline material properties with degraded ones, the effects of the salt water environment on the composite mechanical properties were evaluated. From the experiments, it was confirmed that the difference in aging conditions had very small influence on composite properties. And it was found that tensile strength of carbon/epoxy composites showed little degradation, but much more degradation was observed in glass/epoxy composites. And large degradations on matrix dominant properties were observed. The salt water could damage the fiber-matrix interface, matrix properties and the glass fiber.

Effect of coupling agent on the dielectric and mechanical properties of GFRP (GFRP의 유전적 및 기계적 특성에 미치는 계면결합제의 효과에 관한 연구)

  • 곽영순;신중홍;홍영기;조성수;박정후
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1988.10a
    • /
    • pp.43-45
    • /
    • 1988
  • This paper deals with the effect amino silane coupling agent for the composite insulating material (GFRP). Three kinds of coupling agent treatments are studied, that is treatment on glass fiber, epoxy resin and both glass fiber and epoxy resin. The result shows that the optimum electrical and mechanical properties is obtained for the sample treated on the glass fiber with 0.3% amino silane water solution.

  • PDF

A Study on the Manufacture of the Water Sensor (물방울 감지 센서의 제작에 관한 연구)

  • Kim, Jin Kook;Lee, Yun Min
    • Journal of Korea Society of Digital Industry and Information Management
    • /
    • v.10 no.2
    • /
    • pp.37-45
    • /
    • 2014
  • This paper is a study of the water sensor using a coaxial cavity resonator. This water sensor uses the resonant frequency variation of the coaxial cavity resonator when there is a water drop of the used coaxial cavity resonator. And we made resonant frequencies by controlling the input voltage of the oscillator which will be mainly resonated in the coaxial cavity resonator. First, we made the coaxial cavity resonator by simulating the resonator structure with the proposed size and we expect the resonant frequency from the simulation and then we decide the VCO from the result. Second, we made the water drop detecting sensor circuit and measured the water sensor. We decided the size of the resonator as inner conductor 5mm, outer conductor 14mm, the height of resonator 9.5mm, and the height of the glass 6mm from the simulated result. The simulated resonant frequencies are 3.09GHz and we made the VCO frequency ranges from 2.56GHz to 3.2GHz. The measured resonant frequency is 2.97GHz and the return loss is under -8. 4 dB at the center frequency. When the water is dropped on the glass of the resonator, the voltage has changed from 690mV to 145mV. It shows the proposed water sensor can detect the water by the resonant frequency variation of the resonator.

Adsorption Treatment of Azo Dye Containing Wastewater using Activated Carbon and Glass Fiber as an Adsorbent (활성탄과 유리섬유를 흡착제로 이용한 아조염료 함유 폐수의 처리)

  • Baek, Mi-Hwa;Jeon, Hyein;Lee, Ji-Ae;Kim, Dong-Su
    • Journal of Korean Society on Water Environment
    • /
    • v.25 no.3
    • /
    • pp.370-374
    • /
    • 2009
  • Adsorption characteristics of glass fibers, obtained from the spent lithium primary batteries recycling process, were investigated for the removal of Acid Red 27 dye from aqueous solution. The batch data clearly showed that increasing the initial sorptive concentration apparently enhanced the amount adsorbed and the uptake process followed the pseudo-second order rate model. The equilibrium adsorption data at different initial sorptive concentrations were fitted well to Freundlich and Langmuir adsorption isotherms. Moreover, the increase in temperature, favored the uptake of dye on this solid, indicated the process was endothermic in nature. Further, using the temperature dependence sorption data obtained at different temperatures was used to estimate various thermodynamic parameters.

Comparative Study of Fluidized Bed-type and Assmann Psychrometer (유동층습도계와 아스만습도계의 비교 연구)

  • 강희찬;강민철
    • Korean Journal of Air-Conditioning and Refrigeration Engineering
    • /
    • v.15 no.9
    • /
    • pp.779-785
    • /
    • 2003
  • The present work proposed a newly developed fluidized bed-type psychrometer that could be applicable to the high temperature and contaminant gases. The psychrometer is a device that test gas passes through the water in a glass bottle as a bubbly flow to obtain the adiabatic saturation temperature. A fluidized bed-type psychrometer was made and its characteristics were compared with the Assmann Psychrometer. The characteristic time was in the order of a hundred seconds, and decreased for the decrease of the mass of water and the increase of the air flow rate. The air flow rate and the insulation of the glass bottle were definitely important in the accurate measurement of the wet bulb temperature. The error in wet bulb temperature became less than 5 percent of the difference of dry and wet bulb temperatures if the air velocity in the glass bottle was greater than 1.5m/s.