• 제목/요약/키워드: Warm Deep Drawing

검색결과 68건 처리시간 0.035초

AZ31 합금의 온간 사각 컵 디프 드로잉 공정에서의 성형성에 관한 연구 (A study on formability of AZ31 alloy sheets in square cup deep drawing process at temperature elevated)

  • 김민철;이영선;권용남;김상우;이정환
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2005년도 추계학술대회 논문집
    • /
    • pp.235-238
    • /
    • 2005
  • In this study, it is investigated that the effect of material properties such as strength coefficient and strain hardening exponent on formability of AZ31 alloy sheet in square cup deep drawing process. Mechanical properties of AZ31 alloy sheet at elevated temperature $250^{\circ}C$ are obtained from uniaxial tensile tests and based on these results, a series of square cup deep drawing tests at the same temperature condition are carried out. Also, the possibilities of necking initiation is predicted by the FEM and FLD and compared with experimental results.

  • PDF

Clad Sheet(Mg-Al-SUS) 성형성에 관한 해석 기법의 연구 (A Study of the FEM Method on the Clad Sheet Metal Formability)

  • 정택우;이영선;김대용;문영훈
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2009년도 추계학술대회 논문집
    • /
    • pp.399-402
    • /
    • 2009
  • The Clad sheet is made roll-bonding process of the one or more material with the different property. Good formability is an essential property in order to deform a clad metal sheet to a part or component. In this study, the mechanical properties and formability of a Mg-Al-SUS clad sheet are investigated. The clad sheet was deformed at elevated temperatures because of its poor formability at room temperature. Tensile tests of the each material and clad sheet were performed at various temperatures and at various strain rates. The limited draw ration (LDR) was obtained using a deep drawing test to measure the formability of the clad sheet. A finite element (FE) analysis was performed to predict formability of the cup drawing product, one_layer model and three_layer model.

  • PDF

AZ31B 마그네슘판재의 온간, 열간 딮드로잉 성형성 평가 (The Drawbility Estimation in warm and Hot Forming of AB31B Magnesium Sheet)

  • 추동균;오세웅;이준희;강충길
    • 소성∙가공
    • /
    • 제14권7호
    • /
    • pp.628-634
    • /
    • 2005
  • The drawability of AZ31B magnesium sheet is estimated at various temperatures (200, 250, 300, 350, $400^{\circ}C$), forming speeds (20, 50, 100mm/min), thicknesses (0.8, 1.4mm) and blank holding forces (2.0, 2.8, 3.4kN). The deep drawing process (DDP) of circular cup is used in forming experiments. The results of deep drawing experiments show that the drawability is well at the range from 250 to $300^{\circ}C$, 50mm/min forming speed and 2.0kN blank holding force. The 0.8mm magnesium sheets were deformed better than 1.4 mm. Blank holding force was controlled in order to improve drawability and prevent the change of cup thickness. When blank holding force was controlled, tearing and thickness change were decreased and limit drawing ratio was improved from 2.1 to 3.0.

다이캐스팅 공정의 대체를 위한 마그네슘판재의 온간, 열간 ???K드로잉 성형성 평가 (The Drawbility Estimation in Warm and Rot Sheet Forming Process of Magnesium for Substitution of Die-casting Process)

  • 추동군;오세웅;이준희;강충길
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2005년도 춘계학술대회 논문집
    • /
    • pp.407-410
    • /
    • 2005
  • The drawability of AZ31B magnesium sheet is estimated according to the variable temperatures (200, 250, 300, 350 and $400^{\circ}C$), forming speed (20, 50, 100 mm/min), thickness (0.8, 1.4 t), blank holding force (1.0, 1.4, 1.7kN). The deep drawing process (DDP) of circular cup is used in forming experiments. The results of deep drawing experiences show that the drawability is well at the range from 250 to $300^{\circ}C$, 50mm/min forming speed and 1.4kN blank holding force. The 0.8t magnesium sheets were deformed better than 1.4t. BHF was controlled in order to improve drawability and protect the change of cup thickness. When BHF was controlled, tearing and thickness change were decreased and LDR. was improved from 2.1 to 3.0.

  • PDF

유한요소법과 연성파괴이론에 의한 AZ31합금 판재의 온간 드로잉 공정에서의 파단예측 (Failure Prediction for an AZ31 Alloy Sheet during Warm Drawing using FEM Combined with Ductile Fracture Criteria)

  • 김상우;이영선
    • 소성∙가공
    • /
    • 제21권4호
    • /
    • pp.258-264
    • /
    • 2012
  • The forming failure of AZ31 alloy sheet during deep drawing processes was predicted by the FEM and ductile fracture criteria. Uniaxial tensile tests of round-notched specimens and FE simulations were performed to calculate the critical damage values for three ductile fracture criteria. The critical damage values for each criterion were expressed as a function of strain rate at various temperatures. In order to determine the best criterion for failure prediction, Erichsen cupping test under isothermal conditions at $250^{\circ}C$ were conducted. Based on the plastic deformation histories obtained from the FE analysis of the Erichsen cupping tests and the critical damage value curves, the initiation time and location of fracture were predicted under bi-axial tension deformation. The results indicate that the Cockcroft-Latham criterion had good agreement with the experimental data. In addition, the FE analysis combined with the criterion was applied to another deep drawing process using an irregular shaped blank and these additional results were verified with experimental tests.

마그네슘 합금 AZ31 판재의 온간 사각컵 딥드로잉 성형성의 유한요소 해석 (Finite-Element Analysis of Formability in Warm Square Cup Deep Drawing of Magnesium Alloy AZ31 Sheet)

  • 김흥규;이위로;홍석관;한병기;김종덕
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2005년도 추계학술대회 논문집
    • /
    • pp.122-125
    • /
    • 2005
  • Magnesium alloys are expected to be widely used for the parts of structural and electronic applications due to their lightweight and EMI shielding characteristics. While the die casting has been mainly used to manufacture the parts from the magnesium alloys, the press forming is considered as an alternative to the die casting for saving the manufacturing cost and improving the structural strength of the magnesium alloy parts. However, the magnesium alloy has low formability at room temperature and therefore, in many cases, forming at elevated temperatures is necessary to obtain the required material flow without failure. In the present study, square cup deep drawing tests using the magnesium alloy AZ31 sheet were experimentally conducted at various elevated temperatures as well as room temperature, and the corresponding finite-element simulations, which calculated the damage evolution based on the Oyane's criterion, were conducted using the stress-strain relations from the tensile tests at various temperatures. The formability predictability by the finite-element analysis was investigated by comparing the predicted damage distributions over the deformed AZ31 sheet at elevated temperatures with the corresponding experimental deformations with failures.

  • PDF

가열냉각방법에 의한 마그네슘합금의 판재성형성 개선 (Improvement on the Formability of Magnesium Alloy Sheet by Heating and Cooling Method)

  • 강대민
    • 한국자동차공학회논문집
    • /
    • 제13권6호
    • /
    • pp.93-98
    • /
    • 2005
  • The purpose of this study is to confirm the improvement of formability of AZ31 magnesium alloy sheet by using local heating and cooling technique. For this, the experiments of warm deep drawing were done under the temperatures of $100^{\circ}C\~400^{\circ}C$, and the punch velocity of 10, 100mm/min. Also FE analysis under the temperatures of blankholder and die of $150^{\circ}C,\;225^{\circ}C\;and\;300^{\circ}C$ for tools(holder and die) was executed with considering heat teansfer. From the results, the formability of AZ31 magnesium alloy, espicially the temperatures of $225^{\circ}C\~250^{\circ}C$ for tools(holder and die)improved remarkably. And the experiments and simulations showed that necking under room temperature for tools occured under the part of punch shoulder while at $300^{\circ}C$ for tools, at the part of die shoulder.

마그네슘 합금 AZ31 판재의 온간 사각컵 디프드로잉 공정의 유한요소 해석 (Finite-Element Analysis of Warm Square Cup Deep Drawing Process of Magnesium Alloy AZ31 Sheet)

  • 김흥규;이위로;홍석관;김종덕;한병기
    • 소성∙가공
    • /
    • 제15권3호
    • /
    • pp.232-240
    • /
    • 2006
  • Magnesium alloys are expected to be widely used fur the parts of structural and electronic appliances due to their lightweight and EMI shielding characteristics. While the die casting has been mainly used to manufacture the parts from the magnesium alloys, the press forming is considered as an alternative to the die casting for saving the manufacturing cost and improving the structural strength of the magnesium alloy parts. However, the magnesium alloy has low formability at room temperature and therefore, in many cases, forming at elevated temperatures is necessary to obtain the required material flow without failure. In the present study, square cup deep drawing tests using the magnesium alloy AZ31 sheet were experimentally conducted at various elevated temperatures as well as room temperature, and the corresponding finite-element simulations, which calculated the damage evolution based on the Oyane's criterion, were conducted using the stress-strain relations from the tensile tests at various temperatures. The formability predictability by the finite-element analysis was investigated by comparing the predicted damage distributions over the deformed AZ31 sheet at elevated temperatures with the corresponding experimental deformations with failures.

마그네슘 판재 온간 성형의 파단 예측 모델 비교 연구 (A Comparative Study of Failure Criteria for Magnesium Alloy Sheet under Warm Press Forming Condition)

  • 김흥규;김종덕;허영무;김우진
    • 소성∙가공
    • /
    • 제21권2호
    • /
    • pp.113-118
    • /
    • 2012
  • Magnesium sheet alloys possess limited plastic formability at room temperature but their formability is substantially improved at elevated temperatures and optimum strain rates. In the present paper, three different types of failure criteria, namely, strain-based, stress-based, and work-based criteria, are compared for their applicability to warm press forming of magnesium sheet alloys. Warm deep-drawing experiments were conducted on AZ31 alloy sheet, and the results were used to assess the strength and weakness of the failure criteria.