크랭크 프레스와 유압 프레스에서 스테인리스 강판의 온간 드로잉성 비교 (Comparison of Warm Deep Drawability of Stainless Sheet Between Crank Press and Hydraulic Press)

  • 김종호;최치수;나경환
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1995년도 춘계학술대회논문집
    • /
    • pp.178-185
    • /
    • 1995
  • Warm deep drawing for optimum forming conditions to give the maximum drawing depth is investigated and compared with the results at room temperature. Experiments which draw square cups of STS 304 stainless steel sheet under the constant lubrication condition of teflon film made both in a crank and hydrqulic press for two kinds of specimens . The maximum drawing depth at warm forming condition reaches 1.4 times the drawing depth at room temperature in a crank press, whereas 1.6 times in a hydrqulic press, and also more uniform distribution of thickness in case of warm deep drawn cup is observed. The effects of other factors on formability , such as forming temperature, speed of press and cooling of punch are examinnied and discussed.

  • PDF

온간 쇼트피닝에 의한 압축잔류응력의 변화 (The Improvement of Compressive Residual Stress by Warm Shot Peening)

  • 이승호;심동석;김기전
    • 한국표면공학회지
    • /
    • 제37권5호
    • /
    • pp.273-278
    • /
    • 2004
  • The requirements of getting spring steel with higher fatigue strength have been increased to achieve the weight reduction of a vehicle. As the possible increment in fatigue strength by using the conventional shot peening treatment is found to be limited, it is necessary to modify the shot peening treatment. In this study, to investigate the effects of warm shot peening on increasing fatigue strength, tests are conducted on spring steel SAE9524. By the results of rotating bending fatigue tests, the fatigue strength increases up to 23.8% in warm shot peening specimens at $200^{\circ}C$ compared with conventional shot peening. The major reason why the warm shot peening is effective to the improvement of fatigue strength is the increment of the compressive residual stress, which can be effectively formed by shot peening under the condition of warm temperature than room temperature.

고감성 의류용 Nylon/PP 온감 니트 소재의 물성 (The Physical Property of Nylon/PP Warm-up Knitted Fabric for High Emotional Garment)

  • 김현아;장홍원;허경;김승진;권상준
    • 한국염색가공학회지
    • /
    • 제26권1호
    • /
    • pp.22-31
    • /
    • 2014
  • This study investigated the physical properties of warm up yarns and their knitted fabrics including the dye affinity and color fastness to washing of these knitted fabrics according to the various dyeing times and temperatures on dyeing process. The results were summarized as follows. The tenacity of Nylon/PP warm-up yarn was 4g/d and breaking strain was 4.5%. The wet and dry thermal shrinkages were higher than those of PET warm-up yarn. The maximum heat flow rate(Qmax) of Nylon/PP warm-up knitted fabric was lower than that of PET warm-up knitted fabric and heat keeping rate(a) of Nylon/PP warm-up knitted fabric was higher as 47% than that of PET warm-up knitted fabric. It was shown that the shape retention and wearing comfort of Nylon/PP warm-up knitted fabric were better than those of PET warm-up knitted fabric. The dye-affinity(K/S) of Nylon/PP warm-up knitted fabric showed maximum value at the dyeing condition of 40minute or 50minute dyeing time with $80^{\circ}C$ dyeing temperature, but PET warm-up knitted fabric showed maximum value at the 30minute or 40minute with $110^{\circ}C$ dyeing temperature. Finally, the color fastness to washing of Nylon/PP warm-up knitted fabric showed good value as between 4 and 5 grade.

The Study on the Mechanical Properties with Various Control Cooling Conditions for Ball Joint Socket

  • Bae M.H.;Lee J.Y.;Jeong S.C.;Seo S.Y.;Kang S.W.;Lim K.H.
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2003년도 The 8th Asian Symposium on Precision Forging ASPF
    • /
    • pp.138-142
    • /
    • 2003
  • In this study, to show well favorable characteristics of warm forged material, we compared and analyzed microstructure and mechanical properties of general hot-forged material which finished heat treatment with warm-forged material which was produced by control cooling condition. Along with this, we suggested better direction of control cooling condition to be able to remove heat treatment process while satisfying mechanical properties.

  • PDF

오일팬용 재료의 온간 성형한계도에 관한 연구 (Study on the forming Limit Diagram of Steel Sheets for the Oil Pan of Automobile at the Warm Forming Condition)

  • 이항수;오영근;최치수
    • 소성∙가공
    • /
    • 제9권6호
    • /
    • pp.670-680
    • /
    • 2000
  • The purpose of this study is to provide the database of forming limit diagram applicable to the warm forming of oil pan. The test materials are SCP1 and SCP3C with the thickness of 1.4mm which is used for the oil pan of automobile. The testing temperature is 5$^{\circ}C$~15$0^{\circ}C$ which is In the range of practical usage. The results are the forming limit diagram limiting dome height and the maximum punch load at each temperature such as 5$^{\circ}C$, $25^{\circ}C$, 6$0^{\circ}C$, 9$0^{\circ}C$, 12$0^{\circ}C$ and 15$0^{\circ}C$. From these results, we can see that the forming limit curves are translated depending upon the temperature and that FLC at low temperature is higher than at high temperature. Both of limiting dome height and maximum punch load also decrease as the temperature increases. Present results can be useful for die trial and forming analysis as a tool of evaluating the forming severity for the sheet metal forming processes at the warm working condition by comparing the practical strains with FLC.

  • PDF

Comparison of Sound Absorption Performance between Fresh and Air-dried Leaves by Leaf Composition in Quercus glauca

  • Su Young Jung;Hee-Seop Byeon;Kwang-Soo Lee;Hyun-Soo Kim
    • 한국환경과학회지
    • /
    • 제32권1호
    • /
    • pp.25-35
    • /
    • 2023
  • The purpose of this study was to determine the optimal sound absorption conditions by comparing the sound absorption characteristics of fresh and air-dried leaves of Quercus glauca, the main species of evergreen broadleaf trees (EBLT) in southern Korea. The sound absorption coefficients (SACs) obtained under 18 conditions were comparatively analyzed. The SAC of air-dried leaves improved significantly with increasing leaf layer thickness. The highest average SAC in the fresh leaf group was 0.617, which was observed under the condition of a leaf specimen size of 0.5 × 0.5 cm2 and a leaf layer thickness of 1.75 cm. In a group of air-dried leaves, this was 0.615 under the condition of a leaf specimen size of 0.5 × 0.5 cm2 and a leaf layer thickness of 2.50 cm. The maximum value of SAC for each wavelength was observed under the condition of a leaf layer thickness of 2.50 cm consisting of 0.5 × 0.5 cm2 leaf specimens, ranging from 1,400 Hz to 1,500 Hz.

압연조건에 따른 AZ31 마그네슘합금판재의 변형거동 및 미세조직 변화 (Rolling of AZ31 Alloy and Microstructure of Rolled Plates)

  • 하태권;정효태;성환진;박우진
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2006년도 춘계학술대회 논문집
    • /
    • pp.63-66
    • /
    • 2006
  • The effect of warm rolling under various conditions on the microstructure and mechanical property was investigated using an AZ31 Mg alloy sheet. Several processing parameters such as initial thickness, thickness reduction by a single pass rolling, rolling temperature, roll speed, and roll temperature were varied to elicit an optimum condition for the warm rolling process of AZ31 Mg alloy. Microstructure and mechanical properties were measured for specimens subjected to rolling experiments of various conditions. Warm rolling of 30% thickness reduction per pass was possible without any side-crack at temperatures as low as $200^{\circ}C$ under the roll speed of 30 m/min. The initial microstructure before rolling was the mixed one consisting of partially recrystallized and cast structures. Grain refinement was found to occur actively during the warm rolling, producing a very fine grain size of 7 mm after 50% reduction in single pass rolling at $200^{\circ}C$. Yield strength of 204MPa, tensile strength of 330MPa and uniform elongation of 32% have been obtained in warm rolled sheets.

  • PDF

요소.포름알데히드 수지가공 셀룰로오스계 직물의 열특성 (The Thermal Characteristics of Cellulose Fabrics Finished with Urea-Formaldehyde Resin)

  • Song, Wha Soon
    • 한국염색가공학회지
    • /
    • 제5권4호
    • /
    • pp.79-91
    • /
    • 1993
  • The purpose of this study is to prepare the newer, more comfortable of urea-formaldehyde resin finished fabrics. The methods of this study are by making examinations and comparisons the relations between the thickness, fabrics counts, weight, moisture regain and crease recovery of cotton and viscose rayon fabrics caused by condition of urea-formaldehyde resin finishing and warm retaining ability and warm-cool sense. The analytic results of thermal character in state of fabrics material finished with urea-formaldehyde are as follows: 1. The warm retaining ability has no correlation with mixing ratio of resin but the increase of the warm retaining ability has correlation with the increase of concentration of urea-formaldehyde resin. 2. The result pf multiple regression analysis for effect of physical property according to the concentration of resin to the warm retaining ability revealed as below. As the weight, thickness and density increase and moisture regain decreases, the warm retaining ability increases. 3. The qmax value has no correlation with mixing ratio of resin but the increase of the qmax value has correlation with the increase of resin concentration. In the end, the effect of it promotes cool sense. 4. The result of multiple regression analysis for effect of physical property according to the concentration of resin to the qmax value revealed as below. As he weight and thickness increase, the qmax value decrease. But, as the density and crease recovery increase, the qmax value increase.

  • PDF