• 제목/요약/키워드: Wall Thinning Area

검색결과 48건 처리시간 0.021초

B-Scan 초음파 측정장비를 이용한 원전 배관 침식손상 검사법 개발 (Development of Inspection Methodology for a Nuclear Piping Wall Thinning Caused by Erosion Using Ultrasonic B-Scan Measurement Device)

  • 이대영;서혁기;황경모
    • Corrosion Science and Technology
    • /
    • 제11권3호
    • /
    • pp.89-95
    • /
    • 2012
  • U.S. Electric Power Research Institute (EPRI) has developed CHECWORKS program and applied it to power plant piping lines since some lines were ruptured by flow-accelerated corrosion (FAC) in 1978. Nowadays the CHECWORKS program has been used to manage pipe wall thinning phenomena caused by FAC. However, various erosion mechanisms can occur in carbon-steel piping. Most common forms of erosion are cavitation, flashing, liquid droplet impingement erosion (LDIE), and Solid Particle Erosion (SPE). Those erosion mechanisms cause pipe wall thinning, leaking, rupturing, and even result in unplanned shutdowns of utilities. Especially, in two phase condition, LDIE damages a wide scope of plant pipelines. Furthermore, LDIE is the major culprit to cause such as power runback by pipe leaking. This paper describes the methodologies that manage wall thinning and also predict LDIE wall thinning area. For this study, current properties of two-phase condition are investigated and LDIE areas are selected. The areas are checked by B-Scan method to detect the effect of wall thinning phenomena.

굽힘하중을 받는 배관의 파손에 미치는 감육의 영향 (Effect of Wall Thinning on the Failure of Pipes Subjected to Bending Load)

  • 안석환;남기우
    • 대한기계학회논문집A
    • /
    • 제29권4호
    • /
    • pp.606-613
    • /
    • 2005
  • Effects of circumferentially local wall thinning on the fracture behavior of pipes were investigated by monotonic four-point bending. Local wall thinning was machined on the pipes in order to simulate erosion/corrosion metal loss. The configurations of the eroded area included an eroded ratio of d/t= 0.2, 0.5, 0.6, and 0.8, and an eroded length of ${\ell}\;=10mm,$ 25mm, and 120mm. Fracture type could be classified into ovalization, local buckling, and crack initiation depending on the eroded length and eroded ratio. Three-dimensional elasto-plastic analyses were also carried out using the finite element method, which is able to accurately simulate fracture behaviors excepting failure due to cracking. It was possible to predict the crack initiation point by estimating true fracture ductility under multi-axial stress conditions at the center of the thinned area.

감육된 증기발생기 전열관의 유한요소 해석 (Finite Element Analysis for Wall Thinned Steam Generator Tubes)

  • 성기용;안석환;남기우
    • 동력기계공학회지
    • /
    • 제10권3호
    • /
    • pp.38-44
    • /
    • 2006
  • Failure assessment of steam generator tube are very important for the integrity of energy plants. In pipes of energy plants, sometimes, the local wall thinning may result from severe erosion-corrosion damage. Recently, the effects of local wall thinning on fracture strength and fracture behavior of piping system have been well studied. In this paper, the elasto-plastic analysis is performed by FE code ANSIS on steam generator tube with wall thinning. We evaluated the failure mode, fracture strength and fracture behavior from FE analysis. It was possible to predict the crack initiation point by estimating true fracture ductility under multi-axial stress conditions at the center of the thinned area.

  • PDF

감육예측 및 수치해석 기법을 활용한 소구경 탄소강배관 감육영향 분석에 관한 연구 (Technology Based on Wall-Thinning Prediction and Numerical Analysis Techniques for Wall-Thinning Analysis of Small-Bore Carbon Steel Piping)

  • 이대영;황경모;진태은;박원;오동훈
    • 대한기계학회논문집B
    • /
    • 제34권4호
    • /
    • pp.429-435
    • /
    • 2010
  • 국내를 포함한 전 세계 50여개 원전의 발전사업자는 유동가속부식에 의한 탄소강 배관 감육을 관리하기 위하여 CHECWORKS 프로그램을 이용하고 있다. CHECWORKS 프로그램은 대구경 배관에만 적용 가능한 것으로 알려져 있기 때문에 소구경 배관에 대해서는 현장 배관감육 관리 담당자의 경험과 판단에 따라 배관을 관리하고 있다. 이에 따라 본 논문에서는 국내 원전 소구경 배관 4개 라인그룹에 대하여 CHECWORKS 프로그램과 FLUENT 코드를 이용하여 유동가속부식과 유동 특성을 분석하였다. 그 결과 현장 배관감육 관리 담당자의 기술력에 따라 CHEC- WORKS 프로그램도 소구경 배관 감육 관리에 이용할 수 있는 것으로 나타났다.

급수가열기 추기노즐 충격판 주변의 동체감육 현상규명을 위한 실험 및 수치해석 연구 (A Study on Experiment and Numerical Analysis for Disclosing Shell Wall Thinning of a Feedwater Heater)

  • 김경훈;이우;황경모
    • 대한기계학회논문집B
    • /
    • 제31권1호
    • /
    • pp.1-7
    • /
    • 2007
  • Feedwater heaters of many nuclear power plants have recently experienced severe wall thinning damage, which will increase as operating time progresses. Several nuclear power plants in Korea have experienced wall thinning damage in the area around the impingement baffle - installed downstream of the high pressure turbine extraction steam line - inside number 5A and 5B feedwater heaters. At that point, the extracted steam from the high pressure turbine is two phase fluid at high temperature, high pressure, and high speed. Since it flows in reverse direction after impinging the impingement baffle, the shell wall of the number 5 high pressure feedwater heater may be affected by flow-accelerated corrosion. This paper describes the comparisons between the numerical analysis results using the FLUENT code and the down scale experimental data in an effort to determine root causes of the shell wall thinning of the high pressure feedwater heaters. The numerical analysis and experimental data were also confirmed by actual wall thickness measured by an ultrasonic test.

유동가속부식으로 인한 급수가열기 동체 감육현상 규명과 완화 방안 및 충격판 설계개선에 관한 연구 (A Study on the Shell Wall Thinning by Flow Acceleration Corrosion and Mitigation Plan and Design Modification of a Feedwater Heater Impingement Baffle)

  • 김경훈;황경모;김인태
    • 한국분무공학회지
    • /
    • 제15권2호
    • /
    • pp.83-93
    • /
    • 2010
  • Feedwater heaters of many nuclear power plants have recently experienced severe wall thinning damage, which will increase as operating time progresses. Several nuclear power plants in Korea have experienced wall thinning damage in the area around the impingement baffle inside feedwater heater installed downstream of the turbine extraction stream line. At that point, the extract steam from the turbine is two phase fluid at high temperature, high pressure, and high speed. Since it flows to reverse direction after impinging the impingement baffle, the shell wall of feedwater heaters may be affected by flow-accelerated corrosion. In this paper, to compare degree of shell wall thinning mitigation rate to squared type with mitigation rate of other type baffle plate, four different types of impingement baffle plate-squared, curved, mitigating type and multi-hole type-applied inside the shell. With these comparison data, this paper describes operation of experiments and numerical analysis which is composed similar condition with real feed water heater. And flow visualization is operated for verification of experiments and numerical analysis. In conclusion, this study shows that mitigating type and multi-hole type baffle plate are more effective than other baffle plate about prevention of pressure concentration and pressure value decrease.

급수가열기 동체 감육 현상과 완화 방안 및 충격판 설계개선 (Shell Wall Thinning and Mitigation Plan and Design Modification of a Feedwater Heater Impingement Baffle)

  • 김경훈;황경모;박상훈
    • 한국정밀공학회지
    • /
    • 제27권6호
    • /
    • pp.55-63
    • /
    • 2010
  • Feedwater heaters of many nuclear power plants have recently experienced severe wall thinning damage, which will increase as operating time progresses. Several nuclear power plants in Korea have experienced wall thinning damage in the area around the impingement baffle inside feedwater heater installed downstream of the turbine extraction stream line. At that point, the extract steam from the turbine is two phase fluid at high temperature, high pressure, and high speed. Since it flows to reverse direction after impinging the impingement baffle, the shell wall of feedwater heaters may be affected by flow-accelerated corrosion. In this paper, to compare degree of shell wall thinning mitigation rate to squared type with mitigation rate of other type baffle plate, three different types of impingement baffle plate-squared, curved and mitigating type-applied inside the shell. With these comparison data, this paper describes operation of experiments and numerical analysis which is composed similar condition with real feed water heater. And flow visualization is operated for verification of experiments and numerical analysis. In conclusion, this study shows that mitigating type baffle plate is more effective than other baffle plate about prevention of pressure concentration and pressure value decrease.

내압을 받는 외부 국부 감육 직관의 파손 기준 (Failure Criterion of Straight Pipe with Outer Local Wall Thinning under Internal Pressure)

  • 김수영;남기우
    • 동력기계공학회지
    • /
    • 제18권1호
    • /
    • pp.76-83
    • /
    • 2014
  • This study was carried out an experimental and finite element analysis on the fracture behavior of straight pipes with local wall thinning under internal pressure. Local wall thinning was machined on the pipes in order to simulate erosion/corrosion metal loss. The configurations of the eroded area has an eroded ratio of d/t=0.80~0.92 and an eroded length of l=25, 50 and 102 mm. Three-dimensional elastic-plastic analyses were also carried out using the finite element method, which is able to accurately simulate failure behaviors. In regards to the relation ship between pressure and eroded ratio, the criterion that can be used safely under operating pressure and design pressure were obtained from this calculation. The results of this calculation were in relatively good agreement with that of the experiment.

굽힘하중을 받는 배관의 파손에 미치는 감육의 영향 (Effect of wall Thinning on the Failure of Pipes Subjected to Bending Load)

  • 안석환;이수식;남기우
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2004년도 학술대회지
    • /
    • pp.242-246
    • /
    • 2004
  • Effects of circumferentially local wall thinning on the fracture behavior of pipes were investigated by monotonic four-point bending. Local wall thinning was machined on the pipes in order to simulate erosion/corrosion metal loss. The configurations of the eroded area included an eroded ratio of d/t= 0.2, 0.5, 0.6, and 0.8, and an eroded length of I = 10 mm, 25 mm, and 120 mm. Fracture type could be classified into ovalization, local buckling, and crack initiation depending on the eroded length and eroded ratio. Three-dimensional elasto-plastic analyses were also carried out using the finite element method, which is able to accurately simulate fracture behaviors excepting failure due to cracking. It was possible to predict the crack initiation point by estimating true fracture ductility under multi-axial stress conditions at the center of the eroded area.

  • PDF

두께 감소된 배관 엘보우의 파손 모드에 대한 연구 (A Study on Failure Mode of Pipe Elbows with Wall Thinning)

  • 신규인;윤기봉
    • 한국가스학회지
    • /
    • 제12권2호
    • /
    • pp.57-62
    • /
    • 2008
  • 배관 엘보우의 내호면(intrados)의 과 내부에 국부적으로 두께 감육이 발생한 경우, 내압과 엘보우를 닫는 방향으로의 굽힘하중을 부가하여 파손 모드를 연구하였다. 탄소성해석 시 반력-변위 곡선이 세 그룹으로 나뉘므로 각 그룹의 한 경우씩을 해석하여 소성붕괴에 의한 파손모드의 차이를 확인하였다. 이를 위해 주요 부위에서 하중-국부적응력 곡선이 어떻게 변화하는지 결정하여, 이로부터 관찰된 파손모드와 비교하여 설명하였다. 감육폭이 $90^{\circ}$인 경우 배관은 엘보우 측면부터 소성붕괴가 시작되었으며, $360^{\circ}$인 경우 내호면으로부터 소성변형이 시작되어 서로 다른 파손모드를 보여주었다. 배관의 감육측정에 의한 건전성 평가 시 이와 같은 파손 모드의 차이점을 고려하여 평가를 실시하여야 한다.

  • PDF