It was attempted to improve the wear resistance of Al alloy under the load condition by making a formation of the thick surface hardening alloy layers. The thick surface hardening alloy layers were formed on 6061 Al alloys overlayed by MIG welding process with WC-12%Co powder addition. Effects of the dispersion of WE-12%Co powders on hardness and wear characteristics of alloys were investigated. The following results were obtained. Most of WE-12%Co powders are dispersed nearly uniform as unmelted particles in the matrix alloy. A part of WC-12%Co powders are melted in the molten pool, and during solidification {TEX}$Al_{9}Co_{2}${/TEX} appeared. With increasing addition of WC-12%Co powders, the hardness and specific wear resistance of the overlay weld alloys increased and reached Hv450 at WC-12%Co powder addition rate of 54g/min. It is considered that excellent wear resistance of the overlayed alloys was due to dispersed WC-12%Co powders and increased 10 times at WC-12%Co powder addition rate of 54 g/min than that of the WC-free overlaying layers.
The microstructures and mechanical properties of submicron WC-Co cemented carbides were investigated in relation to cobalt content. To inhibit the WC grain growth during sintering, VC was added as a inhibitor in each alloy with 3 mass% to the cobalt content. The WC-(5, 8, 10, 15, 20) mass% Co compacts were sintered at $1400^{\circ}C$ for 30 min in vacuum. Some of WC-(5, 8, 10) mass% Co sintered compacts were HIPed with 120 atm at 130$0^{\circ}C$ for 1 hr. The shrinkages of all HIPed alloys were increased without depending on the cobalt contents and the sintered densities of them. The relative densities of the alloys were increased with the cobalt content and HIPing. The less the cobalt content, the larger the WC grain. Many contiguities of WC grains were found in WC-5 mass% Co alloy. The sizes and numbers of pores in the alloys were decreased by HIPing. And also the strength and the hardness of each alloy were increased. The maximum hardness was about 18.95 GPa in the WC-5 mass% Co alloy HIPed and the maximum transverse-rupture strength (T.R.S.) 3.2 GPa in the WC-20 mass% Co alloy sintered.
Journal of the Korean Society of Manufacturing Technology Engineers
/
v.6
no.2
/
pp.102-111
/
1997
This paper deals with the machinability based on turning of WC-Co allows with the coated and the sintered diamond tools. The main conclusions obtained are as follows. (1) When machining WC-10%Co alloy, the flank wear of sintered diamond tool increases more largely with the increase of cutting speed in comparison with coated diamond tool. The tool wear decreases with the increase of the grain size and nose radius of sintered diamond tool. (2) When machining WC-20%Co alloy, the tool wear and cutting force decrease with the decrease of rake angle. Their exists a certain cutting speed range to exhibit the smallest tool wear in machining the WC-20%Co alloy, and this critical cutting speed becomes higher by 2 times in the case of coated diamond tool compared with sintered diamond tool. (3) The machinability becomes better with the increase of Co content. The effects of cutting speed and feed rate on the roughness of machined surface become smaller with the increase of Co content.
The purpose of this paper is to investigate polarization characteristics of WC-based alloy coatings in alkaline solution. The coatings were fabricated with WC-CrC-Ni, WC-Co-Cr and WC-Co composite powders by HVOF process. Corrosion tests of coatings and substrate were carried out using potentiostat/galvanostat at solution with pH 8 and pH 13. Corrosion potential(Ecorr) and corrosion current density(Icorr) could be studied from polarization curve, and corrosion behavior was analyzed by SEM and EDS. WC-Co-Cr coating and WC-CrC-Ni coating showed more favorable anti-corrosion characteristics than WC-Co coating and substrate at solution with pH 8 and pH 13.
The aim of this study to investigate polarization characteristics of WC-based alloy coatings fabricated by high velocity oxygen fuel(HVOF) process. The coatings were fabricated by HVOF process with WC-CrC-Ni, WC-Co-Cr, WC-Co composite powders. Corrosion tests were carried out using potentiostat/galvanostat at solution with pH 2 and pH 6. Corrosion potential(Ecorr) and corrosion current density(Icorr) could be analyzed from polarization curve. WC-Co-Cr coating showed more incorrodible characteristics than other coatings at solution pH 2. WC-CrC-Ni coating was more favorable anti-corrosion characteristics than other coatings at solution with pH 6.
The dispersion of WC grains Into the interior of an eutectic liquid has been studied by superimposing the eutectic WC-85wt.%Co liquid on the top surface of presintered WC-l0wt.%Co alloy compacts. The heavy WC grains diffused into the interior of liquid from the WC-l0wt.%Co compacts. According to increasing the treating temperatures and times, the dispersion distance from WC-l0wt.%Co substrates increased. The fine WC grains diffused into the liquid faster than the coarse WC grains. The high microstructural stability of WC-Co alloys having the heavier WC grains dispersed in a lighter Co-rich liquid was attributed to Brownian motion of WC grains in liquid. The motion of WC grains in the liquid appears to be same with the colloid(the disperse phase) in a dispersing medium. The dihedral angle of 0 degree of WC-Co at. toy seems one of key parameters, which enables the WC-Co alloys to have high structural stability without settling the WC grains during liquid phase sintering.
Ultrafine TiC-5%Co powders were synthesized by spray drying of aqueous solution of TiO$(OH)_2$ slurry and cobalt nitrate, followed by calcination and carbothermal reaction. The oxide powders with carbon powder was reduced and carburized at $900^{\circ}C{\sim}1250^{\circ}C$ under hydrogen atmosphere. During reduction, CO gas was mainly evolved by reducing reaction of oxides. Ultrafine TiC-5%Co powders were easily formed by carbothermal reaction at $1250^{\circ}C$ due to using ultrafine powders as raw materials. The ultrafine WC-TiC-Co alloy prepared by sintering of mixed powder of ultrafine WC-13%Co powder and ultrafine TiC-5%Co powder has higher sintered density and mechanical properties than WC-TiC-Co alloy prepared by commercial WC, TiC and Co powders.
Norgren, Susanne;Kusoffsky, Alexandra;Elfwing, Mattias;Eriksson, Anders
Proceedings of the Korean Powder Metallurgy Institute Conference
/
2006.09a
/
pp.338-339
/
2006
The solubility of Cr in cubic carbides in the systems WC-Co-TaC and WC-Co-ZrC has been determined using equilibrium samples. Thermodynamic calculations were used to design the alloys through extrapolations of Gibbs energy expressions. The alloys were designed to have a microstructure containing the following phases: WC, liquid, $M_7C_3$, graphite and cubic carbide. The alloys were investigated using scanning electron microscopy and analyzed using energy-dispersive X-ray spectrometry. The present work shows how the Cr solubility depends on which cubic carbide former that is present. The WC-Co-Cr-Zr alloy has no detectable amount of Cr whereas the WC-Co-Cr-Ta alloy has 12% Cr in the cubic carbide.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.