• Title/Summary/Keyword: WC

Search Result 1,031, Processing Time 0.028 seconds

Effect of Manganese on the Microstructure of Cemented Carbides

  • Weidow, Jonathan;Norgren, Susanne;Elfwing, Mattias;Andren, Hans-Olof
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.348-349
    • /
    • 2006
  • The plastic deformation behavior of cemented carbides is related to the WC grain boundary strength. Ab initio calculations predict that Co and Mn segregate to WC/WC grain boundaries. To experimentally study the effect of Mn, a WC-Co-Mn material was manufactured and compared to a WC-Co material. The microstructure was studied using scanning electron microscopy (SEM), including electron backscatter diffraction (EBSD). Special attention was paid to the WC grain size and the frequency of special low-energy grain boundaries. Mn was found to have negligible effect on both the WC grain growth and the fraction of $\sum2$ WC/WC boundaries in the as-sintered material.

  • PDF

Long-Term Performance Evaluation on the Recycled Asphalt Concrete Using the Steel Slag and Reclaimed Asphalt Pavement Aggregates (제강 슬래그 및 순환골재를 사용한 순환 아스팔트 혼합물의 장기 공용성 평가)

  • Park, Kyung-Won;Jang, Dong-Bok;Lee, Jong-Min;Kang, Byung-Hwa;Kim, Hyung-Bae
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.9 no.4
    • /
    • pp.633-641
    • /
    • 2021
  • The study performed long-term performacne evaluation on the hot mix asphalt using the steel slag aggregates and Reclaimed Asphalt Pavement (RAP). The laboratory comparative evaluation was conducted between conventional Hot Mix Asphalt (HMA) which is entitled WC-2 and HMA containing steel slag and RAP which is entitled ES WC-2(R). Dynamic stability test, dynamic modulus test, and fatigue crack test were conducted during the comparative evaluation process. The dynamic stability test result showed that ES WC-2(R) was 140% higher than WC-2. It is noted that ES WC-2(R) showed no inflection point whereas WC-2 showed inflection point during the dynamic stability test which implies ES WC-2(R) has the higher moisture susceptability than WC-2. The dynamic modulus of ES WC-2(R) were 342.3%, 486.7%, and 350.0% higher than WC-2 at medium temperature of 21℃, low temperature of -10℃, and high temperature of 38℃ respectively. The test result showed that rutting resistance of ES WC-2(R) is higher than WC-2 at all temperature spectrum. The fatigue resistance of ES WC-2(R) were 31.7%, 325.3%, 899.9% higher at low stress level, medium stress level, and high stress level, respectively. The test result showed that ES WC-2(R) is higher than WC-2 at all stress levels. Based on the laboratory comparative evaluation, The in-situ scale Accelerated Pavement Test (APT) was conducted comparing WC-2 and WC-2(R). APT found that the rutting resistance of WC-2(R) was 45% higher than WC-2.

Fabrication of Ultra fine WC-Ni Hard Materials by Rapid Sintering Process

  • Kim Hwan-Cheol;Oh Dong-Young;Shon In-Jin
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2004.11a
    • /
    • pp.98-99
    • /
    • 2004
  • (1) Using high-frequency induction heating sintering and spark plasma sintering method, the densification of WC-Ni hard materials was accomplished using ultra fine power of Ni and WC. (2) Nearly fully dense WC-Ni could be obtained within 1 min. (3) Relative density and mechanical properties of WC-Ni obtained by HFIHS were high than those obtained by SPS. And WC grain size made by HFIHS was smaller than that made by SPS. (4) The fracture toughness and hardness values of WC-8Ni, WC-10Ni, and WC-12Ni made by HFIHS were $13MPa{\cdot}m^{1/2}\;and\;1950kg/mm^2,\;13.5Mpa{\cdot}m^{1/2}\;and\;1810kg/mm^2,\;14.4MPa{\cdot}m^{1/2}\;and\;1690kg/mm^2$, respectively for 60MPa and an induced current for 90% output of total capacity, 15KW. (5) The fracture toughness and hardness values of WC-8Ni, WC-10Ni, and WC-12Ni made by SPS were $12.2MPa{\cdot}m^{1/2}\;and\;1796kg/mm^2,\;12.9MPa{\cdot}m^{1/2}\;and\;1725kg/mm^2,\;13.6MPa{\cdot}m^{1/2}\;and\;1597kg/mm^2$, respectively for 60MPa and the electric current of 2500 A

  • PDF

A Study on Variation of Colony Forming Units of Heterotrophic Bacteria by Input Ratios of Bulking Materials in Aerobic Composting of Food Wastes (음식물류폐기물의 호기성 퇴비화에 있어서 팽화재 투입비에 따른 타가영양세균의 균락형성단위의 변화에 관한 연구)

  • Park, Seok-Hwan
    • Journal of Environmental Health Sciences
    • /
    • v.32 no.4 s.91
    • /
    • pp.353-358
    • /
    • 2006
  • This study was performed to evaluate the effects of input ratios of bulking material in aerobic composting of food wastes on variation of colony forming units of heterotrophic bacteria. Wood chips were used as a bulking material. Volume ratios of food wastes to wood chips in reactor of Control, WC-1 and WC-2 were 10/0, 10/5 and 10/10, respectively. Reactors were operated for 24 days with 1hour stirring by 1rpm and 2 hours of the forced aeration per day. WC-2 reached high temperature range faster than WC-1, and the maximum temperature of WC-2 was higher than that of WC-1. This means that the reaction velocity of composting of WC-2 was faster than that of WC-1. Judging from the profile of pH changes, composting of WC-1 proceeded slowly and continuously. Composting of WC-2 proceeded rapidly in the former half reaction period, and kept steady state of high pH in the latter half reaction period. Namely, composting of WC-2 was nearly completed in the former half reaction period. In the case of WC-1 and WC-2. the maximum temperature was followed by the rapid pH increase in 2-3 days, and this was followed by the maximum Colony Forming Units(CFU) in 3 days. But, these three items of WC-2 always appeared faster and higher than those of WC-1.

EFFECTS OF CO CONTENT AND WC GRAIN SIZE ON WEAR OF WC CEMENTED CARBIDE

  • Saitoh, Hiroyuki;Iwabuchi, Akira;Shimizu, Tomoharu
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2002.10b
    • /
    • pp.213-214
    • /
    • 2002
  • WC cemented carbide are used as many die material to improve abration resistance. Mechanical properties of the cemented carbide were influenced by Co content and WC grain size. In this study, effects of Co content and WC grain size of WC cemented carbide on wear were examied. We prepared 13 cemented carbides with different Co content and WC grain size. Wear test was carried out against S45C under dry condition at 98N and 232mm/s. From the results, we found that wear increased with both Co content and WC grain size. Specific wear rate was range $10^{-7}mm^3/Nm$.

  • PDF

Effect of the WC particle size and Co content on the adhesion property between AIP-TiN coating and WC-Co substrate (AIP-TiN/WC-Co계에서 WC입자크기와 Co함량이 밀착력에 미치는 영향)

  • 한대석;류정민;권식철;김광호
    • Journal of the Korean institute of surface engineering
    • /
    • v.35 no.3
    • /
    • pp.165-171
    • /
    • 2002
  • TiN coating were deposited onto different WC-Co substrates using arc ion plating (AIP) technique. The structure and morphology for the deposited coating were characterized by x-ray diffraction (XRD) and scanning electron microscopy (SEM). The adhesion behavior of the deposited TiN coating was investigated with a conventional scratch test. Effects of WC particle size and Co content on the adhesion strength between the deposited TiN coating and substrate were studied. During the scratch test, the value of critical load was dependent of WC particle size and Co content on substrate. As the WC particle size and Co content on substrate decreased, the critical load increased. The highest critical load, approximately 110N, was obtained at WC particle size of 1$\mu\textrm{m}$ and Co content of 10wt.%.

Effect of WC and group IV Elements of Ti(C,N) on the Intermittent Cutting Performance (Ti(C,N)계 서메트 공구의 WC와 IV족 원소 첨가가 단속 절삭성능에 미치는 영향)

  • 박준석;김경재;권원태;강신후
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 1997.10a
    • /
    • pp.919-922
    • /
    • 1997
  • In this study, the amount of WC and group N elements of Ti(C, N) cermet tool was investigated. The composition of WC was changed from 5 to 20% to determine the effect of WC on the cutting performance of cermet tool. The more WC was added, the longer the tool life of the cermet tool was. The cermet with 20% WC showed the best fracture toughness. The effect of group N elements ; ZrC, ZrN and HfC was also investigated by adding each of them to manufacture the cermet tool with fixed 14% WC composition. The cermet with 1% group N ZrC and 14% WC showed the best cutting performance among the investigated cermet tools.

  • PDF

Consolidation of Binderless and Low-Binder WC hardmetal by Vacuum Sintering (진공 소결공정에 의한 고밀도 바인더리스 및 극저바인더 초경합금의 제조)

  • Min, Byoung-June;Park, Young-Ho;Lee, Gil-Geun;Ha, Gook-Hyeon
    • Journal of Powder Materials
    • /
    • v.14 no.5
    • /
    • pp.315-319
    • /
    • 2007
  • Pure WC or WC with low Co concentration less than 0.5 wt.% is studied to fabricate high density WC/Co cemented carbide using vacuum sintering and post HIP process. Considering the high melting point of WC, it is difficult to consolidate it without the use of Co as binder. In this study, the effect of lower Co addition on the microstructure and mechanical properties evolution of WC/CO was investigated. By HIP process after vacuum sintering, hardness and density was sharply increased. The hardness values was $2,800kgf/mm^2$ using binderless WC.

Contribution of the Interface Energies to the Growth Process of Cemented Carbides WC-Co

  • Lay, Sabine;Missiaen, Jean-Michel;Allibert, Colette H
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.332-333
    • /
    • 2006
  • The driving forces and the probable processes of WC-Co grain growth are reanalysed from recent data of interface energy and microstructure. Grain growth is driven by the disappearing of the high energy WC/WC and WC/Co interfaces with habit planes different from {0001}, ${10\bar{1}0}$ and ${11\bar{2}0}$ facets and by the area decrease of the WC/WC and WC/Co interfaces with {0001} and ${10\bar{1}0}$ habit planes. Grain growth mainly results of dissolution-precipitation. Abnormal grains are likely formed by defects assisted nucleation.

  • PDF

Measurement of WC Grain Size in Nanocrystalline WC-10Co Hardmetal

  • Chenguang, Lin;Guansen, Yuan
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.344-345
    • /
    • 2006
  • The linear intercept (LI) method was used to quantitatively measure the intercepts of WC grains in nano-grained WC-10Co hardmetal. When the surveyed intercept numbers of WC grain exceeded 200, the statistic data for the mean grain size of WC were reproduced. The discriminative minimal grain size of used LI method was 12 nm; the maximum intercept of WC grain was 109 nm; the average intercept of WC grains was 45 nm and the corresponding 3D mean grain size of WC was 70 nm which is agreeable with the XRD outcome.

  • PDF