Effect of Manganese on the Microstructure of Cemented Carbides

  • Weidow, Jonathan;Norgren, Susanne;Elfwing, Mattias;Andren, Hans-Olof
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.348-349
    • /
    • 2006
  • The plastic deformation behavior of cemented carbides is related to the WC grain boundary strength. Ab initio calculations predict that Co and Mn segregate to WC/WC grain boundaries. To experimentally study the effect of Mn, a WC-Co-Mn material was manufactured and compared to a WC-Co material. The microstructure was studied using scanning electron microscopy (SEM), including electron backscatter diffraction (EBSD). Special attention was paid to the WC grain size and the frequency of special low-energy grain boundaries. Mn was found to have negligible effect on both the WC grain growth and the fraction of $\sum2$ WC/WC boundaries in the as-sintered material.

  • PDF

제강 슬래그 및 순환골재를 사용한 순환 아스팔트 혼합물의 장기 공용성 평가 (Long-Term Performance Evaluation on the Recycled Asphalt Concrete Using the Steel Slag and Reclaimed Asphalt Pavement Aggregates)

  • 박경원;장동복;이종민;강병화;김형배
    • 한국건설순환자원학회논문집
    • /
    • 제9권4호
    • /
    • pp.633-641
    • /
    • 2021
  • 본 연구에서는 철강산업 부산물인 제강슬래그 및 폐아스팔트 콘크리트포장 파쇄물인 순환골재를 사용하여 아스팔트 혼합물용 천연골재를 대체 가능성을 파악하고 제강슬래그를 활용한 아스팔트 혼합물의 공용성 평가를 수행하였다. 일반 WC-2와 Slag WC-2(R)에 대한 평가는 동일한 조건으로 수행하였으며, 수행기관은 국가 공인시험기관(KTR) 및 한국도로학회로 각 기관의 연구용역을 통해 평가되었다. 동적안정도, 동탄성계수, 피로균열 시험결과 슬래그 아스팔트 혼합물이 일반 아스팔트 혼합물에 비해 각각 140%, 저온·고온 487·350%, Low·Middle·High Stress Level 32·325·900% 증가하는 것으로 조사되었다. 함부르크 휠 트래킹 시험결과 두 가지 혼합물의 수분저항성이 우수한 것으로 조사되었으나, 슬래그 아스팔트 혼합물 시험결과에 변곡점이 없고 변위발생량이 낮아 일반 혼합물 대비 우수한 것으로 조사되었다. 장기공용성 평가(APT) 결과 슬래그 아스팔트 혼합물에서 소성변형 발생량이 6.5% 적게 발생하였으며, 표층, 기층 및 하부층의 압축량을 분석한 결과 슬래그 포장도로의 표층 소성변형 저항성이 45% 높게 조사되었다.

Fabrication of Ultra fine WC-Ni Hard Materials by Rapid Sintering Process

  • Kim Hwan-Cheol;Oh Dong-Young;Shon In-Jin
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2004년도 International Symposium on Powder Materials and Processing
    • /
    • pp.98-99
    • /
    • 2004
  • (1) Using high-frequency induction heating sintering and spark plasma sintering method, the densification of WC-Ni hard materials was accomplished using ultra fine power of Ni and WC. (2) Nearly fully dense WC-Ni could be obtained within 1 min. (3) Relative density and mechanical properties of WC-Ni obtained by HFIHS were high than those obtained by SPS. And WC grain size made by HFIHS was smaller than that made by SPS. (4) The fracture toughness and hardness values of WC-8Ni, WC-10Ni, and WC-12Ni made by HFIHS were $13MPa{\cdot}m^{1/2}\;and\;1950kg/mm^2,\;13.5Mpa{\cdot}m^{1/2}\;and\;1810kg/mm^2,\;14.4MPa{\cdot}m^{1/2}\;and\;1690kg/mm^2$, respectively for 60MPa and an induced current for 90% output of total capacity, 15KW. (5) The fracture toughness and hardness values of WC-8Ni, WC-10Ni, and WC-12Ni made by SPS were $12.2MPa{\cdot}m^{1/2}\;and\;1796kg/mm^2,\;12.9MPa{\cdot}m^{1/2}\;and\;1725kg/mm^2,\;13.6MPa{\cdot}m^{1/2}\;and\;1597kg/mm^2$, respectively for 60MPa and the electric current of 2500 A

  • PDF

음식물류폐기물의 호기성 퇴비화에 있어서 팽화재 투입비에 따른 타가영양세균의 균락형성단위의 변화에 관한 연구 (A Study on Variation of Colony Forming Units of Heterotrophic Bacteria by Input Ratios of Bulking Materials in Aerobic Composting of Food Wastes)

  • 박석환
    • 한국환경보건학회지
    • /
    • 제32권4호
    • /
    • pp.353-358
    • /
    • 2006
  • This study was performed to evaluate the effects of input ratios of bulking material in aerobic composting of food wastes on variation of colony forming units of heterotrophic bacteria. Wood chips were used as a bulking material. Volume ratios of food wastes to wood chips in reactor of Control, WC-1 and WC-2 were 10/0, 10/5 and 10/10, respectively. Reactors were operated for 24 days with 1hour stirring by 1rpm and 2 hours of the forced aeration per day. WC-2 reached high temperature range faster than WC-1, and the maximum temperature of WC-2 was higher than that of WC-1. This means that the reaction velocity of composting of WC-2 was faster than that of WC-1. Judging from the profile of pH changes, composting of WC-1 proceeded slowly and continuously. Composting of WC-2 proceeded rapidly in the former half reaction period, and kept steady state of high pH in the latter half reaction period. Namely, composting of WC-2 was nearly completed in the former half reaction period. In the case of WC-1 and WC-2. the maximum temperature was followed by the rapid pH increase in 2-3 days, and this was followed by the maximum Colony Forming Units(CFU) in 3 days. But, these three items of WC-2 always appeared faster and higher than those of WC-1.

EFFECTS OF CO CONTENT AND WC GRAIN SIZE ON WEAR OF WC CEMENTED CARBIDE

  • Saitoh, Hiroyuki;Iwabuchi, Akira;Shimizu, Tomoharu
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2002년도 proceedings of the second asia international conference on tribology
    • /
    • pp.213-214
    • /
    • 2002
  • WC cemented carbide are used as many die material to improve abration resistance. Mechanical properties of the cemented carbide were influenced by Co content and WC grain size. In this study, effects of Co content and WC grain size of WC cemented carbide on wear were examied. We prepared 13 cemented carbides with different Co content and WC grain size. Wear test was carried out against S45C under dry condition at 98N and 232mm/s. From the results, we found that wear increased with both Co content and WC grain size. Specific wear rate was range $10^{-7}mm^3/Nm$.

  • PDF

AIP-TiN/WC-Co계에서 WC입자크기와 Co함량이 밀착력에 미치는 영향 (Effect of the WC particle size and Co content on the adhesion property between AIP-TiN coating and WC-Co substrate)

  • 한대석;류정민;권식철;김광호
    • 한국표면공학회지
    • /
    • 제35권3호
    • /
    • pp.165-171
    • /
    • 2002
  • TiN coating were deposited onto different WC-Co substrates using arc ion plating (AIP) technique. The structure and morphology for the deposited coating were characterized by x-ray diffraction (XRD) and scanning electron microscopy (SEM). The adhesion behavior of the deposited TiN coating was investigated with a conventional scratch test. Effects of WC particle size and Co content on the adhesion strength between the deposited TiN coating and substrate were studied. During the scratch test, the value of critical load was dependent of WC particle size and Co content on substrate. As the WC particle size and Co content on substrate decreased, the critical load increased. The highest critical load, approximately 110N, was obtained at WC particle size of 1$\mu\textrm{m}$ and Co content of 10wt.%.

Ti(C,N)계 서메트 공구의 WC와 IV족 원소 첨가가 단속 절삭성능에 미치는 영향 (Effect of WC and group IV Elements of Ti(C,N) on the Intermittent Cutting Performance)

  • 박준석;김경재;권원태;강신후
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1997년도 추계학술대회 논문집
    • /
    • pp.919-922
    • /
    • 1997
  • In this study, the amount of WC and group N elements of Ti(C, N) cermet tool was investigated. The composition of WC was changed from 5 to 20% to determine the effect of WC on the cutting performance of cermet tool. The more WC was added, the longer the tool life of the cermet tool was. The cermet with 20% WC showed the best fracture toughness. The effect of group N elements ; ZrC, ZrN and HfC was also investigated by adding each of them to manufacture the cermet tool with fixed 14% WC composition. The cermet with 1% group N ZrC and 14% WC showed the best cutting performance among the investigated cermet tools.

  • PDF

진공 소결공정에 의한 고밀도 바인더리스 및 극저바인더 초경합금의 제조 (Consolidation of Binderless and Low-Binder WC hardmetal by Vacuum Sintering)

  • 민병준;박용호;이길근;하국현
    • 한국분말재료학회지
    • /
    • 제14권5호
    • /
    • pp.315-319
    • /
    • 2007
  • Pure WC or WC with low Co concentration less than 0.5 wt.% is studied to fabricate high density WC/Co cemented carbide using vacuum sintering and post HIP process. Considering the high melting point of WC, it is difficult to consolidate it without the use of Co as binder. In this study, the effect of lower Co addition on the microstructure and mechanical properties evolution of WC/CO was investigated. By HIP process after vacuum sintering, hardness and density was sharply increased. The hardness values was $2,800kgf/mm^2$ using binderless WC.

Contribution of the Interface Energies to the Growth Process of Cemented Carbides WC-Co

  • Lay, Sabine;Missiaen, Jean-Michel;Allibert, Colette H
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.332-333
    • /
    • 2006
  • The driving forces and the probable processes of WC-Co grain growth are reanalysed from recent data of interface energy and microstructure. Grain growth is driven by the disappearing of the high energy WC/WC and WC/Co interfaces with habit planes different from {0001}, ${10\bar{1}0}$ and ${11\bar{2}0}$ facets and by the area decrease of the WC/WC and WC/Co interfaces with {0001} and ${10\bar{1}0}$ habit planes. Grain growth mainly results of dissolution-precipitation. Abnormal grains are likely formed by defects assisted nucleation.

  • PDF

Measurement of WC Grain Size in Nanocrystalline WC-10Co Hardmetal

  • Chenguang, Lin;Guansen, Yuan
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.344-345
    • /
    • 2006
  • The linear intercept (LI) method was used to quantitatively measure the intercepts of WC grains in nano-grained WC-10Co hardmetal. When the surveyed intercept numbers of WC grain exceeded 200, the statistic data for the mean grain size of WC were reproduced. The discriminative minimal grain size of used LI method was 12 nm; the maximum intercept of WC grain was 109 nm; the average intercept of WC grains was 45 nm and the corresponding 3D mean grain size of WC was 70 nm which is agreeable with the XRD outcome.

  • PDF