• 제목/요약/키워드: Vacuum arc

검색결과 324건 처리시간 0.028초

Fe-30at.%Al-5at.%Cr계 합금의 공식특성에 미치는 플라즈마질화의 영향 (Effects of Plasma-Nitriding on the Pitting Corrosion of Fe-30at%Al-5at%Cr Alloy)

  • 최한철
    • 한국표면공학회지
    • /
    • 제36권6호
    • /
    • pp.480-490
    • /
    • 2003
  • Effects of plasma-nitriding on the pitting corrosion of Fe-30at%Al-5at%Cr alloy containing Ti, Hf, and Zr were investigated using potentiostat in 0.1M HCl. The specimen was casted by the vacuum arc melting. The subsequent homogenization was carried out in Ar gas atmosphere at $1000^{\circ}C$ for 7days and phase stabilizing heat treatment was carried out in Ar gas atmosphere at $500^{\circ}C$ for 5 days. The specimen was nitrided in the $N_2$, and $H_2$, (1:1) mixed gas of $10^{-4}$ torr at $480^{\circ}C$ for 10 hrs. After the corrosion tests, the surface of the tested specimens were observed by the optical microscopy and scanning electron microscopy(SEM). For Fe-30at%Al-5Cr alloy, the addition of Hf has equi-axied structure and addition of Zr showed dendritic structure. For Fe-30at%Al-5Cr alloy containing Ti, plasma nitriding proved beneficial to decrease the pitting corrosion attack by increasing pitting potential due to formation of TiN film. Addition of Hf and Zr resulted in a higher activation current density and also a lower pitting potential. These results indicated the role of dendritic structure in decreasing the pitting corrosion resistance of Fe-30Al-5Cr alloy. Ti addition to Fe-30Al-5Cr decreased the number and size of pits. In the case of Zr and Hf addition, the pits nucleated remarkably at dendritic branches.

Morphology Change of Nanotube and Micropore on the Ti-25Nb-xHf Alloys with Hf Contents after Anodization

  • Kim, Sung-Hwan;Ko, Yeong-Mo;Choe, Han-Cheol
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2012년도 춘계학술발표회 논문집
    • /
    • pp.333-333
    • /
    • 2012
  • In this study, we investigated morphology of nanotube and micropore on the Ti-25Nb-xHf alloys with Hf contents after anodization. Ti-25Nb-xHf ternary alloys contained from (0~15) wt.% Hf contents were manufactured by vacuum arc-melting furnace. The obtained ingots were homogenized in an argon atmosphere at $1000^{\circ}C$ for 12h and then water quenching. The specimens were cut from ingots to 3mm thickness and first ground and polished using SiC paper (grades from 100 to 2000). 2steps anodization treatments on Ti-25Nb-xHf alloys were carried out at room temperature for experiments. Micro-pore formation was performed in Ca+P mixed solution at 265V for 3min. After that, nanotube formation was in 1M $H_3PO_4$ electrolytes containing 0.8wt.% NaF solutionat 10V for 120min. Morphologies of micropore and nanotube depended on the Hf content in Ti-25Nb-xZr ternary system.

  • PDF

Application of a Dynamic-Nanoindentation Method to Analyze the Local Structure of an Fe-18 at.% Gd Cast Alloy

  • Choi, Yong;Baik, Youl;Moon, Byung M.;Sohn, Dong-Seong
    • Nuclear Engineering and Technology
    • /
    • 제49권3호
    • /
    • pp.576-580
    • /
    • 2017
  • A dynamic nanoindentation method was applied to study an Fe-18 at.% Gd alloy as a neutron-absorbing material prepared by vacuum arc-melting and cast in a mold. The Fe-18 at.% Gd cast alloy had a microstructure with matrix phases and an Fe-rich primary dendrite of $Fe_9Gd$. Rietveld refinement of the X-ray spectra showed that the Fe-18 at.% Gd cast alloy consisted of 35.84 at.% $Fe_3Gd$, 6.58 at.% $Fe_5Gd$, 16.22 at.% $Fe_9Gd$, 1.87 at.% $Fe_2Gd$, and 39.49 at.% ${\beta}-Fe_{17}Gd_2$. The average nanohardness of the primary dendrite phase and the matrix phases were 8.7 GPa and 9.3 GPa, respectively. The fatigue limit of the matrix phase was approximately 37% higher than that of the primary dendrite phase. The dynamic nanoindentation method is useful for identifying local phases and for analyzing local mechanical properties.

치과임플란트용 Ti-25Ta-xHf 합금의 플라즈마 전해 산화 (Plasma Electrolytic Oxidation of Ti-25Ta-xHf for Dental Implants)

  • 김정재;최한철
    • 한국표면공학회지
    • /
    • 제51권6호
    • /
    • pp.344-353
    • /
    • 2018
  • Plasma electrolytic oxidation of Ti-25Ta-xHf alloy in electrolyte containing Ca and P for dental implants was investigated using various experimental techniques. Ti-25Ta-xHf (x=0 and 15 wt.%) alloys were manufactured in an arc-melting vacuum furnace. Micropores were formed in PEO films on Ti-25Ta-xHf alloys in 0.15 M calcium acetate monohydrate + 0.02 M calcium glycerophosphate at 240 V, 270 V and 300 V for 3 min, respectively. The microstructure of Ti-25Ta-xHf alloys changed from (${\alpha}^{\prime}+{\alpha}^{{\prime}{\prime}}$) phase to (${\alpha}^{{\prime}{\prime}}+{\beta}$) phase by addition of Hf. As the applied potential increased, the number of pore and the area ratio of occupied by micro-pore decreased, whereas the pore size increased. The anatase phase increase as the applied potential increased. Also, the crystallite size of anatase-$TiO_2$ can be controlled by applied voltage.

Application of ta-C Coating on WC Mold to Molded Glass Lens

  • Lee, Woo-Young;Choi, Ju-hyun
    • Tribology and Lubricants
    • /
    • 제35권2호
    • /
    • pp.106-113
    • /
    • 2019
  • We investigated the application of tetrahedral amorphous carbon (ta-C) coatings to fabricate a glass lens manufactured using a glass molding process (GMP). In this work, ta-C coatings with different thickness (50, 100, 150 and 200 nm) were deposited on a tungsten carbide (WC-Co) mold using the X-bend filter of a filtered cathode vacuum arc. The effects of thickness on mechanical and tribological properties of the coating were studied. These ta-C coatings were characterized by atomic force microscopy, scanning electron microscopy, nano-indentation measurements, Raman spectrometry, Rockwell-C tests, scratch tests and ball on disc tribometer tests. The nano-indentation measurements showed that hardness increased with an increase in coating thickness. In addition, the G-peak position in the Raman spectra analysis was right shifted from 1520 to $1586cm^{-1}$, indicating that the $sp^3$ content increased with increasing thickness of ta-C coatings. The scratch test showed that, compared to other coatings, the 100-nm-thick ta-C coating displayed excellent adhesion strength without delamination. The friction test was carried out in a nitrogen environment using a ball-on-disk tribometer. The 100-nm-thick ta-C coating showed a low friction coefficient of 0.078. When this coating was applied to a GMP, the life time, i.e., shot counts, dramatically increased up to 2,500 counts, in comparison with Ir-Re coating.

고온 코팅용 Cr-Al합금의 미세조직 및 특성에 미치는 Si 첨가의 영향 (Effects of Si Addition on the Microstructure and Properties of Cr-Al alloy for High Temperature Coating)

  • 김정민;김일현;김현길
    • 한국재료학회지
    • /
    • 제29권1호
    • /
    • pp.7-10
    • /
    • 2019
  • Cr-Al alloys are attracting attention as oxidation resistant coating materials for high temperature metallic materials due to their excellent high temperature stability. However, the mechanical properties and oxidation resistance of Cr-Al alloys can be further enhanced, and such attempts are made in this study. To improve the properties of Cr-Al alloys, Si is added up to 5 wt%. Casting specimens with different amounts of Si content are prepared by a vacuum arc remelting method and isothermally heated under steam conditions at $1,100^{\circ}C$ for 1 hour. The as-cast microstructure of low Si alloys is mainly composed of only a Cr phase, while $Al_8Cr_5$ and $Cr_3Si$ phases are also observed in the 5 % Si alloy. In the high Si alloy, only Cr and $Cr_3Si$ phases remain after the isothermal heating at $1,100^{\circ}C$. It is found that Si additions slightly decrease the oxidation resistance of the Cr-Al alloy. However, the microhardness of the Cr-Al alloy is observed to increase with an increasing Si content.

Design of Copper Alloys Preventing Grain Boundary Precipitation of Copper Sulfide Particles for a Copper Disposal Canister

  • Minkyu Ahn;Jinwoo Park;Gyeongsik Yu;Jinhyuk Kim;Sangeun Kim;Dong-Keun Cho;Chansun Shin
    • 방사성폐기물학회지
    • /
    • 제21권1호
    • /
    • pp.1-8
    • /
    • 2023
  • The major concern in the deep geological disposal of spent nuclear fuels include sulfide-induced corrosion and stress corrosion cracking of copper canisters. Sulfur diffusion into copper canisters may induce copper embrittlement by causing Cu2S particle formation along grain boundaries; these sulfide particles can act as crack initiation sites and eventually cause embrittlement. To prevent the formation of Cu2S along grain boundaries and sulfur-induced copper embrittlement, copper alloys are designed in this study. Alloying elements that can act as chemical anchors to suppress sulfur diffusion and the formation of Cu2S along grain boundaries are investigated based on the understanding of the microscopic mechanism of sulfur diffusion and Cu2S precipitation along grain boundaries. Copper alloy ingots are experimentally manufactured to validate the alloying elements. Microstructural analysis using scanning electron microscopy with energy dispersive spectroscopy demonstrates that Cu2S particles are not formed at grain boundaries but randomly distributed within grains in all the vacuum arc-melted Cu alloys (Cu-Si, Cu-Ag, and Cu-Zr). Further studies will be conducted to evaluate the mechanical and corrosion properties of the developed Cu alloys.

ta-C 후막코팅을 이용한 비철금속가공용 절삭 공구류의 수명향상에 관한 연구

  • 장영준;강용진;김동식;이의영;김종국
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2016년도 제50회 동계 정기학술대회 초록집
    • /
    • pp.132-132
    • /
    • 2016
  • 기계 가공품의 정밀화, 경량화 요구로 난색재로 분류되는 비철분야 및 복합재 가공용 공구개발에 대한 수요가 급증하고 있으나, 기존 난삭재 가공 시 절삭공구의 마모가 빠르고, 상대재의 융착 불량 등이 공구 수명 감소의 주요 영향으로 보고된다. 상기문제를 해결하기 위해 절삭가공 공정 중 과다한 절삭유의 사용에 따른 가공비용, 에너지소모 증가, 환경오염 등으로 절삭유의 최소화 또는 절삭유를 사용하지 않는 표면처리기술등의 친환경 가공기술의 개발이 필요하다. 내융착 및 내마모 특성 향상을 위한 표면코팅 방법으로 수소가 포함되지 않은 고경도 비정질 카본 (ta-C)이 있으나, ta-C 코팅 막은 경도 30 - 80 GPa, 잔류응력 3 - 10 GPa 범위로 일반 경질 코팅 막 (AlTiN, TiSiCrN : 평균 3 GPa)에 비해 높고 산업적 활용이 가능한 0.5 - 1.5 um 두께 수준의 후막화가 힘들어 매우 우수한 절삭공구용 코팅 막 특성에도 불구하고 적용사례가 매우 적다. 따라서, 본 연구에서는 아크플라즈마 방식 (Filtered Cathode Vacuum Arc Plasma, FCVA)을 활용한 고경도/무수소 카본 코팅 막을 후막형태로 증착하여 비철금속가공용 절삭 공구류의 수명향상 기법을 제시하고자 한다. ta-C 코팅 막의 기초 공정개발 단계에서는 바이어스 전압, 공정시간을 달리하여 ta-C 코팅 막의 기계적 물성(경도: $50{\pm}3GPa$, 잔류응력: $6{\pm}1GPa$, 밀착력: 30N 이상 및 트라이볼로지 특성: 마찰계수 0.1 이하, 마멸량: $1.85{\times}10-14mm^3$)을 확보하여 절삭공구로의 공정실용화 적용검토를 실시하였다. ta-C 코팅 막은 (1) WC 공구 및 기존 상용품인 (2) TiAlN/TiN/WC 구조에 대해 증착을 실시하였으며 코팅 막의 두께 변화에 따른 실제 절삭환경에서의 내수명 관측을 진행하였다. 시험결과, ta-C/WC의 단일막 구조인 절삭공구의 경우, 실제 절삭환경에서 쉽게 박리가 발생하여 코팅 막으로서의 효과를 나타내지 못하였다. 이는, 기초 공정개발 단계에서의 밀착력 기준이 실제 환경과 부합하지 않는 것을 의미하며 추후 공정개선을 통해 극복하고자 한다. 반면에, 상용품인 (2) TiAlN/TiN/WC 구조의 절삭공구 대비 ta-C/TiAlN/TiN/WC 구조에서 내수명 증가는 약 2.5배 (기존 300회, 코팅 후 800회)로 증가하였으며 ta-C 코팅 막의 두께가 $0.6-0.8{\mu}m$일 때 최대치를 취한 후 감소하였다. 이를 통해, 절삭공구로의 ta-C 코팅 막 효과는 최외각 층의 두께 범위와 모재 강도보강을 할 수 있는 적절한 중간층 막 (TiN/TiAlN 층)이 혼합되어 나타난 것으로 사료되며 현재 산업계로의 적용을 위한 대량생산용 코팅장비의 개발 및 비용절감을 위한 공정개발이 진행 중이다.

  • PDF

Controlling the Work Functions of Graphene by Functionalizing the Surface of $SiO_2$ Substrates with Self-assembled Monolayers

  • 조주미;김유석;차명준;이수일;정상희;송우석;김성환;전승한;박종윤
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2012년도 제43회 하계 정기 학술대회 초록집
    • /
    • pp.400-401
    • /
    • 2012
  • 그래핀(Graphene)은 열 전도도가 높고 전자 이동도(200 000 cm2V-1s-1)가 우수한 전기적 특성을 가지고 있어 전계 효과 트랜지스터(Field effect transistor; FET), 유기 전자 소자(Organic electronic device)와 광전자 소자(Optoelectronic device) 같은 반도체 소자에 응용 가능하다. 그러나 에너지 밴드 갭이 없기 때문에 소자의 전기적 특성이 제한되는 단점이 있다. 최근에는 아크 방출(Arc discharge method), 화학적 기상 증착법(Chemical vapor deposition; CVD), 이온-조사법(Ion-irradiation) 등을 이용한 이종원자(Hetero atom)도핑과 화학적 처리를 이용한 기능화(Functionalization) 등의 방법으로 그래핀을 도핑 후 에너지 밴드 갭을 형성시키는 연구 결과들이 보고된 바 있다. 그러나 이러한 방법들은 표면이 균일하지 않고, 그래핀에 많은 결함들이 발생한다는 단점이 있다. 이러한 단점을 극복하기 위해 자가조립 단층막(Self-assembled monolayers; SAMs)을 이용하여 이산화규소(Silicon oxide; SiO2) 기판을 기능화한 후 그 위에 그래핀을 전사하면 그래핀의 일함수를 쉽게 조절하여 소자의 전기적 특성을 최적화할 수 있다. SAMs는 그래핀과 SiO2 사이에 부착된 매우 얇고 안정적인 층으로 사용된 물질의 특성에 따라 운반자 농도나 도핑 유형, 디락 점(Dirac point)으로부터의 페르미 에너지 준위(Fermi energy level)를 조절할 수 있다[1-3]. 본 연구에서는 SAMs한 기판을 이용하여 그래핀의 도핑 효과를 확인하였다. CVD를 이용하여 균일한 그래핀을 합성하였고, 기판을 3-Aminopropyltriethoxysilane (APTES)와 Borane-Ammonia(Borazane)을 이용하여 각각 아민 기(Amine group; -NH2)와 보론 나이트라이드(Boron Nitride; BN)로 기능화한 후, 그 위에 합성한 그래핀을 전사하였다. 기판 위에 NH2와 BN이 SAMs 형태로 존재하는 것을 접촉각 측정(Contact angle measurement)을 통해 확인하였고, 그 결과 NH2와 BN에 의해 그래핀에 도핑 효과가 나타난 것을 라만 분광법(Raman spectroscopy)과 X-선 광전자 분광법(X-ray photoelectron spectroscopy: XPS)을 이용하여 확인하였다. 본 연구 결과는 안정적이면서 패턴이 가능하기 때문에 그래핀을 기반으로 하는 반도체 소자에 적용 가능할 것이라 예상된다.

  • PDF

Effects of Hole Transport Layer Using Au-ionic Doping SWNT on Efficiency of Organic Solar Cells

  • Min, Hyung-Seob;Jeong, Myung-Sun;Choi, Won-Kook;Kim, Sang-Sig;Lee, Jeon-Kook
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2012년도 제43회 하계 정기 학술대회 초록집
    • /
    • pp.434-434
    • /
    • 2012
  • Despite recent efforts for fabricating flexible transparent conducting films (TCFs) with low resistance and high transmittance, several obstacles to meet the requirement of flexible displays still remain. Indium tin oxide (ITO) thin films, which have been traditionally used as the TCFs, have a serious obstacle in TCFs applications. SWNTs are the most appropriate materials for conductive films for displays due to their excellent high mechanical strength and electrical conductivity. Recently, it has been demonstrated that acid treatment is an efficient method for surfactant removal. However, the treatment has been reported to destroy most SWNT. In this work, the fabrication by the spraying process of transparent SWNT films and reduction of its sheet resistance by Au-ionic doping treatment on PET substrates is researched. Arc-discharge SWNTs were dispersed in deionized water by adding sodium dodecyl sulfate (SDS) as surfactant and sonicated, followed by the centrifugation. The dispersed SWNT was spray-coated on PET substrate and dried on a hotplate. When the spray process was terminated, the TCF was immersed into deionized water to remove the surfactant and then it was dried on hotplate. The TCF film was then was doped with Au-ionic doping treatment, rinsed with deionized water and dried. The surface morphology of TCF was characterized by field emission scanning electron microscopy. The sheet resistance and optical transmission properties of the TCF were measured with a four-point probe method and a UV-visible spectrometry, respectively. This was confirmed and discussed on the XPS and UPS studies. We show that 87 ${\Omega}/{\Box}$ sheet resistances with 81% transmittance at the wavelength of 550 nm. The changes in electrical and optical conductivity of SWNT film before and after Au-ionic doping treatments were discussed. The effects of hole transport interface layer using Au-ionic doping SWNT on the performance of organic solar cells were investigated.

  • PDF