Journal of the Korean Crystal Growth and Crystal Technology
/
v.3
no.2
/
pp.149-156
/
1993
Polycrystalline silicon was produced from metallurgical-grade Si by unidirectional solidification. Variations of impurity concentration and resistivity in the ingots have been investigated. X-ray diffraction analysis has also been performed to examine the crystal orientation. According to the X-ray diffraction analysis on the polycrystalline silicon, preferential orientation was changed from ( 220) into ( III ) with decreasing growth rate. Also, with increasing growth rate and fraction solidified, the resistivity tends to decrease.
Journal of the Korean Crystal Growth and Crystal Technology
/
v.7
no.3
/
pp.349-358
/
1997
meta-Nitroaniline(mNA) crystals were grown from the supercooled melt for the first time. A seed was introduced into the purified mNA melt of 100 ml 0.1 K above the melting temperature ($T_m$ : $112.0^{\circ}C$) and crystal was grown at constant supercooling of 0.1 K. The melt was stirred . mechanically and the crystal was also rotated while the growth proceeds. mNA crystals of size up to $20{\times}15{\times}15 \textrm {mm}^3 and of very high perfection could be grown for the period of one day. The bottom half of the crystal faces are well-faceted and covered by {111} and {021} faces, while the faces of the top half are not well defined. The overall crystal morphology was characterized by the unidirectional growth along one of the polar axes. The absolute direction of preferred growth was determined to be [001] by the pyroelectric measurements. The perfection of the crystal was characterized by synchrotron X-ray topography and optical characterization was made by measuring second harmonic conversion efficiency.
Proceedings of the Korea Association of Crystal Growth Conference
/
2000.06a
/
pp.195-214
/
2000
The high-speed steel (shorten as HSS) consists of Fe and several kinds of transition metal carbides. The cutting tools or wear-resistant materials made from HSS experience relatively high thermal shock because a coolant such as water or oil is flowed over the surface of heated HSS. The purpose of this research is to increase the hardness, strength, fracture toughness and thermal shock resistance of HSS. A possible strategy is to incorporate a hard ceramic material with high strength in HSS matrix. This paper describes the processing, microstructure and mechanical properties of the oriented unidirectional mullite fiber/HSS composite. The unidirectional mullite fibers of 10${\mu}{\textrm}{m}$ diameter were dispersed by the ultrasonic irradiation of 38 kHz in an ethylenglycol suspension containing HSS powder of 11${\mu}{\textrm}{m}$ median size. The dried green composites with 4-68 vol% fibers were hot-pressed for 2h at 100$0^{\circ}C$ in Ar atmosphere under a pressure of 39 MPa. The higher density was achieved in the composite with a lower content of fibers. The oriented unidirectional fibers were well dispersed in the HSS matrix. The average distance between the center of fibers in the cross section was close to the value calculated from the fiber fraction. No reaction occurred at the interfaces between HSS and mullite fibers in the composites. The composite with 13.6 vol% fibers showed 100 MPa of four point flexural strength at room temperature. The thermal expansion of composite with heating was influenced by the orientation of mullite fibers.
Journal of the Korean Crystal Growth and Crystal Technology
/
v.18
no.6
/
pp.232-236
/
2008
Recently the shortage of silicon resources especially for poly-silicon of purity higher than 99.9999% leads to search for the more cheap and quick synthesizing routes for silicon feedstock. In order to solve this situation, we investigated the purification process of metallurgical grade (MG) silicon of purity around 99% by the acid leaching and following the unidirectional solidification. MG-Si lumps are pulverized with a planetary mill, and then leached with HCl/$HNO_3$/HF acid solution. As a result, the concentration of metal impurities including Al, Fe, Ca, Mn, etc. decreased dramatically. This process led to silicon content higher than 99.99%. The purified silicon powders were compacted and have been melted and uni-directionally solidified with heat exchange method (HEM) furnace. The properties of multicrystalline silicon ingots were specific resistance of $0.3{\Omega}{\cdot}cm$ and minority carrier life time (MCLT) of $3.8{\mu}{\cdot}sec$.
The structure of a single crystal, grown by a slow cooling a melt of $Ca_{1.29}Bi_{0.14}VO_4$ composition, was analyzed. The crystals belong to the rhombohedral space group R3c and the dimensions of the unit cells are a = 10.848(1)${\AA}$, c = 38.048(6)${\AA}$, V = 3877.6(8)${\AA}^3$ for the pale yellow crystal, and a = 10.857(1), c = 38.063(6)${\AA}$, V = 3885.6(8)${\AA}^3$ for the yellow crystal, respectively. Unit cell dimensions of the crystal were larger than those of the host crystal, $Ca_3(VO_4)_2$, owing to the Bi that replaced Ca in the unit cell. Ca in the unit cell formed six, eight and nine coordinated polyhedra with O atoms and Bi replacing Ca entered the eight or nine coordinated Ca sites with different crystallographic environments in the unit cell. All the V in the unit cell formed four coordinated tetrahedra with O atoms, however V-O bond lengths in the tetrahedra were different from one another.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.31
no.2
/
pp.90-93
/
2018
This aim of this study was to develop a process for creating bulk single-crystal YBaCuO superconductors in a high magnetic field. To support the bulk unidirectional growth of $YBa_2Cu_3O_{7-y}$, $SmBa_2Cu_3O_{7-y}$ seeds were planted inside YBaCuO composites and samples were produced by melting, enabling the growth of two YBaCuO superconductors. Due to the magnetism generated inside the superconductor of the upper sample, the magnetization inside the superconducting single crystals was evenly distributed, the sharpness of the induced magnetic force was improved, and the superconducting magnetization were significantly improved. This approach is widely applicable for the production of superconducting wires and current leads used for DC power breakers.
The Peltier heat absorbed or evolved at the solidiliquid interface in the unidirectional solidification process could contribute to the increase of temperature gradient in liquid and growth velocity, and the enhancement of crystal orientation. In this study, in order to measure the Peltier heat generated at the solidiliquid interface as a way of application to crystal growth, the thermoelectric effects were investigated on the temperature changes at the solid- and liquid-phase of the same material and its interface. Through the theoretical consideration, it was possible to separate sole Peltier. Thomson or Joule heat from the temperature changes due to current density, polarity, and temperature gradient. Thomson coefficient of solid- and liquid-phase as well as Peltier coefficient at the solid/liquid interface could be obtained.
Journal of the Korean Crystal Growth and Crystal Technology
/
v.8
no.1
/
pp.73-82
/
1998
The exchange anisotropy is the unidirectional magnetic anisotropy which comes from exchange interaction between antiferromagnetic layer and ferromagnetic layer. The application of this phenomenon to MR read head and spin-valve type GMR (Giant Magnetoresistance) head has been studied extensively. In our study, we intended to apply exchange anisotropy of NiO/NiFe bilayer to spin-valve type GMR element. Above all, we studied the exchange anisotropy of NiO/NiFe bilayer, and focused especially on the effect of NiO deposition condition. And we found that Ar pressure during NiO deposition was crucial factor for the exchange anisotropy of NiO/NiFe bilayer. The lower the Ar pressure is, the better the characteristics of exhange anisotropy is. Then, we applied this optimum condition of NiO/NiFe bilayer to spin-valve type GMR element. Finally we got spin-valve type GMR element which had 3.6 % MR ratio, 16 Oe switching field, and 0.25 %/Oe sensitivity.
Thermoelectric effects on the temperature changes at the solid- and liquid-phase and its interface were studied by using the unidirectional solidification of $\textrm{Bi}_{2}\textrm{Te}_{3}$. Cooling or heating effects measured with current density. polarity and current passing time were quite different. By separating sole Peltier, Thomson and Joule heat theoretically and experimentally, the Peltier coefficient at the solid/liquid interface of $\textrm{Bi}_{2}\textrm{Te}_{3}$ was -1.10$\times\textrm{10}^{-1}$V, and the Thomson coefficients of solid- and liquid-phase were 7.31\times\textrm{10}^{-4}V/K, 5.77\times\textrm{10}^{-5}V/K, respectively. When D.C. passed from solid-phase to liquid-phase during the crystal growth of $\textrm{Bi}_{2}\textrm{Te}_{3}$ the crystal with more directionality was obtained owing to increase of the temperature gradient in liquid by the Peltier cooling. But in reverse current direction, the crystallinity was not changed significantly.
Journal of the Korean Crystal Growth and Crystal Technology
/
v.8
no.1
/
pp.169-178
/
1998
The crystal phases precipitated in various compositions glass of CaO-$SiO_2-P_2O_5$ system, were identified by XRD. E composition (CaO 49.4, $SiO_2\;36.8,\;P_2O_5$ 8.8 wt%) glass in which both apatite(($Ca_{10}(PO_4)_6O$ and $\beta$-wollastonite($CaSiO_3$) crystals would precipitate by heating, was selected as an experimental composition to prepare the glass ceramics with high bending strength and good bioactivity to the living bone. Glass powders of E composition were unidirectionally crystallized at $1050^{\circ}$C in the temperature-gadient furnace and the resultant glass ceramics were characterized. Bending strength of the glass ceramics was also measured. To investigate the bond forming ability between the glass ceramics and living bone tissue, soaking test of glass ceramics in simulated body fluid was carried out. Densed glass ceramics composed of apatite and $\beta$-wollastonite crystal were prepared by unidirectional crystallization under the optimum conditions. (2 0 2) plane of $\beta$-wollastonite crystals tended to grow perpendicularly to the crystallization direction. Average bending strength of this glass ceramics was 186.9 MPa, higher than that of the glass ceramics prepared by isothermal (not directional) crystallization In soaking test, a thin layer of apatite crystallite was formed on surface of the glass ceramics in 3 days. Apatite crystals formed on the glass ceramics could be act a role to make the chemical bond between the glass ceramics and living bone tissue.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.