• Title/Summary/Keyword: Uniaxial Compression Test

Search Result 281, Processing Time 0.02 seconds

Interaction between opening space in concrete slab and non-persistent joint under uniaxial compression using experimental test and numerical simulation

  • Vahab Sarfarazi;Kaveh Asgari;Mehdi Kargozari;Pouyan Ebneabbasi
    • Computers and Concrete
    • /
    • v.31 no.3
    • /
    • pp.207-221
    • /
    • 2023
  • In this investigation, the interaction between opening space and neighboring joint has been examined by experimental test and Particle flow code in two dimension (PFC2D) simulation. Since, firs of all PFC was calibrated using Brazilian experimental test and uniaxial compression test. Secondly, diverse configurations of opening and neighboring joint were provided and tested by uniaxial test. 12 rectangular sample with dimension of 10 cm*10 cm was prepared from gypsum mixture. One quarter of tunnel and one and or two joint were drilled into the sample. Tunnel diameter was 5.5 cm. The angularities of joint in physical test were 0°, 45° and 90°. The angularities of joint in numerical simulation were 0°, 30°, 60°, -30°, -45°, -60° and its length were 2cm and 4cm. Loading rate was 0.016 m/s. Tensile strength of material was 4.5 MPa. Results shows that dominant type of crack which took place in the model was tensile cracks and or several shear bands develop within the model. The Final stress is minimum in the cases where oriented angle is negative. The failure stress decrease by decreasing the joint angle from 30° to 60°. In addition, the failure stress decrease by incrementing the joint angle from -30° to -60°. The failure stress was incremented by decreasing the number of notches. The failure stress was incremented by decreasing the joint length. The failure stress was incremented by decreasing the number of notches. Comparing experimental results and numerical one, showed that the failure stress is approximately identical in both conditions.

Experimental Study on Failure Behavior of Plain Concrete - Biaxial Stress Test (콘크리트 파괴거동특성의 실험적 연구I-이축응력시험)

  • 이상근;이상민;박상순;한상훈;송영철
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2003.05a
    • /
    • pp.315-320
    • /
    • 2003
  • Two different strength types of plain concrete plate specimens (200$\times$200$\times$60mm) were tested under different biaxial load combinations. The specimens were subjected to biaxial combinations covering the three regions of compression-compression, compression-tension, and tension-tension. The loading platens with Teflon pads were used to reduce a confining effect in boundary surface between the concrete specimen and the solid platen. The principal deformations in the specimens were recorded, and the failure modes along with each stress ratio were examined. Based on the strength data, the failure envelops were developed for each type of plain concrete. The biaxial stress-strain responses of concrete plate specimens for three biaxial loading regions were also plotted. The test data indicated that the strength of concrete under biaxial compression ($f_2 / f_1$$_1$=-1/-1) is about 17 percent larger than under uniaxial compression.

  • PDF

Weathering Characteristics of Granite by Freeze-Thaw Cyclic Test (동결-융해 시험에 의한 화강암의 풍화 특성 연구)

  • Park, Yeon-Jun;You, Kwang-Ho;Yang, Kwang-Yong;Woo, Ik;Park, Chan;Song, Won-Kyung
    • Tunnel and Underground Space
    • /
    • v.13 no.3
    • /
    • pp.215-224
    • /
    • 2003
  • Weathering in nature was simulated by freeze-thaw cyclic test which represents mechanical weathering. Measured physical properties were elastic wave velocities, absorption rate, volume change and weight change. Uniaxial compression tests were also conducted before and after the weathering tests. The change in weight and volume of the specimens were not clearly related to the weathering process, but P, S wave velocities, uniaxial compression strength and Young's modulus were clearly decreased as weathering progresses. Test result can be used for the assessment of long-term stability of rock slopes.

Investigation of the effects of particle size and model scale on the UCS and shear strength of concrete using PFC2D

  • Haeri, Hadi;Sarfarazi, Vahab;Zhu, Zheming;Lazemi, Hossein Ali
    • Structural Engineering and Mechanics
    • /
    • v.67 no.5
    • /
    • pp.505-516
    • /
    • 2018
  • In this paper, the effects of particle size and model scale of concrete has been investigated on the failure mechanism of PFC2D numerical models under uniaxial compressive test. For this purpose, rectangular models with same particle sizes and different model dimensions, i.e., $3mm{\times}6mm$, $6mm{\times}12mm$, $12mm{\times}24mm$, $25mm{\times}50mm$ and $54mm{\times}108mm$, were prepared. Also rectangular models with dimension of $54mm{\times}108mm$ and different particle sizes, i.e., 0.27 mm, 0.47 mm, 0.67 mm, 0.87 mm, 1.07 mm, 1.87 mm and 2.27 mm were simulated using PFC2D and tested under uniaxial compressive test. Concurrent with uniaxial test, direct shear test was performed on the numerical models. Dimension of the models were $75{\times}100mm$. Two narrow bands of particles with dimension of $37.5mm{\times}20mm$ were removed from upper and lower of the model to supply the shear test condition. The particle sizes in the models were 0.47 mm, 0.57 mm, 0.67 mm and 0.77 mm. The result shows that failure pattern was affected by model scale and particle size. The uniaxial compressive strength and shear strength were increased by increasing the model scale and particle size.

Strengthening of perforated walls in cable-stayed bridge pylons with double cable planes

  • Cheng, Bin;Wu, Jie;Wang, Jianlei
    • Steel and Composite Structures
    • /
    • v.18 no.4
    • /
    • pp.811-831
    • /
    • 2015
  • This paper focuses on the strengthening methods used for improving the compression behaviors of perforated box-section walls as provided in the anchorage zones of steel pylons. Rectangular plates containing double-row continuous elliptical holes are investigated by employing the boundary condition of simple supporting on four edges in the out-of-plane direction of plate. Two types of strengthening stiffeners, named flat stiffener (FS) and longitudinal stiffener (LS), are considered. Uniaxial compression tests are first conducted for 18 specimens, of which 5 are unstrengthened plates and 13 are strengthened plates. The mechanical behaviors such as stress concentration, out-of-plane deformation, failure pattern, and elasto-plastic ultimate strength are experimentally investigated. Finite element (FE) models are also developed to predict the ultimate strengths of plates with various dimensions. The results of FE analysis are validated by test data. The influences of non-dimensional parameters including plate aspect ratio, hole spacing, hole width, stiffener slenderness ratio, as well as stiffener thickness on the ultimate strengths are illustrated on the basis of numerous parametric studies. Comparison of strengthening efficiency shows that the continuous longitudinal stiffener is the best strengthening method for such perforated plates. The simplified formulas used for estimating the compression strengths of strengthened plates are finally proposed.

Compression Fracture Behavior of ATJ Graphite for Rocket Nozzle throat (로켓 노즐목에 사용하는 ATJ 흑연의 압축 파단 특성)

  • Choi, Hoonseok;Kim, Jaehoon;Kim, Yeonwook;Seo, Bohwi;Moon, Soonil
    • Journal of the Korean Society of Propulsion Engineers
    • /
    • v.18 no.4
    • /
    • pp.61-66
    • /
    • 2014
  • Graphite is commonly used for rocket nozzle. The purpose of the present study is to evaluate compression fracture behavior of ATJ graphite. Uniaxial compression test is conducted in accordance with ASTM C 695 in the range of R.T to $900^{\circ}C$. The size effects of specimen on the compressive strength and fracture behavior were investigated. Two types of cylindrical specimen, i.e., where the diameter to length ratio is 1:2 (ASTM C 695 specimen) or 1:1, were tested at room temperature.

Constitutive property behavior of an ultra-high-performance concrete with and without steel fibers

  • Williams, E.M.;Graham, S.S.;Akers, S.A.;Reed, P.A.;Rushing, T.S.
    • Computers and Concrete
    • /
    • v.7 no.2
    • /
    • pp.191-202
    • /
    • 2010
  • A laboratory investigation was conducted to characterize the constitutive property behavior of Cor-Tuf, an ultra-high-performance composite concrete. Mechanical property tests (hydrostatic compression, unconfined compression (UC), triaxial compression (TXC), unconfined direct pull (DP), uniaxial strain, and uniaxial-strain-load/constant-volumetric-strain tests) were performed on specimens prepared from concrete mixtures with and without steel fibers. From the UC and TXC test results, compression failure surfaces were developed for both sets of specimens. Both failure surfaces exhibited a continuous increase in maximum principal stress difference with increasing confining stress. The DP tests results determined the unconfined tensile strengths of the two mixtures. The tensile strength of each mixture was less than the generally assumed tensile strength for conventional strength concrete, which is 10 percent of the unconfined compressive strength. Both concretes behaved similarly, but Cor-Tuf with steel fibers exhibited slightly greater strength with increased confining pressure, and Cor-Tuf without steel fibers displayed slightly greater compressibility.

Experimental and numerical studies of the pre-existing cracks and pores interaction in concrete specimens under compression

  • Haeri, Hadi;Sarfarazi, Vahab;Zhu, Zheming;Marji, Mohammad Fatehi
    • Smart Structures and Systems
    • /
    • v.23 no.5
    • /
    • pp.479-493
    • /
    • 2019
  • In this paper, the interaction between notch and micro pore under uniaxial compression has been performed experimentally and numerically. Firstly calibration of PFC2D was performed using Brazilian tensile strength, uniaxial tensile strength and biaxial tensile strength. Secondly uniaxial compression test consisting internal notch and micro pore was performed experimentally and numerically. 9 models consisting notch and micro pore were built, experimentally and numerically. Dimension of these models are 10 cm*1 cm*5 cm. the length of joint is 2 cm. the angularities of joint are $30^{\circ}$, $45^{\circ}$ and $60^{\circ}$. For each joint angularity, micro pore was situated 2 cm above the lower tip of the joint, 2 cm above the middle of the joint and 2 cm above the upper of the joint, separately. Dimension of numerical models are 5.4 cm*10.8 cm. The size of the cracks was 2 cm and its orientation was $30^{\circ}$, $45^{\circ}$ and $60^{\circ}$. Diameter of pore was 1cm which situated at the upper of the notch i.e., 2 cm above the upper notch tip, 2 cm above the middle of the notch and 2 cm above the lower of the notch tip. The results show that failure pattern was affected by notch orientation and pore position while uniaxial compressive strength is affected by failure pattern.

An Experimental Study on Filling Material for Bored Pile Using High Calcium Ash (고칼슘 연소재를 이용한 매입말뚝의 주면고정액에 관한 실험적 연구)

  • Song, Sang-Hwon;Lim, Yang-Hyun;Seo, Se-Gwan;Cho, Dae-Sung
    • Journal of the Korean Geosynthetics Society
    • /
    • v.16 no.4
    • /
    • pp.13-20
    • /
    • 2017
  • In this study, laboratory tests were performed to evaluate for new filling materials (ZA-Soil) for bored pile that were developed using by high calcium ash. As a result of laboratory test, the uniaxial compression strength of 2 types of ZA-Soil are shown 68.0% and 64.6% compared to ordinary portland cement. And it have a suitable flowability and environmental stability. Also, after 28days, uniaxial compression strength of material mixed with soil and high strength filling material (ZA-Soil) for bored pile is 1.10-1.23 times bigger than material mixed with ordinary portland cement.

Strength and Deformation Characteristics, and Numerial Analysis for Cement Admixed Clay and Composite Ground (시멘트 혼합토 및 복합지반의 강도, 변형 특성 및 수치해석)

  • Jeon, Jesung
    • Journal of the Korean GEO-environmental Society
    • /
    • v.15 no.8
    • /
    • pp.51-58
    • /
    • 2014
  • In this research, the composite grounds including original clay and soil-cement were constructed for conducting uniaxial compression test. Strength and deformation properties were analysed using results of laboratory tests with variations of water content of clay, replacement ratio and cement content. Numerical simulation using 3D distinct element method was conducted for soil cement. For strength of composite ground that contains more than cement contents of 15 %, it is more effective to increase cement content than increase of replacement ratio. Strength and elastic modulus of composite ground could be predicted by regression equations using uniaxial compression strength of clay, cement content of soil cement and replacement ratio. For strength and elastic modulus of soil cement, which is most important things for predicting final strength and elastic modulus of composite ground, numerical simulation using the distinct element method adapted bonding model could be used to verify laboratory test, and predict strength and elastic modulus.