• Title/Summary/Keyword: Ultra-high-strength Steel

Search Result 292, Processing Time 0.025 seconds

FE Analysis of Hot Press Forming Process considering the Phase Transformation (상변태를 고려한 핫프레스포밍 공정의 유한요소해석)

  • Kang, Gyeong-Pil;Lee, Kyung-Hoon
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2008.10a
    • /
    • pp.226-229
    • /
    • 2008
  • Hot press forming is an advanced forming technology fur manufacturing of complex and crash-resistant automotive parts using ultra high strength steels. The 3-dimensional FE analysis of hot press forming process, in which process the deformation, heat transfer and phase transformation behavior are fully coupled, is carried out. The vast amount of material properties for the FE analysis is obtained from material properties calculation software which is based on thermodynamic calculations. The overall methodology for the FE analysis of HPF process and the analysis results are discussed here.

  • PDF

Finite element analysis of longitudinal reinforcement beams with UHPFC under torsion

  • Mohammed, Thaer Jasim;Bakar, B.H. Abu;Bunnori, N. Muhamad;Ibraheem, Omer Farouk
    • Computers and Concrete
    • /
    • v.16 no.1
    • /
    • pp.1-16
    • /
    • 2015
  • The proposed techniques to strengthen concrete members such as steel plates, polymers or concrete have important deficiencies in adherence and durability. The use of UHPFC plates can overtake effectively these problems. In this paper, the possibility of using UHPFC to strengthen RC beams under torsion is investigated. Four specimens of concrete beams reinforced with longitudinal bars only were tested under pure torsion. One of the beams was considered as the baseline specimen, while the others were strengthened by ultra-high-performance fiber concrete (UHPFC) on two, three, and four sides. Finite element analysis was conducted in tandem with experimental work. Results showed that UHPFC enhances the strength, ductility, and toughness of concrete beams under torsional load, and that finite element analysis is in good agreement with the experimental data.

Surface Quality Improvements on the Spherical Shaped Mold using Ball End Milling (볼 엔드밀을 이용한 금형 구면 가공의 표면품질 향상에 관한 연구)

  • Yun, Il-Woo;Hwang, Jong-Dae
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.19 no.3
    • /
    • pp.71-76
    • /
    • 2020
  • Various machining methods are being studied to improve the processing quality of the spherical R shape in press die. In this paper, we confirmed that changes in machining quality were associated with changes in cutting direction, path, and cutting angle, which are commonly used in the machining of molds. We obtained a surface roughness graph with each condition change in one specimen using an instrument that measured geometry and surface roughness simultaneously. The results of the study showed that the best surface roughness in the finish cut of the spherical surface was obtained using upward pick feed machining.

Investigation on the Experimental Results of Anisotropic Fracture Behavior for UHSS 1470 MPa Grade Sheets (초고강도 1470 MPa급 판재의 파단 이방성 실험 결과에 관한 연구)

  • J. Lee;H. J. Bong;D. Kim
    • Transactions of Materials Processing
    • /
    • v.32 no.2
    • /
    • pp.87-91
    • /
    • 2023
  • In the present work, the ductile fracture behaviors of ultra-high strength steel sheets along the different loading directions are investigated under various loading paths. Three loading paths, i.e., in-plane shear, uniaxial tension, plane strain tension deformations, are considered, and the corresponding specimens are described. The experiments are conducted using the digital image correlation (DIC) system to analyze the strain at the onset of the fracture. The experimental results show that the loading path for each specimen sample is linear, and different values of the fracture strains for the loading direction from the plane strain tension are observed. The ductile fracture model of the modified Mohr-Coulomb (MMC) is constructed based on the experimental data and evaluated along the rolling direction and transverse direction under various loading paths.

Effect on the Stabilizing Heat Treatment to Weld Joint for the USC Coal Boiler Tubes(SA213 TP347H) (초초임계 석탄발전 보일러 튜브(SA213 TP347H) 용접부 안정화 열처리 효과)

  • Ahn, Jong-Seok;Park, Jin-Keun;Lee, Gil-Jae;Yoon, Jae-Yeon
    • Journal of Welding and Joining
    • /
    • v.33 no.4
    • /
    • pp.30-36
    • /
    • 2015
  • Austenite stainless steel(SA213-TP347H) has widely been used for the superheater & reheater tube in USC(ultra-supercritica) coal boiler because of its high creep rupture strength and anti-oxidation. But recently, the short-term failures have happened frequently in heat affected zone for only 4,000~15,000hours of service. Many investigations have been conducted to understand the failure mechanism. The root cause of failure was comfirmed to "strain induce participation hardening crack" or "reheat cracking". This mechanism often occurred due to weld residual stress and precipitation of the Cr, Nb carbides in the stabilized stainless steel such as TP347H. This paper presents an analysis of failure tube and effect of the sample tubes that conducting stabilizing heat treatment in site after 11,380hours & 16,961hours of service. Visual inspection was performed. In addition, microscopic characteristics was identified by O.M, SEM, and hardness test was carried out to find out the heat treatment effects. Failures seem to happen because of being not conducted stabilizing heat treatment in site. And another cause is inadequate weld parameter such as pass, ampere, voltage, inter-pass temperature. Thus, this paper has the purpose to describe that how to prevent similar failures in those weld-joints.

Process Design for Manufacturing 1.5wt%C Ultrahigh Carbon Workroll: Void Closure Behavior and Bonding Strength (1.5wt%C 초고탄소 워크롤 제조를 위한 단조 공정 설계: 기공압착 및 접합강도 분석)

  • Lim, H.C.;Lee, H.;Kim, B.M.;Kang, S.H.
    • Transactions of Materials Processing
    • /
    • v.22 no.5
    • /
    • pp.269-274
    • /
    • 2013
  • Experiments and numerical simulations of the incremental upsetting test were carried out to investigate void closure behavior and mechanical characteristic of a 1.5wt%C ultra-high carbon steel. The experimental results showed that the voids become quickly smaller as the reduction ratio increases. The simulation results confirmed this behavior and indicated that the voids were completely closed at a reduction ratio of about 40~45% during incremental upsetting. After the completion of the incremental upsetting tests, the process of diffusion bonding was employed to heal the closed voids in the deformed specimens. To check the appropriate temperature for diffusion bonding, deformed specimens were kept at 800, 900, 1000 and $1100^{\circ}C$ for an hour. In order to investigate the effect of holding time for diffusion bonding at $1100^{\circ}C$, specimens were kept at 10, 20, 30, 40, 50 and 60minutes in the furnace. A distinction between closed and healed voids was clearly established using microstructural observations. In addition, subsequent tensile tests demonstrated that complete healing of a closed void was achieved for diffusion bonding temperatures in the range $900{\sim}1100^{\circ}C$ with a holding time larger than 1 hour.

Crash Analysis of the ULSAB-AVC Model with Considering Forming Effects (박판성형가공을 고려한 자동차 충돌해석)

  • Huh, H.;Yoon, J.H.;Bao, Y.D.;Kim, S.H.;Park, S.H.
    • Transactions of Materials Processing
    • /
    • v.15 no.8 s.89
    • /
    • pp.556-561
    • /
    • 2006
  • Most of auto-body members are composed of stamping parts. These parts have the non-uniform thickness and plastic work hardening distribution during the forming process. This paper is concerned with the side impact analysis of the ULSAB-AVC model according to the US-SINCAP in order to compare the crashworthiness between the model with and without considering the forming effect. The forming effect is ca]ciliated by one-step forming analysis for several members. The crashworthiness is investigated by comparing the deformed shape of the cabin room the energy absorption characteristics and the intrusion velocity of a car. The result of the crash analysis demonstrates that the crash mode, the load-carrying capacity and energy absorption can be affected by the forming effect. It is noted that the design of an autobody should be carried out considering the forming effect for accurate assessment of crashworthiness.

Comparison of Wear Amount of Surface Coating Layers on Dies for Cold-Stamped Products with MART1470 (MART1470 판재 냉간 프레스 성형용 금형 코팅층의 마모량 비교)

  • Son, M.K.;Kim, S.H.
    • Transactions of Materials Processing
    • /
    • v.31 no.1
    • /
    • pp.11-16
    • /
    • 2022
  • In this paper, wear characteristics of PVD coatings were compared on the die surface for cold stamping of MART1470 steel sheet with the finite element analysis and the pin-on-disc wear test. Three types of PVD coatings (CrN, TiAlCrN, and MoS2TiCr(W)N) were considered for the tool surface made of STD11 material. The stamping process of an auto-body part was analyzed with the finite element method. Ranges of process variables for the wear test such as contact pressure, relative speed, and sliding distance were predicted from analysis results. In order to quantitatively analyze wear characteristics of each coating, the amount of wear was measured and compared according to process variables with the pin-on-disc wear test. The influence of each process variable was investigated and the wear characteristics of the three coating layers were quantitatively compared. It was confirmed that the wear characteristics of MoS2TiCr(W)N coating were better than those of CrN and TiAlCrN. It was noted that the proposed prediction approach could predict and respond to the wear phenomenon occurring in the stamping process.

Effect of Compressive Strength and Curing Condition on the Direct Tensile Strength Properties of Ultra High Performance Concrete (압축강도 및 양생조건에 따른 초고성능 콘크리트의 직접인장강도 특성)

  • Park, Ji Woong;Lee, Gun Cheol
    • Journal of the Korea Institute of Building Construction
    • /
    • v.17 no.2
    • /
    • pp.175-181
    • /
    • 2017
  • The purpose of this study is evaluating the characteristics of tensile strength of UHPC and examining tensile performance of notched specimens by direct tensile test. For test variables, 120, 150, and 180MPa of target design standard strength were aimed at. With general water curing and $90^{\circ}C$ high temperature steam as curing conditions, the properties were reviewed. Overall, it was represented that the specimens of notch-type direct tensile strength concrete was effective in inducing central cracks compared with existing direct tension specimens. Through this, it was judged that data construction with high reliability was possible. Above all, in a graph of direct tensile strength and strain, in the case of steam curing at high temperature, there was great difference of initial tensile strength compared with water curing. As passing of ages, an aspect that the difference gradually decreased was shown. Maximum tensile strength was found to increase steadily with increasing age for all target design strengths in water curing, in the case of steam curing, the tendency to increase significantly due to the initial strength development effect at 7 days of age. The initial crack strength increases with age in case of underwater curing, in the case of steam curing, it was higher than that of water curing in 7 days, while the strength of 28 days was lowered. In this part, it is considered necessary to examine the arrangement condition of the steel fiber.

Performance of Fresh and Hardened Ultra High Performance Concrete without Heat Treatment (상온 양생한 초고성능 콘크리트(UHPC)의 경화 전과 후의 성능 관계)

  • Kang, Sung-Hoon;Hong, Sung-Gul
    • Journal of the Korea Concrete Institute
    • /
    • v.26 no.1
    • /
    • pp.23-34
    • /
    • 2014
  • This study investigates the relationship between the performance of fresh and hardened Ultra-High Performance Concrete (UHPC) without heat treatment. The performance of fresh UHPC is determined by the slump flow test related to the fluidity of concrete mixtures, and the air content test. The variables of these tests are the water to binder ratio, superplasticizer dosages and volume fractions of steel fiber. Generally, insufficient fluidity and excessive air contents in concrete mixtures lead to the insufficient packing density related to the performance of harden concrete. The performance of hardened UHPC is determined by the compressive and flexural tensile tests. The results of the fresh UHPC tests show that there is the linear correlation between each variable and the slump flow diameter, and that the slump flow diameter is linearly decreased as the air content ratio increase. Using these results, the formula is developed to predict the fresh performance before mixing UHPC. The results of the hardened UHPC tests show that the hardened performance is not influenced by the air content ratio in the range of 3.2 to 4.2 per cent. However, the flexural tensile strength dominantly influenced by the volume fractions of steel fiber.