• Title/Summary/Keyword: Tube Tensile Test

Search Result 99, Processing Time 0.029 seconds

Hydroformability and mechanical properties of A16061 tubes on different extrusion type (알루미늄 6061 압출재의 제조공정에 따른 온간액압성형성과 기계적 특성 연구)

  • Yi, H.K.;Jang, J.H.;Kwon, S.O.;Lee, Y.S.;Moon, Y.H.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2007.05a
    • /
    • pp.254-257
    • /
    • 2007
  • In this study, hydroformability and mechanical properties of pre- and post- heat treated Al6061 tubes at different extrusion type were investigated. For the investigation, as-extruded, full annealed and T6-treated Al 6061 tubes at different extrusion type were prepared. To evaluate the hydroformability, uni-axial tensile test and free bulge test were performed at room temperature and $200^{\circ}C$. Also mechanical properties of hydroformed part at various pre- and post-heat treatments were estimated by tensile test. And the tensile test specimens were obtained from hexagonal prototype hydroformed tube at $200^{\circ}C$. As for the heat treatment, hydroformability of full annealed tube is 25% higher than that of extruded tube. The tensile strength and elongation were more than 330MPa and 12%, respectively, when hydroformed part was post-T6 treated after hydroforming of pre- full annealed tube. However, hydroformed part using T6 pre treated tube represents high strength and low elongation, 8%. Therefore, the T6 treatment after hydroforming for as-extruded tube is cost-effective. Hydroformability of Al6061 tube showed similar value for both extrusion types. But flow stress of seam tube showed $20{\sim}50MPa$ lower value.

  • PDF

Effect of process type and heat treatment conditions on warm hydroformability (온간액압성형특성에 미치는 압출제조공정과 열처리 조건의 영향)

  • Yi, H.K.;Kwon, S.O.;Park, H.K.;Yim, H.S.;Lee, Y.S.;Moon, Y.H.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2007.10a
    • /
    • pp.132-135
    • /
    • 2007
  • In this study, hydroformability and mechanical properties of pre- and post- heat treated Al6061 tubes at different extrusion type were investigated. For the investigation, as-extruded, full annealed and T6-treated Al6061 tubes at different extrusion type were prepared. To evaluate the hydroformability, uni-axial tensile test and free bulge test were performed at room temperature and $250^{\circ}C$. Also mechanical properties of hydroformed part at various pre- and post-heat treatments were estimated by tensile test. And the tensile test specimens were obtained from hexagonal prototype hydroformed tube at $250^{\circ}C$. As for the heat treatment, hydroformability of full annealed tube is 25% higher than that of extruded tube. The tensile strength and elongation were more than 330MPa and 12%, respectively, when hydroformed part was post-T6 treated after hydroforming of pre- full annealed tube. However, hydroformed part using T6 pre treated tube represents high strength and low elongation, 8%. Therefore, the T6 treatment after hydroforming for as-extruded tube is cost-effective. Hydroformability of Al6061 tube showed similar value for both extrusion types. But flow stress of seam tube showed $20{\sim}50MPa$ lower value.

  • PDF

Tensile capacity of mortar-filled rectangular tube with various connection details

  • Kim, Chul-Goo;Kang, Su-Min;Eom, Tae-Sung;Baek, Jang-Woon
    • Steel and Composite Structures
    • /
    • v.44 no.3
    • /
    • pp.339-351
    • /
    • 2022
  • A mortar-filled rectangular hollow structural section (RHS) can increase a structural section property as well as a compressive buckling capacity of a RHS member. In this study, the tensile performance of newly developed mortar-filled RHS members was experimentally evaluated with various connection details. The major test parameters were the type of end connections, the thickness of cap plates and shear plates, the use of stud bolts, and penetrating bars. The test results showed that the welded T-end connection experienced a brittle weld fracture at the welded connection, whereas the tensile performance of the T-end connection was improved by additional stud bolts inserted into the mortar within the RHS tube. For the end connection using shear plates and penetrating stud bolts, ductile behavior of the RHS tube was achieved after yielding. The penetrating bars increased load carrying capacity of the RHS. Based on the analysis of the load transfer mechanism, the current design code and test results were compared to evaluate the tensile capacity of the RHS tube according to the connection details. Design considerations for the connections of the mortar-filled RHS tubes were also recommended.

A study on the deformation characteristic of heat-treated 6061,7075 aluminum alloy with changes of elevated temperature and strain rate for warm hydroforming (열처리된 알루미늄 6061, 7075 합금의 온간 액압 성형 적용을 위한 온도 및 변형 속도 변화에 따른 변형 특성 연구)

  • Yi H. K.;Moon Y. H.;Sohn S. M.;Lee M. Y.;Suh D. W.;Lee S. Y.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2004.10a
    • /
    • pp.23-26
    • /
    • 2004
  • The deformation behaviors of fully annealed or T6-treated 6061 and 7075 aluminum tubes are investigated at elevated temperature using uniaxial tensile test. Fully annealed 6061 and 7075 tube, and T6-treated 7075 tube do not show sharp local necking with an elongation of $50\%$ at tensile temperature of $300^{\circ}C$, accordingly, it is expected that warm hydroforming process can be applied. The increase of tensile temperature does not significantly affect the total elongation of T6-treated 6061 tube.

  • PDF

Effect of Steady-State Oxidation on Tensile Failure of Zircaloy Cladding

  • Kim, Taeho;Choi, Kyoung Joon;Yoo, Seung Chang;Lee, Yunju;Kim, Ji Hyun
    • Journal of Nuclear Fuel Cycle and Waste Technology(JNFCWT)
    • /
    • v.20 no.2
    • /
    • pp.161-170
    • /
    • 2022
  • The effect of oxidation time on the characteristics and mechanical properties of spent nuclear fuel cladding was investigated using Raman spectroscopy, tube rupture test, and tensile test. As oxidation time increased, the Raman peak associated with the tetragonal zirconium oxide phase diminished and merged with the Raman peak associated with the monoclinic zirconium oxide phase near 333 cm-1. Additionally, the other tetragonal zirconium oxide phase peak at 380 cm-1 decreased after 100 d of oxidation, whereas the zirconium monoclinic oxide peak became the dominant peak. The oxidation time had no effect on the tube rupture pressure of the oxidized zirconium alloy tube. However, the yield and tensile stresses of the oxidized nuclear fuel cladding tube decreased after 100 d of oxidation. The results of the scanning electron microscopy and transmission electron microscopy were represented with the in-situ Raman analysis result for the oxide characteristics generated on the cladding of spent nuclear fuel.

Hydrogen Embrittlement of Zr-2.5Nb PT with Temperature (Zr-2.5Nb 압력관의 온도변화에 따른 수소취화 파괴거동)

  • Oh, Dong-Joon;Ahn, Sang-Bok;Kim, Young-Suk
    • Proceedings of the KSME Conference
    • /
    • 2003.04a
    • /
    • pp.78-83
    • /
    • 2003
  • The aim of this study is to investigate the effect of hydrogen embrittlement od Zr-2.5Nb CANDU pressure tube. The test were performed at three hydrogen contents for transverse tensile and CCT specimens while the test temperatures were changed (RT to 300$^{\circ}C$). The specimens were directly machined from the tube retaining original curvature using electric discharge machine. Both the transverse tensile and the fracture toughness tests showed the hydrogen embrittlement clearly at RT but this phenomenon was disappeared while the test temperature arrived over 250$^{\circ}C$. From the fracture toughness test, it was found that fracture toughness dJ/da was increased up to 200$^{\circ}C$ and then decreased.

  • PDF

A Study on the Characteristics of Aluminum Tube Hydroformed Products (알루미늄 튜브를 이용한 액압성형품 특성연구)

  • Yi, Hyae-Kyung;Lee, Gun-Yeop;Lee, Sung-Mun;Lee, Young-Seon;Moon, Young-Hoon
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.32 no.11
    • /
    • pp.1010-1015
    • /
    • 2008
  • In this study, the characteristics of aluminum tube hydroformed products at different extrusion type and heat treatment conditions were investigated. For the investigation, as-extruded, full annealed and T6-treated Al 6061 tubes at different extrusion type were prepared. To evaluate the hydroformability, free bulge test was performed at room temperature to $300^{\circ}C$. Also mechanical properties of hydroformed products at various pre- and post-heat treatments were estimated by hexagonal prototype hydroforming test at $250^{\circ}C$. And the tensile test specimens were obtained from hexagonal prototype hydroformed tube. As a results, hydroformability of full annealed tube is $5{\sim}8%$ higher than that of extruded and T6-treated tube. The tensile strength and elongation of T6-post heat treated indirect extrusion tube were more than 330MPa and 12%, respectively. However, T6 pre treated hydroformed product represents high strength, 330MPa and low elongation, 8%. Therefore, Hydroformability of Al6061 tube showed similar value for both extrusion types. However flow stress of direct tube showed $20{\sim}50MPa$ lower value than indirect tube.

Evaluation of Tensile Properties of Alloy 690TT Steam Generator Tube at Room Temperature and 343℃ (상온과 343℃에서 Alloy 690TT 증기발생기 전열관의 인장물성치 평가)

  • Eom, Ki Hyeon;Kim, Jin Weon
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.38 no.6
    • /
    • pp.655-662
    • /
    • 2014
  • This study conducted tensile tests on an Alloy 690TT tube at room temperature (RT) and at $343^{\circ}C$ using tube- and ring-type specimens to investigate the stress-strain behavior and tensile properties of a steam generator (SG) tube in the axial and circumferential directions at RT and at the design temperature of a nuclear power plant (NPP). The results of the axial tensile test showed that yield point phenomena appeared at both RT and $343^{\circ}C$, and serrated flow in the stress-strain curve appeared at $343^{\circ}C$. Yield and tensile strengths for both directions were clearly lower at $343^{\circ}C$ compared to RT; however, the elongations were approximately the same at both test temperatures. Regardless of the test temperature, the strengths in the circumferential direction were lower by approximately 5~10 % than those in the axial direction. In addition, the test data revealed that the reduction in the yield and tensile strengths of the Alloy 690TT SG tube with the test temperature was more significant than that estimated by the temperature correction factor of ASME Sec.II.

A study on the formability with heat treatment and deformation temperature in warm hydroforming of Al 6061 tube (Al6061 tube의 열처리조건과 온도에 따른 액압성형성에 관한 특성 연구)

  • Yi H. K.;Lee Y. S.;Moon Y. H.;Lee J. H.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2005.10a
    • /
    • pp.255-258
    • /
    • 2005
  • In this study, the effect of heat treatment conditions and deformation temperature on the formability were investigated in warm hydroforming of Al 6061 tube. Full annealing and T6-treatment for heattreatment of Al6061 tube were used in this study. To evaluate the hydroformability, uniaxial tensile test and bulge test were performed between room temperature and $300^{\circ}C$. And measured flow stress was used to simulate the hydroforming of Al 6061. A commercial FEM code, DEFORM2D, was used to calculate the damage and strain variation. The calculated values were efficient to predict the forming limit in hydroforming for real complex shaped part.

  • PDF

Effect of Heat Treatment Conditions on Formability and Property of Warm Hydroformed Parts for Al 6061 Extruded Tube (Al6061압출재를 이용한 온간액압성형품의 성형성 및 물성에 미치는 열처리조건의 영향)

  • Yi, Hyae-Kyung;Kwon, Seung-O;Jang, Jeong-Hwan;Lee, Young-Seon;Moon, Young-Hoon
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.20 no.4
    • /
    • pp.181-186
    • /
    • 2007
  • Effect of heat treatment conditions on formability and property of warm hydroformed parts for Al 6061 extruded tubes was investigated in this study. For the investigation, as-extruded, fully annealed and T6-treated Al 6061 seamless tubes were prepared. To evaluate the warm hydroformability, uni-axial tensile test and free bulge test were performed at various pre- and post-heat treatment conditions. And the tensile test specimens were obtained from hexagonal prototype hydroformed parts at $250^{\circ}C$. As a result, hydroformability of fully annealed tube is 25% higher than that of extruded tube. The tensile strength and strain of hydroformed part reach to 330 MPa and 12%, respectively, when the part was T6 treated after warm hydroforming. However, the hydroformability of T6 pre-treated tube is relatively low due to the decreased elongation, 8%.