New sources of barley (Hordeum vulgare L.) resistant to spot blotch, caused by Cochliobolus sativus, are needed to provide effective resistance because of the rapid change pathotype patterns of C. sativus in fields. The purposes of our study were to develop a method to screen barley for resistance to spot blotch disease and then use this methodology to screen barley genotypes for resistance to the major virulent pathotype Pt4 in barley populations in Syria. A transparent tape method, in which a conidial suspension of C. sativus was dropped onto transparent tape and placed, treated-side down, on the second leaf surface of barley plants. Disease symptoms of fungus were easily detected on the leaves covered by the transparent tape after 48h of inoculation. The transparent tape method was repeatable and the disease scores obtained were correlated (r = 0.91, P = 0.001) with those obtained by the seedling assay. This method may be beneficial in various plant pathology breeding programs.
To fabricate green sheet of transparent dielectric for PDP front panel, dispersion of transparent dielectric slurry, density, and mechanical properties of green sheets have been investigated as a function of amount and composition of organic additives. Measurements of sedimentation and viscosity were employed to determine a proper dispersant and its amount for a well dispersed transparent dielectric powders in non-aqueous system. Green sheets, having various ratios of transparent dielectric powders to transparent dielectric powders+ binder+plasticizer and binder to binder+plasticizer, were fabricated. All the tape casting slurries showed shear thinning effect, that is, the apparent viscosity decreased with the increase of shear rate. It was found that the amount and composition of organic additives were main variables to affect densities and mechanical properties of transparent dielectric green sheets for PDP.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.17
no.10
/
pp.1107-1113
/
2004
Dry film method for large size of PDP(Plasma Display Panel) module has been actively investigated. This method for lead-free transparent dielectric formation depends on green sheet technology. By adjusting the composition of transparent dielectric powders and organics, uniformly dispersed slurry was fabricated, Viscosity of the slurry exhibited pseudoplastic behavior for tape casting, Cast green sheets were tested under tensile condition at room temperature. It was found that the increase in transparent dielectric powder and binder ratio leads to decrease in strain to failure of green sheets from 120 % to 34 % and from 255 % to 4 %, respectively. Tensile strength of green sheets decreased abruptly with increase of transparent dielectric powder ratio, with minimum at 0.13 MPa. On the other hand, tensile strength increased continuously from 0.1 MPa to 2.4 MPa with increase of binder ratio. The green sheets were attached on the glass substrate and heated by following firing schedule. As a result, the best result was obtained when fired at 580 $^{\circ}C$ for 15 min and had transmittance of 78 % in visible range 550 nm.
Journal of the Microelectronics and Packaging Society
/
v.27
no.3
/
pp.73-76
/
2020
Silver nanowires (AgNWs) intrinsically possess high conductivity, ductility, and network structure percolated in a low density, which have led to many advanced applications of transparent and flexible electronics. Most of these applications require patterning of AgNWs, for which photolithographic and printing-based techniques have been widely used. However, several drawbacks such as high cost and complexity of the process disturb its practical application with patterning AgNWs. Herein, we propose a novel method for the patterning of AgNWs by employing UV-curable adhesive tape with a structure of liner/adhesive layer/polyolefin (PO) film and UV irradiation to simplify the process. First, the UV-curable adhesive tape was attached to AgNWs/polyurethane (PU), and then selectively exposed to UV irradiation by using a photomask. Subsequently, the UV-curable adhesive tape was peeled off and consequently AgNWs were patterned on PU substrate. This facile method is expected to be applicable to the fabrication of a variety of low-cost, shape-deformable transparent and wearable devices.
Ceramic green sheets consisting Bi-based glass frit were fabricated for an application to PDP transparent dielectric front panel. The dispersion condition of the slurry for tape casting was pre-examined, and two kinds of hinder and plasticizer were used in the non-aqueous slurry system. In the fabrication process for the frit film, the properties such as dry and firing shrinkage, elongation, and transmittance were examined at the condition of various mixing ratio of plasticizers. In the mixing ratio of polyethylene glycol to dibutyl phthalate of 3:5wt%, a good adhesion, elongation and transmittance were observed at the firing temperature of $580^{\circ}C$. The photograph for the cross section of the interface was also showed a dense microstructure.
Recently, electronic devices with bendable electronic devices based on flexible substrates are being sold, and therefore, the purpose of this study is to evaluate the possibility of flexible substrates of conductive transparent tapes. As a transparent electrode, carbon nanotube (CNT) was formed by the coating method developed by the research team, and samples coated up to 5 times were fabricated. The surface resistance and transmittance of the substrate were measured, and both resistance and transmittance decreased as the number of CNT coatings increased. After the tape was detached from the glass, the surface resistance slightly increased in all samples, and the transmittance increased by about 10% in all measured wavelength ranges because the glass was removed. Next, the tape coated with CNT twice was used to a bending test 20,000 times under the condition of a radius of curvature of 2 mm. The electrical and optical properties before and after bending did not change, which means that there was no change in CNT properties due to bending.
Bi$_{2}Sr_{2}CaCu_{2}O_{\delta}$ superconducting films were rapidly fabricated on copper tape by liquid reaction between a Cu-free precursor and Cu tape (LiReac-PreCu) method. Those thick films were well oriented along the c-axis. The precursor was made by melt-quenched technology using twin roller. The melt-quenched films were transparent and glossy yellow in appearance. These films which were the compostion of Bi$_2SrCaO_y$, Bi$_3Sr_2CaO_z$ were placed on copper tape and then heated at various temperatures for several minutes in air. They were analyzed using X-ray powder diffraction, SEM, a DC four-probe method. The mechanism of superconducting phase formation . from the melt-quenched precursor on Cu tape was studied
Journal of the Korea Academia-Industrial cooperation Society
/
v.6
no.6
/
pp.497-501
/
2005
Dry film method was applied to fabricate lead-free transparent dielectric fur PDP(Plasma Display Panel). From various slurry compositions, it was able to find out the. best composition for producing high density green sheet. The slurry exhibited shear thinning characteristics which are known to be suitable fur producing a high quality green sheet. The thermal expansion coefficient of the fabricated transparent dielectric was measured to be $97{\times}10^{-7}/^{\circ}C$ which is close to the value of the glass substrate(PD-200). Cross sectional SEM of the transparent dielectric layer on PD-200 showed that the two layers were well attached each other with no observable gaps between them.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
1995.11a
/
pp.302-305
/
1995
ITO(indium tin oxide) that is both conductive in electricity and transparent to the visible ray is called transparent conducting thin film. Nowaday, according to the development of flat panel display such as LCD(Liquid Crystal display, EL(electolumine- scence display), PDP(plasma display panel), ECD(electrocromic display), the higher quality in the low temperature process has been asked to reduce the production cost and to have a good uniformity on a large substrate. In this study, we prepared indium tin oxide(ITO) by a cylindrical DC magnetron sputtering with Indium-tin (9:1) alloy target instead of indium-tin oxide target. To reduce the defact in ITO, the effect on ITO by varing the magnetic field intensity and the applied voltage ares studied. the resistivity of the film deposited in oxygen partial pressure of 5% and substrate temperature of 140$^{\circ}C$. is 1.6${\times}$10$\^$-1/$\Omega$$.$cm with 85% optical transmission in viaible ray.
Kwak, Seung-Hoon;Kwak, Min-Gi;Hong, Sung-Jei;Ju, Byeong-Kwon;Han, Jeong In
Current Photovoltaic Research
/
v.2
no.1
/
pp.14-17
/
2014
In this paper, indium reduced materials for transparent conductive electrodes (TCE) were fabricated and their physical properties were evaluated. Two of materials, indium-zinc-tin oxide (IZTO) and aluminum (Al) were selected as TCE materials. In case of IZTO nanoparticles, composition ratios of In, Zn and Sn is 8:1:1 were synthesized. Size of the synthesized IZTO nanoparticles were less than 10 nm, and specific surface areas were about $90m^2/g$ indicating particle sizes are very fine. Also, the IZTO nanoparticles were well crystallized with (222) preferred orientation despite it was synthesized at the lowered temperature of $300^{\circ}C$. Composition ratios of In, Zn and Sn were very uniform in accordance with those as designed. Meanwhile, Al was deposited onto glass by sputtering in a vacuum chamber for mesh architecture. The Al was well deposited onto the glass, and no pore was observed from the Al surface. The sheet resistance of Al on glass was about $0.3{\Omega}/{\square}$ with small deviation of $0.025{\Omega}/{\square}$, and adhesion was good on the glass substrate since no pelt-off part of Al was observed by tape test. If the Al mesh is combined with ink coated layer which is consistent of IZTO nanoparticles, it is expected that the good and reliable metal mesh architecture for TCE will be formed.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.