• Title/Summary/Keyword: Total Strain Intensity Factor

Search Result 17, Processing Time 0.02 seconds

A Study on the Initiation and Growth Behaviors of Surface Crack in a Type 304 Stainless Steel at Room Temperature (SUS 304鋼 의 常溫下 表面피勞균열 의 發생.成長 擧動 에 관한 硏究)

  • 서창민;김규남
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.8 no.3
    • /
    • pp.195-200
    • /
    • 1984
  • In-plane tension fatigue tests(R=0.1) were carried out to investigate the initiation and growth behaviors of very small surface fatigue cracks on smooth unnotched surfaces of type 304 stainless steel at room temperature. The present paper deals with the unification of two approaches to the analysis of fatigue: the one approach is based on fracture mechanics concept and the other on low-cycle fatigue concept. The results are;(1)Maximum crack length, 2 $a_{max}$, initiated at a very small surface scratch not exceeding 20 .mu.m which can exist on the surface after buffing. And the density of small surface crack is remarkably low compared to that of mild steel. (2) The growth rate, d(2a)/dN, of very small fatigue cracks can be represented by one straight line as a function of either stress intensity factor range, .DELTA. $K_{I}$ or cyclic total strain intensity factor range, .DELTA. $K_{\epsilon}$$_{I}$/, for various values of the nominal stress range.e.e.e.e.

Dynamic Fracture Properties of Nylon Thermoplastic Material Depending on Notch Angle with Charpy Impact Machine and Finite Element Method (유한요소법과 샤피충격시험기에 의한 노치각도에 따른 나일론 열가소성 플라스틱 재료의 파괴특성)

  • Park, Myung-Kyun;Lee, Jung-Won;Kim, Tae-Ok
    • Journal of the Korean Institute of Gas
    • /
    • v.12 no.1
    • /
    • pp.1-6
    • /
    • 2008
  • The notched Charpy impact test is one of the most prevalent techniques used to characterize the effect of high impulse loads on polymeric materials. In this study, a method of analysis in nylon plastic materials is suggested to evaluate the critical strain energy release rate for variation of notch angles from the Charpy impact energy measurement. Instrumented Charpy impact tester was used to extract ancillary information concerning fracture parameters in addition to total fracture properties and maximum critical load. The dynamic stress intensity factor of nylon plastic material was calculated for the ASTM Charpy specimen from the obtained maximum critical load. Also, the finite element model was developed to figure out the stress distributions for Charpy specimen with different notch angles subject to 3 point bending load which is equivalent to the load applied in the experiment.

  • PDF

A Study on Growth Characteristics of the Surface Fatigue Crack Propagated from a Small Surface Defect in Carbon Steels (탄소강재(炭素鋼材)의 작은 표면결함(表面缺陷)에서 성장(成長)하는 표면피로(表面疲勞)균열의 성장특성(成長特性)에 관한 연구(硏究))

  • Chang-Min,Suh;Yong-Goo,Kang
    • Bulletin of the Society of Naval Architects of Korea
    • /
    • v.21 no.1
    • /
    • pp.35-42
    • /
    • 1984
  • In the present study, rotating bending fatigue tests have been carried out in three kinds of carbon steel specimens; an annealed low carbon steel, an annealed high carbon steel and quenched-tempered high carbon steel; with a small artificial surface defect that might exist in real structures. Fatigue crack lengths have been observed by a method of replication in order to investigate the growth characteristic of fatigue crack in the viewpoints of strength of materials and fracture mechanics. The main results obtained are as follows: 1) The effect of a small surface defect upon the reduction of fatigue limit is considerably large, and the rate of fatigue limit reduction grows in the following order; annealed low carbon steel(mild steel), annealed high carbon steel, quenched-tempered high carbon steel. 2) When the growth rate of surface crack length(2a) was investigated in the viewpoints of fracture mechanics based upon $ ${\Delta}K_{\varepsilon}$, the dependence of stress level and of surface defect size disappear, and there exists a linear relationships between d(2a)/dN and ${\Delta}K_{{\varepsilon}t},\;\Delta_{{\varepsilon}t}\sqrt{{\pi}a}$, on log. plot, i.e, $d(2a)/dN={C{\cdot}{\Delta}K_{\varepsilon}}^3_t$, where ${\Delta}_{{\varepsilon}t}\sqrt{{\pi}a}$ a is the cyclic total strain intensity factor range.

  • PDF

Surface Crack Behavior and the Fatigue Life Prediction of Notched Specimens (표면균열의 거동과 피로수명예측에 관한 연구)

  • 서창민;이정주;정은화;박희범
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.12 no.5
    • /
    • pp.1097-1103
    • /
    • 1988
  • This paper deals with surface crack behavior and the fatigue life prediction of notched specimens using the relation between surface crack length, a, and the cycle ratio, $N/N_{f}$. From the $a-N\;/\;N_{f}$ curves, UC(the upper limit curve), LC(the lower limit curve) and MC(the middle limit curve) were assumed and utilized to predict the fatigue life and crack growth rate. The data computed from the three assumed curves were compared with the experimental data. It has been found that in the stable crack growth region ($N/N_{f}=0.3-0.8$) fatigue life can be predicted within 20% errors. Using the characteristics of $a-N\;/\;N_{f}$ curve, it is possible to predict the $da/dN-K_{max}$ curve, the $da/dN-{\Delta}K_{{\varepsilon}_t}$ curve, and the $S-N_{f}$ curve.

Production of Concentrated Blueberry Vinegar Using Blueberry Juice and Its Antioxidant and Antimicrobial Activities (블루베리 농축식초 제조 및 이들의 항산화 및 항균 활성)

  • Oh, Hyeonhwa;Jang, Sowon;Jun, Hyun-Il;Jeong, Do-Youn;Kim, Young-Soo;Song, Geun-Seoup
    • Journal of the Korean Society of Food Science and Nutrition
    • /
    • v.46 no.6
    • /
    • pp.695-702
    • /
    • 2017
  • This study was carried out to investigate the effects of seed vinegar on antioxidant activity and antimicrobial activities of concentrated blueberry vinegar (CBV). Of the nine strains of yeast and six strains of acetic acid bacteria provided by the Microbial Institute for Fermentation Industry, each strain of yeast (Saccharomyces cerevisiae SRCM 100610, showing the highest ethanol content) and acetic acid bacteria (Acetobacter pasteurianus SRCM 101342, showing the highest total acidity) was selected for production of CBVs. Sugar content, pH, total acidity, total phenolic content (TPC), and browning intensity (280 nm and 420 nm) in CBVs using concentrated blueberry juice were $11.05{\sim}12.70^{\circ}Brix$, 2.63~2.98, 1.65~5.72%, 3.03~4.24 mg/mL, 0.95~1.50, and 0.11~0.20, respectively. Sugar content and total acidity of CBVs increased upon addition of seed vinegar, whereas pH, TPC, and browning intensity decreased. Of all CBVs with various additions of seed vinegar, the control showed the lowest $EC_{50}$ values in DPPH radical scavenging assay, ABTS radical scavenging assay, and reducing power (23.80, 19.48, and 79.21 dilution factor, respectively), whereas the 40% seed vinegar group showed the highest clear zone diameter values for Escherichia coli, Staphylococcus aureus, Listeria monocytogenes, and Bacillus cereus (4.31, 4.59, 5.81, and 3.97, respectively). Antioxidant activities of CBVs were closely correlated with their TPC, browning intensity at 280 nm, pH, and total acidity values, showing correlation determination coefficient ($R^2$) values higher 0.82. However, antimicrobial activities of CBVs were closely correlated with their pH and total acidity values, showing higher $R^2$ values more than 0.92. These results suggest that CBVs using concentrated blueberry juice, S. cerevisiae SRCM 100610, and A. pasteurianus SRCM 101342 may be useful as potentially functional foods for enhancing health.

The Effect of the Replacement of Grinded Fly Ash according to Curing Temperature on Repair Mortar Based on Polymer Admixture (폴리머수지 기반 보수모르타르에서 양생온도에 따른 미분쇄된 플라이애시 치환율의 영향)

  • Sim, Jae-Il;Mun, Ju-Hyun;Yun, In-Gu;Jeon, Young-Su
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.19 no.4
    • /
    • pp.116-124
    • /
    • 2015
  • The objective of this study is to evaluate the effects of the replacement levels of grinded fly-ash on the repaired mortar based on a polymer. The main parameters are the curing temperature and replacement levels of grinded fly-ash. The curing temperature and the replacement levels of grinded fly-ash are varied at $40^{\circ}C$, $20^{\circ}C$ and $5^{\circ}C$, and between 0% and 35% of the total binder by weight, respectively. The flow in fresh mortar and compressive strengths according to ages, the relationship of stress-strain, elastic modulus and modulus rupture in hardened mortar, as well as scanning the electron microscopy and the X-ray diffraction of mortar, were measured, respectively. The test results showed that the flow, elastic modulus and modulus rupture are great in mortar specimens with 20~30% of the replacement levels of grinded fly-ash. In addition, compressive strengths according to ages were affected by the replacement levels of grinded fly-ash and the curing temperature indicated that the strength development ratio of mortar with 20% of the replacement levels of grinded fly-ash was greater than others. In the prediction of the compressive strength specified by the ACI 209 code, the strength development at an early and late age can be generalized by the functions of the replacement levels of grinded fly-ash and the curing temperature. In the analysis of scanning the electron microscopy and the X-ray diffraction, the number and intensity of peaks increased and the form of CSH gels on the surface of the particle of grinded fly-ash was observed.

An Analytical Study on Crack Behavior Inside Standard Compact Tension Specimen with Holes (구멍들을 가진 표준 CT 시험편 내에서의 크랙 거동에 대한 해석적 연구)

  • Lee, Jung Ho;Cho, Jae Ung
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.40 no.6
    • /
    • pp.531-537
    • /
    • 2016
  • The damage and fracture of machine or structure are caused by the crack happened from the defect existed at the inside of material. The properties of crack propagation and growth characteristic must be considered because there are many cases at which these cracks are densely existed. Therefore, this study investigates the fracture property due to the position of crack and hole inside the standard compact tension (C. T.) specimen. When the concentrated load is applied eccentrically at the standard C. T. specimen, the fracture mechanical behavior due to the existence or non-existence and the position of hole near crack is investigated. As the result of analysis study, model 3 (in case of the distance of 2mm on the horizontal direction between the end part and hole as the specimen model existed with one hole near the crack) has the maximum deformation, stress and deformation energy of the most values among three models. As the distance between the crack and hole inside the specimen becomes nearer, the maximum stress becomes higher in cases of three models. Apart from the number of holes, it is seen that the maximum stress becomes higher near the crack when the hole exists near the crack inside the specimen. If the hole inside the machine or the mechanical structure is punctured by using the result of this study, it is thought that the occurred breakage or breakdown can be prevented by reducing the fracture stress happened at the specimen.