• 제목/요약/키워드: TiC content

검색결과 453건 처리시간 0.02초

Al-7Si 합급의 결정립 미세화에 미치는 TiC 첨가의 영향 (Study on Grain Refinement of Al-7Si Based Alloys with TiC)

  • 한윤성;최창옥
    • 한국주조공학회지
    • /
    • 제23권2호
    • /
    • pp.63-68
    • /
    • 2003
  • Al-Ti-C grain refiner form a relatively new alternative to the existing class of Al-Ti-B type grain refiners for achieving fine equiaxed structures in aluminum alloys during casting and solidification. The present study was carried out to investigate the influence of Al-Ti-C master alloys on the grain structure of Al-7Si alloys. The present study also investigates the relationship between grain refining efficiency and concentrations of Fe and Si in hypo-eutectic Al-Si alloys using Al-3Ti-0.13C master alloys. It is found that several parameters affect significantly the grain refining performance in silumin alloys. The present study reports the influence of various parameters such as alloy content, master alloy addition level, melt holding time and superheat on the grain refining efficiency in Al-7Si alloys.

Si 함량에 따른 Ti-Al-Si-C-N 코팅막의 미세구조와 기계적 특성의 변화에 관한 연구 (Effect of Si on the Microstructure and Mechanical Properties of Ti-Al-Si-C-N Coatings)

  • 홍영수;권세훈;김광호
    • 한국표면공학회지
    • /
    • 제42권2호
    • /
    • pp.73-78
    • /
    • 2009
  • Quinary Ti-Al-Si-C-N films were successfully synthesized on SUS 304 substrates and Si wafers by a hybrid coating system combining an arc ion plating technique and a DC reactive magnetron sputtering technique. In this work, the effect of Si content on the microstructure and mechanical properties of Ti-Al-C-N films were systematically investigated. It was revealed that the microstructure of Ti-Al-Si-C-N coatings changed from a columnar to a nano-composite by the Si addition. Due to the nanocomposite microstructure of Ti-Al-Si-C-N coatings, the microhardness of The Ti-Al-Si-C-N coatings significantly increased up to 56 GPa. In addition the average friction coefficients of Ti-Al-Si-C-N coatings were remarkably decreased with Si addition. Therefore, Ti-Al-Si-C-N coatings can be applicable as next-generation hard-coating materials due to their improved hybrid mechanical properties.

에폭시수지 복합재료의 기계적.열적 성질에 대한 $TiO_2$ 나노입자의 영향 (Effect of $TiO_2$ Nanoparticle on the Mechanical and Thermal Properties of Epoxy Resin Composites)

  • 문용재;최정영;김부안;문창권
    • 동력기계공학회지
    • /
    • 제14권4호
    • /
    • pp.68-75
    • /
    • 2010
  • The effect of dispersion agent, the content and size of nanoparticle on the mechanical and thermal properties has been investigated in $TiO_2$ nanoparticle/epoxy resin composites(nanocomposites). The weight fraction of fabricated nanocomposites were 0, 1, 3, 5%, respectively. The glass transition temperature was lower than pure epoxy resin and decreased with the increasing of nanopaticle content. This is considered that the cross link of epoxy resin during solidification was hindered by the presence of nanoparticles. Nanocomposites of 3wt% content with dispersion agent showed the best tensile strength. The tensile strength of 20㎚ $TiO_2$ nanocomposites were higher than one of 200nm $TiO_2$ nanocomposites.

Ti 첨가강 열영향부 조직과 인성에 미치는 질소의 영향 (Effects of Nitrogen on the Microstructure and Toughness of HAZ in Ti-Containing Steel)

  • 김병철;방국수
    • Journal of Welding and Joining
    • /
    • 제20권3호
    • /
    • pp.91-97
    • /
    • 2002
  • Variation of HAZ toughness of Ti-containing steel with nitrogen content was investigated and interpreted in terms of its microstructure and the amount of soluble nitrogen present. The amounts of Ti and Al combined in TiN and AlN, respectively, in HAZ at $1400^{\circ}C$ peak temperature were less than those in base plate; 55~88% in TiN and 21~28% in AlN, indicating the dissolution of nitrifies in HAZ. The calculated amounts of soluble nitrogen using the thermodynamic analysis showed a good agreement with the measured values in other experiment. Therefore, the analysis can be used to estimate the amount of soluble nitrogen in HAZ. Simulated HAZ toughness was influenced not only by its microstructure but also by the amount of soluble nitrogen present after the formation of BN during the cooling cycle of welding. It showed maximum value when the nitrogen content is in stoichiometric ratio with titanium content, showing that soluble nitrogen in HAZ is detrimental to its toughness.

고압연소소결(HPCS)법을 이용한 Ti-C-Mo계 탄화물 복합체의 제조 (Preparation of Carbide Composites for Ti-C-Mo system by HPCS(High-Pressure self-Combustion Sintering) Process)

  • 최장민;이근행;류종화;조원승;최상욱
    • 한국세라믹학회지
    • /
    • 제36권4호
    • /
    • pp.451-458
    • /
    • 1999
  • TiC-Mo2C composites were prepared from Ti-C-Mo system by HPCS which has a great advantage of simulataneous synthesis and sintering In this study physical properties and microstructures of the com-posites were measured and observed to compare the sintering effects of Ni and Co each other : The results showed that the role of 5 wt% Ni in the sintering of the carbide composites was superior to that of 5wt% Co and the optimum content of Mo in the Ti-C-Mo system was 20wt% The carbide composites prepared under these two conditions had the best properties with 1.0% in apparent porosity 97.6% in relative density 19.1GPa in Vickers hardness and 5.3MPa$.$m1/2 in fracture toughness.

  • PDF

가압 소결법으로 합성된 Ti3SiC2 소결체의 기계적 특성 (Mechanical Properties of Bulk Ti3SiC2 Synthesized by a Hot Press Sintering)

  • 조경선;황성식;권혁보;박상환
    • 한국세라믹학회지
    • /
    • 제47권6호
    • /
    • pp.560-565
    • /
    • 2010
  • Nano laminated bulk $Ti_3SiC_2$ was synthesized by hot press process using TiCx/Si powder mixture at the temperature range of $1300^{\circ}C\sim1500^{\circ}C$. pure $Ti_3SiC_2$ was synthesized by a hot pressing above $1400^{\circ}C$, while unreacted TiCx were remained in bulk $Ti_3SiC_2$ which synthesized below $1400^{\circ}C$. The sintering density of bulk $Ti_3SiC_2$ were varied with the amount of TiCx. It was found that the mechanical properties and micro structures of bulk $Ti_3SiC_2$ were closely related to the amounts of TiCx which was controlled by the hot pressing temperature. The TiCx increase the flexural strength of bulk $Ti_3SiC_2$, while the fracture toughness and thermal shock resistance of bulk $Ti_3SiC_2$ were decreased with the content of TiCx. The plastic deformations of bulk $Ti_3SiC_2$ were appeared above $1000^{\circ}C$.

새로운 고경도 Ti-Mo-Si-N 코팅막의 합성 및 기계적 특성 (Synthesis and Characteristics of New Quaternary Superhard Ti-Mo-Si-N Coatings)

  • 전진우;홍승균;김광호
    • 한국표면공학회지
    • /
    • 제39권6호
    • /
    • pp.245-249
    • /
    • 2006
  • In this study, ternary Ti-Mo-N and new quaternary Ti-Mo-Si-N coatings were synthesized on steel substrates(AISI D2) and Si wafers by a hybrid coating system of arc ion plating (AIP) using Ti target and d.c. magnetron sputtering technique using Mo and Si targets in $N_2/Ar$ gaseous mixture. Ternary Ti-Mo-N coatings were substitutional solid-solution of (Ti, Mo)N and showed maximum hardness of approximately 30 GPa at the Mo content of ${\sim}10$. %. The Ti-Mo-Si-N coating with the Si content of 8.8 at. % was a composite consisting of fine (Ti, Mo)N crystallites and amorphous $Si_3N_4$ phase. The hardness of the Ti-Mo-Si(8.8 at. %)-N coatings exhibited largely increased hardness value of ${\sim}48$ GPa due to the microstructural evolution to the fine composite microstructure and the refinement of (Ti, Mo)N crystallites. The average friction coefficient of the Ti-Mo-Si-N coatings largely decreased with increase of Si content. The microstructures of Ti-Mo-Si-N coatings were investigated with instrumental analyses of XRD, XPS, and HRTEM in this work.

MOD법에 의한 Sr modified $PbTiO_3$ 박막 제조 및 Tunable microwave device 응용 특성 연구 (Sr modified $PbTiO_3$ thin films for tunable microwave device application)

  • 강동헌;조수철;차훈주;조봉희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집 Vol.3 No.2
    • /
    • pp.749-751
    • /
    • 2002
  • $(Pb_{1-x}Sr_x)TiO_3$ $(0.6{\leq}x{\leq}0.8)$ thin films were prepared by the MOD method for tunable microwave device application and their characteristics were investigated as a function of Sr content(x) and applied field. Thin films showed a homogeneous microstructure and the tetragonality(c/a) was slightly decreased with increasing Sr content. With increasing Sr content, Curie temperature of the thin films showed a decreasing tendency. For the PST thin films, the dielectric constant at room temperature, Tc, and $tan{\delta}$ were 750~1900, $-70^{\circ}{\sim}-30^{\circ}C$ and 0.025~0.04, respectively.

  • PDF

Electrically Conductive Silicon Carbide without Oxide Sintering Additives

  • Frajkorova, Frantiska;Lences, Zoltan;Sajgalik, Pavol
    • 한국세라믹학회지
    • /
    • 제49권4호
    • /
    • pp.342-346
    • /
    • 2012
  • This work deals with the preparation of dense SiC based ceramics with high electrical conductivity without oxide sintering additives. SiC samples with different content of conductive Ti-NbC phase were hot pressed at $1850^{\circ}C$ for 1 h in Ar atmosphere under mechanical pressure of 30 MPa. The conductive phase is a mixture of Ti-NbC in weight ratio of Ti/NbC 1:4. Composite with 50% of conductive Ti-NbC phase showed the highest electrical conductivity of $30.6{\times}10^3\;S{\cdot}m^{-1}$, while the good mechanical properties of SiC matrix were preserved (fracture toughness 4.5 $MPa{\cdot}m^{1/2}$ and Vickers hardness 18.7 GPa). The obtained results show that use of NbC and Ti as sintering and also electrically conductive additives is appropriate for the preparation of SiC-based composite with sufficient electrical conductivity for electric discharge machining.

증착온도와 RF Power가 TiCN박막의 플라즈마 화학증착에 미치는 영향 (The Effects of Deposition Temperature and RF Power on the Plasma Assisted Chemical Vapor Deposition of TiCN Films)

  • 김시범;김광호;김상호;천성순
    • 한국세라믹학회지
    • /
    • 제26권3호
    • /
    • pp.323-330
    • /
    • 1989
  • Wear restance titanium carbonitride (TiCN) films were deposited on the SKH9 tool steels and WC-Co cutting tools by plasma assisted chemical vapor deposition (PACVD) using a gaseous mixture of TiCl4, CH4, N2, H2 and Ar. The effects of the deposition temperature and RF(Radio Frequency) power on the deposition rate, chlorine content and crystallinity of the deposited layer were studied. The experimental results showed that the stable and adherent films could be obtained above the deposition temperature of 47$0^{\circ}C$ and maximum deposition rate was obtained at 485$^{\circ}C$. The deposition rate was much affected by RF power and maximum at 40W. The crystallinity of the deposited layer was improved with increasing the deposition temperature and RF power. The TiCN films deposited by PACVD contained much chlorine. The chlorine content in the TiCN films was affected by deposition conditions and decreased with improving the crystallinity of the deposited layer. The deposited TiCN films deposited at the deposition temperature of 52$0^{\circ}C$ and RF power of 40W had an uniform surface with very fine grains of about 500$\AA$ size. The microhardness of the deposited layer was 2,300Kg/$\textrm{mm}^2$.

  • PDF