• Title/Summary/Keyword: Ti-Ta-Nb

Search Result 125, Processing Time 0.038 seconds

Cell response to a newly developed Ti-10Ta-10Nb alloy and its sputtered nanoscale coating

  • Kim, Young-Min;Vang, Mong-Sook;Yang, Hong-So;Park, Sang-Won;Lim, Hyun-Pil
    • The Journal of Advanced Prosthodontics
    • /
    • v.1 no.1
    • /
    • pp.56-61
    • /
    • 2009
  • STATEMENT OF PROBLEM. The success of titanium implants is due to osseointegration or the direct contact of the implant surface and bone without a fibrous connective tissue interface. PURPOSE. The purpose of this study was to evaluate the osteoblast precursor response to titanium-10 tantalum-10 niobium(Ti-Ta-Nb) alloy and its sputtered coating. MATERIAL AND METHODS. Ti-Ta-Nb coatings were sputtered onto the Ti-Ta-Nb disks. Ti6-Al-4V alloy disks were used as controls. An osteoblast precursor cell line, were used to evaluate the cell responses to the 3 groups. Cell attachment was measured using coulter counter and the cell morphology during attachment period was observed using fluorescent microscopy. Cell culture was performed at 4, 8, 12 and 16 days. RESULTS. The sputtered Ti-Ta-Nb coatings consisted of dense nanoscale grains in the range of 30 to 100 nm with alpha-Ti crystal structure. The Ti-Ta-Nb disks and its sputtered nanoscale coatings exhibited greater hydrophilicity and rougher surfaces compared to the Ti-6Al-4V disks. The sputtered nanoscale Ti-Ta-Nb coatings exhibited significantly greater cell attachment compared to Ti-6Al-4V and Ti-Ta-Nb disks. Nanoscale Ti-Ta-Nb coatings exhibited significantly greater ALP specific activity and total protein production compared to the other 2 groups CONCLUSIONS. It was concluded that nanoscale Ti-Ta-Nb coatings enhance cell adhesion. In addition, Ti-Ta-Nb alloy and its nanoscale coatings enhanced osteoblast differentiation, but did not support osteoblast precursor proliferation compared to Ti-6Al-4V. These results indicate that the new developed Ti-Ta-Nb alloy and its nanoscale Ti-Ta-Nb coatings may be useful as an implant material.

Chemical Design of Highly Water-Soluble Ti, Nb and Ta Precursors for Multi-Component Oxides

  • Masato Kakihana;Judith Szanics;Masaru Tada
    • Bulletin of the Korean Chemical Society
    • /
    • v.20 no.8
    • /
    • pp.893-896
    • /
    • 1999
  • Novel citric acid based Ti, Nb and Ta precursors that are highly stable in the presence of water were developed. No alkoxides of Ti, Nb and Ta were utilized in the preparation, instead much less moisture-sensitive metallic Ti, NbCl5 and TaCl5 were chosen as starting chemicals for Ti, Nb and Ta, respectively. The feasibility of these chemicals as precursors is demonstrated in the powder synthesis of BaTi4O9, Y3NbO7 and LiTaO3. The water-resistant Ti precursor was employed as a new source of water-soluble Ti in the amorphous citrate method, and phase pure BaTi4O9 in powdered form was successfully synthesized at 800 ?. The Pechini-type polymerizable complex method using the water-resistant Nb and Ta precursors was applied to the synthesis of Y3NbO7 and LiTaO3, and both the powder materials in their pure form were successfully synthesized at reduced tempera-tures, viz. 500-700 ?. The remarkable retardation of hydrolysis of these water-resistant precursors is explained in terms of the partial charge model theory.

Biological response of primary rat calvarial cell by surface treatment of Ti-8Ta-8Nb alloy (Ti-8Ta-3Nb 합금의 표면처리에 의한 백서 두개관 세포의 반응)

  • Kim, Hae-Jin;Son, Mee-Kyoung;Park, Ji-Il;Chung, Hyun-Ju;Kim, Young-Joon
    • Journal of Periodontal and Implant Science
    • /
    • v.38 no.4
    • /
    • pp.595-602
    • /
    • 2008
  • Purpose: Ti-6Al-4V alloy is widely used as an implant material because of its good biocompatibility and good mechanical property compared with commercial pure titanium. Otherwise, toxicity of aluminum and vanadium in vivo has been reported. Ti-8Ta-3Nb alloy is recently developed in the R&D Center for Ti and Special Alloys and it was reported that this alloy has high mechanical strength, no cytotoxicity and similar biocompatibility to commercial pure titanium, but many studies are needed for its clinical use. In these experiment, we carried out different surface treatment on each Ti-8Ta-3Nb alloy disks, then cultured cell on it and assessed biological response. Materials and Methods: cpTi, Ti-6Al-4V, Ti-8Ta-3Nb alloy disks were prepared and carried out sandblasting and acid etching (SLA) or alkali-heat treatment (AH) on the Ti-8Ta-3Nb alloy disks. We cultured primary rat calvarial cells on each surface and assessed early cell attachment and proliferation by scanning electron microscopy, cell proliferation, alkaline phosphatase activity. Result: The rates of cell proliferation on the cpTi, Ti-8Ta-3Nb AH disks were higher than others (p<0.05) and alkaline phosphatase activity was significantly enhanced on the Ti-STa-8Nb AH disks(p<0.05). Conclusion: Most favorable cell response was shown on the Ti-8Ta-3Nb AH surfaces. It is supposed that alkali-heat treatment of the Ti-8Ta-3Nb alloy could be induced earlier bone healing and osseointegration than smooth surface.

Dielectric Properties of Ti-doped K(Ta,Nb)O3 Thin Films for Tunable Microwave Applications

  • Bae Hyung-Jin;Koo Jayl;Hong Jun-Pyo
    • Journal of Electrical Engineering and Technology
    • /
    • v.1 no.1
    • /
    • pp.120-126
    • /
    • 2006
  • Ferroelectric materials have been widely investigated for high density dynamic random access memories, opto-electrics, and tunable microwave devices due to their properties. In this study, we have investigated the dielectric properties of Ti doped $K(Ta,\;Nb)O_3$ thin films. By doping Ti Into the $K(Ta,Nb)O_3$ system, Ti with a valence value of +4 will substitute Ta or Nb ions with a valence value of +5. This substitution will introduce an acceptor state. Therefore, this introduced acceptor state will reduce dielectric loss by trapping electrons. Using 3% Ti-doped $K(Ta,Nb)O_3\;targets,\;K(Ta,Nb)O_3$:Ti films were grown in MgO(001) crystals using pulsed laser deposition. First, growth conditions were optimized. A reduction in the loss tangent was observed for Ti-doped $K(Ta,Nb)O_3$ relative to undoped films, although a reduction in tunability is also seen. The crystallinity, morphology, and tunability of $K(Ta,Nb)O_3$:Ti films are reported.

THE EVALUATION OF CYTOTOXICITY AND BIOCOMPATIBILITY OF TI-TA-NB-BASE ALLOY (Ti-Ta-Nb계 합금의 세포독성과 생체적합성의 평가)

  • Cui De-Zhe;Vang Mong-Sook;Yoon Taek-Rin
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.44 no.2
    • /
    • pp.250-263
    • /
    • 2006
  • Statement of problem: Ti-alloy has been used widely since it was produced in the United States in 1947 because it has high biocompatibility and anticorrosive characteristics. Purpose: The pure titanium, however, was used limitedly due to insufficient mechanical charateristics and difficult manufacturing process. Our previous study was focused on the development of a new titanium alloy. In the previous study we found that the Ti-Ta-Nb alloy had better mechanical characteristics and similar anticorrosive characteristics to Ti-6Al-4V Material and methods: In this study, the cytotoxicity of the Ti-Ta-Nb alloy was evaluated by MTT assay using MSCs(Mesenchaimal stem cells) and L929 cells(fibroblast cell line). The biocompatibility of the Ti-Ta-Nb alloy was performed by inserting the alloy into the femur of the rabbits and observing the radiological and histological changes surrounding the alloy implant. Results: 1. In the cytotoxicity test using MSCs, the 60% survival rate was observed in pure titanium, 84% in Ti-6Al-4V alloy and 95% in Ti-10Ta-10Nb alloy. 2. In the animal study, the serial follow-up of the radiographs showed no separation or migration revealing gradual bone ingrowth surrounding the implants. Similar radiographic results were obtained among three implant groups pure titanium, Ti-6Al-4V alloy and Ti-10Ta-10Nb alloy. 3. In the histologic examination of the bone block containing the implants. the bone ingrowth was prominent around the implants with the lapse of time. There was no signs of any tissue rejection, degeneration, or inflammation. Active bone ingrowth was observed around the implants. In the comparison of the three groups, the rate of bone ingrowth was better in the Ti-10Ta-10Nb alloy group than those in pure titanium group or Ti-6Al-4V alloy group. In conclusion, Ti-10Ta-10Nb alloy revealed better biocompatibility in survival rate of the cells and bone ingrowth around the implants. Therefore we believe a newly developed Ti-10Ta-10Nb alloy can replace currently used Ti-6Al-4V alloy to increase biocompatibility and to decrease side effects. Conclusion: In conclusion, Ti-10Ta-10Nb alloy revealed better biocompatibility in survival rate of the cells and bone ingrowth around the implants. Therefore we believe a newly developed Ti-10Ta-10Nb alloy can replace currently used Ti-6Al-4V alloy to increase biocompatibility and to decrease side effects.

Study for Fatigue Crack Propagation Behavior of Ti-alloy (Ti 합금의 피로 특성 고찰)

  • 정화일;조규종
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 1997.10a
    • /
    • pp.786-789
    • /
    • 1997
  • Ti-6Al-4V has been used widely in biomedical field. But because of its toxicity, the ${\beta}$ stabilizing element, V, in Ti-6Al-4V has been replaced by Nb, Ta. Ti-10Ta-10Nb has been developed for biomedical applications. The fatigue crack propagation behavior of Ti-alloy(Ti-10Ta-10Nb) was investigated, in comparison with that of pure Ti. In order to better understand the fundamental fatigue behavior of Ti-10Ta-10Nb, rotating bending fatigue tests have been carried out. Ti-10Ta-10Nb has a better fatigue strength than pure Ti. In this paper, fatigue life has been predicted with Nisitani's equation of the fatigue crack propagation that can be established by measuring fatigue crack growth rates.

  • PDF

Microstructure of $SrBi_2(Ta,Nb)_2O_9$ Thin Films on $SrTiO_3$(001) Single Crystal ($SrTiO_3$(001) 단결정 위에 제조된 $SrBi_2(Ta,Nb)_2O_9$ 박막의 미세구조)

  • 이지현
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.10
    • /
    • pp.1008-1013
    • /
    • 2000
  • SrTi $O_3$(001) 단결정 기판 위에 졸-겔 스핀코팅으로 $SrBi_2(Ta,Nb)_2O_9$ 박막을 도포하고 그 결정화 과정을 고온 X-선 회절분석 (HTXRD)으로 추적하면서 Pt(111)/Ti/ $SiO_2$/Si 위에 성장한 박막과 비교하였다. SrTi $O_3$(001) 단결정 기판 위에 도포된 $SrBi_2Nb_2O_{9}$ 박막은 fluorite-like phase와 같은 transient phase를 거치지 않고 곧바로 순수한 $SrBi_2Nb_2O_9$ 상으로 결정화가 시작되었으며 결정화가 시작되는 온도인 ${\sim}540^{\circ}C$부터 c축 배향성장하였다. 또한 $SrB i_2(Ta,Nb)_2O_9$ 박막은 Ta/Nb 비에 관계없이 $SrTiO_3$(001) 위에서 모두 $(00{\ell})$로 배향되었으며, 코팅 횟수가 늘어나 필름의 두께가 증가함에 따라 c축 배향성은 미세한 감소를 보였다. $SrBi_2Nb_2O_9/SrTiO_3$단면을 TEM으로 관찰한 결과 $SrBi_2Nb_2O_9$은 대체로 불규칙한 크기의 다결정체로 되어 있었으나 계면 부근에서는 [001]$_{SBN}$//[001]$_{SrTi}$ $O_3$/, [100]$_{SBN}$//[100]$_{SrTi}$ $O_3$/라는 결정학적 관계를 가지며 에피탁샬 성장했음을 알 수 있었다.있었다.

  • PDF

Effect of multi-layered HA/Ti coating on biological Ti-30Ta-xNb alloys (생체용 Ti-30Ta-xNb 합금의 HA/Ti 복합코팅의 영향)

  • Jeong, Yong-Hun;Choe, Han-Cheol;Go, Yeong-Mu
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2007.11a
    • /
    • pp.51-51
    • /
    • 2007
  • 기존에 있는 Ti 합금의 여러 가지 단점을 보완하기 위해 골과의 탄성계수 차이를 줄이고 독성이 없는 Ta, Nb와 같은 ${\beta}$형 안정화 원소를 Ti 와 합금하여 Ti-30Ta-(3${\sim}$15wt%)Nb 합금을 제조하여 RF-magnetron sputter를 이용하여 Ti/HA 복합코팅을 하여 코팅된 합금의 전기화학적 특성을 조사하였다.

  • PDF

Study on the mechanical Properties of Ti-8Ta-3Nb Alloys for Biomaterials (생체재료용 Ti-8Ta-3Nb 합금의 물성변화 고찰)

  • 이경원;반재삼;유영선;조규종
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2003.06a
    • /
    • pp.1374-1377
    • /
    • 2003
  • Ti-8Ta-3Nb is made for biomaterial. The experimental speciments are as-cast Ti-8Ta-3Nb and Ti-8Ta-3Nb swaged. The solution treatment in the range 760-96$0^{\circ}C$have been carried out. The microstructural investigations have been carried out on the specimens after the solution treatment. and the hardness have been measured. And the specific heat and the dilatometer of Ti-8Ta-3Nb swaged have been measured. From the result, the $\beta$ transus of the alloy was determined to be 880-86$0^{\circ}C$.

  • PDF

Electrochemical Properties of Ti-30Ta-(3~15)Nb Alloys Coated by HA/Ti Compound Layer (HA/Ti 복합층 코팅한 Ti-30Ta-(3~15)Nb 합금의 전기화학적 특성)

  • Jeong, Yong-Hoon;Choe, Han-Cheol;Ko, Yeong-Mu
    • Journal of the Korean institute of surface engineering
    • /
    • v.41 no.2
    • /
    • pp.57-62
    • /
    • 2008
  • Electrochemical properties of Ti-30Ta-$(3{\sim}15)$Nb alloys coated by HA/Ti compound layer have been studied by various electrochemical method. Ti-30Ta binary alloys contained 3, 7, 10, and 15 wt% Nb contents were manufactured by the vacuum furnace system. The specimens were homogenized for 24 hrs at $1000^{\circ}C$. The samples were cut and polished for corrosion test and coating. It was coated with HA/Ti compound layer by magnetron sputter. The HA/Ti non-coated and coated morphology of Ti alloy were analyzed by x-ray diffractometer(XRD) and filed emission scanning electron microscope(FE-SEM). The corrosion behaviors were investigated using potentiodynamic method in 0.9% NaCl solution at $36.5{\pm}1^{\circ}C$. The homoginazed Ti-30Ta-$(3{\sim}15wt%$)Nb alloys showed the ${\alpha}+{\beta}$ phase, and ${\beta}$ phase peak was predominantly appeared with increasing Nb content. The microstructure of Ti alloy was transformed from needle-like structure to equiaxed structure as Nb content increased. HA/Ti composite surface showed uniform coating layer with 750 nm thickness. The corrosion resistance of HA/Ti composite coated Ti-alloys were higher than those of the non-coated samples in 0.9% NaCl solution at $36.5{\pm}1^{\circ}C$. Especially, corrosion resistance of Ti-Ta-Nb system increased as Nb content increased.