ECAP 강소성 가공에 의한 구조재료 초미세립화 (Fabrication of Ultrafine Grained Structure Materials by Equal Channel Angular Pressing)

  • 김우겸;안정용;신동혁;박경태;고영건;이종수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2005년도 추계학술대회 논문집
    • /
    • pp.126-129
    • /
    • 2005
  • Microstructures and tensile properties of low carbon steels, 5083 Al alloy and Ti-6Al-4V alloy fabricated by equal channel angular pressing (ECAP) were examined in order to understand their deformation response associated with a formation of an ultrafine grained (UFG) structure. Room temperature tensile properties of UFG low carbon ferrite/pearlite steels and UFG ferrite/martensite dual phase steel were compared for exploring a feasibility enhancing the strain hardening capability of UFG materials. In addition, low temperature and high strain rate superplasticity of the two grades of the UFG 5083 Al alloy, and Ti-6Al-4V alloy were presented. From the analysis of a series of experiments, it was found that UFG materials exhibited the enhanced mechanical properties compared to coarse grained counterparts.

  • PDF

TiN/Ti 다층막 코팅된 생체용 Ti-30Ta-xZr 합금의 부식특성 (Corrosion Characteristics of TiN/Ti Multilayer Coated Ti-30Ta-xZr Alloy for Biomaterials)

  • 김영운;조주영;최한철
    • Corrosion Science and Technology
    • /
    • 제8권4호
    • /
    • pp.162-169
    • /
    • 2009
  • Pure titanium and its alloys are drastically used in implant materials due to their excellent mechanical properties, high corrosion resistance and good biocompatibility. However, the widely used Ti-6Al-4V is found to release toxic ions (Al and V) into the body, leading to undesirable long-term effects. Ti-6Al-4V has much higher elastic modulus than cortical bone. Therefore, titanium alloys with low elastic modulus have been developed as biomaterials to minimize stress shielding. For this reason, Ti-30Ta-xZr alloy systems have been studied in this study. The Ti-30Ta containing Zr(5, 10 and 15 wt%) were 10 times melted to improve chemical homogeneity by using a vacuum furnace and then homogenized for 24 hrs at $1000^{\circ}C$. The specimens were cut and polished for corrosion test and Ti coating and then coated with TiN, respectively, by using DC magnetron sputtering method. The analyses of coated surface were carried out by field emission scanning electron microscope(FE-SEM). The electrochemical characteristics were examined using potentiodynamic (- 1500 mV~+ 2000 mV) and AC impedance spectroscopy(100 kHz~10 mHz) in 0.9% NaCl solution at $36.5{\pm}1^{\circ}C$. The equiaxed structure was changed to needle-like structure with increasing Zr content. The surface defects and structures were covered with TiN/Ti coated layer. From the polarization behavior in 0.9% NaCl solution, The corrosion current density of Ti-30Ta-xZr alloys decreased as Zr content increased, whereas, the corrosion potential of Ti-30Ta-xZr alloys increased as Zr content increased. The corrosion resistance of TiN/Ti-coated Ti-30Ta-xZr alloys were higher than that of the TiN-coated Ti-30Ta-xZr alloys. From the AC impedance in 0.9% NaCl solution, polarization resistance($R_p$) value of TiN/Ti coated Ti-30Ta-xZr alloys showed higher than that of TiN-coated Ti-30Ta-xZr alloys.

Ni/MH 2차전지용 TiFe1-xNix 합금전극의 방전특성에 대한 열처리의 영향 (Effects of Heat-treatments on Discharge Characteristics of TiFe1-xNix Alloy Electrodes for Ni/MH Secondary Battery)

  • 정순돌;정상식;안효준;김기원
    • 한국수소및신에너지학회논문집
    • /
    • 제9권4호
    • /
    • pp.135-141
    • /
    • 1998
  • Fe-Ti계 수소저장합금 전극의 방전특성을 개선하기 위하여 Ni을 첨가한 $TiFe_{1-x}Ni_x$ 합금을 제조하여 방전특성과 열처리 온도에 따른 변화를 조사하였다. 합금의 조성은 x = 0.1에서 0.6까지 0.1 단위씩 변화시킨 6가지 조성을 선택하여 각각에 대한 초기방전용량과 충방전사이클에 따른 용량변화를 조사하였다. 초기방전용량은 Ni의 조성이 클수록 증가하다가 x = 0.6 에서 다시 감소하였으며 Ni의 조성이 증가함에 따라 사이클특성은 전반적으로 매우 악화되었다. 열처리온도가 사이클 특성에 미치는 영향을 조사하기 위하여 초기용량이 가장 우수한 $TiFe_{0.5}Ni_{0.5}$ 합금에 대하여 $700{\sim}900^{\circ}C$ 의 온도범위에서 열처리를 시행한 후 방전특성을 조사하였다. 열처리에 의해서 초기용량은 감소되지만 사이클 특성은 현저히 개선되었다. $700{\sim}850^{\circ}C$의 온도범위에서 1시간 열처리한 전극의 경우에 사이클이 진행되면서 방전용량이 크게 회복되었으며, 열처리한 표면조직을 SEM 으로 관찰해 본 결과 이는 충분한 전극강도 및 기공율에 기인한 것으로 생각되었다. $900^{\circ}C$에서 1시간 열처리한 전극은 충분한 기공율을 갖지 못하여 방전특성이 좋지 않음을 알 수 있었다.

  • PDF

Effects of Alloying Element and Heat Treatment on Properties of Cu-Ti Alloys

  • Suk, Han-Gil;Hong, Hyun-Seon
    • 한국표면공학회지
    • /
    • 제42권5호
    • /
    • pp.246-249
    • /
    • 2009
  • Cu-Ti alloys with titanium in the range of 0.5-6.0 wt% were developed to evaluate the effect of the titanium content and heat treatment on microstructure, hardness, and electrical conductivity. The hardness of the Ti-added copper alloys generally increased with the increase in titanium content and hardening was effective up to the 2.5 wt%-Ti addition. Microstructural examination showed that the second phase of $Cu_4Ti$ started to precipitate out from the 3.0 wt% Ti-addition, and the precipitate size and volume fraction increased with further Ti addition. Aging of the present Cu-Ti alloys at $450^{\circ}C$ for 1 h increased the hardness; however, the further aging up to 10 h did not much change the hardness. In the present study, it was inferred that in optimal Ti addition and aging condition Cu-Ti alloy could have the hardness and electrical conductivity values which are comparable to those of commercial Cu-Be alloy.

펄스전류 활성 소결에 의한 나노구조의 TiAl 합금 제조와 기계적 성질 (Mechanical Properties and Fabrication of TiAl Alloy by Pulsed Current Activated Sintering)

  • 두송이;김나리;김원백;조성욱;손인진
    • 한국분말재료학회지
    • /
    • 제17권5호
    • /
    • pp.373-378
    • /
    • 2010
  • Nanostuctured TiAl powder was synthesized by high energy ball milling. A dense nanostuctured TiAl was consolidated using pulsed current activated sintering method within 2 minutes from mechanically synthesized powders of TiAl and horizontally milled powders of Ti+Al. The grain size and hardness of TiAl sintered from horizontally milled Ti+Al powders and high energy ball milled TiAl powder were 35 nm, 20 nm and 450 kg/$mm^2$, 630 kg/$mm^2$, respectively.

폴리머 코팅된 NiTi합금 교정선의 표면특성 (Surface Characteristics of Polymer Coated NiTi Alloy Wire for Orthodontics)

  • 조주영;김원기;최환석;이호종;최한철
    • 한국표면공학회지
    • /
    • 제43권3호
    • /
    • pp.132-141
    • /
    • 2010
  • NiTi alloy has been used for orthodontic wire due to good mechanical properties, such as elastic strength and frictional resistance, combined with a high resistance to corrosion. Recently, these wire were coated by polymer and ceramic materials for aesthetics. The purpose of this study was to investigate surface characteristics of polymer coated NiTi alloy wire for orthodontics using various instruments. Wires (round type and rectangular type) were used, respectively, for experiment. Polymer coating was carried out for wire. Specimen was investigated with field emission scanning electron microscopy(FE-SEM), energy dispersive x-ray spectroscopy(EDS) and atomic force microscopy(AFM). The phase transformation of non-coated NiTi wire from martensite to austenite occurred at the range of $14{\sim}15^{\circ}C$, in the case of coated wire, it occurred at the range of $16{\sim}18^{\circ}C$. Polymer coating on NiTi wire surface decreased the surface defects such as scratch which was formed at severe machined surface. From the AFM results, the average surface roughness of non-coated and coated NiTi wire was 13.1 nm, and 224.5 nm, respectively. From convetional surface roughness test, the average surface roughness of non-coated and coated NiTi wire was $0.046{\mu}m$, and $0.718{\mu}m$, respectively.

Ni-MH 2차 전지용 Zr계 수소저장합금전극의 특성에 미치는 치환원소(Co, Cr, Fe)의 영향 (The effect of substitution elements(Co, Cr, Fe) on the properties of Zr-based hydrogen storage alloy electrode for Ni-MH secondary battery)

  • 최승준;정소이;서찬열;최전;박충년
    • 한국수소및신에너지학회논문집
    • /
    • 제10권3호
    • /
    • pp.185-189
    • /
    • 1999
  • Effects of alloy modification with the $Zr_{0.6}Ti_{0.4}V_{0.4}Ni_{1.2}Mn_{0.4}$ alloy for an electrode use have been investigated. For the alloy composition, a part of Mn was substituted by Co, Cr and Fe. The experimental results showed that Co accelerated activation of alloy, and Fe and Cr improved the discharge capacity. These results agree with P-C-T curves of each alloy. But substituting Fe for Mn showed the decrease of the discharge capacity when discharged at high rate (60mA, about 1C rate). Considering both the discharge capacity and the high rate discharge property, $Zr_{0.6}Ti_{0.4}V_{0.4}Ni_{1.2}Mn_{0.3}Cr_{0.1}$ alloy was found to be the best alloy among the alloys subjected to the test.

  • PDF

Quasi-Static and Dynamic Loading Responses of Ti-6Al-4V Titanium Alloy: Experiments and Constitutive Modeling

  • Suh, Yeong-Sung;Akhtar S. Khan
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2003년도 추계학술대회논문집
    • /
    • pp.191-194
    • /
    • 2003
  • The results from a systematic study of the response of a Ti-6Al-4V alloy under quasi-static and dynamic loading at different strain rates and temperatures are presented. It has been shown that the work-hardening rate decreased as the strain rate and the strain increased. The correlations and predictions using modified KHL (Khan-Huang-Liang) viscoplastic constitutive model are compared with those from JC (Johnson-Cook) model and experimental observations. Overall, KHL model correlations and predictions compared much more favorably than the corresponding JC model predictions and correlations.

  • PDF

열간 등가압 소결에 의한 Ti-6Al-4V 분말의 치밀화 거동 (Densification Behavior of Ti-6Al-4V Power Compacts by Hot Isostatic Pressing)

  • 양훈철;김기태
    • 대한기계학회논문집A
    • /
    • 제24권2호
    • /
    • pp.394-402
    • /
    • 2000
  • Densification behavior of titanium alloy powder was investigated under hot isostatic pressing at various pressures and temperatures. Uniaxial creep responses of a dense specimen were also obtained at high temperatures. The densification model of Abouaf and co-workers was implemented into a Finite element program (ABAQUS) to compare with experimental data for titanium alloy powder. The agreements between finite element calculations and experimental data for deformation and densification of titanium alloy powder were good during hot isostatic pressing.

차동식 NiTi-형상기억합금 액츄에이터의 동특성연구 (A study on Bidirectional NiTi-Shape Memory Alloy Actuator)

  • 정상화;김현욱;장우양;김경석;신현성;차경래;나윤철
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 2001년도 추계학술대회(한국공작기계학회)
    • /
    • pp.75-79
    • /
    • 2001
  • In the recent years, as the research and the development of micro and precision machinery become active, the interest of micro actuators using SMA(Shape Memory Alloy) has been increased. The dynamic characteristic analysis of SMA is necessary for actuator application and many common researches report the material characteristics of SMA sufficiently. However, the research on dynamic characteristics is very deficient. In this paper, the helical spring are fabricated with NiTi SMA wire of high resistivity, The force, response speed, temperature, and displacement are measured by digital force gauge, infrared thermometer, and laser displacement sensor so that the dynamic characteristics of this SMA is analyzed. Also, bidirectional actuator was fabricated and experimented for its performance.

  • PDF