• Title/Summary/Keyword: Ti-Al alloy

Search Result 647, Processing Time 0.026 seconds

A Study on the Deformation Induced Microstructure $L1_2$-ordered $Ni_3Al$ Containing Fine Precipitates (미세석출상을 포함하는 $L1_2$형 규칙 $Ni_3Al$의 변형조직에 관한 연구)

  • Han, Chang-Suk;Lee, Joon
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.21 no.5
    • /
    • pp.251-258
    • /
    • 2008
  • A transmission electron microscope investigation has been performed on the morphology of dislocations in deformed ${\gamma}^{\prime}-Ni_3(Al,Ti)$ alloys containing fine dispersion of disordered ${\gamma}$ particles. Superlattice dislocations dissociate into fourfold Shockley partial dislocations in a uniform supersaturated solid solution of the ${\gamma}^{\prime}$ phase. Dislocations are attracted into the disordered ${\gamma}$ phase and dissociate further in the particles. At any stage of aging, dislocations cut through the particles and the Orowan bypassing process does not occur even in the over-aged stage of this alloy system. The work necessary to pull the dislocation away from the disordered particles into the ordered matrix should mainly contribute to increase the strength of the ${\gamma}^{\prime}$ phase containing fine dispersion of the disordered ${\gamma}$ phase.

플라즈마 전해산화 공정에 있어서 전해액 내 실리콘 이온이 표면특성에 미치는 영향

  • Kim, Seong-Cheol;Yun, Sang-Hui;Seong, Gi-Hun;Gang, Du-Hong;Min, Gwan-Sik;Cha, Deok-Jun;Kim, Jin-Tae;Yun, Ju-Yeong
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.02a
    • /
    • pp.290-290
    • /
    • 2013
  • 플라즈마 전해산화(Plasma Electrolytic Oxidation)란 저 농도의 알칼리 전해액을 매개로, 고전압을 가해 미세 플라즈마 방전을 유도하여 Al, Mg, Ti 등의 금속표면을 산화시켜 고내식성, 초경합금 수준의 내마모성, 탁월한 절연성과 고경도성을 가지는 산화막을 형성시키는 기술로 전자, 자동차, 의료, 섬유, 해양, 석유화학 산업에 이르기까지 광범위한 분야에 적용되어 우수한 물성을 확보할 수 있는 차세대의 표면처리 기술이다. 본 연구에서는 6061 알루미늄 합금을 이용하여 다양한 전해액 조건에서 플라즈마 전해산화 공정으로 Al2O3 산화막을 형성시켰다. 산화막의 조성 및 미세구조는 XRD와 FE-SEM, EDS를 이용하여 분석하였다. 형성된 산화막은 회색에서 밝은 회색으로 시편 전면에 고르게 나타났다. 전해액 조성을 바꾸어줌에 따라 각기 다른 표면 특성을 가지는 산화막을 얻을 수 있었고, 그에 따른 물성 변화를 분석하였다. 특히 Si 이온 농도를 조절함으로써 피막 성장인자와 표면 미세구조를 제어할 수 있었다.

  • PDF

Hydrogen Evolution Ability of Selected Pure Metals and Galvanic Corrosion Behavior between the Metals and Magnesium

  • Luo, Zhen;Song, Kaili;Li, Guijuan;Yang, Lei
    • Journal of Electrochemical Science and Technology
    • /
    • v.11 no.4
    • /
    • pp.323-329
    • /
    • 2020
  • The cathodic hydrogen evolution ability of different pure metals and their long term galvanic corrosion behavior with pure Mg were investigated. The hydrogen evolution ability of pure Ti, Al, Sn and Zr is weak, while that of Fe, W, Cr, and Co is very strong. Initial polarization test could not completely reveal the cathodic behavior of the tested metals during long term corrosion. The cathodic hydrogen evolution ability may vary significantly in the long term galvanic tests for different metals, especially for Al whose cathodic current density reduced to 1/50 of the initial value. The anodic polarization shows that Al and Sn as alloying elements are supposed to provide relatively good passive effect for Mg alloy, while Ag can provide a slight passive effect and Zn has little passive effect.

Cavitation damage characteristics of plasma electrolytic oxidation coatings prepared on marine grade Al alloy (플라즈마 전해 산화 처리된 해양환경용 Al 합금의 캐비테이션 손상 특성)

  • Lee, Jeong-Hyeong;Kim, Yong-Hwan;Kim, Yeon-Ju;Kim, Seong-Jong
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2017.05a
    • /
    • pp.132.2-132.2
    • /
    • 2017
  • 플라즈마 전해 산화(Plasma Electrolytic Oxidation, PEO)는 Al, Ti, Mg 합금과 같은 경량 금속소재에 대한 표면처리기술로서 주목을 받고 있다. PEO 처리에 의해 표면에 치밀하게 형성되는 세라믹 산화층은 우수한 내식성, 내마모성을 보유하기 때문에, 이와 같은 특성이 요구되는 분야에 적용하기 위한 연구가 활발하다. 특히 PEO 세라믹 코팅층의 응착마모(adhesive wear)와 절삭마모(abrasive wear)에 관한 연구는 상당부분 이루어지고 있으나, 캐비테이션 침식과 같은 침식마모(erosive wear) 특성에 관한 연구는 부족한 실정이다. 본 연구에서는 알루미늄 합금 소지에 제작된 PEO 코팅층의 캐비테이션 손상 특성을 고찰하였으며, 전해액 조성이 PEO 코팅층의 미세조직과 캐비테이션 손상 특성에 미치는 영향을 살펴보았다. PEO 처리를 위해 사용된 소재는 상용 5083-O합금 판재로서 $2cm{\times}2cm$로 절단하여, 에머리페이퍼로 1000번까지 연마하여 사용하였다. 사용된 전해액은 증류수에 KOH(1 g/L)을 base로 하여 $Na_2SiO_3$(2 g/L)의 첨가유무를 변수로 하였다. 시편을 양극으로 하고 STS304를 음극으로 하여 각각 DC 전원 공급기의 +극과 -극에 연결하였으며, 정전류 조건에서 30분간 $0.1A/cm^2$의 전류밀도를 인가하였다. PEO 처리후 시편은 SEM, EDS, XRD를 이용하여 표면 특성 평가를 실시하였다. PEO코팅층의 캐비테이션 특성 평가는 초음파 진동식 캐비테이션 발생 장치를 이용하였으며, 캐비테이션 실험 후 시간에 따른 표면 거칠기의 변화 거동을 분석하였다.

  • PDF

플라즈마 전해산화 공정 중 전해액 내의 인산염 변화에 따른 알루미늄 합금 산화피막의 형성

  • Yun, Sang-Hui;Kim, Seong-Cheol;Seong, Gi-Hun;Gang, Du-Hong;Min, Gwan-Sik;Cha, Deok-Jun;Kim, Jin-Tae;Yun, Ju-Yeong
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.02a
    • /
    • pp.298-298
    • /
    • 2013
  • 플라즈마 전해산화기술은 알루미늄 소재에 대해 기존의 양극 산화막, 전해 경질크롬 도금 및 플라즈마 세라믹 용사기술 등에 의해 구현할 수 없는 고기능성을 부여하여 월등히 우수한 경도, 내부식, 내마모, 전기절연, 열저항, 피로강도 등을 얻을 수 있는 획기적인 기술이다. 또한 최근 환경에 대한 관심이 점차 높아지면서 친환경적 공정과정과 경금속 소재의 제품에 내구성을 향상시킬 필요성이 높아지고 있다. 이러한 요구에 부합하는 플라즈마 전해 산화기술은 알칼리 수용액 중에서 Al, Ti, Mg 등의 표면에 산화 피막을 형성시키는 기술로써 기존의 양극산화(Anodizing)을 대체 할 수 있다. 본 연구에서는 Al6061을 이용하여 플라즈마 전해산화 공정에 사용되는 전해액의 종류 및 농도, 시간의 변화에 따른 산화 피막의 변화를 내전압 측정 및 FE-SEM, EDS, XRD를 통해 분석하였다. 전해액에 sodium hexameta phosphate과 potassium phosphate를 이용하여 phosphate 종류의 변화에 따른 피막 특성의 변화를 연구하였다. 그로인해 phosphate의 종류 및 농도, 시간 변화를 이용하여 플라즈마 전해산화공정의 산화 피막 물성 제어를 할 수 있다.

  • PDF

THE BOND CHARACTERISTICS OF PORCELAIN FUSED BY TITANIUM SURFACE MODIFICATION (타이타늄의 표면개질에 따른 도재 결합 특성)

  • Choi, Taek-Huw;Park, Sang-Won;Vang, Mong-Sook;Yang, Hong-So;Park, Ha-Ok;Lim, Hyun-Pil;Oh, Gye-Jeong;Kim, Hyun-Seung;Lee, Kwang-Min;Lee, Kyung-Ku
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.45 no.2
    • /
    • pp.169-181
    • /
    • 2007
  • Statement of problem: Titanium is well known as a proper metal for the dental restorations, because it has an excellent biocompatibility, resistance to corrosion, and mechanical property. However, adhesion between titanium and dental porcelains is related to the diffusion of oxygen to the reaction layers formed on cast-titanium surfaces during porcelain firing and those oxidized layers make the adhesion difficult to be formed. Many studies using mechanical, chemical and physical methods to enhance the titanium-ceramic adhesion have been actively performed. Purpose: This study meant to comparatively analyse the adhesion characteristics depending on different titanium surface coatings after coating the casts and wrought titanium surfaces with Au and TiN. Material and method: In this study, the titanium specimens (CP-Ti, Grade 2, Kobe still Co. Japan) were categorized into cast and wrought titanium. The wrought titanium was cast by using the MgO-based investment(Selevest CB, Selec). The cast and wrought titanium were treated with Au coating($ParaOne^{(R)}$., Gold Ion Sputter, Model PS-1200) and TiN coating(ATEC system, Korea) and the ultra low fusing dental porcelain was fused and fired onto the samples. Biaxial flection test was done on the fired samples and the porcelain was separated. The adhesion characteristics of porcelain and titanium after firing and the specimen surfaces before and after the porcelain fracture test were observed with SEM. The atomic percent of Si on all sample surfaces was comparatively analysed by EDS. In addition, the constituents of specimen surface layers after the porcelain fracture and the formed compound were evaluated by X-ray diffraction diagnosis. Result: The results of this study were obtained as follows : 1. The surface characteristics of cast and wrought titanium after surface treatment(Au, TiN, $Al_2O_3$ sandblasting) were similar and each cast and wrought titanium showed similar bonding characteristics. 2. Before and after the biaxial flection test, the highest atomic weight change of Si component was found in $Al_2O_3$ sandblasted wrought titanium(28.6at.% $\rightarrow$ 8.3at.%). On the other hand, the least change was seen in Au-Pd-In alloy(24.5at.% $\rightarrow$ 9.1at.%). 3. Much amount of Si components was uniformly distributed in Au and TiN coated titanium, but less amount of Si's was unevenly dispersed on Al2O3 sandblasting surfaces. 4. In X-ray diffraction diagnosis after porcelain debonding, we could see $Au_2Ti$ compound and TiN coating layers on Au and TiN coated surfaces and $TiO_2$, typical oxide of titanium, on all titanium surfaces. 5. Debonding of porcelain on cast and wrought titanium surface after the biaxial flection is considered as a result of adhesion deterioration between coating layers and titanium surfaces. We found that there are both adhesive failure and cohesive failure at the same time. Conclusion: These results showed that the titanium-ceramic adhesion could be improved by coating cast and wrought titanium surfaces with Au and TiN when making porcelain fused to metal crowns. In order to use porcelain fused to titanium clinically, it is considered that coating technique to enhance the bonding strength between coating kKlayers and titanium surfaces should be developed first.

Effects of the Precipitation of Carbides and Nitrides on the Textures in Extra Low Carbon Steel Sheets containing B, Nb and Ti(l) (B,Nb 및 Ti 를 함유한 극저탄소강에서 탄화물 및 질화물의 석출이 집합조직에 미치는 영향(I)-집합조직과 기계적 성질-)

  • Lee, Jong-Mu;Yoon, Kuk-Hoon;Lee, Do-Hyeong
    • Korean Journal of Materials Research
    • /
    • v.3 no.1
    • /
    • pp.43-49
    • /
    • 1993
  • Excellent deep drawability and strain aging rsistance are obtained by the addition of alloying elements such as Ti and Nb which can form carbide and nitride easily into Al killed extra low carbon steel. Recrystallization textures and mechanical properties of the three different extra low carbon steels with B containing Nb only, Ti only, and both Nb and Ti, respectively, along with have been compared. Inverse pole figure shows that (100) and (111) texture intensities of Nb containing steel changed a lot during the annealing treatment and the degree of texture-structural change in the steel containing both Nb and Ti is about the same as that in the Ti-containing 5teel. After annealing the pole figure shows that the {Ill} < 110 > and {112} < 110> textures are the strongest in the cold rolled state and the annealed state, respectively. However, there is little difference in texture structure among the three kinds of steels. There is a tendency that the steel containing both Nb and Ti the grain size of which is the smallest is the highest in hardness. Nb-containing steel is the next and Ti -containing steel is the last in hardness.

  • PDF

Improvement of the Quality of Cryogenic Machining by Stabilization of Liquid Nitrogen Jet Pressure (액체질소 분사 안정화를 통한 극저온가공 품질 향상)

  • Gang, Myeong Gu;Min, Byung-Kwon;Kim, Tae-Gon;Lee, Seok-Woo
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.34 no.4
    • /
    • pp.247-251
    • /
    • 2017
  • Titanium alloy has been widely used in the aerospace industry because of its high strength and good corrosion resistance. During cutting, the low thermal conductivity and high chemical reactivity of titanium generate a high cutting temperature and accelerates tool wear. To improve cutting tool life, cryogenic machining by using a liquid nitrogen (LN2) jet is suggested. In cryogenic jet cooling, evaporation of LN2 in the tank and transfer tube could cause pressure fluctuation and change the cooling rate. In this work, cooling uniformity is investigated in terms of liquid nitrogen jet pressure in cryogenic jet cooling during titanium alloy turning. Fluctuation of jet spraying pressure causes tool temperature to fluctuate. It is possible to suppress the fluctuation of the jet pressure and improve cooling by using a phase separator. Measuring tool temperature shows that consistent LN2 jet pressure improves cryogenic cooling uniformity.

Springback FE modeling of titanium alloy tubes bending using various hardening models

  • Shahabi, Mehdi;Nayebi, Ali
    • Structural Engineering and Mechanics
    • /
    • v.56 no.3
    • /
    • pp.369-383
    • /
    • 2015
  • In this study, effect of various material hardening models based on Holloman's isotropic, Ziegler's linear kinematic, non-linear kinematic and mixture of the isotropic and nonlinear kinematic hardening laws on springback prediction of titanium alloy (Ti-3Al-2.5V) in a tube rotary draw bending (RDB) process was investigated with presenting the keynotes for a comprehensive step by step ABAQUS simulation. Influence of mandrel on quality of the final product including springback, wall-thinning and cross-section deformation of the tube was investigated, too. Material parameters of the hardening models were obtained based on information of a uniaxial test. In particular, in the case of combined iso-nonlinear kinematic hardening the material constants were calibrated by a simple approach based on half-cycle data instead of several stabilized cycles ones. Moreover, effect of some material and geometrical parameters on springback was carried out. The results showed that using the various hardening laws separately cannot describe the material hardening behavior correctly. Therefore, it is concluded that combining the hardening laws is a good idea to have accurate springback prediction. Totally the results are useful for predicting and controlling springback and cross-section deformation in metal forming processes.

Single Walled Carbon Nanotubes-Reinforced Metal Matrix Composite Materials Fabricated by Spark Plasma Sintering (방전플라즈마 소결공정으로 제조된 단일벽탄소나노튜브 강화 금속기지 복합재료)

  • Kwon, Hansang
    • Journal of Power System Engineering
    • /
    • v.21 no.4
    • /
    • pp.94-99
    • /
    • 2017
  • Single walled carbon nanotubes were mixed with various metal powders by mechanical ball milling and sintered by spark plasma sintering processes. Two compositional (0.1 and 1 vol%) of the single walled carbon nanotubes were dispersed onto the pure aluminum, 5052 aluminum alloy, pure titanium, Ti6Al4Vanadium alloy, pure copper, and stainless steel 316L. Each composite powders were spark plasma sintered at $600^{\circ}C$ and well synthesized regardless of the matrices. Vickers hardness of the composite materials was measured and they exhibited higher values regardless of the carbon nanotubes composition than those of the pure materials. Moreover, single walled carbon nanotubes reinforced copper matrix composites showed highest enhancement between the other metal matrices system. We believe that low energy mechanical ball milling and spark plasma sintering processes are useful tool for fabricating of the carbon nanotubes-reinforced various metal matrices composite materials. The single walled carbon nanotubes-reinforced various metal matrices composite materials could be used as an engineering parts in many kind of industrial fields such as aviation, transportation and electro technologies etc. However, detail strengthening mechanism should be carefully investigated.