  • Nanotubular structure formation on the Ti-6Al-4V and Ti-Ta alloy surfaces by electrochemical methods has been studied using the anodizing method. A nanotube layer was formed on Ti alloys in 1.0 M $H_3PO_4$ electrolyte with small additions of $F^-$ ions. The nanotube nucleation and growth of the ${\alpha}$-phase and ${\beta}$-phase appeared differently, and showed different morphology for Cp-Ti, Ti-6Al-4V and Ti-Ta alloys. In the ${\alpha}$-phase of Cp-Ti and martensite ${\alpha}^{\prime}$ and in the ${\alpha}^{{\prime}{\prime}}$ and ${\beta}$-phase of the Ti-Ta alloy, the nanotube showed a clearly highly ordered $TiO_2$ layer. In the case of the Ti-Ta alloy, the pore size of the nanotube was smaller than that of the Cp-Ti due to the ${\beta}$-stabilizing Ta element. In the case of the Ti-6Al-4V alloy, the ${\alpha}$-phase showed a stable porous structure; the ${\beta}$-phase was dissolved entirely. The nanotube with two-size scale and high order showed itself on Ti-Ta alloys with increasing Ta content.

Ti-6Al-4V 합금의 고온성형시 미세조직 예측에 관한 연구 (Prediction of Microstructure During High Temperature Forming of Ti-6Al-4V Alloy)

  • 이유환;신태진;황상무;박노광;심인옥;이종수
    • 소성∙가공
    • /
    • 제12권4호
    • /
    • pp.290-295
    • /
    • 2003
  • High temperature deformation behavior and prediction of final microstructure after forming of Ti-6Al-4V alloy were investigated in this study. Equiaxed and Widmanstatten microstructures of Ti-6Al-4V alloys were prepared as initial microstructures and compression tests were performed to obtain the flow curves at high temperatures (700∼110$0^{\circ}C$) and various strain rates (10$^{-4}$ ∼10$^2$/s). From the results of compression test, strain rate sensitivity (m) and activation energy (Q) were calculated and used to establish constitutive equation. To predict the final microstructure after farming, finite element analysis was performed considering the microstructural parameters such as grain size and volume fraction of second phase.

CaO 도가니에 의한 Ti-6Al-4V 합금의 용해와 주조결함 (Melting of Ti-6Al-4V Alloy Using CaO Crucible and Internal Defects of its Casting)

  • 세이주우치다;킨야카나타;나오히로타나카;오사무야나기사와
    • 한국주조공학회지
    • /
    • 제24권6호
    • /
    • pp.314-322
    • /
    • 2004
  • The CaO crucible is expected to serve as a useful tool for melting Ti and its alloys due to its thermodynamic stability. However, tjere still remain problems that need to be resolved in the melting of Ti and its alloys to enable commerical use. The cause of the defects of Ti-6AI-4V alloy castings melted in the CaO crucible were examined and compared with induction skull melting. The key factors of the melting technique using the CaO crucible, affecting the quality of Ti-6AI-4V alloy castings, were investigated. Defects of the Ti-6AI-4V alloy castings are caused by the chemical reduction of CaO by Ti. Pressurizing with argon gas in a vacuum induction chamber is effective for reducing the defects. Preheating of the charged material in the crucible and quick pouring into a mold of lower temperature, just after melting down, are important for produsing sound Ti-6AI-4V castings.

Ti-6Al-4V 합금의 고온성형 시 미세조직 예측에 관한 연구 (Prediction of microstructure during high temperature forming of Ti-6Al-4V alloy)

  • 이유환;신태진;황상무;이종수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2003년도 춘계학술대회논문집
    • /
    • pp.57-60
    • /
    • 2003
  • The purpose of this study is to investigate the high temperature deformation behavior of Ti-6Al-4V alloy and to predict the final microstructure under given forming conditions. Equiaxed and widmanstatten of Ti-6Al-4V alloys were prepared as initial microstructure and the compression tests were performed to obtain the flow curves at high temperatures (700∼1100$^{\circ}C$) and various strain rates (10$\^$-4/∼10$^2$/s). Form the results of compression test various parameters such as strain rate sensitivity (m) and activation energy (Q) were calculated and used to establish constitutive equations. To predict the final microstructure after forming, finite element analysis was performed considering the microstructural parameters such as the grain size and the volume fraction of second phase.

  • PDF

Blended Elemental P/M Synthesis of Titanium Alloys and Titanium Alloy-based Particulate Composites

  • Hagiwara, Masuo;Emura, Satoshi
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1030-1031
    • /
    • 2006
  • Titanium alloys and Titanium alloy-based particulate composites were synthesized using the blended elemental P/M route. First, processing conditions such as the fabrication of master alloy powder were investigated. Ti-6Al-4V, Ti-5Al-2.5Fe, Ti-6Al-2Sn-4Zr-2Mo, IMI685, IMI829, Timetal 1100 and Timetal 62S, and Ti-6Al-2Sn-4Zr-2Mo/ 10%TiB and Timetal 62S/10%TiB were then synthesized using the optimal processing conditions obtained. The microstructures and mechanical properties such as tensile strength and high cycle fatigue strength were evaluated.

  • PDF

생체용 타이타늄 합금의 산화거동 및 세포독성에 관한 연구 (A Study on Oxidation Behavior and Cytotoxicity Test of Ti-10Ta-10Nb Alloy)

  • 조홍규;이도재;이광민;이경구
    • 대한치과기공학회지
    • /
    • 제26권1호
    • /
    • pp.97-104
    • /
    • 2004
  • A new Ti-10Ta-10Nb alloy has designed and examined some possibility of forming more passive oxide film by oxidation treatment which is closely related to corrosion resistance and biocompatibility. Ti-6Al-4V and Ti-10Ta-10Nb alloys were prepared by consumable vacuum arc melting and homogenized at 1050$^{\circ}C$ for 24hours. Alloy specimens were oxidized at the temperature range of 400 to 750$^{\circ}C$ for 30minutes, and the oxide films on Ti alloys were analysed by optical microscope, SEM, XPS and TGA. Cytotoxicity test was performed in MTT assay treated L929 fibroblast cell culture by indirect method. It is found out that the oxide film on Ti-10Ta-10Nb alloy is denser and thinner compared to Ti-6Al-4V alloy. The weight gain during the oxidation was increased rapidly at the temperature above 650$^{\circ}C$ for Ti-6Al-4V alloy and above 700$^{\circ}C$ for Ti-10Ta-10Nb alloy respectively. It was analysed that the passive film of the Ti alloys consisted of TiO2 through X-ray photoelectron spectroscopy (XPS) analysis. It is found out by cytotoxicity test that moderate oxidation treatment lowers cell toxicity, and Ti-10Ta-10Nb alloy showed better result compared to Ti-6Al-4V alloy.

  • PDF

Ti-6Al-4V 합금에 2nd ATO 처리 후 플라즈마 전해 산화법에 의한 생체활성표면형성 (Formation of Bioactive Surface by PEO-treatment after 2nd ATO Technique of Ti-6Al-4V Alloy)

  • Lim, Sang-Gyu;Cho, Han-Cheol
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2018년도 춘계학술대회 논문집
    • /
    • pp.74-74
    • /
    • 2018
  • Ti-6Al-4V alloys have been widely used as orthopedic materials because of their excellent corrosion resistance and mechanical properties. However, it does not bind directly to the bone, so it requires a surface modification. This problem can be solved by nanotube and micropore formation. Plasma electrolytic oxidation (PEO) treatment for micropore, which combines high-voltage spark and electrochemical oxidation, is a new way of forming a ceramic coating on light metals such as titanium and its alloys. This method has excellent reproducibility and can easily control the shape and size of the Ti alloy. In this study, formation of bioactive surface by PEO-treatment after $2^{nd}$ ATO technique of Ti-6Al-4V alloy was invesgated by various instrument. Nanotube oxide surface structure was formed on the surface by anodic oxidation treatment in 0.8 wt.% NaF and 1M $H_3PO_4$ electrolytes. After nanotube formation, nanotube layer was removed by ultrasonic cleaning. PEO-treatment was carried out at 280V for 3 minutes in the electrolytic solution containing the bioactive substance (Mg, Zn, Mn, Sr, and Si). The surface of Ti-6Al-4V alloy was observed by field emission scanning electron microscopy (FE-SEM, S-4800 Hitachi, Japan). An energy dispersive X-ray spectrometer (EDS, Inca program, Oxford, UK) was used to analyze the spectra of physiologically active Si, Mn, Mg, Zn, and Sr ions. The PEO film formed on the Ti-6Al-4V alloy surface was characterized using an X-ray diffractometer (TF-XRD, X'pert Philips, Netherlands). It is confirmed that bioactive ions play an essential role in the normal bone growth and metabolism of the human skeletal tissues.

  • PDF

열산화 처리된 Ti-Ag 합금의 세포적합성 (CYTOCOMPATIBILITY OF THERMALLY OXIDIZED TI-AG ALLOYS)

  • 김호중;오근택;이지환;김경남;한동후
    • 대한치과보철학회지
    • /
    • 제42권4호
    • /
    • pp.333-343
    • /
    • 2004
  • Statement of problem: In its preceding work, change in surface characteristics were investigated in consideration that both microtopograpy and macroscopic configuration of implants surface are two of the most important factors, in that they can construct agreeable environment by raising surface energy, to affect osseointegration and biocompatibility explained by cell proliferation. Purpose: This study focused on examining cytocompatibility of dental implants materials Ti-Ag alloys, of which mechanical and electrochemical superiority to cp-Ti or Ti6Al4V were verified, in comparison with that of cp-Ti, and Ti6Al4V. Materials and methods: In this regard, MTT tests for L-929, the fibroblast connective tissues and cell proliferation tests for osteoprogenitor cells, MC3T3-E1 were performed on cp-Ti, Ti6Al4V, and Ti-Ag alloys following thermal oxidation according to appropriate heat treatment temperature(untreated, 400, 600, $800^{\circ}C$) and heat treatment duration(untreated, 0.5, 1, 4 hr). Results: The MTT tests on fibroblasts L-929 resulted in cell viability of over 90% in all experimental group entities, where, especially, the 100% of the viability for Ti-Ag alloys specimens accounted for the slightest adverse effect of ions release from those alloys on the cell. In MC3T3-E1 proliferation tests, the population of cells in the experimental group was roughly increased as experimentation proceeded, after two to four days. Proliferation showed highest viability for most of specimens, including Ti2.0Ag, treated at $600^{\circ}C$. Conclusion: In conclusion, it is the heat treatment temperature, not the duration that has considerable effects on thermal oxidation of specimens. Ti-Ag alloys treated at $600^{\circ}C$ proved to have the best surface morphology as well as cytocompatibility when compared with Ti or Ti6Al4V for short-term biocompatibility tests.

알루미나이드 코팅된 티타늄 합금의 동적산화거동 (Dynamic Oxidation Behaviors of Aluminide Coated Titanium Alloys)

  • 손영일;박진수;박준식
    • 한국추진공학회지
    • /
    • 제19권5호
    • /
    • pp.84-90
    • /
    • 2015
  • 티타늄 합금은 고온 추진체의 부품에 사용될 경우, 고온의 화염에서 순간적으로 노출될 수 있음으로, 고온의 화염하에서의 내산화특성을 평가할 필요가 있다. 본 연구에서는 Ti64 합금 (Ti-6%Al-4%V) 및 코팅된 Ti64 합금을 고온화염하에서 산화손상 및 내산화 특성을 평가하고자 하였다. Ti64 합금의 코팅은 알루미늄 확산코팅법을 사용하여 코팅을 수행하였다. 표면에 알루미나이드층이 코팅되지 않은 Ti64 합금은 고온의 화염 노출시에 표면 박리현상이 발생하였으나, 코팅된 시험편은 표면박리현상이 나타나지 않았고 알루미나이드 층의 산화물 생성으로 인하여 표면이 보호됨을 관찰할 수 있었다. 화염노출시 코팅층의 역할을 고찰하기 위하여 코팅층을 분석하였으며, 조직의 변화를 고찰하고 논의하였다.

치과주조용 Ti-20%Zr-X%Cr(X=0,5)계 합금의 기계적 성질 (Mechanical Properties of Ti-20%Zr-X%Cr(X=0,5) Based Alloys for Dental Casting)

  • 정종현
    • 대한치과기공학회지
    • /
    • 제25권1호
    • /
    • pp.81-87
    • /
    • 2003
  • Ti-20%Zr-X%Cr(X=0,5) based alloys not containing hamful Al and V were newly designed in order to reveal their possibility for dental casting alloys, and melted in argon-arc casting machine. The mechanical properties were evaluated by using universal testing machine. The tensile strength and %elongaton of the alloys markedly increased with Cr content. The Ti-20%Zr-5%Cr alloy showed a similar tendency with Ti-6%Al-4%V alloy in tensile strength, but surpassed in %elongation. From these results, it was concluded that new alloys for successful dental casting materials should be designed as Ti-Zr-Cr based alloys.