• 제목/요약/키워드: Three point bend test specimens

검색결과 21건 처리시간 0.025초

동적 파괴에 대한 가속장치의 보정 및 시험장치 설계 (Calibration of Acceleration Plant and Test Rig Design to Dynamic Fracture)

  • 조재웅;한문식
    • 한국공작기계학회논문집
    • /
    • 제17권3호
    • /
    • pp.47-52
    • /
    • 2008
  • The force transducer in the acceleration plant due to dynamic fracture is calibrated by dynamically using the stress pulses from a longitudinal bar. The bar is supported by two strings attached to the ceiling. The bar velocities before and after impact are measured and a full bridge at bar and transducer is formed by the four strain gauges. A transient recorder is used to store the stress pulse signals of force transducer and bar. For the first test series, three point bend test specimens can be chosen by means of test rig design and the inspection as sample experiment in this presented paper is sufficient for proving with the numerical simulation of the specimen model.

생체주입용 Ni-Ti 합금의 시효특성(I) (Characteristics of Aging of Ni-Ti Alloy Used for Implant Fabrications(I))

  • 조형준;이준희;박기룡
    • 대한의용생체공학회:의공학회지
    • /
    • 제10권3호
    • /
    • pp.261-268
    • /
    • 1989
  • The characteristics of aging of near-equiatomic Ni-Ti alloy has been studied by the three point bend test and the measurement of Differential Scanning Calorimetry(DSC). The DSC is used to measure precise transformation temperatures and the amount of thermal energy required for the corresponding phase transformation. The effort of hardness on aging treatment in saline solution of $37^{\circ}C$ was higher for the annealed than solution treated specimens. As the testing temperature inc- rease from under $M_f$ to above $A_f$ temperature, the elastic stiffness increased. Almost full recovery can be achieved after bending below Belo outer fiber strain. Total bend recovery decreased gradually as aging time and bend angle is increased.

  • PDF

Determination of Double-K Fracture Parameters of Concrete Using Split-Tension Cube: A Revised Procedure

  • Pandey, Shashi Ranjan;Kumar, Shailendra;Srivastava, A.K.L.
    • International Journal of Concrete Structures and Materials
    • /
    • 제10권2호
    • /
    • pp.163-175
    • /
    • 2016
  • This paper presents a revised procedure for computation of double-K fracture parameters of concrete split-tension cube specimen using weight function of the centrally cracked plate of finite strip with a finite width. This is an improvement over the previous work of the authors in which the determination of double-K fracture parameters of concrete for split-tension cube test using weight function of the centrally cracked plate of infinite strip with a finite width was presented. In a recent research, it was pointed out that there are great differences between a finite strip and an infinite strip regarding their weight function and the solution of infinite strip can be utilized in the split-tension specimens when the notch size is very small. In the present work, improved version of LEFM formulas for stress intensity factor, crack mouth opening displacement and crack opening displacement profile presented in the recent research work are incorporated. The results of the double-K fracture parameters obtained using revised procedure and the previous work of the authors is compared. The double-K fracture parameters of split-tension cube specimen are also compared with those obtained for standard three point bend test specimen. The input data required for determining double-K fracture parameters for both the specimen geometries for laboratory size specimens are obtained using well known version of the Fictitious Crack Model.

금속/세라믹 계면 물성 분석 (Metal/ceramic Interface Mechanical Property Analysis)

  • 김송희;강형석
    • 산업기술연구
    • /
    • 제24권A호
    • /
    • pp.9-15
    • /
    • 2004
  • The flexural strength from 3-point bend test and fatigue properties were measured to evaluate mechanical properties of metal/ceramic interface of the multilayer ceramic package produced through tape casting. From the results, the specimens with three electrode layers showed the highest strength. The temperature distribution with time during thermal cycle and thermal stresses with the change of electrode's shape have been estimated by mathematical modelling. Specimen affected by thermal shock, produced microcracks by the difference of thermal expansion coefficient. The results of tensile test and fatigue test showed the rupture at pin. The fact that the pin brazed specimens were always fractured at the pin proved the good bonding condition between pin and electrode.

  • PDF

Cocure/Precure 경화공정에 의해 제조된 Carbon/Epoxy 복합재료의 미시적 파손거동에 대한 AE 특성 (AE Characteristics on Microscopic Failure Behavior of Carbon/Epoxy Comosite Prepared by Cocure and Precure Process)

  • 이진경;이준현;이민래;최흥섭
    • 대한기계학회논문집A
    • /
    • 제24권10호
    • /
    • pp.2520-2528
    • /
    • 2000
  • Mechanical and physical properties of composite materials make a great difference due to their cure process condition. In order to clarify the effect of cure process condition on the microscopic damage behavior and failure mechanism of Carbon/Epoxy composites, three point bend test has been performed. For this purpose, two kinds of specimens with single adhesive and multiple adhesive layers were prepared. For single adhesive layer, four different types of specimen were used, that is, non-sanding, sanding, cocured, laminated specimens. Three different types of specimen were also used for the multiple adhesive layer, non-sanding, sanding, cocured specimens. Acoustic emission technique has also been employed to monitor the damage progresses associated with each micro-failure mechanism. The characteristics of AE parameters associated with micro-failure mechanism of each specimen were discussed.

Alloy Wheel용 저압 주조 A356-T6 합금의 기계적 특성 (Mechanical Properties of Low-Pressure Die Cast A356-T6 alloys for Automotive Wheels)

  • 유봉준;김정호;윤형석;어순철
    • 한국주조공학회지
    • /
    • 제34권1호
    • /
    • pp.6-13
    • /
    • 2014
  • The mechanical properties of low-pressure die cast (LPDC) A356-T6 automotive road wheels are evaluated and correlated with their corresponding microstructures. In this study, two types of alloy wheels processed using different LPDC gating system are investigated. The yield stress, tensile stress, and elongation values tested at room temperature are correlated with the secondary dendrite arm spacing (SDAS) with respect to the gating system, and are also compared with similar studies. The SDAS and precipitates are examined using optical microscopy, scanning electron microscopy (SEM) and energy-dispersive spectroscopy. The phase information is also investigated using X-ray diffraction. Charpy impact tests are also performed from $-100^{\circ}C$ to $200^{\circ}C$, and the fracture surfaces are examined using SEM. The impact energy is demonstrated to increase with increasing temperatures without exhibiting specific transition behaviors as in other nonferrous alloys. The fracture toughness is also evaluated using three point bend test with single-edged bend specimens. The obtained fracture toughness values are in good agreement with those in similar studies.

Glass ionomer cement 표면의 산부식 효과에 관한 연구 (THE EFFECT OF ACID ETCHING ON GLASS IONOMER CEMENT SURFACES)

  • 한승원;박상진;민병순;최호영;최기운
    • Restorative Dentistry and Endodontics
    • /
    • 제18권1호
    • /
    • pp.1-26
    • /
    • 1993
  • The purpose of this study was to investigate the effect of acid etching on the surface appearance and fracture toughness of five glass ionomer cements. Five kinds of commercially available glass ionomer cements including chemical curing filling type, chemical curing lining type, chemical curing metal reinforced type, light curing tilling type and light curing lining type were used for this study. The specimens for SEM study were fabricated by treating each glass ionomer cement with either visible light curing or self curing after being inserted into a rubber mold (diameter 4mm, depth 1mm). Some of the specimens were etched with 37% phosphoric acid for 0, 15, 30, 60, go seconds, at 5 minutes, 1 hour and 1 day after mixing of powder and liquid. Unetched ones comprised the control group and the others were the experimental groups. The surface texture was examined by using scanning electron microscope at 20 kV. (S-2300, Hitachi Co., Japan). The specimens for fracture toughness were fabricated by curing of each glass ionomer cement previously inserted into a metal mold for the single edge notch specimen according to the ASTME399. They were subjected to a three-point bend test after etching for 0, 30, 60, and 90 seconds at 5 minutes-, 1 hour-and 1 day-lapse after the fabrication of the specimens. The plane strain fracture toughness ($K_{IC}$) was determined by three-point bend test which was conducted with cross-head speed of 0.5 mm/min using Instron universal testing machine (Model No. 1122) following seven days storage of the etched specimens under $37^{\circ}C$, 100% humidity condition. Following conclusions were drawn. 1. In unetched control group, crack was present, but the surface was generally smooth. 2. Deterioration of the surface appearance such as serious dissolving of gel matrix and loss of glass particles occured as the etching time was increased beyond 15 s following Immediate etching of chemical curing type of glass ionomer cements. 3. Etching after 1 h, and 1 d reduced surface damage, 15 s, and 30s etch gave rough surface appearance without loss of glass particle of chemical curing type of glass ionomer cements. 4. Light curing type glass ionomer cement was etched by acid, but there was no difference in surface appearances according to various waiting periods. 5. It was found that the value of plane stram fracture toughness of glass ionomer cements was highest in the light curing filling type as $1.79\;MNm^{-1.5}$ followed by the light curing lining type, chemical curing metal reinforced type, chemical curing filling type and chemical curing lining type. 6. The value of plane stram fracture toughness of the chemical curing lining type glass ionomer cement etched after 5 minutes was lower than those of the cement etched after 1 hour or day or unetched (P < 0.05). 7. Light curing glass ionomer cement showed Irregular fractured surface and chemical curing cement showed smooth fractured surface.

  • PDF

콘크리트 삼점 휨시험편의 성장하는 균열에 대한 저항곡선 (Resistance Curves of Propagating Cracks for Concrete Three-Point Bend Specimens)

  • 연정흠
    • 콘크리트학회논문집
    • /
    • 제13권6호
    • /
    • pp.568-574
    • /
    • 2001
  • 콘크리트 시험편에 대한 삼점휨실험을 실시하여 여러 실험에 대해 측정된 반응의 평균값을 계산하곤 계산된 평균거동으로부터 삼점휨 시험편이 완전히 파손될 때까지 연속적으로 성장하는 균열에 대한 파괴거동이 분석되었다. 이 연구에서 사용된 실험변수는 25.4mm와 6.4mm의 초기균열길이 그리고 2000sec와 20sec의 실험기간이며, 초기균열길이는 파괴진행대(FPZ) 크기의 영향과 시험편의 기하학적 특성 및 경계조건에 대한 영향을 분석하기 위한 것이다. 실험기간은 초기 크리프(creep)의 영향을 위해 설정되었으나, 이 연구의 하중점-변위 속도에서는 심각한 영향이 관측되지 않았다. 여러 실험의 평균 외부일로부터 평균하중이 계산되었으며, 변형률 게이지를 사용하여 평균 균열길이를 측정하였다. 최대하중 이전의 저항곡선은 파괴진행대의 크기에 대해 유사한 값을 보였다. 그러나 최대하중 직후에는 초기균열의 크기에 관계없이 0.088~0.154mm의 하중점-변위에서 88mm의 불안정 균열성장이 발생되었으며, 평균 파괴에너지율 $G_{F}$$^{ave}$ = 115N/m은 이 불안정 균열성장 동안에 발생되었다. 균열길이 111mm에서 완전한 파괴진행대가 형성되었고, 25.4mm와 6.4mm의 초기균열길이에 대해 파괴진행대의 크기는 각각 86mm와 105mm이었다. 완전한 파괴진행대의 형성이후 저항곡선의 평균 파괴에너지율은 25.4mm와 6.4mm의 초기균열길이에 대해 각각 229N/m로 284N/m로 $G_{F}$$^{ave}$의 두 배 이상이었다.이었다.이었다.

음향방출 기법을 이용한 탄소섬유시트강화 콘크리트의 미시적 손상 거동에 관한 연구 (A Study on Microscopic Damage Behavior of Carbon Fiber Sheet Reinforced Concrete using Acoustic Emission Technique)

  • 이진경;이준현;정성륜
    • Composites Research
    • /
    • 제12권4호
    • /
    • pp.62-70
    • /
    • 1999
  • 건축 구조물의 재령이 증가함에 따른 손상은 구조물의 안전성 및 신뢰성 확보에 매우 심각한 문제이다. 최근에는 이렇게 손상을 입은 콘크리트 구조물의 보수 보강을 위해 탄소섬유시트가 광범위하게 사용되고 있지만 탄소섬유시트를 보강한 콘크리트의 파괴기구가 명확하게 규명되지 않았다. 따라서 본 연구에서는 탄소섬유시트를 보강한 콘크리트의 손상거동 및 미시적 파손기구를 이해하기 위해 4가지 경우의 시험편, 즉 순수한 콘크리트, 철근 보강 콘크리트, 탄소섬유시트 보강 콘크리트, 철근과 탄소섬유시트 보강 콘크리트 시험편에 대하여 3점 굽힘 시험을 실시하였다. 이러한 시험편들의 파손기구를 명확히 하기 위해 음향방출기법이 사용되었으며 균열 발생, 성장을 모니터링하기 위해 2차원 AE 발생원 위치추정 기법이 적용되었다.

  • PDF

피라미드 트러스형 금속 샌드위치 판재의 적외선 브레이징을 이용한 효율적 적층식 제작 및 특성에 관한 연구 (Efficient Layered Manufacturing Method of Metallic Sandwich Panel with Pyramidal Truss Structures using Infrared Brazing and its Mechanical Characteristics)

  • 이세희;성대용;양동열
    • 한국정밀공학회지
    • /
    • 제27권8호
    • /
    • pp.76-83
    • /
    • 2010
  • Metallic sandwich panels with pyramidal truss structures are high-stiffness and high-strength materials with low weight. In particular, bulk structures have enough space for additional multi-functionalities. In this work, in order to fabricate 3-D structures efficiently, Layered Manufacturing Method (LMM) which was composed of three steps, including crimping process, stacking process and bonding process using rapid infrared brazing, was proposed. The joining time was drastically reduced by employing infrared brazing of which heating rate and cooling rate were faster than those of conventional furnace brazing. By controlling the initial cooling rate slowly, the bonding strength was improved up to the level of strength by conventional vacuum brazing. The observation of infrared brazed specimens by optical microscope and SEM showed no defect on the joining sections. The experiments of 1-layered pyramidal structures and 2-layered pyramidal structures subject to 3-point bending were conducted to determine structural advantages of multilayered structures. From the results, the multi-layered structure has superior mechanical properties to the single-layered structure.