• Title/Summary/Keyword: Thermal hysteresis

Search Result 192, Processing Time 0.024 seconds

Design of the Wire Rope Type Snubber for Earthquake and Vibration of Piping System (Wire Rope형 배관 지진$\cdot$진동완충기의 설계)

  • 김영중
    • Proceedings of the Earthquake Engineering Society of Korea Conference
    • /
    • 1998.10a
    • /
    • pp.173-179
    • /
    • 1998
  • The piping system of a power plant suffers not only thermal expansion according to the temperature variation, but also many kinds of load: steady state vibrations due to the equipment operation or fluid flow, and transient vibrations due to the earthquake or explosion, etc. The snubbers are usually installed on the piping system to allow thermal expansion, and to reduce dynamic responses. Most snubbers are kinds of hydraulic and mechanical type, which can be degraded by leakage and abrasion, and required much cost for maintenance and replacement. Recently the wire rope type snubbers are developed and applied to the power plant, and proved as effective to reduce piping system vibration. Wire rope type snubber uses the bending rigidity and energy dissipation properties of ropes. This paper presents the procedure of design, and the method to apply hysteresis curve to the dynamic response analysis. Experiments were also conducted to confirm design results.

  • PDF

초정밀 선형 모터의 열.진동 분석

  • 임경화;이우영;설진수;김현철
    • Proceedings of the Korean Society Of Semiconductor Equipment Technology
    • /
    • 2004.05a
    • /
    • pp.163-168
    • /
    • 2004
  • Linear motor can directly apply to the system needed linear mot ions without rotary mot ions. To control a high-speed and high-resolution, the development of the linear motors is recently required in the high-integrated and speed process industry. This paper presents vibration analyses as well as measurement standards of the newly developed linear motors through analyzing the vibration characteristics and thermal behaviors of the advanced products. Vibration experiments are conducted for identifying the hysteresis and vibration level during operation. They are also included in the modal test to analyze the vibration. Analytic data using Finite Element Method (FEM) are compared with the results of the modal. Loss of temperature generated the linear motor leads to a serious deformation within its parts. The thermal behaviors are very important factor in linear motor. The FEM and experiments make it possible to understand these characteristics.

  • PDF

A Study on the Shape Memory Characteristic Behaviors of Ti-42.5at%Ni-10at.% Cu Alloys (Ti-42.5at.%Ni-10at.%Cu합금의 형상기억특성에 관한 연구)

  • Woo, Heung-Sik;Park, Yong-Gyu
    • Journal of the Korean Society of Safety
    • /
    • v.24 no.1
    • /
    • pp.26-30
    • /
    • 2009
  • Shape memory recoverable stress and strain of Ti-42.5at%Ni-10at%Cu alloys were measured by means of constant temperature tensile tests. The alloys' transformation behavior is B2 - B19 by DSC result. The strain by tensile stress were perfectly recovered by heating at any testing conditions but shape memory recoverable stress increased to 66MPa and then slightly decreased. Transformation temperatures from thermal cycling under constant uniaxial applied tensile loads linearly increased by increasing tensile load and their thermal hysteresis are about 110K and their maximum recoverable strain is 6.5% at 100MPa condition.

Fabrication of PZT ferroelectric thin films by rapid thermal annealing (급속 열처리에 의한 PZT 강유전 박막의 제작)

  • Paik, Dong-Soo;Kim, Hyun-Gwon;Choi, Hyung-Wook;Kim, Jun-Han;Park, Chang-Yub;Shin, Hyun-Yong
    • Proceedings of the KIEE Conference
    • /
    • 1993.07b
    • /
    • pp.1106-1109
    • /
    • 1993
  • Ferroelectric thin films of PZT with differnt Zr/Ti ratio were prepared by sol-gel processing and annealed by rapid-thermal-annealing at $500^{\circ}C-700^{\circ}C$ for 10sec-1min. The structure of the annealed films were examined by X-ray diffraction and SEM. Maximum remnant polarization of 10.24 ${\mu}m/cm^2$ and coercive field of 70 KV/cm were obtained from hysteresis curve or the film.

  • PDF

Grain Boundary Microcracking in ZrTiO4-Al2TiO5 Ceramics Induced by Thermal Expansion Anisotropy

  • Kim, Ik-Jin;Kim, Hyung-Chul;Lee, Kee-Sung;Han, In-Sub
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.2
    • /
    • pp.109-112
    • /
    • 2003
  • The grain-boundary microcracking materials in the system $Al_2$TiO$_{5}$ -ZrTiO$_4$(ZAT) is influenced by the thermal expansion anisotropy. The range of ZAT compositions investigated had showed very low thermal expansions of 0.3~1.3$\times$10$^{-6}$ K loin compared to 8.29$\times$10$^{6}$ K of pure ZrTiO$_4$and 0.68$\times$10$^{6}$ K of polycrystalline $Al_2$TiO$_{5}$ , respectively, compared with the theoretical thermal expansion coefficient for a single crystal of $Al_2$TiO$_{5}$ , 9.70$\times$10$^{6}$ K. The low thermal expansion and microcraking temperature are apparently due to a combination of thermal contraction and expansion caused by the large thermal expansion anisotropy of the crystal a ies of the $Al_2$TiO$_{5}$ phase.

Erratum to: "Grain Boundary Microcracking in ZrTiO4-Al2TiO5 Ceramics Induced by Thermal Expansion Anisotropy"

  • Kim, Ik-Jin;Kim, Hyung-Chul;Lee, Kee-Sung;Han, In-Sub
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.3
    • /
    • pp.317-321
    • /
    • 2003
  • The grain-boundary microcracking materials in the system A1$_2$Ti $O_{5}$ -ZrTi $O_4$(ZAT) is influenced by the thermal expansion anisotropy. The range of ZAT compositions investigated had showed very low thermal expansions of 0.3~1.3$\times$10$^{-6}$K compared to 8.29$\times$10$^{-6}$K of pure ZrTi $O_4$and 0.68$\times$10$^{-6}$K of polycrystalline A1$_2$Ti $O_{5}$ , respectively, compared with the theoretical thermal expansion coefficient for a single crystal of A1$_2$Ti $O_{5}$ , 9.70$\times$10$^{-6}$K. The low thermal expansion and microcraking temperature are apparently due to a combination of thermal contraction and expansion caused by the large thermal expansion anisotropy of the crystal axes of the A1$_2$Ti $O_{5}$ phase.

A study on the thermal-mechanical fatigue life prediction of 12 Cr steel (12 Cr 강의 열피로 수명단축에 관한 연구)

  • Ha, Jeong-Soo;Kim, Kun-Young;Ahn, Hye-Thon
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.11 no.4
    • /
    • pp.114-125
    • /
    • 1994
  • Fatigue behavior and life prediction method were presented for themal-mechanical and isothermal low cycle fatigue of 12 Cr forged steel used for high temperature applications. In-phase and out-of-phase thermal-mechanical fatigue test from 350 .deg. C to 600 .deg. C and isothermal low cycle fatigue test at 600 .deg. C, 475 .deg. C, 350 .deg. C were conducted using smooth cylindrical hollow specimen under strain-control with total strain ranges from 0.006 to 0.015. The phase difference between temperature and strain in thermal-mechanical fatigue resulted in significantly shorter fatigue life for out-of-phase than for in-phase. Thermal-mechanical fatigue life predication was made by partitioning the strain ranges of the hysteresis loops and the results of isothermal low cycle fatigue tests which were performed under the combination of slow and fast strain rates. Predicted fatigue lives for out-of-phase using the strain range partitioning method showed an excellent agreement with the actual out-of-phase thermal-mechanical fatigue lives within a factor of 1.5. Conventional strain range partitioning method exhibited a poor accuracy in the prediction of in-phase range partitioning method in a conservative way. By the way life prediction of thermal-mechanical fatigue by Taira's equivalent temperature method and spanning fartor method showed good agreement within out-of-phase thermal-mechanical fatigue.

  • PDF

Cloning, expression, and activity of type IV antifreeze protein from cultured subtropical olive flounder (Paralichthys olivaceus)

  • Lee, Jong Kyu;Kim, Hak Jun
    • Fisheries and Aquatic Sciences
    • /
    • v.19 no.8
    • /
    • pp.33.1-33.7
    • /
    • 2016
  • Antifreeze proteins (AFPs) lower the freezing point but not the melting point of aqueous solutions by inhibiting the growth of ice crystals via an adsorption-inhibition mechanism. However, the function of type IV AFP (AFP IV) is questionable, as its antifreeze activity is on the verge of detectable limits, its physiological concentration in adult fish blood is too low to function as a biological antifreeze, and its homologues are present even in fish from tropic oceans as well as freshwater. Therefore, we speculated that AFP IV may have gained antifreeze activity not by selective pressure but by chance. To test this hypothesis, we cloned, expressed, and assayed AFP IV from cultured subtropical olive flounder (Paralichthys olivaceus), which do not require antifreeze protein for survival. Among the identified expressed sequence tags of the flounder liver sample, a 5'-deleted complementary DNA (cDNA) sequence similar to the afp4 gene of the longhorn sculpin was identified, and its full-length cDNA and genome structure were examined. The deduced amino acid sequence of flounder AFP IV shared 55, 53, 52, and 49 % identity with those of Pleuragramma antarcticum, Myoxocephalus octodecemspinosus, Myoxocephalus scorpius, and Notothenia coriiceps, respectively. Furthermore, the genomic structure of this gene was conserved with those of other known AFP IVs. Notably, the recombinant AFP IV showed a weak but distinct thermal hysteresis of $0.07{\pm}0.01^{\circ}C$ at the concentration of 0.5 mg/mL, and ice crystals in an AFP IV solution grew star-shaped, which are very similar to those obtained from other polar AFP IVs. Taken together, our results do not support the hypothesis of evolution of AFP IV by selective pressure, suggesting that the antifreeze activity of AFP IV may have been gained by chance.

Effect of Phenyl Vinyl Methyl Silicone (PVMQ) on Low Temperature Sealing Performance of Fluorosilicone Composites

  • Lee, Jin Hyok;Bae, Jong Woo;Choi, Myoung Chan;Yun, Yu-Mi;Jo, Nam-Ju
    • Elastomers and Composites
    • /
    • v.56 no.4
    • /
    • pp.209-216
    • /
    • 2021
  • In this study, we observed the mechanical properties, thermal stability, and low temperature sealing performance of fluorosilicone elastic composites. When the blend ratio of Phenyl vinyl methyl silicone (PVMQ) was increased, the tensile strength, modulus at 100%, and compression set were decreased. The thermal stability of fluorosilicone elastic composites showed a similar tendency. These were caused by poorer green strength of PVMQ than Fluorosilicone rubber (FVMQ). The change in the tensile strength and elongation at -40℃ showed a decreasing tendency with increasing PVMQ blend ratio. By increasing the PVMQ blend ratio, low-temperature performance was improved. The Dynamic mechanical analysis (DMA) results showed that Tg was decreased and low-temperature performance was improved with increasing PVMQ blend ratio. However tanδ was decreased becaused of the poor green strength and elasticity of PVMQ. From a hysteresis loss at -40℃, the hysteresis loss value was increased and fluorosilicone elastic composites showed the decreasing tendency of elasticity with increasing PVMQ blend ratio. From the TR test, TR10 was decreased with increasing PVMQ blend ratio. FS-4 (45% PVMQ blended composites) showed a TR10 of -68.0℃ that was 5℃ lower than that of FS-1 (100% FVMQ). The gas leakage temperature was decreased with increasing PVMQ blend ratio. The gas leakage temperature of FS-4 was -69.2℃ that was 5℃ lower than that of FS-1. Caused by the polymer chain started to transfer from a glassy state to a rubbery state and had a mobility of chain under Tg, the gas leakage temperature showed a lower value than Tg. The sealing performance at low temperature was dominated by Tg that directly affected the mobility of the polymer chain.

Si(100)기판 위에 증착된$CeO_2$(200)박막과 $CeO_2$(111) 박막의 전기적 특성 비교

  • 이헌정;김진모;김이준;정동근
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2000.02a
    • /
    • pp.67-67
    • /
    • 2000
  • CeO2는 cubic 구조의 일종인 CaR2 구조를 가지고 있으며 격자상수가 Si의 격장상수와 매우 비슷하여 Si 기판위에 에피텍셜하게 성장할 수 있는 가능성이 매우 크다. 따라서 SOI(silicon-on-insulator)구조의 실현을 위하여 Si 기판위에 CeO2 박막을 에피텍셜하게 성장시키려는 많은 노력이 있어왔다. 또한 metal-ferroelectric-semiconductor field effect transistor)에서 ferroelectric 박막과 Si 기판사이의 완충층으로 사용된다. 이러한 CeO2의 응용을 위해서는 Si 기판 위에 성장된 CeO2 박막의 방위성 및 CeO2/Si 구조의 전기적 특성을 알아보는 것이 매우 중요하다. 본 연구에서는 Si(100) 기판위에 CeO2(200)방향으로 성장하는 박막과 EcO2(111) 방향으로 성장하는 박막을 rf magnetron sputtering 방법으로 증착하여 각각의 구조적, 전기적 특성을 분석하였다. RCA 방법으로 세정한 P-type Si(100)기판위에 Ce target과 O2를 사용하여 CeO2(200) 및 CeO2(111)박막을 증착하였다. 증착후 RTA(rapid thermal annealing)방법으로 95$0^{\circ}C$, O2 분위기에서 5분간 열처리를 하였다 이렇게 제작된 CeO2 박막의 구조적 특성을 XRD(x-ray diffraction)방법으로 분석하였고, Al/CeO2/Si의 MIS(metal-insulator-semiconductor)구조를 제작하여 C-V (capacitance-voltage), I-V (current-voltage) 특성을 분석하였으며 TEM(transmission electron microscopy)으로 증착된 CeO2막과 Si 기판과의 계면 특성을 연구하였다. C-V특성에 있어서 CeO2(111)/Si은 CeO2(111)의 두께가 증가함에 따라 hysteresis windows가 증가한 방면 CeO2(200)/Si은 hysteresis windows가 아주 작을뿐만 아니라 CeO2(200)의 두께가 증가하더라도 hysteresis windos가 증가하지 않았다. CeO2(111)/Si과 CeO2(200)/Si의 C-V 특성의 차이는 CeO2(111)과 CeO2(200)이 Si 기판에 의해 받은 stress의 차이와 이에 따른 defect형성의 차이에 의한 것으로 사료된다.