Rietveld 해석법에의한 YBCO 초전도체의 결정 구조 전이 연구 (The crystal structure transition in YBCO superconductor by Rietveld analysis Method)

  • 채기병;전용우;소대화
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1996년도 춘계학술대회 논문집
    • /
    • pp.239-243
    • /
    • 1996
  • In this paper, we have tried to focus on the optimum conditions of crystal structure parameters on YBCO high Tc oxide-superconductor as an excel lent electronic parts. When we verify the characteristic improvement of superconductance and accurate reproduction and so forth, we have made use of RIETAN. We have varied the lattice constant with oxygen content from 6.0 to 7.0 as for transition of orthogonal structure and tetragonal structure for the superconductor. As the result of above, we have preyed that transition from orthogonal structure to tetragonal structure is made at the point of 6.6(oxygen content) by using the simulation.

  • PDF

Fe-Se-Te계의 특성 연구 (A Study on the Properties of Fe-Se-Te System)

  • 최승한
    • 한국재료학회지
    • /
    • 제9권8호
    • /
    • pp.854-857
    • /
    • 1999
  • Fe-Se-Te계(FeSe(sub)1-xTe(sub)x, x=0.2, 0.5, 0.8)의 특성을 X-선 회절법 및 Mossbauer 분광법에 의해 조사하였다. 결정구조는 세 시료 모두 주된 tetragonal PbO 구조와 hexagonal NiAs 구조가 일부 혼합된 형태를 보였으며 x=0.5의 경우 tetragonal 구조의 격자상수 값은 a=3.795$\AA$, c=5.896$\AA$ 이며 c/a=1.55로 나타났다. 다양한 온도변화에 의해 측정된 Mossbauer 스펙트럼은 전체 시료 모두 초미세 자기구조를 갖지 않는 강한 이중선(doublet)이 관측되었다. 조성 및 온도변화에 대해 뚜렷한 선형(line shape)의 변화는 관측되지 않았으나 결합상태에 약간의 변화를 보였다. 이성질체 이동(isomer shift)값과 사중극자 분열(quadrupole splitting)값 및 온도의존성을 분석한 결과 Fe는 low spin이 +2가 상태로 존재하며 강한 공유 결합상태임을 알 수 있었다. x=0.8의 경우 이성질체 이동값의 온도변화는 제2차 도플러 효과(second order Doppler effect)의 영향인 것으로 나타났다.

  • PDF

공침법으로 제조한 $ZrO_2$+3m/o $Y_2O_3$계 분체의 특성(I) : 정방정 Zirconia분체의 안정성 (Properties of the System $ZrO_2$+3m/o $Y_2O_3$ Powder Prepared by Co-precipitation Method(I) : Stability of Tetragonal ZrO2 Powder)

  • 홍기곤;이홍림
    • 한국세라믹학회지
    • /
    • 제27권3호
    • /
    • pp.361-368
    • /
    • 1990
  • The properties of the powder of ZrO2+3m/o Y2O3 system prepared by co-precipitation method at the pH values of 7, 9, 10 and 11 were investigated. ZrOCl2.8H2O and YCl3.6H2O were used as starting materials and NH4OH as a precipitation agent. Zirconium hydroxide near by Zr(OH)4 structure showed more excellent crystallinity and lower formation temperature of tetragonal ZrO2. In the range of this study, cubic ZrO2 was not formed and stability of tetragonal ZrO2 prepared in the conditiion of pH 7 was most excellent. Average particle sizes and specific surface areas of tetragonal ZrO2 powders, prepared as calcining amorphous zirconium hydroxides at $600^{\circ}C$ for 1h, were 0.6-0.8${\mu}{\textrm}{m}$ and 45-70$m^2$/g, respectively.

  • PDF

La와 Nd가 치환된 PZT 세라믹의 구조 및 전기적 성질 (Structure and Electric Properties of PZT Ceramics Substituted by La and Nd)

  • 정수철;박휴범;김정;김건;김시중
    • 한국세라믹학회지
    • /
    • 제31권2호
    • /
    • pp.155-160
    • /
    • 1994
  • PZT ceramics substituted by La3+ and Nd3+ were fabricated according to the formula: [Pb1-x(La or Nd)x][Zr0.58Ti0.42]1-x/4$\square$x/4O3(x=0.00, 0.02, 0.05, 0.08, 0.15, 0.20). The crystal structure and microstructure were investigated by XRD and SEM. It was observed that the phase transitions among rhombohedral, tetragonal, and cubic symmetry occured as the substitutional quantity increased. Dielectric constant, dissipation factor and piezoelectric coefficient (d33), of each sample were measured. The dielectric properties were changed as the substitutional quanity of rare earth ion increased. These changes could be explained by crystal structure and compositional fluctuaction. Its d33 was higher at tetragonal region near to phase boundry between rhombohedral and tetragonal, which was explained by reorientation of domain wall.

  • PDF

Bi-2223/Ag HTS 장선재의 Ic 특성 향상 공정 연구 (Study on fabrication process of long length of Bi-2223/Ag MTS wires for high critical current)

  • 하동우;양주생;황선역;이동훈;최정규;하홍수;오상수;권영길
    • 한국초전도저온공학회:학술대회논문집
    • /
    • 한국초전도저온공학회 2003년도 학술대회 논문집
    • /
    • pp.105-108
    • /
    • 2003
  • Long length of Bi-2223 superconducting wires were fabricated by stacking, drawing process with different precursor owders and different heat-treatment histories. The precursor powders were 2 kinds of Pb content. And a part of the tapes were experienced pre-annealing process which caused tetragonal structure of Bi-2212 phase to orthorhombic structure of it was during drawing process. We confirmed the transformation of Bi-2212 phase from tetragonal structure to orthorhombic structure and reduction of second phases. We designed and made a continuous Ic measurement system for Bi-2223/Ag HTS tape. We could achieve best Ic of 65 A at the Bi-2223/Ag tape using low Pb content of precursor powder and experienced pre-annealing process.

  • PDF

$TlGa_xIn_{1-x}Se_2$ Solid Solution의 광학적 특성 및 상전이에 관한 연구 (Study on Optical Properties and Phase Transition of $TlGa_xIn_{1-x}Se_2$ Solid Solutions)

  • 윤창선;김병호;차덕준
    • 한국진공학회지
    • /
    • 제2권2호
    • /
    • pp.220-226
    • /
    • 1993
  • Bridgman 방법으로 성장된 $TlGa_xIn_{1-x}Se_2$ 단결정의 격자상수와 energy gap의 성분의존성을 조사하였다. $TlGa_xIn_{1-x}Se_2$ solid solution의 불연속 특성이 tetragonal과 monoclinic 구조를 가진 0.25$0.0{\leq}X{\leq}0.25$)로부터 monoclinic 구조($0.65{\leq}X{\leq}1.0$)로 변하는 구조적 상전이가 이 성분영역에서 관측되었다. $TlGaSe_2$ 단결정의 energy gap과 유전상수의 온도의존성으로부터 각각 1차 및 2차 상전이에 상당하는 107 K와 120 K에서 변칙특성을 발견하였다.

  • PDF

$SiH_2$$CI_2$ 환원에 의해 형성된 WSix 박막 특성 (Characteristics of Tungsten Silicide Film Formed by Dichlorosilane Reduction)

  • 최동규;고철기
    • 전자공학회논문지A
    • /
    • 제29A권9호
    • /
    • pp.15-19
    • /
    • 1992
  • Tungsten silicied (WSix) has been widely used for interconnection line to improve the speed and reliability of devices. It is known that WSix formed by silane reduction has poor step coverage and poor adhesion. In this research, WSix by dichlorosilane reduction showed excellent adhesion in cellophane adhesive tape test, and improved step coverage by two times. The crystal structure of the as-deposited WSix film by silane reduction was transformed from the hexagonal to the tetragonal structure during annealing treatment, while that by dichlorosilane reduction kept the stable tetragonal structure. The fluorine concentration in the WSix film by dichlorosilane was lower than that by silane.

  • PDF

Sol-Gel법으로 제작된 PLZT박막의 Raman 연구 (Raman spectroscopy of PLZT thin films prepared by Sol-Gel processing)

  • 방선웅;장낙원;박정흠;마석범;박창엽;최형욱
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1997년도 추계학술대회 논문집
    • /
    • pp.52-55
    • /
    • 1997
  • In this study, PLZT stock solutions were prepared by sol-gel processing to fabricate PLZT thin films. The stock solutions were spin-coated on ITO-glass and the film were annealed by rapid thermal annealing(RTA). The variation of tile crystallographic structure of the thin films and the phase transition with respect to it were observed using Raman spectra. Raman result showed that the band of spectra are broad as the amount of Zr substitution increased and specially, abrupt change occurs in the raman spectra upon crossing the tetragonal-rhombohedral phase boundry at 2/55/45 PLZT thin film. So, the fact that the crystallographic structure was transitted from tetragonal to rhombohedral structure was certified.

  • PDF

Synthesis, Structural and Electrical Characterizations of $Pr_{2-x}Ba_xNiO_{4{\pm}\delta}{^\$}$

  • 장영기;권영구;변송호
    • Bulletin of the Korean Chemical Society
    • /
    • 제16권2호
    • /
    • pp.120-125
    • /
    • 1995
  • Solid solutions of Pr2-xBaxNiO4±δ with K2NiF4-type structure were prepared in air and characterized by powder X-ray diffraction, Rietveld refinements, iodometry titrations, and conductivity measurements. The range of the solid solution was 0 ≤ x < 0.5. The crystal structure changes from orthorhombic (Fmmm) for x ≤ 0.1 to pseudo-tetragonal (I4/mmm) for x ≥ 0.2. The orthorhombic structure of x=0.1 transforms to tetragonal at low temperature. The bond distances obtained from the Rietvel analyses did not vary significantly with the Ba content except that of Ni-O (parallel to the c-axis) which showed an abrupt increase from x=0.1 to 0.2. The excess oxygen content (δ) decreases from 0.241 to 0.03 with increasing substituted Ba contents within the solution range. The samples are all semiconductors at the temperature range 4 < T < 300 K.

이온 분극률과 결정구조에 따른 Aluminum Magnesium Tantalate 고용체의 마이크로파 유전특성 (Microwave Dielectric Characteristics of Aluminum Magnesium Tantalate Solid Solutions with Variations of Ionic Polarizability and Crystal Structure)

  • 최지원;하종윤;강종윤;윤석진;윤기현;김현재
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집
    • /
    • pp.119-122
    • /
    • 2002
  • The calculated and measured dielectric constant of (1-x)(Al$\sub$1/2/Ta$\sub$1/2/)O$_2$-x(Mg$\sub$1/3/Ta$\sub$2/3/)O$_2$(O$\leq$x$\leq$1.0) solid solutions were investigated by variations of ionic polarizability and crystal structure. (Al$\sub$1/2/Ta$\sub$1/2/)O$_2$ and (Mg$\sub$1/3/Ta$\sub$2/3/)O$_2$were orthorhombic and tetragonal trirutile structure, respectively. When (Al$\sub$1/2/Ta$\sub$1/2/)O$_2$ was substituted by (Mg$\sub$1/3/Ta$\sub$2/3/)O$_2$, the phase transformed to tetragonal structure over 60 mole%. Because the ionic radius of (Mg$\sub$1/3/Ta$\sub$2/3/)O$_2$was slightly bigger than one of (A1$\sub$1/2/Ta$\sub$1/2)O$_2$, the cell parameters increased with an increase of (Mg$\sub$1/3/Ta$\sub$2/3/)O$_2$ substitution. The measured dielectric constant increased with an increase of (Mg$\sub$1/3/Ta$\sub$2/3/)O$_2$ substitution and coincided with dielectric mixing rule and the calculated dielectric constant with the molecular additivity rule. There were some differences between the measured and the calculated dielectric constant. The reason of the lowered dielectric constant comparing with the calculated one was compressed stress due to the electronic structure of tantalum.

  • PDF