3성분계 무기결합재의 W/B 및 규산나트륨 첨가율 변화에 따른 유동 및 강도특성 (Flowing and Strength Properties of Ternary System Inorganic Composite According to the Change of W/B and Addition Ratio of Na2SiO3)

  • 배상우;문지환;이윤성;이강필;이상수;송하영
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2011년도 추계 학술논문 발표대회
    • /
    • pp.49-50
    • /
    • 2011
  • This study tried to utilize basic data for developing the cement substitute material through ternary system inorganic composite properties of flowing and strength. W/B and addition ratio of Na2SiO3 have been changed in ternary system inorganic composite combined blast furnace slag, red mud and fly ash. As to the experimental result inorganic composite, the flowing and intensity improvement effect was showed to be bigger than W/B according to the addition ratio change of the Na2SiO3. When particularly the Na2SiO3 addition ratio was 6%, the rapid flowing and strength improvement effect was confirmed.

  • PDF

순환잔골재 치환율 변화에 따른 3성분계 무기결합재 모르타르의 유동 및 강도특성 (Flowing and Strength Properties of Ternary System Inorganic Composite Mortar according to the Change of Replacement Ratio of Recycled Sand)

  • 배상우;박종필;김규용;이상수;송하영
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2012년도 춘계 학술논문 발표대회
    • /
    • pp.99-100
    • /
    • 2012
  • This study tried to present the appropriate replacement ratio of the recycled sand through the properties of the ternary system inorganic composite mortar according to replacement ratio change of the recycled sand about the natural sand through test verification. The flowing and compressive strength was degraded as the replacement ratio of the experimental result recycled sand increased. The appropriate replacement ratio of the recycled sand according to it was shown up less than 15%.

  • PDF

Preparation and capacitance properties of graphene based composite electrodes containing various inorganic metal oxides

  • Kim, Jeonghyun;Byun, Sang Chul;Chung, Sungwook;Kim, Seok
    • Carbon letters
    • /
    • 제25권
    • /
    • pp.14-24
    • /
    • 2018
  • Electrochemical properties and performance of composites performed by incorporating metal oxide or metal hydroxide on carbon materials based on graphene and carbon nanotube (CNT) were analyzed. From the surface analysis by field emission scanning electron microscopy and field emission transmission electron microscopy, it was confirmed that graphene, CNT and metal materials are well dispersed in the ternary composites. In addition, structural and elemental analyses of the composite were conducted. The electrochemical characteristics of the ternary composites were analyzed by cyclic voltammetry, galvanostatic charge-discharge tests, and electrochemical impedance spectroscopy in 6 M KOH, or $1M\;Na_2SO_4$ electrolyte solution. The highest specific capacitance was $1622F\;g^{-1}$ obtained for NiCo-containing graphene with NiCo ratio of 2 to 1 (GNiCo 2:1) and the GNS/single-walled carbon $nanotubes/Ni(OH)_2$ (20 wt%) composite had the maximum specific capacitance of $1149F\;g^{-1}$. The specific capacitance and rate-capability of the $CNT/MnO_2/reduced$ graphene oxide (RGO) composites were improved as compared to the $MnO_2/RGO$ composites without CNTs. The $MnO_2/RGO$ composite containing 20 wt% CNT with reference to RGO exhibited the best specific capacitance of $208.9F\;g^{-1}$ at a current density of $0.5A\;g^{-1}$ and 77.2% capacitance retention at a current density of $10A\;g^{-1}$.

폐자기와 3성분계 무기결합재의 혼합비율 변화에 따른 인조석재의 역학적 특성 (The Dynamic Properties of the Artificial Stone According to the Mixed Ratio Change of the Inorganic Composite and Waste Porcelain)

  • 유용진;배상우;이상수;송하영
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2012년도 추계 학술논문 발표대회
    • /
    • pp.95-96
    • /
    • 2012
  • This study makes with the environment-friendly artificial stone which doesn't use the cement and natural aggregate and increases the blast furnace slag that is the eco-friendly material that is the industrial byproduct, fly ash, and availability of the red mud and applies the coares aggregate substitute material as the cleistothecium. The experimental plan according to it indicated the compressive strength and flexural strength which is the most excellent in the mixied ratio 40% of the result degree of closeness magnetism of experimenting with the optimal mix obtained through the preceding stude.

  • PDF

Simultaneous Biofiltration of H2S, NH3 and Toluene using an Inorganic/Polymeric Composite Carrier

  • Park, Byoung-Gi;Shin, Won-Sik;Chung, Jong-Shik
    • Environmental Engineering Research
    • /
    • 제13권1호
    • /
    • pp.19-27
    • /
    • 2008
  • Simultaneous removal of ternary gases of $NH_3$, $H_2S$ and toluene in a contaminated air stream was investigated over 180 days in a biofilter. A commercially available inorganic/polymeric composite chip with a large void volume (bed porosity > 0.80) was used as a microbial support. Multiple microorganisms including Nitrosomonas and Nitrobactor for nitrogen removal, Thiobacillus thioparus (ATCC 23645) for $H_2S$ removal and Pseudomonas aeruginosa (ATCC 15692), Pseudomonas putida (ATCC 17484) and Pseudomonas putida (ATCC 23973) for toluene removal were used simultaneously. The empty bed residence time (EBRT) ranged from 60 - 120 seconds and the inlet feed concentration was $0.0325\;g/m^3-0.0651\;g/m^3$ for $NH_3$, $0.0636\;g/m^3-0.141\;g/m^3$ for $H_2S$, and $0.0918\;g/m^3-0.383\;g/m^3$ for toluene, respectively. The observed removal efficiency was 2% - 98% for $NH_3$, 2% - 100% for $H^2S$, and 2% - 80% for toluene, respectively. Maximum elimination capacity was about $2.7\;g/m^3$/hr for $NH_3$, > $6.4\;g/m^3$/hr for $H_2S$ and $4.0\;g/m^3$/hr for toluene, respectively. The inorganic/polymeric composite carrier required 40 - 80 days of wetting time for biofilm formation due to the hydrophobic nature of the carrier. Once the surface of the carrier was completely wetted, the microbial activity became stable. During the long-term operation, pressure drop was negligible because the void volume of the carrier was two times higher than the conventional packing materials.

SO3를 다량 함유한 폐석고보드 미분말을 첨가한 3성분계 무기결합재의 길이변화 특성 (The Length Change Characteristic of the Ternary System Inorganic Composites adding the Waste Gypsum Board Micro Powder containing SO3 the great quantity)

  • 김윤미;박종필;이상수;송하영
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2012년도 추계 학술논문 발표대회
    • /
    • pp.65-66
    • /
    • 2012
  • The cement used in the construction industry of the manufacturing process, large amounts of the greenhouse gas, CO2 and is currently being studied for cement substitutes that reduce greenhouse gas issue. Therefore, the this study as a replacement for cement industrial by-product of blast furnace slag, red mud, silica fume and alkali-activator, using only inorganic composites without high-temperature calcination process were manufactured. The waste gypsum board micro powder added to compensate for the shrinkage cracks, the compressive strength and flow, and length change characteristics were investigated. Consequently, The setting time was shortened as GB added And liquidity was reduced. GB 2%, 7 days curing the added strength of specimens was the highest. Came out, and change the length of the Plain least.

  • PDF

섬유의 종류에 따른 폐유리와 무기결합재 인조석재의 역학적 특성 (Mechanical Properties of the artificial Stone According to the Ternary System Inorganic Composite and Waste Glass and Fiber type)

  • 유용진;김헌태;이상수;송하영
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2013년도 춘계 학술논문 발표대회
    • /
    • pp.321-322
    • /
    • 2013
  • Recently, the exhaustion of resource and environmental damage is serious due to the global warming because of the CO2 exhaust and each type the natural aggregate picking described below. meanwhile, The rest is the actual condition gone to the dumping ground that there is nearly no use which the waste glass can recycle and it is recycled. This research applied the waste glass as the cement substitute material the inorganic binder and coares aggregate substitute material. It utilizes the substitute material of the cement according to it and natural aggregate and tries to develop the environment-friendly artificial stone. The inorganic binder used the blast furnace slag, red mud, and fly ash. The straight type steel fiber, PVA fiber, PA fiber, and cellulosic fiber were used with a kind of fiber. As to the experimental item according to it, the compressive strength is the flexural strength and compressive strength.

  • PDF