• Title/Summary/Keyword: Tempering Temperature

Search Result 168, Processing Time 0.029 seconds

Low Cycle Fatigue Characteristics of High Strength Low Alloy Steel (고강도 저합금강의 저주기 피로특성)

  • Kim, Jae-Hoon;Kim, Duck-Hoi;Lee, Jong-Hyun;Cho, Seong-Seock;Jeon, Byoung-Hwan
    • Proceedings of the KSME Conference
    • /
    • 2001.06a
    • /
    • pp.169-174
    • /
    • 2001
  • Low cycle fatigue tests are performed on high strength low alloy steels that be developed for submarine material. The relation between absorbed plastic strain energy and numbers of cycle to failure is examined in order to predict the low cycle fatigue life of structural steels by using plastic strain energy method. The cyclic properties are determined by a least square fit techniques. The life predicted by the plastic strain energy method is found to coincide with experiment data and results obtained from the Coffin-Manson method. Also the cyclic behavior of structural steels is characterized by cyclic softening with increasing number of cycle at room temperature. Especially, low cycle fatigue characteristics and microstructural changes of structural steels are investigated according to changing tempering temperatures. In the case of PFS steels, the $\varepsilon$-Cu is formed in 550C of tempering temperature and enhances the low cycle fatigue properties.

  • PDF

The Effect of Heat treating Conditions on Wear Characteristics of High Speed Steel by Powder Metallurgy (분말고속도공구강의 미끄럼마모특성에 미치는 열처리조건의 영향)

  • 이한영;노정균;배종수;김용진
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2000.06a
    • /
    • pp.48-53
    • /
    • 2000
  • The effects of added elements, such as Co or Nb, on wear properties of high speed steel by powder metallurgy(PM-HSS) had been evaluated in previous paper. The wear properties of materials, in fact, have been a]so influenced by heat-treating conditions. In this paper, the effects of heat-treating conditions on wear properties of PM-HSS have been evaluated. The wear tests have been performed as same conditions as previous paper using PM-HSS(5%Co-1%Nb) heat-treated under different quenching and tempering temperature. The result of this paper shows that wear resistance of PM-HSS is improved with relatively high quenching temperature. However tempering temperature is not sensitve to the wear resistance in range of high quenching temperature. It may be deduced by the fact that the shear strength of matrix by strengthening mechanisms of quenching aging in addition to dispersion-hardening is improved.

  • PDF

Effects of Austenitizing Temperature and Cooling Rate on Precipitation Behavior and Tensile Properties of Pressure Vessel Steels (압력용기용 강의 석출거동과 인장특성에 미치는 오스테나이트화 온도 및 냉각속도의 영향)

  • Shin, Jae Woong;Lee, Sang Min;Kim, Yong Jin;Lee, Sang Woo
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.29 no.1
    • /
    • pp.15-23
    • /
    • 2016
  • The effects of austenitizing temperature and cooling rate on precipitation behavior and tensile properties were investigated in an Mn-Mo-Nb-V pressure vessel steel. During austenitizing, it was shown that the austenite coarsening was somewhat suppressed by undissolved NbC. After cooling from austenitizing, the microstructure of all the steels mainly consisted of upper bainite. However, the steel comprised a little lower bainite and martensite in the case of aqua oil quenching from $1000^{\circ}C$, which would be due to increased hardenability by partly dissolved Nb and comparatively large austenite grains. The average size of NbC in austenite at higher temperature was analyzed to be smaller than that at lower temperature because of the more dissolution. It was found that the NbC did not grow much during fast cooling from austenitizing. Meanwhile, the NbC grew much during slow cooling, probably due to wide temperature range of cooling and sufficiently long time for NbC to grow. It was conjectured the V precipitates newly formed and/or grew during cooling from austenitizing and during tempering. On the other hand, the formation of NbC was almost completed before tempering and little more precipitated during tempering. Among the tempered steels, the steel which was fast cooled from $1000^{\circ}C$ showed the highest tensile strength, which seemed to come from the microstructure of fine upper bainite and some low temperature phases as well as the comparatively fine NbC precipitates.

Effects of Tempering Treatment on Microstructure and Mechanical Properties of Cu-Bearing High-Strength Steels (템퍼링에 따른 Cu 첨가 고강도강의 미세조직과 기계적 특성)

  • Lee, Sang-In;Hwang, Byoungchul
    • Korean Journal of Materials Research
    • /
    • v.24 no.10
    • /
    • pp.550-555
    • /
    • 2014
  • The present study deals with the effects of tempering treatment on the microstructure and mechanical properties of Cu-bearing high-strength steels. Three kinds of steel specimens with different levels of Cu content were fabricated by controlled rolling and accelerated cooling, ; some of these steel specimen were tempered at temperatures ranging from $350^{\circ}C$ to $650^{\circ}C$ for 30 min. Hardness, tensile, and Charpy impact tests were conducted in order to investigate the relationship of microstructure and mechanical properties. The hardness of the Cu-added specimens is much higher than that of Cu-free specimen, presumably due to the enhanced solid solution hardening and precipitation hardening, result from the formation of very-fine Cu precipitates. Tensile test results indicated that the yield strength increased and then slightly decreased, while the tensile strength gradually decreased with increasing tempering temperature. On the other hand, the energy absorbed at room and lower temperatures remarkably increased after tempering at $350^{\circ}C$; and after this, the energy absorbed then did not change much. Suitable tempering treatment remarkably improved both the strength and the impact toughness. In the 1.5 Cu steel specimen tempered at $550^{\circ}C$, the yield strength reached 1.2 GPa and the absorbed energy at $-20^{\circ}C$ showed a level above 200 J, which was the best combination of high strength and good toughness.

A Study on Die Wear Model considering Thermal Softening(I) -Construction of Wear Model (열연화를 고려한 금형마멸모델에 관한 연구(I)-마멸모델의 정립)

  • Kang, Jong-Hun;Park, In-Woo;Jae, Jin-Soo;Kang, Seong-Soo
    • Transactions of Materials Processing
    • /
    • v.7 no.3
    • /
    • pp.274-281
    • /
    • 1998
  • The service life of tools in metal forming process is to a large extent limited by wear, fatigue fracture and plastic deformation. In elevated temperature forming processes wear is the predominant factor for tool operating life. To predict tool life by wear Achard's model is generally applied. Usually hardness of die is considered to be a function of temperature. But hardness of die is a function of not only tem-perature but also operating time of die. To consider softening of die by repeated operation it is necessary to express hardness of die by a function of a function of temperature and time. By experiment of reheating of die softening curve was obtained and applied to suggest modified Archard's Model in which hardness is a function of main tempering curve.

  • PDF

Combined Heat Treating characteristics of Hot Work Tool Steel (열간금형 공구강의 복합열처리 특성에 관한 연구)

  • Kim, Y.H.;Kim, D.K.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.11 no.4
    • /
    • pp.315-323
    • /
    • 1998
  • This study has been conducted to develope the combined heat treating technique of gas carburising - gas nitriding and gas carburising to improve the hot working performance of type H3 hot work tool steel. Case depth and carbrides coarsening were increased with increasing carburising temperature and time, respectively. Surface hardness showed decreasing tendency with increasing 2nd tempering temperature after carburising treatment. After carburising, 2nd treatment at 500 to 600 was chosen according to a hardness demand of final product. High temperature tempering resistance showed more excellent quality during such carburising-nitriding or carburising than complex treatment as after conventional hardening.

  • PDF

Milling and Rice Flour Properties of Tempering Condition on Moisture Content of Rice (쌀의 수분함량별 Tempering에 따른 제분 및 쌀가루의 특성)

  • 김형열;이병영;유효숙;함승시
    • Food Science and Preservation
    • /
    • v.6 no.1
    • /
    • pp.76-80
    • /
    • 1999
  • Power consumption, mesh size, moisture content, color difference, amylogram of rice flour milled with the water soaked rice were compared with that of rice using dry pin mill process. The rice was soaked in 23, 24, 25, 26% of water for 10hr, independently. The more rice had moisture content, the less power consumption was needed. Power consumption to mill the rice soaked in 25% of water was less than that of dry rice by 6.8kW/100Kg. Moisture content of rice flour from the rice soaked with 25% of water was 2% higher than that of rice flour from the rice soaked with 23% of, water. Population of flour particle from the rice soaked with 24-25% of water was 45.7∼46.25 of 60 mesh, 9.7∼10.4% of 80∼100 mesh and 7.7∼8.1% of 100 mesh. Gelatinization temperature of rice flour from the rice soaked with 23% and 24∼25% of water was 65.70C and 64.50C, independently. Temperature of rice flour from the rice soaked with 23% 24∼25% of water sith minimum viscosity was 85.50C and 88.4∼88.70C, independently. Brightness and whiteness of the rice flour from the rice soaked with 24∼25% of water were 95.90∼95.95 and 905.82∼95.94, independently. Brightness and whiteness of the rice flour from the soaked rice were 1.2 and 1.7 higher than that of rice flour from the dry rice, independently.

  • PDF

The Effects of the Tempering Temperatures on the Mechanical Properties of the Carbon Tool Steel(SK5M) for Flat Spring (박판 스프링용 탄소공구강대(SK5M)의 기계적 성질에 미치는 뜨임 온도의 영향)

  • Won S.T.;Sim K.S.;Lim C.R.
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2006.05a
    • /
    • pp.95-96
    • /
    • 2006
  • This study examined the effects of the tempering temperatures($360-420^{\circ}C$) on the mechanical properties of the carbon tool steel (SK4M) for flat spring. Hardness test, tensile test and fatigue test were performed at room temperature($20^{\circ}C$). The tensile strength and yield strength of $390^{\circ}C\;and\;420^{\circ}C$ tempered SK5M were 0.93-0.97 times and 0.81-0.87 times those of $360^{\circ}C$ tempered SK5M, respectively. The fatigue limit of $360-420^{\circ}C$ tempered SK5M were 35-40% of tensile strength of $360-420^{\circ}C$ tempered SK5M, respectively.

  • PDF

Effects of Alloying Element and Tempering on the Mechanical Properties of Cr-Mo Plastic Mold Steels (Cr-Mo계 금형강의 기계적 성질에 미치는 합금원소 및 템퍼링의 영향)

  • Kim, Nam-Kyu;Kim, Byoung-Ok;Lee, Oh-Yeon
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.25 no.4
    • /
    • pp.196-205
    • /
    • 2012
  • The purpose of this study is to enhance the hardenability and the mechanical properties by the addition of alloying elements such as Ni, Cr, Mo and B for the development of Cr-Mo plastic mold steel with uniform hardness and microstructure. The ingots were prepared by vacuum induction melting and forged to ${\Phi}35mm$ round bar. Forged bars were quenched and tempered at $200{\sim}600^{\circ}C$ for 1.5 hour. Jominy test, boron distribution observation, microstructual observation, tensile test and charpy impact test were conducted. It was confirmed that the hardenablity of these steels was improved by increasing of alloying elements and further promoted by the addition of boron. The critical rate of cooling required to obtain the bainitic structure for 0.27C-1.23Cr-0.28Mo-B steel was $0.5^{\circ}C/sec$. Hardness and strength of Cr-Mo steels decreased with increasing tempering temperature, but elongation and reduction of area increased with increasing tempering temperature. However, impact energy tempered at $400^{\circ}C$ showed the lowest value in the range $200{\sim}600^{\circ}C$ due to the temper embrittlement.

Effect of tempering on the repeated impact fatique life of the steel (강재의 충격피로파괴수명에 미치는 tempering 효과에 관한 연구)

  • 정재천
    • Journal of the korean Society of Automotive Engineers
    • /
    • v.3 no.3
    • /
    • pp.30-38
    • /
    • 1981
  • The fatigue characteristics of Si-Mn spring steel (AISI 9260-H, JIS SUP-6) were investigated on several heat treatment conditions. Repeated impact loads of 10kg-cm and 15kg-cm energy were applied with a cam roller drop hammer type impact fatigue testing machine. Specimens were oil-quenched, and tempered at 350.deg. C, 450.deg. C and 500.deg. C, respectively. Results obtained in these experiments are summarized as follows.; 1) The fatigue life of the specimen is decreased as the magnitude of constant impact energy is increased, regardless of heat treatment. 2) Generally, the fatigue life of the specimen is decreased as the tensile strength of the materials is increased. 3) Within the limit of these experiments, the fatigue life showed abrupt decrease at the tempering temperature of about 400.deg. C 4) The fatigue life is increased as the initial value of applied stress intensity factor(K$_{1}$) is decreased. This tendency is apparent for the low tensile strength materials.

  • PDF